Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “STRESS AND LOAD”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 1,351 records · Page 75

Burner liner thermal/structural load modelling

The objective of this program is to develop a thermal data transfer computer program module for the burner liner thermal structural load modeling program. This will be accomplished by (1) reviewing existing methodologies for thermal data transfer and selecting three heat transfer codes for application in this program; (2) evaluating the selected codes to establish criteria for developing a computer program module to transfer thermal data from the heat transfer codes to selected stress analysis codes; (3) developing the automated thermal load transfer module; and (4) verifying and documenting the module. In aircraft turbine engine hot section components, cyclic thermal stresses are the most important damage mechanism. Consequently, accurate and reliable prediction of thermal loads is essential to improving durability. To achieve this goal, a considerable effort over the past 20 years has been devoted to the acquisition of engine temperature test data, as well as the development of accurate, reliable, and efficient computer codes for the prediction of steady state and transient temperatures and for the calculation of elastic and inelastic cyclic stresses and strains in hot section components. There is a need for continued development of these codes, because the availability of more accurate analysis techniques for complex configurations has enabled engine designers to use more sophisticated designs to achieve higher cycle efficiency and reduce weight.

Maffeo, R. J.↗

Dislocation generation in diamond under extreme loading

Diamond is, by virtue of its high bonding forces and Peierls-Nabarro barrier stresses, among the hardest materials on earth due to the difficulty of generating and moving dislocations. We demonstrate, using molecular dynamics and analytical calculations, that the generation of defects is dependent on loading orientation. Shock-loading single-crystal diamond along [001] and [011] to a stress of 137 GPa did not reveal dislocations, whereas loading along [111] generated profuse dislocations. The introduction of a void at the latter orientation generated dislocations at 72.6 GPa. Two slip systems were identified: <011>{100} and <112>{111}. The threshold for plastic deformation in diamond is orientation dependent and significantly lower than reported in previous studies: 0.14 G (shear modulus). The void collapse generated localized amorphization for [001]. In conclusion, these results on the anisotropy of plasticity and void effects have relevance for the improvement of symmetry in the collapse of diamond capsules in inertial fusion experiments.

36 MATERIALS SCIENCE↗

Prediction of service life of aircraft structural components using the half-cycle method

The service life of aircraft structural components undergoing random stress cycling was analyzed by the application of fracture mechanics. The initial crack sizes at the critical stress points for the fatigue-crack growth analysis were established through proof load tests. The fatigue-crack growth rates for random stress cycles were calculated using the half-cycle method. A new equation was developed for calculating the number of remaining flights for the structural components. The number of remaining flights predicted by the new equation is much lower than that predicted by the conventional equation.

Ko, William L.↗

An approximate analytical solution for interlaminar stresses in angle-ply laminates

An improved approximate analytical solution for interlaminar stresses in finite width, symmetric, angle-ply laminated coupons subjected to axial loading is presented. The solution is based upon statically admissible stress fields which take into consideration local property mismatch effects and global equilibrium requirements. Unknown constants in the admissible stress states are determined through minimization of the complementary energy. Typical results are presented for through-the-thickness and interlaminar stress distributions for angle-ply laminates. It is shown that the results represent an improved approximate analytical solution for interlaminar stresses.

Rose, Cheryl A.↗

A Method of Strengthening Composite/Metal Joints

The term tape setback method denotes a method of designing and fabricating bonded joints between (1) box beams or other structural members made of laminated composite (matrix/ fiber) materials and (2) metal end fittings used to fasten these structural members to other structural members. The basic idea of the tape setback method is to mask the bonded interface between the metallic end fitting and composite member such that the bond does not extend out to the free edges of the composite member. The purpose served by the tape setback method is to strengthen the joints by decoupling stress concentrations from edge defects, which can cause premature failures. A related prior method that serves a similar purpose, involving the use of tapered adherends at the joints, can be too difficult and costly to be acceptable in some applications. The tape setback method offers an easier, less costly alternative. The structural members to which the method was originally applied were box beams in the form of composite tubes having flat faces with rounded corners. The end fittings were plugs made of a low-thermal- expansion nickel/iron alloy (see figure). In computational-simulation studies of tensile and compressive loading of members without tape setback, stresses were found to be concentrated at the free end edges of the composite tubes, and inspection of members that had been subjected to real tension and compression tests showed that cracks started at the free end edges. As applied to these members, the tape setback method makes them less vulnerable to initiation of failure at edge defects produced during fabrication. In real tension tests of comparable members without and with tape setback, the average mean tensile strength of the members with tape setback was found to be 1.9 times that of the members without tape setback.

