Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “dissolution”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 1,351 records · Page 75

Geochemical Assessment for Carbon Sequestration in the Conasauga Group, Northwest Georgia, USA

Sedimentary geological formations are known to be great candidates for geological carbon sequestration. Published studies suggest the southeast of the United States contains many formations suitable for carbon storage. The Cassville 1 Stratigraphic Borehole well could act as a potential carbon reservoir for nearby energy resource facilities in Georgia, United States. Although studies have shown that porous formations are adequate for geological carbon sequestration, it is important to understand possible geochemical reactions between CO 2 and the targeted geological formation before injecting any fluids. In this study, a sandstone sample from the Cassville 1 well is being considered for geological carbon sequestration in the Conasauga Group in Northwest Georgia. Here, the collected sandstone sample, consisting of quartz, K-feldspar, micas, kaolinite, and carbonate minerals such as calcite and dolomite, has a 6% porosity. Leveraging the formation composition and porosity, a one-dimensional continuum reactive transport model was built using CrunchFlow to assess possible geochemical reactions between injected CO 2 and the geological formation. Simulation results show that the carbonate minerals, calcite and dolomite, dissolve during the injection period of 10,000 days, increasing formation porosity from 6% to as much as 30%. The rate and extent of carbonate mineral dissolution and resulting porosity increase are highly sensitive to mineral reactive surface area values. No evidence of mineral precipitation was observed, suggesting that dissolution reactions will control porosity evolution during the CO 2 injection period.

42 ENGINEERING↗

Integrated modeling of CO2 storage and leakage scenarios including transitions between super- and sub-critical conditions, and phase change between liquid and gaseous CO2

Storage of CO{sub 2} in saline aquifers is intended to be at supercritical pressure and temperature conditions, but CO{sub 2} leaking from a geologic storage reservoir and migrating toward the land surface (through faults, fractures, or improperly abandoned wells) would reach subcritical conditions at depths shallower than 500-750 m. At these and shallower depths, subcritical CO{sub 2} can form two-phase mixtures of liquid and gaseous CO{sub 2}, with significant latent heat effects during boiling and condensation. Additional strongly non-isothermal effects can arise from decompression of gas-like subcritical CO{sub 2}, the so-called Joule-Thomson effect. Integrated modeling of CO{sub 2} storage and leakage requires the ability to model non-isothermal flows of brine and CO{sub 2} at conditions that range from supercritical to subcritical, including three-phase flow of aqueous phase, and both liquid and gaseous CO{sub 2}. In this paper, we describe and demonstrate comprehensive simulation capabilities that can cope with all possible phase conditions in brine-CO{sub 2} systems. Our model formulation includes: (1) an accurate description of thermophysical properties of aqueous and CO{sub 2}-rich phases as functions of temperature, pressure, salinity and CO{sub 2} content, including the mutual dissolution of CO{sub 2} and H{sub 2}O; (2) transitions between super- and subcritical conditions, including phase change between liquid and gaseous CO{sub 2}; (3) one-, two-, and three-phase flow of brine-CO{sub 2} mixtures, including heat flow; (4) non-isothermal effects associated with phase change, mutual dissolution of CO{sub 2} and water, and (de-) compression effects; and (5) the effects of dissolved NaCl, and the possibility of precipitating solid halite, with associated porosity and permeability change. Applications to specific leakage scenarios demonstrate that the peculiar thermophysical properties of CO{sub 2} provide a potential for positive as well as negative feedbacks on leakage rates, with a combination of self-enhancing and self-limiting effects. Lower viscosity and density of CO{sub 2} as compared to aqueous fluids provides a potential for self-enhancing effects during leakage, while strong cooling effects from liquid CO{sub 2} boiling into gas, and from expansion of gas rising towards the land surface, act to self-limit discharges. Strong interference between fluid phases under three-phase conditions (aqueous - liquid CO{sub 2} - gaseous CO{sub 2}) also tends to reduce CO{sub 2} fluxes. Feedback on different space and time scales can induce non-monotonic behavior of CO{sub 2} flow rates.

