Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “Alloy Design”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 1,351 records · Page 75

Multiscale fatigue crack initiation in hierarchical additively manufactured alloys

Bioinspired hierarchical microstructures offer a route toward engineered fatigue resistance in additively manufactured alloys. However, it remains unclear how discrete structural constituents independently govern damage accumulation, particularly during the critical fatigue initiation regime where short cracks strongly interact with local microstructure. Here, we investigate multiscale fatigue initiation in a dual-phase, nanolamellar AlCoCrFeNi 2.1 high-entropy alloy. By comparing microscale specimens that isolate the nanolamellar structure against macroscale specimens containing the full melt-pool architecture, we identify size-dependent fatigue initiation mechanisms. We find that failure is dictated by nanolamellar interfaces at the microscale, whereas mesoscale melt pool boundaries serve to initiate fatigue at the macroscale. This mechanistic shift is accompanied by a transition from macroscale quasi-brittle failure to microscale plasticity-driven crack extension. Our results provide a physical framework for understanding how structural hierarchy governs the transition from discrete microstructural deformation to continuum fatigue fracture behavior, informing the design of damage-tolerant, additively manufactured alloys.

36 MATERIALS SCIENCE↗

AN INITIAL ASSESSMENT OF THE CREEP-RUPTURE STRENGTHS FOR WELDMENTS WITH ALLOY 800H BASE METAL AND ALLOY 617 FILLER METAL

In Section III, Division 5 of the American Society of Mechanical Engineers Boiler and Pressure Vessel Code, Alloy 800H is qualified for elevated-temperature nuclear construction for temperatures up to 760°C (1,400°F) and a maximum service life of 300,000 hours. There are two permissible filler metals for Alloy 800H weldments specified in Division 5: ENiCrFe-2 (Alloy A) and ERNiCr-3 (Alloy 82). Low creep-rupture strengths of these weldments at the upper limits of the qualified temperatures and service lives may restrict the design envelope for elevated-temperature nuclear construction with Alloy 800H. As a result, an alternative filler metal is desired to improve the creep-rupture strengths of Alloy 800H weldments for the qualified temperatures and service lives. This work investigates an overmatched filler metal. Specifically, a weldment with Alloy 800H base metal and Alloy 617 filler metal fabricated by semiautomated gas tungsten arc welding is investigated. A scoping creep-rupture test program was conducted of cross-weld specimens at temperatures ranging from 750 to 1,000°C (1,292 to 1,832°F). Preliminary results on the creep-rupture strengths of the Alloy 800H weldment with Alloy 617 filler metal do not show significant improvement compared to the filler metals currently qualified in Division 5 for Alloy 800H weldments. Consequently, work is in progress to investigate a matching filler metal.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

GCR: Development of Improved Alloy 800H Weldment

In Section III, Division 5 of the American Society of Mechanical Engineers Boiler and Pressure Vessel Code, Alloy 800H is qualified for elevated-temperature nuclear construction for temperatures up to 760°C (1400°F) and a maximum service life of 300,000 hours. There are two permissible filler metals for Alloy 800H weldments specified in Division 5: ENiCrFe-2 (Alloy A) and ERNiCr-3 (Alloy 82). Low creep-rupture strengths of these weldments at the upper limits of the qualified temperatures and service lives may restrict the design envelope for elevated-temperature nuclear construction with Alloy 800H. As a result, an alternative filler metal is desired to improve the creep-rupture strengths of Alloy 800H weldments for the qualified temperatures and service lives. This work investigates an overmatched filler metal. Specifically, a weldment with Alloy 800H base metal and Alloy 617 filler metal fabricated by semiautomated gas tungsten arc welding is investigated. A scoping creep-rupture test program was conducted of cross-weld specimens at temperatures ranging from 750 to 1000°C (1292 to 1832°F). Preliminary results on the creep-rupture strengths of the Alloy 800H weldment with an Alloy 617 filler metal do not show significant improvement compared to the filler metals currently qualified in Division 5 for Alloy 800H weldments. Consequently, work is in progress to investigate a matching filler metal, UTP A 2133 Mn.

