At least 1,333 records · Page 74

Trowelable ablative coating composition and method of use

A trowelable ablative coating composition is disclosed. The composition comprises an epoxy resin, an amide curing agent, glass microspheres and ground cork. A method for protecting a substrate is also disclosed. The method comprises applying the trowelable ablative coating discussed above to a substrate and curing the coating composition.

Headrick, Stephen E.↗

Investigation of Fiber Waviness in a Thick Glass Composite Beam Using THz NDE

Fiber waviness in laminated composite material is introduced during manufacture because of uneven curing, resin shrinkage, or ply buckling caused by bending the composite lay-up into its final shape prior to curing. The resulting waviness has a detrimental effect on mechanical properties, therefore this condition is important to detect and characterize. Ultrasonic characterization methods are difficult to interpret because elastic wave propagation is highly dependent on ply orientation and material stresses. By comparison, the pulsed terahertz response of the composite is shown to provide clear indications of the fiber waviness. Pulsed Terahertz NDE is an electromagnetic inspection method that operates in the frequency range between 300 GHz and 3 THz. Its propagation is influenced by refractive index variations and interfaces. This work applies pulsed Terahertz NDE to the inspection of a thick composite beam with fiber waviness. The sample is a laminated glass composite material approximately 15mm thick with a 90-degree bend. Terahertz response from the planar section, away from the bend, is indicative of a homogeneous material with no major reflections from internal plies, while the multiple reflections at the bend area correspond to the fiber waviness. Results of these measurements are presented for the planar and bend areas.

Anastasi, Robert F.↗

Processing and Properties of a Phenolic Composite System

Phenolic resin systems generate water as a reaction by-product via condensation reactions during curing at elevated temperatures. In the fabrication of fiber reinforced phenolic resin matrix composites, volatile management is crucial in producing void-free quality laminates. A commercial vacuum-bag moldable phenolic prepreg system was selected for this study. The traditional single-vacuum-bag (SVB) process was unable to manage the volatiles effectively, resulting in inferior voidy laminates. However, a double vacuum bag (DVB) process was shown to afford superior volatile management and consistently yielded void-free quality parts. The DVB process cure cycle (temperature /pressure profiles) for the selected composite system was designed, with the vacuum pressure application point carefully selected, to avoid excessive resin squeeze-outs and achieve the net shape and target resin content in the final consolidated laminate parts. Laminate consolidation quality was characterized by optical photomicrography for the cross sections and measurements of mechanical properties. A 40% increase in short beam shear strength, 30% greater flexural strength, 10% higher tensile and 18% higher compression strengths were obtained in composite laminates fabricated by the DVB process.

Hou, Tan-Hung↗

Stretch-Orientation of LaRC(TM) RP 50 Polyimide Film

An addition-curable poly(amic acid) film was subjected to various thermal pretreatments and then to uniaxial or biaxial drawing. Hot-stretching to 300% of the initial length produced better than twofold increases in tensile modulus and strength of partially-cured films. Most of the improvement was maintained upon completion of the curing at constant length.

Hawkins, Brian P.↗

The Manufacturing Process for the NASA Composite Crew Module Demonstration Structure