54 ENVIRONMENTAL SCIENCES↗

Development of molecular cluster models to probe pyrite surface reactivity

Abstract The recent discovery that anaerobic methanogens can reductively dissolve pyrite and utilize dissolution products as a source of iron and sulfur to meet their biosynthetic demands for these elements prompted the development of atomic‐scale nanoparticle models, as maquettes of reactive surface sites, for describing the fundamental redox steps that take place at the mineral surface during reduction. The given report describes our computational approach for modeling n (FeS 2 ) nanoparticles originated from mineral bulk structure. These maquettes contain a comprehensive set of coordinatively unsaturated Fe (II) sites that are connected via a range of persulfide (S 2 2− ) ligation. In addition to the specific maquettes with n = 8, 18, and 32 FeS 2 units, we established guidelines for obtaining low‐energy structures by considering the pattern of ionic, covalent, and magnetic interactions among the metal and ligand sites. The developed models serve as computational nano‐reactors that can be used to describe the reductive dissolution mechanism of pyrite to better understand the reactive sites on the mineral, where microbial extracellular electron‐transfer reactions can occur.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Understanding Discharge‐Driven Growth of Cathode Impedance in Ni‐Rich NMC Cathodes

Degradation of LiNi x Mn y Co 1-x-y O 2 (NMC)-based lithium-ion batteries depends strongly on cut-off voltage ranges. In addition to the high upper cut-off voltage, a high depth of discharge (i.e., lower cut-off voltage) significantly worsens cathode impedance growth and capacity fade during long-term cycling. However, there is currently no consensus on the mechanism behind the negative role of a deep discharge. Here, this phenomenon was investigated in graphite||NMC cells with single-crystal cathodes (LiNi 0.6 Co 0.2 Mn 0.2 O 2 (NMC622) or LiNi 0.76 Co 0.14 Mn 0.10 O 2 (NMC76)) using targeted aging protocols (constant high-voltage holds vs. charge–discharge cycling), while monitoring transition-metal (TM) dissolution, cathode-electrolyte interface (CEI) impedance, and NMC surface composition. We demonstrate a correlation between discharge-driven CEI impedance growth and increased TM dissolution. Furthermore, this degradation pathway is more pronounced in lower-Ni NMC622 than in higher-Ni (NMC76) under comparable delithiation states at charge, with both compositions undergoing the H2→H3 phase transition. X-ray photoelectron spectroscopy (XPS) reveals NMC composition-dependent evolution of surface lattice oxygen and restructured surface layer composition between charged and discharged states. These findings add mechanistic depth to the role of discharge as an active driver of interfacial degradation and provide new insights into its composition dependence.

25 ENERGY STORAGE↗

Chemical evolution of groundwater in the Wilcox aquifer of the northern Gulf Coastal Plain, USA

The Wilcox aquifer is a major groundwater resource in the northern Gulf Coastal Plain (lower Mississippi Valley) of the USA, yet the processes controlling water chemistry in this clastic aquifer have received relatively little attention. The current study combines analyses of solutes and stable isotopes in groundwater, petrography of core samples, and geochemical modeling to identify plausible reactions along a regional flow path ∼300 km long. The hydrochemical facies evolves from Ca-HCO{sub 3} upgradient to Na-HCO{sub 3} downgradient, with a sequential zonation of terminal electron-accepting processes from Fe(III) reduction through SO{sub 4}{sup 2−} reduction to methanogenesis. In particular, decreasing SO{sub 4}{sup 2−} and increasing δ{sup 34}S of SO{sub 4}{sup 2−} along the flow path, as well as observations of authigenic pyrite in core samples, provide evidence of SO{sub 4}{sup 2−} reduction. Values of δ{sup 13}C in groundwater suggest that dissolved inorganic carbon is contributed both by oxidation of sedimentary organic matter and calcite dissolution. Inverse modeling identified multiple plausible sets of reactions between sampled wells, which typically involved cation exchange, pyrite precipitation, CH{sub 2}O oxidation, and dissolution of amorphous Fe(OH){sub 3}, calcite, or siderite. These reactions are consistent with processes identified in previous studies of Atlantic Coastal Plain aquifers. Contrasts in groundwater chemistry between the Wilcox and the underlying McNairy and overlying Claiborne aquifers indicate that confining units are relatively effective in limiting cross-formational flow, but localized cross-formational mixing could occur via fault zones. Consequently, increased pumping in the vicinity of fault zones could facilitate upward movement of saline water into the Wilcox.