36 MATERIALS SCIENCE↗

Demonstration of a Desktop Liquid Direct Metal Write Additive Manufacturing System (CRADA NFE-17-06531 Final Report)

ORNL worked with PrintSpace 3D to demonstrate cost effective electromagnetic induction melting of aluminum alloys on their desktop Altair 3D printer. An electromagnetic coil design and susceptor have been optimized and paired with a high frequency power supply to melt Al-Ce alloys. The manufacturing feasibility of Al-Ce wire was also proven to be successful and precise process control of electro-magnetic heating was demonstrated. The system was found to have inherent safety benefits, requiring no powder handling and with very localized heating. Further research will demonstrate the ability to use DMW technology to print high temperature engine components for the transportation industry.

36 MATERIALS SCIENCE↗

Simplified Optimum Sizing and Cost Analysis for Compact heat Exchanger in VHTR

In this study, the optimum size of the compact heat exchanger has been developed based on its weight and pumping power for the reference design of 600 MWt very high temperature gas-cooled reactor (VHTR) system. Alloy 617 was selected as a construction material. The optimum size and a number of configurations for the reference design of the VHTR with an intermediate heat exchanger (IHX) were investigated and our initial calculations indicated that it has an unrealistically too large aspect ratio of the length and height due to its small-sized channels, which might cause manifolding problems and a large number of parallel modules with high thermal stress. The flow area and channel diameter were then adjusted to achieve a smaller aspect ratio in this paper. Achievement of this aspect ratio resulted in higher cost, but the cost increase was less than would have occurred by simply reducing the flow area by itself. The appropriate channel diameter is estimated to be less than 5.00 mm for the reference system. The effect of channel waviness enhanced the compactness and heat transfer performance, but unfavorably increased the aspect ratio. Therefore, the waviness should be carefully determined based on performance and economics. In this study, the waviness of the IHX is recommended to be selected between 1.0 and 2.5. Calculations show that reducing the duty dramatically decreases the aspect ratio, indicating that the compact heat exchanger is easy to be optimally designed for low duty, but many modules are required for high duty operation proportional to the operating power. Finally, the effect of working fluids was investigated, and it reveals that using carbon dioxide instead of helium in the secondary side reduces the size and cost by about 20% due to the lower pumping power in spite of its lower heat transfer capability by a factor of 4.

99 GENERAL AND MISCELLANEOUS↗

Development of Low Density Titanium Alloys for Structural Applications

In this report the results of a program designed to reduce the density of titanium by adding magnesium are presented. Because these two elements are immiscible under conventional ingot metallurgy techniques, two specialized powder metallurgy methods namely, mechanical alloying (MA) and physical vapor deposition (PVD) were implemented. The mechanical alloying experiments were done both at the University of Idaho and at the Defense Research Agency in UK. Since titanium is reactive with interstitial elements, a secondary goal of this research was to correlate solubility extensions with interstitial contamination content, especially oxygen and nitrogen. MA was carried out in SPEX 8000 shaker mils and different milling containers were utilized to control the level of contamination. Results showed that solubilities of Mg in Ti were obtained up to 28 at.% (16.4 wt. %) Mg in Ti for Ti-39.6 at. % (25 wt. %) Mg alloys, which greatly exceed those obtained under equilibrium conditions. This reflects a density reduction of approximately 26 %. Contamination of oxygen and nitrogen seemed to increase the solubility of magnesium in titanium in some cases; however, we were not able to make a clear correlation between contamination levels with solubilities. Work at the DRA has emphasized optimization of present PVD equipment, specifically composition and temperature control. Preliminary PVD data has shown Ti-Mg deposits have successfully been made up to 2 mm thick and that solubility extensions were achieved. The potential for density reduction of titanium by alloying with magnesium has been demonstrated; however, this work has only scratched the surface of the development of such low density alloys. Much research is needed before such alloys could be implemented into industry. Further funding is required in order to optimize the MA/PVD processes including contamination control, determination of optimal alloy compositions, microstructure development, and mechanical property determination.