This paper will describe the approaches and methods selected in fabrication of a carbon composite demonstration structure for the Composite Crew Module (CCM) Program. The program is managed by the NASA Safety and Engineering Center with participants from ten NASA Centers and AFRL. Multiple aerospace contractors are participating in the design development, tooling and fabrication effort as well. The goal of the program is to develop an agency wide design team for composite habitable spacecraft. The specific goals for this development project are: a).To gain hands on experience in design, building and testing a composite crew module. b) To validate key assumptions by resolving composite spacecraft design details through fabrication and testing of hardware. This abstract is based on Preliminary Design data..The final design will continue to evolve through the fall of 2007 with fabrication mostly completed by conference date. From a structures perspective, the.CCM can be viewed as a pressure module with variable pressure time histories and a series of both impact and quasi-static, high intensity point, line, and area distributed loads. The portion of the overall space vehicle being designed and. fabricated by the CCM team is just the pressure module and primary loading points. The heaviest point loads are applied and distributed to the pressure module at.an aluminum Service Module/Alternate Launch Abort System (SM/ALAS) fittings and at Main and Drogue Chute fittings. Significant line loads with metal to metal impact is applied at.the Lids ring. These major external point and line loads as well as pressure impact loads (blast and water landing) are applied to the lobed floor though the reentry shield and crushable materials. The pressure module is divided into upper and lower. shells that mate together with a bonded belly band splice joint to create the completed structural assembly. The benefits of a split CCM far outweigh the risks of a joint. These benefits include lower tooling cost and less manufacturing risk. Assembly of the top and bottom halves of the pressure shell will allow access to the interior of the shell throughout remaining fabrication sequence and can also potentially permit extensive installation of equipment and .crew facilities prior to final assembly of the two shell halves. A Pi pre-form is a woven carbon composite material which is provided in pre-impregnated form and frozen for long term storage. The cross-section shape allows the top of the pi to be bonded to a flat or curved surface with a second flat plate composite section bonded between two upstanding legs of the Pi. One of the regions relying on the merits of the Pi pre-form is the backbone. All connections among plates of the backbone structure, including the upper flanges, and to the lobe base of the pressure shell are currently joined by Pi pre-forms. The intersection of backbone composite plates is formed by application of two Pi pre-forms, top flanges and lobed surfaces are bonded with one Pi pre-form. The process of applying the pre-impregnated pi-preform will be demonstrated to include important steps like surface preparation, forming, application of pressure dams, vacuum bagging for consolidation, and curing techniques. Chopped carbon fiber tooling was selected over other traditional metallic and carbon fiber tooling. The requirement of schedule and cost economy for a moderate reuse cure tool warranted composite tooling options. Composite tooling schedule duration of 18 weeks compared favorably against other metallic tooling including invar tooling. Composite tooling also shows significant cost savings over low CTE metallic options. The composite tooling options were divided into two groups and the final decision was based on the cost, schedule, tolerance, temperature, and reuse requirements.

Pelham, Larry↗

Modeling the Non-Linear Response of Fiber-Reinforced Laminates Using a Combined Damage/Plasticity Model

The present work is concerned with modeling the non-linear response of fiber reinforced polymer laminates. Recent experimental data suggests that the non-linearity is not only caused by matrix cracking but also by matrix plasticity due to shear stresses. To capture the effects of those two mechanisms, a model combining a plasticity formulation with continuum damage has been developed to simulate the non-linear response of laminates under plane stress states. The model is used to compare the predicted behavior of various laminate lay-ups to experimental data from the literature by looking at the degradation of axial modulus and Poisson s ratio of the laminates. The influence of residual curing stresses and in-situ effect on the predicted response is also investigated. It is shown that predictions of the combined damage/plasticity model, in general, correlate well with the experimental data. The test data shows that there are two different mechanisms that can have opposite effects on the degradation of the laminate Poisson s ratio which is captured correctly by the damage/plasticity model. Residual curing stresses are found to have a minor influence on the predicted response for the cases considered here. Some open questions remain regarding the prediction of damage onset.

Schuecker, Clara↗

Improved Joining of Metal Components to Composite Structures

Systems requirements for complex spacecraft drive design requirements that lead to structures, components, and/or enclosures of a multi-material and multifunctional design. The varying physical properties of aluminum, tungsten, Invar, or other high-grade aerospace metals when utilized in conjunction with lightweight composites multiply system level solutions. These multi-material designs are largely dependent upon effective joining techAn improved method of joining metal components to matrix/fiber composite material structures has been invented. The method is particularly applicable to equipping such thin-wall polymer-matrix composite (PMC) structures as tanks with flanges, ceramic matrix composite (CMC) liners for high heat engine nozzles, and other metallic-to-composite attachments. The method is oriented toward new architectures and distributing mechanical loads as widely as possible in the vicinities of attachment locations to prevent excessive concentrations of stresses that could give rise to delaminations, debonds, leaks, and other failures. The method in its most basic form can be summarized as follows: A metal component is to be joined to a designated attachment area on a composite-material structure. In preparation for joining, the metal component is fabricated to include multiple studs projecting from the aforementioned face. Also in preparation for joining, holes just wide enough to accept the studs are molded into, drilled, or otherwise formed in the corresponding locations in the designated attachment area of the uncured ("wet') composite structure. The metal component is brought together with the uncured composite structure so that the studs become firmly seated in the holes, thereby causing the composite material to become intertwined with the metal component in the joining area. Alternately, it is proposed to utilize other mechanical attachment schemes whereby the uncured composite and metallic parts are joined with "z-direction" fasteners. The resulting "wet" assembly is then subjected to the composite-curing heat treatment, becoming a unitary structure. It should be noted that this new art will require different techniques for CMC s versus PMC's, but the final architecture and companion curing philosophy is the same. For instance, a chemical vapor infiltration (CVI) fabrication technique may require special integration of the pre-form and