Polis, Daniel L.↗

Improved Heat-Stress Algorithm

NASA Dryden presents an improved and automated site-specific algorithm for heat-stress approximation using standard atmospheric measurements routinely obtained from the Edwards Air Force Base weather detachment. Heat stress, which is the net heat load a worker may be exposed to, is officially measured using a thermal-environment monitoring system to calculate the wet-bulb globe temperature (WBGT). This instrument uses three independent thermometers to measure wet-bulb, dry-bulb, and the black-globe temperatures. By using these improvements, a more realistic WBGT estimation value can now be produced. This is extremely useful for researchers and other employees who are working on outdoor projects that are distant from the areas that the Web system monitors. Most importantly, the improved WBGT estimations will make outdoor work sites safer by reducing the likelihood of heat stress.

Teets, Edward H., Jr.↗

Resizing procedure for optimum design of structures under combined mechanical and thermal loading

An algorithm is reported for resizing structures subjected to combined thermal and mechanical loading. The algorithm is applicable to uniaxial stress elements (rods) and membrane biaxial stress members. Thermal Fully Stressed Design (TFSD) is based on the basic difference between mechanical and thermal stresses in their response to resizing. The TFSD technique is found to converge in fewer iterations than ordinary fully stressed design for problems where thermal stresses are comparable to the mechanical stresses. The improved convergence is demonstrated by example with a study of a simplified wing structure, built-up with rods and membranes and subjected to a combination of mechanical loads and a three dimensional temperature distribution.

Adelman, H. M.↗

Thermal loading effects on chalk hydromechanical behavior for nuclear waste disposal

Safe disposal of heat-generating nuclear waste depends on host rock stability under thermal, hydrological, and mechanical stresses. This study investigates the effect of thermal loading on mechanical behavior of the shallowly buried Ghareb formation chalk through triaxial and hydrostatic constant strain rate and creep tests at temperatures up to 100 ˚C and effective pressures up to 20.7 MPa. Experimental results show that thermal loading reduces the elastic moduli of chalk by 50–75%, and a transition occurs above 60 ˚C where creep rates increase rapidly. Water saturation nearly doubles the thermally induced strain compared to dry conditions and strongly decreases material rigidity. Thermal loading also leads to significant pore pressure increases under undrained conditions and leads to reductions in the apparent permeability during drained conditions. Laboratory experimental data were used to parameterize and develop a preliminary constitutive model for predicting future deformation during repository operations in the Ghareb. The strongly coupled effects – mechanical weakening, fluid pressure fluctuations, and permeability modification – demonstrate that elevated repository temperatures will have a pronounced effect on the near field Ghareb behavior during waste disposal operations. The findings indicate that the coupled interactions must be considered in predictive models and repository design to ensure long-term nuclear waste isolation and safety.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Mechanical property anisotropy in superalloy El-929 directionally solidified by an exothermic technique

Directional solidification (DS) of the nickel-based superalloy El-929 was carried out by employing the exothermic technique for preparing several 150 mm long x 55 mm diameter rods. Specimens machined from blanks cut at 0, 45, 75 and 90 deg to the chill surface were tensile and stress-rupture tested at different temperatures. The air-melted DS alloy, when loaded parallel to the growth direction, shows considerable improvement in stress-rupture life and tensile ductility as compared with the vacuum induction melted, forged and heat-treated alloy. However, these property advantages rapidly degrade with the increasing deviation of the load axis from the growth direction.

Pradhan, D. C.↗

A torque, tension and stress corrosion evaluation of high strength A286 bolts

The problems associated with overtorque applied to the Booster Separation Motor (BSM) Igniter Adapter high strength 200 KSI (1379 Mpa) A286 CRES bolts and the threaded holes of the 7075-T73 aluminum alloy BSM cases are addressed. The evaluation included torque, tensile, and stress corrosion tests incorporating the A286 CRES bolts and the 7075-T73 aluminum alloy BSM cases. The tensile test data includes ultimate tensile load (UTL), Johnson's 2/3 yield load (J2/3YL), proportional limit load (PLL), and total bolt stretch. Torque tension data includes torque, torque induced load, and positive and negative break-away torque. Stress corrosion test data reflect the overtorque and the resulting torque induced loads sustained by the A286 CRES bolts torqued into a 7075-T73 aluminum alloy forged dome with threaded holes. After 60 days of salt fog exposure, the positive and the negative break-away torques, the subsequent mechanical property tensile test results, and the BSM dome threaded hole axial tensile pullout loads are reported.