Froes, F. H.↗

Handbook of the Materials Properties of FeCrAl Alloys For Nuclear Power Production Applications

FeCrAl alloys are a class of alloys that have seen increased interest for nuclear power applications including as accident tolerant fuel cladding, structural components for fast fission reactors, and as first wall and blanket structures for fusion reactors. FeCrAl alloys are under consideration for these applications due to their inherent corrosion resistance, stress corrosion cracking resistance, radiation-induced swelling resistance, and high temperature oxidation resistance. A substantial amount of research effort has been completed to design, develop, and begin commercial scaling of FeCrAl alloys for nuclear power applications over the past half a century. These efforts have led to the development of an extensive database on material properties and process knowledge for FeCrAl alloys but not within a consolidated format. The following report is the first edition of a materials handbook to consolidate the state-of-the-art on FeCrAl alloys for nuclear power applications. This centralized database focuses solely on wrought FeCrAl alloys, oxide dispersion strengthened alloys, although discussed in brief, are not covered. Where appropriate, recommendations for applications of the data is provided and current knowledge gaps are identified.

21 SPECIFIC NUCLEAR REACTORS AND ASSOCIATED PLANTS↗

Handbook on the Material Properties of FeCrAl Alloys for Nuclear Power Production Applications (FY18 Version: Revision 1)

FeCrAl alloys are a class of alloys that have seen increased interest for nuclear power applications including accident tolerant fuel cladding, structural components for fast fission reactors, and as first wall and blanket structures for fusion reactors. FeCrAl alloys are under consideration for these applications due to their inherent corrosion resistance, stress corrosion cracking resistance, radiation-induced swelling resistance, and high temperature oxidation resistance. A substantial amount of research effort has been completed to design, develop, and begin commercial scaling of FeCrAl alloys for nuclear power applications over the past half a century. These efforts have led to the development of an extensive database on material properties and process knowledge for FeCrAl alloys but not within a consolidated format. The following report is the first edition of a materials handbook to consolidate the current state of knowledge on FeCrAl alloys for nuclear power applications. This centralized database focuses solely on wrought FeCrAl alloys, oxide dispersion strengthened alloys, although discussed in brief, are not covered. Where appropriate, recommendations for applications of the data is provided and current knowledge gaps are identified.

36 MATERIALS SCIENCE↗

Geometric Limitation and Tensile Properties of Wire and Arc Additive Manufacturing 5A06 Aluminum Alloy Parts

Wire and arc additive manufacture (WAAM), as an emerging and promising technology of metal additive manufacturing, it lacks of experimental works to clarify the feature of geometrical configuration, microstructure and tensile properties, which can be used for further evaluating whether the as-deposited part can be used directly, and providing design reference for structure optimization. Taking 5A06 aluminum alloy additive manufacturing for example, in this paper, the geometric limitation and tensile property criteria are characterized using experimental method. The minimum angle and curvature radius that can be made by WAAM are 20° and 10 mm when the layer width is 7.2 mm. It shows isotropy when loading in build direction and perpendicular one. When loading in the direction of parallel and perpendicular to texture orientation, the tensile properties are anisotropic. The difference between them is 22 MPa.

36 MATERIALS SCIENCE↗

Electrical conductive polymer binder for Si alloy materials

A Poly(1-pyrenemethyl methacrylate-co-dopamine methacrylamide) PPyDMA polymer binder has been designed and fabricated, and has demonstrated an excellent performance for silicon (Si), graphite and a metal alloy anode materials. The PPyDMA polymer binder demonstrates the great potential of a catechol moiety for use in a lithium-ion battery.

36 MATERIALS SCIENCE↗

Influence of chemical disorder on energy dissipation and defect evolution in advanced alloys

We report that historically, alloy development with better radiation performance has been focused on traditional alloys with one or two principal element(s) and minor alloying elements, where enhanced radiation resistance depends on microstructural or nanoscale features to mitigate displacement damage. In sharp contrast to traditional alloys, recent advances of single-phase concentrated solid solution alloys (SP-CSAs) have opened up new frontiers in materials research. In these alloys, a random arrangement of multiple elemental species on a crystalline lattice results in disordered local chemical environments and unique site-to-site lattice distortions. Based on closely integrated computational and experimental studies using a novel set of SP-CSAs in a face-centered cubic structure, we have explicitly demonstrated that increasing chemical disorder can lead to a substantial reduction in electron mean free paths, as well as electrical and thermal conductivity, which results in slower heat dissipation in SP-CSAs. The chemical disorder also has a significant impact on defect evolution under ion irradiation. Considerable improvement in radiation resistance is observed with increasing chemical disorder at electronic and atomic levels. Finally, the insights into defect dynamics may provide a basis for understanding elemental effects on evolution of radiation damage in irradiated materials and may inspire new design principles of radiation-tolerant structural alloys for advanced energy systems.