Semmes, Edmund↗

Vapor-Gas Bubble Evolution and Growth in Extremely Viscous Fluids Under Vacuum

Formation of vapor and gas bubbles and voids is normal and expected in flow processes involving extremely viscous fluids in normal gravity. Practical examples of extremely viscous fluids are epoxy-like filler materials before the epoxy fluids cure to their permanent form to create a mechanical bond between two substrates. When these fluids flow with a free liquid interface exposed to vacuum, rapid bubble expansion process may ensue. Bubble expansion might compromise the mechanical bond strength. The potential sources for the origin of the gases might be incomplete out-gassing process prior to filler application; regasification due to seal leakage in the filler applicator; and/or volatiles evolved from cure reaction products formed in the hardening process. We embarked on a study that involved conducting laboratory experiments with imaging diagnostics in order to deduce the seriousness of bubbling caused by entrained air and volatile fluids under space vacuum and low gravity environment. We used clear fluids with the similar physical properties as the epoxy-like filler material to mimic the dynamics of bubbles. Another aspect of the present study was to determine the likelihood of bubbling resulting from dissolved gases nucleating from solution. These experimental studies of the bubble expansion are compared with predictions using a modified Rayleigh- Plesset equation, which models the bubble expansion.

Kizito, John↗

The Effect of Water on the Work of Adhesion at Epoxy Interfaces by Molecular Dynamics Simulation

Molecular dynamics simulation can be used to explore the detailed effects of chemistry on properties of materials. In this paper, two different epoxies found in aerospace resins are modeled using molecular dynamics. The first material, an amine-cured tetrafunctional epoxy, represents a composite matrix resin, while the second represents a 177 C-cured adhesive. Surface energies are derived for both epoxies and the work of adhesion values calculated for the epoxy/epoxy interfaces agree with experiment. Adding water -- to simulate the effect of moisture exposure -- reduced the work of adhesion in one case, and increased it in the other. To explore the difference, the various energy terms that make up the net work of adhesion were compared and the location of the added water was examined.

Hinkley, J.A.↗

High Temperature VARTM of Phenylethynyl Terminated Imides

Fabrication of composite structures using vacuum assisted resin transfer molding (VARTM) is generally more affordable than conventional autoclave techniques. Recent efforts have focused on adapting VARTM for the fabrication of high temperature composites. Due to their low melt viscosity and long melt stability, certain phenylethynyl terminated imides (PETI) can be processed into composites using high temperature VARTM (HT-VARTM). However, one of the disadvantages of the current HT-VARTM resin systems has been the high porosity of the resultant composites. For aerospace applications, the desired void fraction of less than 2% has not yet been achieved. In the current study, two PETI resins, LaRC PETI-330 and LaRC PETI-8 have been used to make test specimens using HT-VARTM. The resins were infused into ten layers of IM7-6K carbon fiber 5-harness satin fabric at 260 C or 280 C and cured at 371 C. Initial runs yielded composites with high void content, typically greater than 7% by weight. A thermogravimetric-mass spectroscopic study was conducted to determine the source of volatiles leading to high porosity. It was determined that under the thermal cycle used for laminate fabrication, the phenylethynyl endcap was undergoing degradation leading to volatile evolution. By modifying the thermal cycle used in laminate fabrication, the void content was reduced significantly (typically approximately 3%). Densities of the composites were determined using a density gradient column and the glass transition temperatures of the cured composites were measured by dynamic mechanical analysis. Photomicrographs of the panels were taken and void contents were determined by acid digestion. The results of this work are presented herein.