Montano, J. W.↗

Design and Analysis of an Advanced Three-Point Bend Test Approach for Miniature Irradiated Disk Specimens

Candidate tungsten armor materials in a magnetic confinement fusion device must be able to withstand thermal variation that leads to internal stresses caused by the impinging heat load. In addition, the thermomechanical properties of these materials are degraded by irradiation-induced defect accumulation. Fission reactor–based irradiation data are used to predict the fusion neutron damage and property change. This study examines the motivation and design of a custom-designed three-point bend test for neutron-irradiated disk specimens that are 3 mm in diameter to be able to define the flexural strength of advanced tungsten materials, alloys, and composites—and to the extent that embrittlement occurs after neutron irradiation. The theory provided shows a calculation for the flexural deflection and shear deflection due to the small-geometry constraints. A finite element deformation analysis is performed to evaluate the mechanical stress field of disk bend specimens. The stress values above 80% of the maximum stress are concentrated in 2.4 mm of the 3.0-mm length of the centerline across the tungsten disk diameter. A bend test fixture has been designed and fabricated to enable testing of these specimens with precisely engineered tolerance and minimal machine compliance. This fixture will be able to be placed inside a universal testing frame at elevated temperatures for the mechanical property evaluation of future neutron-irradiated disk specimens.

36 MATERIALS SCIENCE↗

Finite element stress analysis of a notched coupon specimen for in-plane shear behaviour of composites

The results of a linear elastic, plane stress finite element investigation of the stress distribution in a double V-notched coupon specimen are presented for an isotropic material (steel) and five graphite/polyimide laminates: (0), (90), (0/90)s, (plus or minus 45)s and (0/90/plus or minus 45)s. Stress contours, stress profiles, and stress concentration factors are presented for specimens loaded through rigid fixtures. It is shown that the finite element analysis predicts a region of essentially uniform pure shear in the central portion of the specimen for all laminates considered. Stress concentrations vary considerably with laminate configuration. The influences of elastic fixtures and thermal stresses on the stress distribution in (0) laminates are also investigated. The (0) laminate is predicted to exhibit maximum pure shear in the center of the test section for both rigid and elastic fixtures. It is concluded that the specimen is a practicable candidate for use as a composite shear specimen.

Herakovich, C. T.↗

Structural behavior of the space shuttle SRM Tang-Clevis joint

The space shuttle Challenger accident investigation focused on the failure of a tang-clevis joint on the right solid rocket motor. The existence of relative motion between the inner arm of the clevis and the O-ring sealing surface on the tang has been identified as a potential contributor to this failure. This motion can cause the O-rings to become unseated and therefore lose their sealing capability. Finite element structural analyses have been performed to predict both deflections and stresses in the joint under the primary, pressure loading condition. These analyses have demonstrated the difficulty of accurately predicting the structural behavior of the tang-clevis joint. Stresses in the vicinity of the connecting pins, obtained from elastic analyses, considerably exceed the material yield allowables indicating that inelastic analyses are probably necessary. Two modifications have been proposed to control the relative motion between the inner clevis arm and the tang at the O-ring sealing surface. One modification, referred to as the capture feature, uses additional material on the inside of the tang to restrict motion of the inner clevis arm. The other modification uses external stiffening rings above and below the joint to control the local bending in the shell near the joint. Both of these modifications are shown to be effective in controlling the relative motion in the joint.

Greene, W. H.↗

Structural behavior of the space shuttle SRM tang-clevis joint

The space shuttle Challenger accident investigation focused on the failure of a tang-clevis joint on the right solid rocket motor. The existence of relative motion between the inner arm of the clevis and the O-ring sealing surface on the tang has been identified as a potential contributor to this failure. This motion can cause the O-rings to become unseated and therefore lose their sealing capability. Finite element structural analyses have been performed to predict both deflections and stresses in the joint under the primary, pressure loading condition. These analyses have demonstrated the difficulty of accurately predicting the structural behavior of the tang-clevis joint. Stresses in the vicinity of the connecting pins, obtained from elastic analyses, considerably exceed the material yield allowables indicating that inelastic analyses are probably necessary. Two modifications have been proposed to control the relative motion between the inner clevis arm and the tang at the O-ring sealing surface. One modification, referred to as the capture feature, uses additional material on the inside of the tang to restrict motion of the inner clevis arm. The other modification uses external stiffening rings above and below the joint to control the local bending in the shell near the joint. Both of these modifications are shown to be effective in controlling the relative motion in the joint.