58 GEOSCIENCES↗

Effects of mass reduction, flow reduction and enhanced biodecay of DNAPL source zones

A mathematical model and an analytical solution are presented to describe field-scale dense non-aqueous phase liquid (DNAPL) source dissolution and source zone biodecay rates coupled with advective-dispersive dissolved plume transport. The model is employed to investigate various source remediation options on source zone mass depletion, net source mass flux, and dissolved plume attenuation for different source zone 'architectures' (i.e., pools versus residual DNAPL) and compliance criteria. Remediation options considered include partial source mass removal, source flow reduction, and source zone enhanced biodecay. Partial mass reduction reduces the source zone mass flux and downgradient concentrations for residual DNAPL sources and pools, which can significantly reduce dissolved plume size and time to reach compliance criteria. Source zone flow reduction decreases the rate of source mass depletion, but can facilitate compliance, if concentrations at compliance locations are not too high initially. Increase in source biodecay rate, especially with concomitant increases in dissolution kinetics, can decrease the time to achieve compliance criteria over biodecay alone.

54 ENVIRONMENTAL SCIENCES↗

Macroscopic and molecular-scale assessment of soil lead contamination impacted by seasonal dove hunting activities

Environmental contamination of lead (Pb) in soils and sediments poses serious threats to human and ecological health. The objective of this study is to investigate the effect of seasonal dove sports hunting activities on Pb contamination in acid forest soils. A grid sampling method was used to investigate the spatial distribution of Pb contamination in surface soils. Soils were analyzed for total metal(loid) concentration and characterized for physicochemical properties and mineralogy. Adsorption isotherm experiments were also conducted to understand the reactivity and retention capacity of Pb(II) in soils. Finally, synchrotron-based X-ray microprobe and X-ray absorption spectroscopy were used to understand the chemical speciation of Pb that controls the retention/release mechanisms of Pb in soils. There was no excessive accumulation of Pb at the site. However, the concentration of Pb in surface soils was greater than the background level (<16 mg kg{sup -1}). The contamination level of Pb was as high as 67 mg kg{sup -1} near a patch of corn field where lime was frequently applied. A microfocused X-ray microprobe analysis showed the presence of Pb pellet fragments that predominantly contain oxidized Pb(II), suggesting that oxidative dissolution was occurring in soils. Dissolved Pb(II) can be readily retained in soils up to {approx}3,600 mg kg{sup -1} via inner-sphere and outer-sphere surface complexation on carbon and aluminol functional groups of soil components, suggesting that partitioning reactions control the concentration of Pb in soil solution. The fate of Pb is likely to be controlled by (1) oxidative dissolution process of Pb(0) pellets and (2) the release of outer-sphere and/or inner-sphere Pb surface complexes in humic substances and aluminosilicate/Al oxyhydroxides. Although no remedial actions are immediately required, the long-term accumulation of Pb in soils should be carefully monitored in protecting ecosystem and water quality at the dove hunting field.

54 ENVIRONMENTAL SCIENCES↗

Wetting Behavior of Calcium Ferrite Slags on Cristobalite Substrates

Calcium ferrite (CF) is a significant intermediate adhesive phase in high-basicity sinters. The wettability between calcium ferrite (CF) and gangue plays an important role in the assimilation process. The wettability of CF-based slags, in which a constant amount (2 mass pct.) of Al{sub 2}O{sub 3}, MgO, SiO{sub 2}, and TiO{sub 2} was added, on solid SiO{sub 2} (cristobalite) substrates at 1523 K (1250 °C) was investigated. The interfacial microstructure and spreading mechanisms were discussed for each sample. All the tested slag samples exhibited good wettability on the SiO{sub 2} substrate. The initial apparent contact angles were in the range of 20 to 50 deg, while the final apparent contact angles were ~ 5 deg. The wetting process could be divided into three stages on the basis of the change in diameter, namely the “linear spreading” stage, “spreading rate reduction” stage, and “wetting equilibrium” stage. It was found that the CF-SiO{sub 2} wetting system exhibits dissolutive wetting and the dissolution of SiO{sub 2} into slag influences its spreading process. The spreading rate increases with a decrease in the ratio of viscosity to interfacial tension, which is a result of the addition of Al{sub 2}O{sub 3}, MgO, SiO{sub 2}, and TiO{sub 2}. After cooling, a deep corrosion pit was formed in the substrate and a diffusion layer was generated in front of the residual slag zone; further, some SiO{sub 2} and Fe{sub 2}O{sub 3} solid solutions precipitated in the slag.

