Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “Microstructure”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 1,333 records · Page 74

Microstructure and partitioning behavior characteristics in low carbon steels treated by hot-rolling direct quenching and dynamical partitioning processes

In this work, a new process and composition design are proposed for “quenching and partitioning” or Q&P treatment. Three low carbon steels were treated by hot-rolling direct quenching and dynamical partitioning processes (DQ&P). The effects of proeutectoid ferrite and carbon concentration on microstructure evolution and mechanical properties were investigated. The present work obtained DQ&P prototype steels with good mechanical properties and established a new notion on compositions for Q&P processing. Microstructures were characterized by means of electro probe microanalyzer (EPMA), scanning electron microscopy (SEM), electron backscatter diffraction (EBSD), transmission electron microscopy (TEM) and X-ray diffraction (XRD), especially the morphology and size of retained austenite. Mechanical properties were measured by uniaxial tensile tests. The results indicated that introducing proeutectoid ferrite can increase the volume fraction of retained austenite and thus improve mechanical properties. TEM observation showed that retained austenite included the film-like inter-lath austenite and blocky austenite located in martensite/ferrite interfaces or surrounded by ferrites. It was interesting that when the carbon concentration is as low as ~ 0.078%, the film-like inter-lath untransformed austenite cannot be stabilized to room temperature and almost all of them transformed into twin martensite. The blocky retained austenite strengthened the interfaces and transformed into twin martensite during the tensile deformation process. The PSEs of specimens all exceeded 20 GPa.%. - Highlights: •This study focused on a new process: Q&P process applying dynamical partitioning. •Ferrite can increase the volume fraction of retained austenite. •The film-like austenite and the blocky austenite were observed. •The low carbon steels treated by new process reached PSEs higher than 20 GPa.%.

36 MATERIALS SCIENCE↗

Analysis of heterogeneities in strain and microstructure in aluminum alloy and magnesium processed by high-pressure torsion

Two distinct bulk light metals were opted to study the shear strain evolution and associated heterogeneities in texture/microstructure development during torsional straining by high pressure torsion (HPT): a face centered cubic Al alloy (A5086) and a hexagonal commercial purity Mg. Relatively thick disk samples - four times thicker than usually employed in HPT process - were processed to 180° and 270° rotations. With the help of X-ray tomography, the shear strain gradients were examined in the axial direction. The results showed strongly localized shear deformation in the middle plane of the disks in both materials. These gradients involved strong heterogeneities in texture, microstructure and associated hardness, in particular through the thickness direction at the periphery of the disk where the interplay between significant strain hardening and possible dynamic recrystallization could occur. - Highlights: •HPT processing was conducted on bulk specimens thicker than the usual thin-disks. •The Al alloy (A5086) and commercial purity magnesium samples were compared. •Distributions of strain and microhardness were evaluated in the radial and axial direction. •Plastic deformation is highly localized in the middle plane at outer edge in both materials. •Different DRX rates governed the differences in microstructure and hardening behavior.

36 MATERIALS SCIENCE↗

Impact of microstructure on the thermoelectric properties of the ternary compound Ce{sub 3}Cu{sub 3}Sb{sub 4}

We present detailed structural and thermoelectric studies of the ternary compound Ce{sub 3}Cu{sub 3}Sb{sub 4}. This material is of interest due to previously reported considerable thermopower above room temperature (∼ 100 μV/K) and low thermal conductivity (2 W/(m K)). Here, we present detailed studies concerning microstructural and thermoelectric data, their variation across the samples and possible explanations for the observed behaviour. We have used X-ray diffraction, scanning electron microscopy (SEM), and time-of-flight secondary ion mass spectrometry (TOF-SIMS) for microstructural analysis. The thermoelectric properties were examined using a physical property measurement system (PPMS). We analyse the impact of the sample quality on the thermoelectric properties. The most unstable parameter is the material resistivity which varies between 1.5 and 15 mΩ cm at room temperature. The properties variability is mainly due to structural defects caused by stresses during material preparation and also due to formation of foreign phases CeCuSb{sub 2} and CeSb. The figure of merit ZT is also strongly dependent on the quality of the sample. The largest value ZT ≈ 0.15 at 400 K is determined for the almost stoichiometric sample with small amounts of a impurity phases. - Highlights: •The Ce{sub 3}Cu{sub 3}Sb{sub 4} has considerable thermoelectric properties and potential for further chemical and/or structural modification. •The control over foreign phases formation is challenging. •The defects arising during arc melting process highly deteriorate ZT of material.