Cano, Roberto J.↗

Protective Skins for Aerogel Monoliths

A method of imparting relatively hard protective outer skins to aerogel monoliths has been developed. Even more than aerogel beads, aerogel monoliths are attractive as thermal-insulation materials, but the commercial utilization of aerogel monoliths in thermal-insulation panels has been inhibited by their fragility and the consequent difficulty of handling them. Therefore, there is a need to afford sufficient protection to aerogel monoliths to facilitate handling, without compromising the attractive bulk properties (low density, high porosity, low thermal conductivity, high surface area, and low permittivity) of aerogel materials. The present method was devised to satisfy this need. The essence of the present method is to coat an aerogel monolith with an outer polymeric skin, by painting or spraying. Apparently, the reason spraying and painting were not attempted until now is that it is well known in the aerogel industry that aerogels collapse in contact with liquids. In the present method, one prevents such collapse through the proper choice of coating liquid and process conditions: In particular, one uses a viscous polymer precursor liquid and (a) carefully controls the amount of liquid applied and/or (b) causes the liquid to become cured to the desired hard polymeric layer rapidly enough that there is not sufficient time for the liquid to percolate into the aerogel bulk. The method has been demonstrated by use of isocyanates, which, upon exposure to atmospheric moisture, become cured to polyurethane/polyurea-type coats. The method has also been demonstrated by use of commercial epoxy resins. The method could also be implemented by use of a variety of other resins, including polyimide precursors (for forming high-temperature-resistant protective skins) or perfluorinated monomers (for forming coats that impart hydrophobicity and some increase in strength).

Leventis, Nicholas↗

Multifunctional, High-Temperature Nanocomposites

In experiments conducted as part of a continuing effort to incorporate multifunctionality into advanced composite materials, blends of multi-walled carbon nanotubes and a resin denoted gPETI-330 h (wherein gPETI h is an abbreviation for gphenylethynyl-terminated imide h) were prepared, characterized, and fabricated into moldings. PETI-330 was selected as the matrix resin in these experiments because of its low melt viscosity (<10 poise at a temperature of 280 C), excellent melt stability (lifetime >2 hours at 280 C), and high temperature performance (>1,000 hours at 288 C). The multi-walled carbon nanotubes (MWCNTs), obtained from the University of Kentucky, were selected because of their electrical and thermal conductivity and their small diameters. The purpose of these experiments was to determine the combination of thermal, electrical, and mechanical properties achievable while still maintaining melt processability. The PETI-330/MWCNT mixtures were prepared at concentrations ranging from 3 to 25 weight-percent of MWCNTs by dry mixing of the constituents in a ball mill using zirconia beads. The resulting powders were characterized for degree of mixing and thermal and rheological properties. The neat resin was found to have melt viscosity between 5 and 10 poise. At 280 C and a fixed strain rate, the viscosity was found to increase with time. At this temperature, the phenylethynyl groups do not readily react and so no significant curing of the resin occurred. For MWCNT-filled samples, melt viscosity was reasonably steady at 280 C and was greater in samples containing greater proportions of MWCNTs. The melt viscosity for 20 weightpercent of MWCNTs was found to be .28,000 poise, which is lower than the initial estimated allowable maximum value of 60,000 poise for injection molding. Hence, MWCNT loadings of as much as 20 percent were deemed to be suitable compositions for scale-up. High-resolution scanning electron microscopy (HRSEM) showed the MWCNTs to be well dispersed in the polymer matrices, while high-resolution transmission electron microscopy shows splits in the walls of the MWCNTs but no catastrophic breakage of tubes. To further assess processing characteristics prior to scale-up, samples containing 10, 15, and 20 weight-percent of MWCNTs were processed through a laboratory melting extruder. HRSEM of the extruded fibers shows significant alignment of MWCNTs in the flow direction (see figure). For the samples containing 20 weight-percent of MWCNTs, difficulties were encountered during feeding, and the temperature of a rotor in the extruder rose to 245 C because of buildup of frictional heat; this indicates that materials of this type having MWCNT concentrations .20 weight- percent may not be melt-processable. On the basis of the results from the foregoing characterizations, samples containing 10, 15, and 20 weight-percent of MWCNTs were scaled up to masses of .300 g and used to make specimens having dimensions of 10.2 by 15.2 by 0.32 cm. These specimens were molded by (1) injecting the mixtures, at temperatures between 260 and 280 C, into a tool made of the low-thermal-expansion alloy InvarR and then (2) curing for 1 hour at 371 C. The tool was designed to impart shear during the injection process in an attempt to achieve some alignment of the MWCNTs in the flow direction.