36 MATERIALS SCIENCE↗

Effects of Static Recrystallization and Precipitation on Mechanical Properties of 00Cr12 Ferritic Stainless Steel

The 00Cr12 ferritic stainless steel samples were isothermally held at different temperatures in the range of 700 °C to 1000 °C to investigate the effect of static recrystallization and precipitation on mechanical properties, such as microhardness, tensile strength, and yield strength. The results show that the formation of the fine recrystallized grain, as well as precipitation, coarsening, and dissolution of the second-phase particles, influences the mechanical properties remarkably. The fine recrystallized grain can provide a positive grain boundary-strengthening effect in the sample under a relatively high holding temperature. Coarsening and dissolution of M{sub 23}C{sub 6} result in partial depletion of precipitate hardening. In contrast, the size and number density of MX particles are almost constant, regardless of the holding temperature; therefore, it can provide a better precipitation-hardening effect.

36 MATERIALS SCIENCE↗

Fundamentals of Hydrogen Solubility in Calcium-Alumino-Silicate Molten Fluxes Containing NaF

The effect of the NaF and CaO/SiO{sub 2} ratio (mass percentage ratio) on hydrogen solubility in a CaO-SiO{sub 2}-Al{sub 2}O{sub 3}-NaF system was studied and correlated to the structural units of the molten flux. Fourier transformed infrared, Raman, and X-ray photoelectron spectroscopy analyses were used to evaluate the structural units with NaF additions and various CaO/SiO{sub 2} ratios. At a CaO/SiO{sub 2} ratio of 0.8, the incorporated-hydroxyl dissolution mechanism is dominant, whereas the free-hydroxyl mechanism is pronounced at higher CaO/SiO{sub 2} ratio. At low NaF contents, the hydrogen solubility as a function of the CaO/SiO{sub 2} ratio showed a parabolic trend with a minimum typical of a change from incorporated- to a free-hydroxyl dissolution mechanism. The addition of network-modifying NaF depolymerizes the structural units of the flux, reducing the available sites for incorporated-hydroxyl groups. The hydrogen solubility behavior in the flux system correlates well with the structural analysis, where a high NaF content and CaO/SiO{sub 2} ratio are shown to depolymerize the complex structural units of the molten flux.

36 MATERIALS SCIENCE↗

Influence of Al{sub 2}O{sub 3} Level in CaO-SiO{sub 2}-MgO-Al{sub 2}O{sub 3} Refining Slags on Slag/Magnesia-Doloma Refractory Interactions

The influence of the Al{sub 2}O{sub 3} level in CaO-SiO{sub 2}-MgO-Al{sub 2}O{sub 3} (CSMA) stainless steel refining slags on the degradation of magnesia-doloma refractories was investigated through static refractory finger corrosion tests. The tests were performed at 1620 °C under Ar atmosphere, using slags with Al{sub 2}O{sub 3} contents of 5, 10, and 20 wt pct, respectively. The results indicate that the formation of 2CaO·SiO{sub 2} at the slag/refractory interface was suppressed by increasing the Al{sub 2}O{sub 3} content to 20 wt pct, thereby changing the corrosion mechanism from an indirect dissolution to a direct dissolution of CaO and MgO from the refractories. The increased solubility limit of MgO by the Al{sub 2}O{sub 3}-rich CSMA slags results in an overall higher corrosion rate of the MgO-doloma refractory.

36 MATERIALS SCIENCE↗

Oxidation Behavior of Carbon Steel: Effect of Formation Temperature and pH of the Environment

The nature of surface oxide formed on carbon steel piping used in nuclear power plants affects flow-accelerated corrosion. In this investigation, carbon steel specimens were oxidized in an autoclave using demineralized water at various temperatures (150-300 °C) and at pH levels (neutral, 9.5). At low temperatures (< 240 °C), weight loss of specimens due to dissolution of iron in water occurred to a greater extent than weight gain due to oxide formation. With the increase in temperature, the extent of iron dissolution reduced and weight gain due to oxide formation increased. A similar trend was observed with the increase in pH as was observed with the increase in temperature. XRD and Raman spectroscopy confirmed the formation of magnetite. The oxide film formed by precipitation process was negligible at temperatures from 150 to 240 °C compared to that at higher temperatures (> 240 °C) as confirmed by scanning electron microscopy. Electrochemical impedance measurement followed by Mott–Schottky analysis indicated an increase in defect density with exposure duration at 150 °C at neutral pH but a low and stable defect density in alkaline environment. The defect density of the oxide formed at neutral pH at 150-300 °C was always higher than that formed in alkaline environment as reported in the literature.