36 MATERIALS SCIENCE↗

Understanding the role of carbon atoms on microstructure and phase transformation of high Nb containing TiAl alloys

The microstructure and solidification behavior of high Nb containing TiAl alloys with the composition of Ti-46Al-8Nb-xC (x = 0.1, 0.7, 1.4, 2.5 at.%) prepared by arc-melting method have been investigated in this work. The results give evidence that the addition of carbon changes the solidification behavior from solidification via the β phase to the peritectic solidification. And carbon in solid solution enriches in the α{sub 2} phase and increases the microhardness. As the carbon content increases to 1.4 at.%, plate-shape morphology carbides Ti{sub 2}AlC (H phase) precipitate from the TiAl matrix which leads to the refinement microstructure. By aging at 1173 K for 24 h after quenching treatment, fine needle-like and granular shape Ti{sub 3}AlC (P phase) carbides are observed in the matrix of Ti-46Al-8Nb-2.5C alloy, which distribute along the lamellar structure or around the plate-shape Ti{sub 2}AlC. Transmission electron microscope observation shows that the Ti{sub 3}AlC carbides precipitate at dislocations. The phase transformation in-situ observations indicate that the Ti{sub 2}AlC carbides partly precipitate during the solid state phase transformation process. - Highlights: •Carbon changes the solidification behavior from β phase to peritectic solidification. •Dislocations in solution treated γ phase act as nucleation sites of Ti{sub 3}AlC precipitations. •Ti{sub 3}AlC precipitates as fine needle-like or granular shape in the solution treated matrix. •Ti{sub 2}AlC carbides precipitate during the solid state phase transformation process.

36 MATERIALS SCIENCE↗

Microstructural and microchemical studies of phase stability in V-O solid solution

Over the last couple of decades vanadium and V-based alloys have received significant attention as a potential structural material for fusion power applications because of their favourable mechanical properties under irradiation and at elevated temperatures. They are also considered as the advanced options of storage materials for hydrogen and its isotopes. However, the higher affinity of V for O, C and N poses critical challenges in its engineering applications since they lead to degradation of mechanical properties. They can further interact with the matrix to produce metallic oxy-carbo-nitride precipitates. To a certain limit, these precipitates are beneficial and can be exploited to enhance the mechanical behaviour of the alloy through suitable microstructural design. However, this requires a prior knowledge of the interaction between the alloy and the impurity solutes. In the present work vanadium specific experiments have been designed and carried out to bring out the V-interstitial solute interaction by charging oxygen in the near surface region of vanadium. Microstructural and microchemical behaviour of the V-O solid solution has been studied through HRTEM (high resolution transmission electron microscopy) and HAADF (high angle annular dark field) coupled with EELS. Quantitative electron microscopy has been carried out to study structural modification of the alloy in atomic level caused by O charging. - Highlights: •Controlled experiments were carried out in pulsed laser ablation set-up to promote V-O interaction. • As a consequence of O dissolution, V transformed into a bct structure which is otherwise a bcc structure. •In V-O solid solution, dissolved O in the V matrix introduces significant amount of lattice strain. • Present work can be extended for introducing interstitial O in other pure transition metals and their alloys.

36 MATERIALS SCIENCE↗

Effect of borides on hot deformation behavior and microstructure evolution of powder metallurgy high borated stainless steel

To investigate borides effect on the hot deformation behavior and microstructure evolution of powder metallurgy high borated stainless steel, hot compression tests at the temperatures of 950– 1150 °C and the strain rates of 0.01– 10 s{sup −1} were performed. Flow stress curves indicated that borides increased the material's stress level at low temperature but the strength was sacrificed at temperatures above 1100 °C. A hyperbolic-sine equation was used to characterize the dependence of the flow stress on the deformation temperature and strain rate. The hot deformation activation energy and stress exponent were determined to be 355 kJ/mol and 3.2, respectively. The main factors leading to activation energy and stress exponent of studied steel lower than those of commercial 304 stainless steel were discussed. Processing maps at the strains of 0.1, 0.3, 0.5, and 0.7 showed that flow instability mainly concentrated at 950– 1150 °C and strain rate higher than 0.6 s{sup −1}. Results of microstructure illustrated that dynamic recrystallization was fully completed at both high temperature-low strain rate and low temperature-high strain rate. In the instability region cracks were generated in addition to cavities. Interestingly, borides maintained a preferential orientation resulting from particle rotation during compression. - Highlights: •The decrement of activation energy was affected by boride and boron solution. •The decrease of stress exponent was influenced by composition and Cottrell atmosphere. •Boride represented a preferential orientation caused by particle rotation.