Connell, John W.↗

Gratings Fabricated on Flat Surfaces and Reproduced on Non-Flat Substrates

A method has been developed for fabricating gratings on flat substrates, and then reproducing the groove pattern on a curved (concave or convex) substrate and a corresponding grating device. First, surface relief diffraction grating grooves are formed on flat substrates. For example, they may be fabricated using photolithography and reactive ion etching, maskless lithography, holography, or mechanical ruling. Then, an imprint of the grating is made on a deformable substrate, such as plastic, polymer, or other materials using thermoforming, hot or cold embossing, or other methods. Interim stamps using electroforming, or other methods, may be produced for the imprinting process or if the same polarity of the grating image is required. The imprinted, deformable substrate is then attached to a curved, rigid substrate using epoxy or other suitable adhesives. The imprinted surface is facing away from the curved rigid substrate. As an alternative fabrication method, after grating is imprinted on the deformable substrate as described above, the grating may be coated with thin conformal conductive layer (for example, using vacuum deposition of gold). Then the membrane may be mounted over an opening in a pressured vessel in a manner of a membrane on a drum, grating side out. The pressure inside of the vessel may be changed with respect to the ambient pressure to produce concave or convex membrane surface. The shape of the opening may control the type of the surface curvature (for example, a circular opening would create spherical surface, oval opening would create toroidal surface, etc.). After that, well-known electroforming methods may be used to create a replica of the grating on the concave or convex membrane. For example, the pressure vessel assembly may be submerged into an electro-forming solution and negative electric potential applied to the metal coated membrane using an insulated wire. Positive electric potential may be then applied to a nickel or other metal plate submerged into the same solution. Metal ions would transfer from the plate through the solution into the membrane, producing high fidelity metal replica of the grating on the membrane. In one variation, an adhesive may be deposited on the deformable substrate, and then cured without touching the rigid, curved substrate. Edges of the deformable substrate may be attached to the rigid substrate to ensure uniform deformation of the deformable substrate. The assembly may be performed in vacuum, and then taken out to atmospheric pressure conditions to ensure that no air is trapped between the deformable and rigid substrates. Alternatively, a rigid surface with complementary curvature to the rigid substrate may be used to ensure uniform adhesion of the deformable substrate to the rigid substrate. Liquid may be applied to the surface of the deformable substrate to uniformly distribute pressure across its surface during the curing or hardening of the adhesive, or the film may be pressed into the surface using a deformable object or surface. After the attachment is complete, the grooves may be coated with reflective or dielectric layers to improve diffraction efficiency.

Content, David↗

The Effects of Temperature, Humidity and Aircraft Fluid Exposure on T800H/3900-2 Composites Bonded with AF-555M Adhesive

Fiber reinforced resin matrix composites and structural adhesives have found increased usage on commercial and military aircraft in recent years. Due to the lack of service history of these relatively new material systems, their long-term aging performance has not been well established. In this study, single lap shear specimens (SLS) were fabricated by secondary bonding of Scotch-Weld(TradeMark) AF-555M between pre-cured adherends comprised of T800H/3900-2 uni-directional laminates. The adherends were co-cured with wet peel-ply for surface preparation. Each bond-line of the SLS specimen was measured to determine thickness and inspected visually using an optical microscope for voids. A three-year environmental aging plan for the SLS specimens at 82 C (180 F) and 85% relative humidity was initiated. SLS strengths were measured for both controls and aged specimens at room temperature and 82 C. The effect of this exposure on lap shear strength and failure modes to date is reported. In addition, the effects of water, saline water, deicing fluid, JP-5 jet fuel and hydraulic fluid on both the composite material and the adhesive bonds were investigated. The up to date results on the effects of these exposures will be discussed.

Miner, Gilda A.↗

Environmental Aging of Scotch-Weld(TradeMark) AF-555M Structural Adhesive in Composite to Composite Bonds

Fiber reinforced resin matrix composites have found increased usage in recent years. Due to the lack of service history of these relatively new material systems, their long-term aging performance is not well established. In this study, adhesive bonds were prepared by the secondary bonding of Scotch-Weld(TradeMark) AF-555M between pre-cured adherends comprised of T800H/3900-2 uni-directional laminate. The adherends were co-cured with wet peel-ply for surface preparation. Each bond-line of single-lap-shear (SLS) specimen was measured to determine thickness and inspected visually for voids. A three-year environmental aging plan for the SLS specimens at 82 C and 85% relative humidity was initiated. SLS strengths were measured for both controls and aged specimens at room temperature and 82 C. The aging results of strength retention and failure modes to date are reported.