Greene, William H.↗

Accelerated Testing Methodology Developed for Determining the Slow Crack Growth of Advanced Ceramics

Constant stress-rate ("dynamic fatigue") testing has been used for several decades to characterize the slow crack growth behavior of glass and structural ceramics at both ambient and elevated temperatures. The advantage of such testing over other methods lies in its simplicity: strengths are measured in a routine manner at four or more stress rates by applying a constant displacement or loading rate. The slow crack growth parameters required for component design can be estimated from a relationship between strength and stress rate. With the proper use of preloading in constant stress-rate testing, test time can be reduced appreciably. If a preload corresponding to 50 percent of the strength is applied to the specimen prior to testing, 50 percent of the test time can be saved as long as the applied preload does not change the strength. In fact, it has been a common, empirical practice in the strength testing of ceramics or optical fibers to apply some preloading (<40 percent). The purpose of this work at the NASA Lewis Research Center is to study the effect of preloading on measured strength in order to add a theoretical foundation to the empirical practice.

Choi, Sung R.↗

The influence of modifications of a fatigue loading history program on fatigue lifetime

Rectangular specimens of 7075 and 2014 aluminum alloys with two holes (stress concentration factor of 3.24) have been tested under axial fatigue loading on a six-rod test bed with modifications of the loading program, the surface particulars, and the frequency. The length of the precrack stage was investigated by use of a new crack detector. In most cases the two alloys behaved similarly, with similar life to crack start under the same loading. Some overloads lengthened the life. Truncation by omission of the lowest peak loads should be limited to about 20 percent of the ultimate load. Simplifying counting methods gave misleading results. Very thin surface layers of anodizing, protection by vinyl, dry nitrogen atmosphere, as well as stepwise reaming or grinding the surface of the holes, lengthened the life; thick anodized layers shortened the life. Compressing the hole surface by rolling had no influence. Frequencies at about 210 to 240 cpm produced shorter lives than those at 40 cpm. At 5.4 cpm the life was considerably longer. A model to better understand the precrack-stage fatigue mechanism is discussed.

Branger, J.↗

Fatigue Behavior of a Third Generation PM Disk Superalloy

The fatigue behavior of a 3rd generation PM disk alloy, LSHR, was studied at 1300 F. Tensile, creep, and fatigue tests were run on smooth and notched (Kt = 2) bars under a variety of conditions. Analysis of smooth bar fatigue data, run under strain and load control with R ratios of 0 and -1, showed that a stress based Smith-Watson-Topper approach could collapse the data set. While the tensile and creep data showed substantial notch strengthening at 1300 F, the fatigue data showed a life deficit for the notch specimens. A viscoplastic finite element model, which accounted for stress relaxation at the notch tip, provided the best correlation between the notched and smooth bar behavior, although the fatigue data was not fully rationalized based on this simplified viscoplastic model of the stresses at the notch tip.Inclusion of a 90 sec dwell at peak load was found to dramatically decrease notch fatigue life. This result was shown to be consistent with a simple linear creep-fatigue damage rule, where creep damage dominated at low stresses and fatigue damage was more prevalent at higher stresses.

Gayda, John↗

Investigation of the Leak Response of a Carbon-Fiber Laminate Loaded in Biaxial Tension

Designers of pressurized structures have been reluctant to use composite materials because of concerns over leakage. Biaxial stress states are expected to be the worst-case loading condition for allowing leakage to occur through microcracks. To investigate the leakage behavior under in-plane biaxial loading, a cruciform composite specimen was designed that would have a relatively large test section with a uniform 1:1 biaxial loading ratio. A 7.6-cm-square test section was desired for future investigations of the leakage response as a result of impact damage. Many iterations of the cruciform specimen were evaluated using finite element analysis to reduce stress concentrations and maximize the size of the uniform biaxial strain field. The final design allowed the specimen to go to relatively high biaxial strain levels without incurring damage away from the test section. The specimen was designed and manufactured using carbon/epoxy fabric with a four-ply-thick, quasi-isotropic, central test section. Initial validation and testing were performed on a specimen without impact damage. The specimen was tested to maximum biaxial strains of approximately 4500micro epsilon without apparent damage. A leak measurement system containing a pressurized cavity was clamped to the test section and used to measure the flow rate through the specimen. The leakage behavior of the specimen was investigated for pressure differences up to 172 kPa

Jackson, Wade C.↗