36 MATERIALS SCIENCE↗

The effect of heat treatment on microstructure evolution in artificially aged carbon nanotube/Al2024 composites synthesized by mechanical alloying

Although carbon nanotubes/aluminum (CNT/Al) composites are promising materials in the production of structural components, their mechanical behavior under overaging conditions has not been considered. In this paper the effect of CNTs on the microstructural and mechanical behavior of a 2024 aluminum alloy (Al2024) synthesized by mechanical alloying (MA) and powder metallurgy routes is discussed, as well as the effect of aging heat treatments at different temperatures and aging times. The mechanical behavior of composites was screened by hardness measurements as function of aging time. After 96 h of aging time, composites showed mechanical stability in their hardness performance. Images from transmission electron microscopy showed that the mechanical stability of composites was due to a homogeneous dispersion of CNTs in the aluminum matrix and a subsequent alteration in the kinetics of precipitation is due to their presence in the aluminum matrix. Even though strengthening precipitation took place during aging, this was not the main strengthening mechanism observed in composites. - Highlights: • Dispersion of carbon nanotubes during mechanical alloying • Microstructural evolution observed by HRTEM. • Mechanical performance evaluated through micro-hardness test. • Increased mechanical performance at high working temperatures • Acceleration of kinetics of precipitation due to CNTs, and milling conditions.

36 MATERIALS SCIENCE↗

Phase transformation and microstructure evolution of the deformed Ti-30Zr-5Nb shape memory alloy

The phase transformation and microstructures of the deformed Ti-30Zr-5Nb shape memory alloy were investigated. The X-ray diffraction measurements indicated that the Ti-30Zr-5Nb alloy was composed of a single orthorhombic α″-martensite phase. The alloy exhibited one yielding behavior in the tensile test, with a critical stress of ~ 600 MPa and a tensile strain of approximately 15%. A shape memory recovery accompanied by a permanent strain was exhibited in the deformed alloys when heated at 873 K. The permanent strain increased with increasing pre-strain. The microstructure evolution of the deformed alloy was investigated by transmission electron microscopy. The results showed that the martensite reorientation occurred and the dislocations were generated during deformation. The alloy displayed a reversible martensite transformation start temperature as high as 763 K. However, no strain-induced martensite stabilization was found in the deformed alloy with different pre-strain levels, potentially because the large chemical energy of the Ti-30Zr-5Nb alloy depressed the effects of the elastic energy and the dissipative energy. - Highlights: • Ti-30Zr-5Nb alloy is composed of single orthorhombic α″-martensite phase with M{sub s} of 721 K. • No martensite stabilization has been found in Ti-30Zr-5Nb alloy with different pre-strain. • Ti-30Zr-5Nb shows the maximum shape memory effect of 2.75% with a pre-strain of 8%.

36 MATERIALS SCIENCE↗

Microstructure characterization of recycled IN718 powder and resulting laser clad material

Highlights: • A simple and efficient recycling procedure of IN718 powder has been defined for the laser cladding process. • Characterization of wasted and cleaned powder and comparison with new IN718 powder pointed out a slight diameter increase. • Microstructure characterization of clad builds showed differences between builds with new and recycled powders. • Clad microstructure and porosity increase remain constant static properties but decrease rupture strain after 3 reuses. • Without special precautions for cladding, the recycled powder can be reused twice without modifying the properties of IN718. - Abstract: The possibility to reuse the metal powder wasted in Laser Material Deposition (LMD) process has been evaluated and a simple procedure developed. LMD uses metal powder which is fed through a nozzle into the focal point of a laser, where it melts the powder and the substrate material. During the process, a high ratio of particles hits against an unmelted area and directly bounces off the deposited area. The efficiency ratio of deposition can drop to 40% depending on the configuration and spot size. This work deals with the design of a procedure to recollect and reuse the wasted powder of a nickel based superalloy IN718. After usage, powder is recollected, undesired fractions are magnetically segregated and aggregates are removed by sieving. The particles are mixed again and ready for reuse. In order to study the effectiveness of the process, no new powder has been added to the recovered fraction, and this procedure has been repeated five times. Experimental tests show that deposited material present similar properties than those obtained with new powder grains. But, after 3 reuses, the porosity content increases consequently and the rupture strain decreases strongly. The implementation of this process allows the improvement of the final efficiency, reducing costs and decreasing the hazardous powder amount.