36 MATERIALS SCIENCE↗

Experimental investigation on the moving characteristics of molten metal droplets impacting coolant

This paper reports the results of an experimental investigation on the moving characteristics of molten metal droplets impacting coolant free surface. A visualization experimental facility of molten fuel coolant interactions (MFCI) is designed and set up in the present study. The lead-bismuth (Pb-Bi) alloys are employed as the metal materials. An automatic control circuit is designed and applied to control the release of the molten droplets. High-speed camera is employed to record the movement of the molten metal droplets falling down and into a coolant pool. Based on the analysis of the experimental data, a so-called ''J-region'' of the droplet's velocity-time curves was found and the melt droplet enters the ''J-region'' when it impacts the free water surface. In the ''J-region'', the velocity of the melt droplet decreases rapidly and suddenly at first, and then increases again. The droplet gradually reaches a comparatively steady velocity when it leaves the ''J-region''. The present study provides essential information for further study on the fragmentation behavior of high-temperature molten droplets in coolant. (author)

22 GENERAL STUDIES OF NUCLEAR REACTORS↗

Review—Effects of Solution and Alloy Composition on Critical Crevice Temperature

Critical temperature for localized corrosion can be a good design parameter because localized corrosion is not likely to occur below that temperature. The critical temperature depends on alloy composition, microstructure, and environment chemistry (including its redox potential). This paper reviews the literature on critical temperature for localized corrosion, expressed either as Critical Pitting Temperature (CPT) or Critical Crevice Temperature (CCT). A history of various testing methods is presented. Different approaches for modeling the temperature of transition to active pit growth are reviewed, including probabilistic aspects of critical temperature. A semi-empirical, electrolyte-based, model is described that can be useful in predicting CCT in service environments that differ from standard laboratory test environments. The model predictions are compared to experimental data for various alloys. The effect of solvent on CCT/CPT is described briefly and future avenues of research are recommended.

02 PETROLEUM↗

Microstructure characteristics of LPBF&HIP fabricated graded composite transition joint between ferritic steel and austenitic stainless steel

Graded composite transition joints (GCTJs) offer a promising alternative to conventional dissimilar metal welds (DMWs) by enabling smooth compositional and microstructural transitions. However, GCTJs fabricated solely through additive manufacturing (AM) face challenges such as heat accumulation, complex parameter control, and elemental segregation. In this study, we propose a novel approach that relies on AM to design a spatially graded structure in one alloy and then employs hot isostatic pressing (HIP) as a diffusion bonding method to join it with a second alloy. Here, this method combines the flexibility of AM with the powder net-shaping advantage of HIP. Specifically, a series of closely packed austenitic stainless steel 304 conical structures were printed using laser powder bed fusion (LPBF) and then combined with ferritic steel P91 powder via HIP. By using electron backscatter diffraction (EBSD), electron probe microanalysis (EPMA), and transmission electron microscopy (TEM) techniques, the microstructure characteristics of the GCTJ of 304&P91, especially the interdiffusion zone (IDZ), have been systematically investigated. The microstructure at the interface transitions from austenite-ferrite (A+F) to austenite-martensite-ferrite (A+M+F), and finally to martensite-ferrite (M+F) due to diffusion. Additionally, the diffusion width between 304 and P91 increases with the volume fraction of P91. This unique design also ensures a gradual transition in both hardness and thermal expansion coefficient from 304 to P91, thereby enabling a smooth gradient in functional properties. Overall, this study proposes a novel approach for fabricating GCTJs and contributes to advancing design concepts in the field of dissimilar metal joining.