36 MATERIALS SCIENCE↗

Pitting Corrosion of 10Ni8CrMoV High-Strength Steel Induced by a Potential Perturbation

Pitting corrosion of high-strength steel 10Ni8CrMoV under square wave polarization (SWP) in simulated deep-sea environment is investigated and the possible mechanism is proposed. The results show that potential perturbation generates periodic intensification effect on both anodic and cathodic processes by frequently breaking the electrode equilibrium state. The intensity of periodic intensification effect essentially depends on the concentration gradient of Fe{sup 2+} cations at the steel/solution interface which acts as the forced electrochemical oscillator. The concentration gradient and the resulting concentration polarization effect increase periodically with the increase in SWP potential range. The morphology observation of the pitting and electric charge calculation indicate that the periodic intensification effect can promote the initiation and growth of pits by enhancing the anodic dissolution even under cathodic protection, but it is ineffective below the hydrogen evolution potential. The decrease in either upper or lower potential can mitigate anodic dissolution. Through the statistical analysis of pitting size, it is found that the wide potential range tends to activate the metastable pitting formed under hydrostatic pressure, forming densely distributed pitting. Meanwhile, it is more favorable to the formation of fully grown pits with high size dispersion degree when the proportion of electric charge in the anodic process is higher.

36 MATERIALS SCIENCE↗

Applying Improved Optical Recognition with Machine Learning on Sorting Cu Impurities in Steel Scrap

Annually, 20–55 million tons of electronic waste (e-waste) is produced worldwide (5% of all municipal solid waste). Although e-waste embodies only 2% of America’s municipal waste, it accounts for a significantly larger proportion of the heavy metals and flame retardants present in the waste stream. Currently, less than 20% of all e-waste is recycled in the United States because the heterogeneity of the feedstock limits the opportunity for reuse in high value products and processing of the waste itself is often too costly to justify handling. To address this concern, the aims of this study are: 1) to identify the major plastic and metal compositions within electronic shredder residue (ESR), 2) to formulate solvents and processing conditions to separate 90% of the plastics targeted from consumer shred ESR, and 3) to develop a process design model to estimate the cost and energy efficiency of the proposed solvent-based processing. In this study, a pre-sorted heterogeneous ESR feedstock (one where aluminum, magnetic components, and hazardous battery materials removed by an e-waste recycling facility) was used, with the major compositions of the ESR characterized. It was found that 25 wt.% of the feedstock was composed of plastics, 6 wt.% rubber, 27 wt.% printed circuit boards, 23% wire, and the remainder metals and capacitors. Within the plastic portion, polystyrene (PS, 40 wt.%), acrylonitrile butadiene styrene (ABS, 25 wt.%), and styrene-acrylonitrile (SAN, 9wt.%) were identified to compose the majority of the screened plastics using Fourier transform infrared spectroscopy (FTIR). Next, selective solvents were screened using Hansen Solubility Parameter Theory (HSP) for dissolving PS and ABS. The pre-screening results show that methylene chloride (dichloromethane, DCM) and tetrahydrofuran (THF) are capable of dissolving the most PS and ABS, while methanol (MeOH) and ethylene glycol (EG) are capable of precipitating the most PS and ABS. These solvents were subsequently used to recover polymers and remove. flame retardants within the ESR feedstock. By optimizing the dissolution time and the solvents used, the highest polymer dissolution yield (99 wt.%%) was achieved using DCM for 48 hr. Both pre-screened anti-solvents (MeOH and EG) showed the highest polymer precipitation yield (71 wt.%). In terms of flame retardant removal rate, EG was found to have a high phosphorus-containing flame retardant removal rate (up to 98%). Characterization shows that the proposed solvent-based processing can preserve a high molecular weight fraction of the polymers and effectively remove flame retardants. Cost analysis indicates that the amount of the solvent/anti-solvent recovered after the reaction would play a critical role in reducing the operating costs. The energy analysis shows that the proposed solvent-based processes can save up to 60% of the embodied energy used to manufacture plastics used in electronics (PS and ABS were used for calculations). The results from this project prove the potential of solvent-based processing to produce secondary materials (plastics and metals) from e-waste for cross-industry reuse.