36 MATERIALS SCIENCE↗

Effect of quenching rate on the microstructure and mechanical behavior of Ce75Al21Ga4 glassy alloy

Highlights: • Structural and microstructural changes with respect to quenching rate have been reported. • Ribbons synthesized at slow cooling rate shows higher hardness and yield strength. • Study is focused on the correlation between quenching rate and mechanical behavior. • Metallic glass synthesized at faster quenching rate contains the highest shear band density. - Abstract: The present study deals with the structural and microstructural changes with respect to the quenching rate and their correlation with mechanical behavior of melt-spun Ce{sub 75}Al{sub 21}Ga{sub 4} glassy alloys. The ribbons of the alloy have been synthesized at different quenching rates obtained through different wheel speeds (44, 36, 29, 22 and 15 m/s). The glass forming indicators and mechanical properties have been investigated at different quenching rates. The higher quenching rate obtained through high wheel speed (44, 36 and 29 m/s) has led to phase separation giving rise to nano-amorphous domains in a glassy matrix while the lower quenching rate obtained through lower wheel speed (22 and 15 m/s) produces nano-crystalline grains with size ranges from 25 ± 1 to 120 ± 1 nm. It has been found that the size of the nano-amorphous domains decreases with decrease in wheel speed. The mechanical behavior has been studied using micro-indentation technique. The indentation test indicates that with the same chemical composition, the ribbons synthesized at slow quenching rate exhibits higher hardness and yield strength than those synthesized at faster quenching rate. The ribbons synthesized at 44 m/s contains the large free volume and has the highest shear band density.

36 MATERIALS SCIENCE↗

TEM analysis of the deformation microstructure of polycrystalline cobalt plastically strained in tension

Highlights: • Deformation of cobalt was studied by TEM and AE. • Basal dislocation glide is the main deformation mechanism in first straining stage. • Twinning mechanism becomes predominant in the second stage. • Statistical analysis was performed in data set generated by electron diffraction. • Tensile {10 2-bar 1} twins are the most common twins in cobalt. - Abstract: The microstructure evolution of hexagonal close-packed cobalt at different stages of work hardening has been studied. The deformation microstructure of polycrystalline samples upon a tension test was investigated by Transmission Electron Microscopy (TEM). Corresponding straining mechanisms were also identified by acoustic emission measurements. It was shown that dislocation glide is the predominant deformation mechanism during the first stage of plastic deformation, while twinning becomes the prominent strain accommodation mechanism in the later stage. A detailed TEM study using electron diffraction allowed identifying different types of twins activated during tensile testing. Four single twinning modes were identified, from which two types correspond to tensile strain and two types to compressive strain (with respect to the c direction), double twins were also observed. A relative importance of various systems is estimated and it is shown that the vast majority of twins correspond to the {10 1-bar 2} twinning system.

36 MATERIALS SCIENCE↗

Effect of gadolinium addition on microstructural evolution and solidification characteristics of Al-15%Mg2Si in-situ composite

Highlights: • The Al{sub 3}Gd is the heterogeneous nucleation of primary Mg{sub 2}Si in Al-15%Mg{sub 2}Si composite. • Addition of Gd to Al-15%Mg{sub 2}Si resulted in the formation of Al{sub 2}Si{sub 2}Gd and AlSiGd intermetallic compounds. • Absorption of Gd atoms preferentially on {100} facets of Mg{sub 2}Si crystals changed its growth manners. • Primary Mg{sub 2}Si transformed from coarse-dendritic to perfect truncated octahedral shape after treating with 1.0 wt% Gd. • Gd addition increased the nucleation and growth temperatures of primary Mg{sub 2}Si. - Abstract: The current study investigated the effects of gadolinium (Gd) addition (0, 0.3, 0.5, 1.0, and 2.0 wt%) on microstructural development and solidification characteristics of hypereutectic Al-15%Mg{sub 2}Si in-situ composite. Microstructural examinations were carried out via optical microscopy (OM), scanning electron microscopy (SEM), X-ray diffraction (XRD), transmission electron microscopy (TEM), and electron backscattered diffraction (EBSD). The results showed that an addition of 1.0 wt% Gd, changed the morphology of primary Mg{sub 2}Si from coarse dendritic to fine truncated octahedral shape. Furthermore, the average size of primary Mg{sub 2}Si particles decreased from 40 μm to 20 μm and density increased from 495 to 1167 particles/mm{sup 2}. Besides that, cooling curve thermal analysis (CCTA) technique revealed that Gd addition increased nucleation and growth temperatures of primary Mg{sub 2}Si phase. It is proposed that modification and refinement mechanism of Gd addition are mainly attributed to formation of tiny Al{sub 3}Gd particles as the heterogeneous nucleation substrates for primary Mg{sub 2}Si, which results in a refined distribution of these particles and poisoning effect by adsorbing Gd atoms, preferentially on {100} facets of Mg{sub 2}Si crystals. Moreover, it is believed that formation of Gd intermetallic compounds is responsible for refinement of primary Mg{sub 2}Si particles.