Additively manufacturing (AM)↗

Aging Optimization of Aluminum-Lithium Alloy L277 for Application to Cryotank Structures

Compared with aluminum alloys such as 2219, which is widely used in space vehicle for cryogenic tanks and unpressurized structures, aluminum-lithium alloys possess attractive combinations of lower density and higher modulus along with comparable mechanical properties and improved damage tolerance. These characteristics have resulted in the successful use of the aluminum-lithium alloy 2195 for the Space Shuttle External Tank, and the consideration of newer U.S. aluminum-lithium alloys such as L277 and C458 for future space vehicles. A design of experiments aging study was conducted for plate and a limited study on extrusions. To achieve the T8 temper, Alloy L277 is typically aged at 290 F for 40 hours. In the study for plate, a two-step aging treatment was developed through a design of experiments study and the one step aging used as a control. Based on the earlier NASA studies on 2195, the first step aging temperature was varied between 220 F and 260 F. The second step aging temperatures was varied between 290 F and 310 F, which is in the range of the single-step aging temperature. For extrusions, two, single-step, and one two-step aging condition were evaluated. The results of the design of experiments used for the T8 temper as well as a smaller set of experiments for the T6 temper for plate and the results for extrusions will be presented.

Sova, B. J.↗

Low-Density, Creep-Resistant Single-Crystal Superalloys

Several recently formulated nickel-base superalloys have been developed with excellent high-temperature creep resistance, at lower densities than those of currently used nickel-base superalloys. These alloys are the latest products of a continuing effort to develop alloys that have even greater strength-to-weight ratios, suitable for use in turbine blades of aircraft engines. Mass densities of turbine blades exert a significant effect on the overall weight of aircraft. For a given aircraft, a reduction in the density of turbine blades enables design reductions in the weight of other parts throughout the turbine rotor, including the disk, hub, and shaft, as well as supporting structures in the engine. The resulting total reduction in weight can be 8 to 10 times that of the reduction in weight of the turbine blades. The approach followed in formulating these alloys involved several strategies for identifying key alloying elements and the range of concentration of each element to study. To minimize the number of alloys needed to be cast, a design-of--experiments methodology was adopted. A statistics-based computer program that models the effects of varying compositions of four elements, including effects of two-way interactions between elements, was used to test all possible alloys within the design space. The starting points for the computational analysis were three alloy compositions mandated by engineering consensus. After likewise identification of key alloying elements to vary and the allowed ranges of concentrations, the computer program then selects a minimum number of alloys within the design space to allow determination of effects for all four elements and their interactions.

MacKay, Rebecca A.↗

Re Doping in 2D Transition Metal Dichalcogenides as a New Route to Tailor Structural Phases and Induced Magnetism

Alloying in 2D results in the development of new, diverse, and versatile systems with prospects in bandgap engineering, catalysis, and energy storage. Tailoring structural phase transitions using alloying is a novel idea with implications in designing all 2D device architecture as the structural phases in 2D materials such as transition metal dichalcogenides are correlated with electronic phases. In this paper, this study develops a new growth strategy employing chemical vapor deposition to grow monolayer 2D alloys of Re-doped MoSe 2 with show composition tunable structural phase variations. The compositions where the phase transition is observed agree well with the theoretical predictions for these 2D systems. Finally, it is also shown that in addition to the predicted new electronic phases, these systems also provide opportunities to study novel phenomena such as magnetism which broadens the range of their applications.

2D materials↗

Effects of 3d electron configurations on helium bubble formation and void swelling in concentrated solid-solution alloys

Currently, elemental specific chemical complexity is known to play a vital role in microstructure development in single-phase concentrated solid-solution alloys (SP-CSAs), including both He bubble formation and irradiation-induced void swelling. While cavity formation and evolution under ion irradiation at elevated temperature are complex nonequilibrium processes, chemical effects are revealed at the level of electrons and atoms herein in a simplified picture, using Ni and a special set of Ni-based SP-CSAs composed of 3d transition metals as model alloys. Based on Ni and the model alloys with minimized variables (e.g., atomic mass, size, and lattice structure), we report on the effects of chemically-biased energy dissipation, defect energetics, sluggish diffusion, and atomic transport on cavity formation and evolution under both self-ion Ni irradiation and He implantation. The observed difference in microstructure evolution is attributed to the effects of d electron interactions in their integrated ability to dissipate radiation energy. The exhibited impact of alloying 3d transition metals with larger differences in the outermost electron counts suggests a simple design strategy for tuning defect properties to improve radiation tolerance in structural alloys.

36 MATERIALS SCIENCE↗