36 MATERIALS SCIENCE↗

Microstructure chemistry and mechanical properties of Ni-based superalloy Rene N4 under irradiation at room temperature

Nickel superalloys with cubic L12 structured γ' (Ni 3 (Al, Ti)) precipitates exhibit high strength at high temperatures and excellent corrosion resistance when exposed to water. Unlike prior studies on irradiation damage of other Ni-based superalloys, our study on Rene N4 involves much larger γ' precipitates, ~450 nm in size, a size regime where the irradiation-induced disordering and dissolution kinetics and the corresponding mechanical property evolution are unknown. Under heavy ion irradiation at room temperature, the submicron-sized γ' precipitates were fully disordered at ~0.3 dpa and only later partially dissolved after 75 dpa irradiation. Nanoindentation experiments indicate that the mechanical properties of the alloy change significantly, with a dramatic decrease in hardness, with irradiation dose. Three contributions to the change in hardness were examined: defect clusters, disordering and dissolution. Moreover, the generation of defect clusters in the matrix and precipitates slightly increased the indentation hardness, while disordering of the submicron-sized γ' precipitates resulted in a dramatic decrease in the total hardness, which decreased further during the early stages of the intermixing between γ' precipitates and matrix (<18 dpa). As a result, controlling the long-range-ordering and chemical intermixing can be used to tailor the mechanical properties of Ni-based superalloys under irradiation.

36 MATERIALS SCIENCE↗

Composition, stability, and measurement of reduced uranium phases for groundwater bioremediation at Old Rifle, CO

Reductive biostimulation is currently being explored as a possible remediation strategy for uranium (U) contaminated groundwater, and is currently being investigated at a field site in Rifle, CO, USA. The long-term stability of the resulting U(IV) phases is a key component of the overall performance and depends upon a variety of factors, including rate and mechanism of reduction, mineral associations in the subsurface, and propensity for oxidation. To address these factors, several approaches were used to evaluate the redox sensitivity of U: measurement of the rate of oxidative dissolution of biogenic uraninite (UO{sub 2(s)}) deployed in groundwater at Rifle, characterization of a zone of natural bioreduction exhibiting relevant reduced mineral phases, and laboratory studies of the oxidative capacity of Fe(III) and reductive capacity of Fe(II) with regard to U(IV) and U(VI), respectively.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

A new approach in quantitative in-situ XRD of cement pastes: Correlation of heat flow curves with early hydration reactions

XRD measurements of the hydration of synthetical cement (SyCem) were used to calculate the resulting heat flow from changes in the phase content. Calculations were performed by application of thermodynamic data. The comparison with data recorded from heat flow calorimetry was in good agreement with the calculated heat flow. The initial maximum of heat flow mainly is caused by the aluminate reaction. During the entire main period the silicate reaction dominates hydration with a high and long first maximum of heat flow. The second but less intense heat flow maximum - only visible as a shoulder in most of the technical cements - can be attributed to an acceleration of the aluminate reaction with the enhanced dissolution of C{sub 3}A and the final formation of ettringite. Moreover, the investigation showed that the dissolution process of C{sub 3}A is directly controlled by the availability of the calcium sulfate phases.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Kinetics of lime/bentonite pozzolanic reactions at 20 and 50 °C: Batch tests and modeling

The effects of duration (1–100 days) and temperature (20 and 50 °C) were assessed from batch tests for Ca-bentonite mixed with 10 wt.% lime. The pozzolanic processes were monitored over time by {sup 29}Si NMR (Cement Concr. Res. 42, 2012), TGA-DTA, XRD and chemical analysis. Modeling considered kinetics and thermodynamics of mineralogical transformations and cation exchange. Kinetic laws were dependent on pH and temperature (Arrhenius energy). Lime hydration occurs within hours, modifying the bentonite exchangeable population and increasing the pH. These alkaline conditions initiate the pozzolanic reactions in a second stage. The rate-limiting step is the dissolution kinetics of the bentonite minerals, i.e. a relatively fast and total consumption of cristobalite in parallel to a long-term slower dissolution of montmorillonite. First C–S–H and then C–A–S–H are formed consequently. Temperature speeds up the pozzolanic reaction kinetics by a factor 5 from 20 to 50 °C, corresponding to an apparent activation energy of 40–50 kJ/mol.

36 MATERIALS SCIENCE↗