36 MATERIALS SCIENCE↗

Fabrication, microstructure, and wear performance of WC-Fe composite/metal coating fabricated by resistance seam welding

Highlights: • WC-Fe/metal coating consisted of WC-Fe layer and metal interlayer was fabricated by resistance seam welding. • The microstructure, hardness and wear performance of coatings with different WC particles size were analyzed. • The wear mechanism of coatings showed huge difference following various sliding distance. - Abstract: WC-Fe composite/metal coatings consisting of a WC-Fe composite layer and a metal interlayer were successfully fabricated on an Al 6061 substrate by resistance seam welding. The microstructures and phase compositions of the WC-Fe composite/metal coatings with different WC particle sizes (nano, fine, and coarse) were investigated. The WC-Fe composite layer consisted of WC particles and a Fe-C-Si super hard alloy (SHA) component, whereas the metal interlayer was composed of SHA, FeAl{sub 3}, Fe{sub 2}Al{sub 5}, and Al 6061. The surface microhardness of the WC-Fe composite/metal coating increased with increasing WC particle size. The wear performance of the coatings tested with different sliding distances is discussed in detail. Coating-C (coarse) showed the best wear resistance. The wear rates of both coating-N (nano) and coating-C decreased as the sliding distance increased, while coating-F (fine) demonstrated the opposite behavior. The wear mechanisms of the coatings were drastically different owing to the significantly different WC particle behavior at various sliding distances.

36 MATERIALS SCIENCE↗

Microstructures and deformation mechanisms of Cr26Mn20Fe20Co20Ni14 alloys

Highlights: • The single-phase FCC alloy as the annealing temperature exceeding 1015 °C • The dual-phase structure as the annealing temperature lower than 1000 °C • The σ phases grow primarily at grain boundaries. • The single-phase alloy deforms via dislocations and twins. • In-situ tensile experiment reveals twinning at the crack tip. - Abstract: We investigated microstructures and tension properties of Cr{sub 26}Mn{sub 20}Fe{sub 20}Co{sub 20}Ni{sub 14} alloys that were produced by arc-melting and subsequent thermal-mechanical processing—hot-rolling → cold-rolling → annealing at different temperatures ranging from 500 °C to 1100 °C for 1 h → air cooling. Microstructure characterization shows the single-phase solid solution with face centered cubic structure as the annealing temperature exceeding 1015 °C while the dual-phase structure (Cr-rich σ phase and FCC solid solution) as the annealing temperature lower than 1000 °C. The σ phases grow primarily at grain boundaries and act as precipitation strengthening units to enhance strain hardening rate. The single-phase solid solution deforms plastically via dislocations and twins. Twin boundaries associated with deformation twinning impede dislocation motion, enhancing the strain hardening capacity. In-situ tensile experiment in transmission electron microscope further reveals that twinning occurs at the crack tip and facilitates the deflection of crack propagation towards twinning shear direction. This work implies that a strength-ductility combination can be realized by coupling precipitation strengthening and twinning-induced plasticity in multiple principle elements alloys.

36 MATERIALS SCIENCE↗

Hot-worked microstructure and hot workability of cold-work tool steels

Highlights: • Hot compression tests were conducted for D2 and an 8% Cr steel. • Processing maps were constructed for the evaluation of their hot workability. • They had similar hot workability concerning the flow instability. • The 8% Cr steel exhibited a larger resistance to dynamic recrystallization. - Abstract: The hot workability of two cold-work tool steels were evaluated and compared. A D2 and an advanced alloy based on 8% Cr steels (TDx) were deformed at high temperatures between 900 and 1100 °C with strain rates 0.001–10 s{sup − 1} via hot compression test. From the flow curves, processing maps were constructed based on the dynamic material model. The deformed microstructures were observed and compared in various scales with respect to the deformation conditions. Although the two alloys exhibited a large similarity in the flow instability consideration of the processing map, their behavior in microstructure evolution was different. While both alloys exhibited a tendency of strain localization in the conditions of instability, the efficiency of power dissipation in the processing maps showed an intricate correlation with the progress of dynamic recrystallization and carbide precipitation. TDx showed a distinctive behavior of carbide precipitation and a larger resistance to dynamic recrystallization, which implied a requirement on more delicate control of hot working conditions.

36 MATERIALS SCIENCE↗

Microstructural characterization of laser micro-welded Nitinol wires

Highlights: • FIB technique was used in the preparation of TEM foils of laser micro-welded joint. • Phase content in various zones of laser micro-welded Nitinol wires was revealed. • Welding induces the R-phase formation in HAZ and intermetallics precipitation in FZ. - Abstract: Laser micro-welding has been considered one of the most promising joining methods of manufacturing Nitinol biomedical devices. However, there is still a lack of understanding about how laser micro-welding influences the microstructure. This work attempts to reveal the phase content within various microstructural zones of laser micro-welded crossed Nitinol wires by transmission electron microscopy (TEM) with the assistance of the focused ion beam (FIB) technique. The base metal is composed of a single austenite phase (B2). The fusion zone exhibits the coexistence of austenite matrix and several intermetallics (T{sub 2}Ni, TiNi{sub 3} and Ti{sub 3}Ni{sub 4}). The precipitation of R-phase was observed in HAZ with B2 matrix due to thermally induced stresses during welding.

36 MATERIALS SCIENCE↗

Effect of microstructure on exfoliation corrosion resistance in an Al-Zn-Mg alloy

Highlights: • A quantitative method was proposed to characterize EXCO resistance. • The EXCO product lead to strain in ND and elongation in RD on nearby grains. • Recrystallized grains are more susceptible to EXCO than fibrous grains. • High fraction of high-angle grain boundaries reduces EXCO resistance. • High coverage ratio of η phases on high-angle grain boundaries reduces EXCO resistance. - Abstract: In this work, the effect of microstructure on exfoliation corrosion (EXCO) resistance in an Al-Zn-Mg alloy were investigated using standard EXCO test, together with detailed microstructural examinations mainly by scanning electron microscopy (SEM) and high-angle annular detector dark-field scanning transmission electron microscopy (HAADF-STEM). An EXCO product model was built based on morphologies of EXCO product on longitudinal section and cross section for further measurement and analysis. A quantitative characterization of EXCO resistance by measuring average thickness of EXCO product was conducted, showing average results of 6.94 μm, 10.21 μm and 18.14 μm, which are corresponding to EXCO ratings of P, EA and EB under ASTM G34 standard, respectively. It was concluded that recrystallization, high fraction of high-angle grain boundaries (HAGBs) and high coverage ratio of η phases on HAGBs reduced EXCO resistance.

36 MATERIALS SCIENCE↗

Effects of friction stir processing and minor Sc addition on the microstructure, mechanical properties, and damping capacity of 7055 Al alloy

Highlights: • Good mechanical and damping properties were obtained in the 7055 after FSP and Sc addition. • The strengthening and damping mechanisms of FSP 7055(-Sc) were analyzed. • FSP and Sc addition were found to be strategy of preparing 7xxx alloys with well damping and mechanical properties. - Abstract: This study investigated the effects of friction stir processing (FSP) and addition of 0.25% (mass ratio) Sc on the microstructure, mechanical properties, and damping capacity of AA 7055 alloy. Microstructure analyses revealed that a low tool rotation rate of 300 rpm effectively inhibited the grain coarsening in the recrystallization of the alloy during FSP. Sc addition prevented the coarsening of grains and precipitated η phase and the annihilation of dislocations in the FSP AA 7055 alloy. After being subjected to FSP at 300 rpm, the AA 7055 alloy containing Sc exhibited good mechanical and damping properties, which were mainly attributed to the fine recrystallized grain structure, fine precipitated η phase, and large number of nano-sized Al{sub 3}(Sc, Zr) particles located at the grain boundaries and dislocations. This work provides an effective strategy for preparing commercial Al alloys with excellent damping capacity and mechanical properties.

36 MATERIALS SCIENCE↗