Hou, Tan-Hung↗

Phenylethynyl Terminated Imide (PETI) Composites Made by High Temperature Vartm

The use of composites as primary structures on aerospace vehicles has increased dramatically over the past decade. As these advanced structures increase in size and complexity, their production costs have grown significantly. A major contributor to these manufacturing costs is the requirement of elevated pressures, during high temperature processing, to create fully consolidated composite parts. Recently, NASA Langley has licensed a series of low viscosity Phenyl Ethynyl Terminated Imide, PETI, oligomers that possess a wide processing window to allow for Resin Transfer Molding, RTM, processing. These resins, PETI-8 and PETI-330, demonstrate void fractions of approx.1% under elevated pressure consolidation. However, when used with a standardized thermal curing cycle in a High Temperature Vacuum Assisted RTM (HT-VARTM) process, they display undesirable void contents in excess of 7%. It was determined previously that under the thermal cycles used for laminate fabrication, the phenylethynyl endcap underwent degradation leading to volatile evolution. Modifications to the processing cycle used in the laminate fabrication have reduced the void content significantly (typically less than 3%) for carbon fiber biaxially woven fabric. For carbon fiber uniaxial fabric, void contents of less than 2% have been obtained using both PETI-8 and PETI-330. The resins were infused into carbon fiber preforms at 260 C and cured between 316 C and 371 C. Photomicrographs of the panels were taken and void contents were determined by acid digestion. Mechanical properties of the panels were determined at both room and elevated temperatures. These include short beam shear and flexure tests. The results of this work are presented herein.

Ghose, Sayata↗

Effects of Hygrothermal Cycling on the Chemical, Thermal, and Mechanical Properties of 862/W Epoxy Resin

The hygrothermal aging characteristics of an epoxy resin were characterized over 1 year, which included 908 temperature and humidity cycles. The epoxy resin quickly showed evidence of aging through color change and increased brittleness. The influence of aging on the material s glass transition temperature (Tg) was evaluated by Differential Scanning Calorimetry (DSC) and Dynamic Mechanical Analysis (DMA). The Tg remained relatively constant throughout the year long cyclic aging profile. The chemical composition was monitored by Fourier Transform Infrared Spectroscopy (FTIR) where evidence of chemical aging and advancement of cure was noted. The tensile strength of the resin was tested as it aged. This property was severely affected by the aging process in the form of reduced ductility and embrittlement. Detailed chemical evaluation suggests many aging mechanisms are taking place during exposure to hygrothermal conditions. This paper details the influence of processes such as: advancement of cure, chemical degradation, and physical aging on the chemical and physical properties of the epoxy resin.

Miller, Sandi G.↗

Making a Metal-Lined Composite-Overwrapped Pressure Vessel

process has been devised for the fabrication of a pressure vessel that comprises a composite-material (matrix/fiber) shell with a metal liner on its inner surface. The use of the composite material makes it possible for the tank to be strong enough to withstand the anticipated operating pressure and yet weigh less than does an equivalent all-metal tank. The metal liner is used as a barrier against permeation: In the absence of such a barrier, the pressurized gas in the tank could leak by diffusing through the composite-material shell. The figure depicts workpieces at four key stages in the process, which consists of the following steps: 1. A mandrel that defines the size and shape of the pressure vessel is made by either molding or machining a piece of tooling wax. 2. Silver paint is applied to the surface of the mandrel to make it electrically conductive. 3. The ends of the mandrel are fitted with metal bosses. 4. The mandrel is put into a plating bath, wherein the metal liner is electrodeposited. Depending on the applications, the liner metal could be copper, nickel, gold, or an alloy. Typical liner thicknesses range from 1 to 10 mils (0.025 to 0.25 mm). 5. The wax is melted from within, leaving the thin metal liner. 6. A hollow shaft that includes holes and fittings through which the liner can be pressurized is sealed to both ends of the liner. The liner is pressurized to stiffen (and hence stabilize) it for the next step. 7. The pressurized liner is placed in a filament-winding machine, which is then operated to cover the liner with multiple layers of an uncured graphite-fiber/epoxy-matrix or other suitable composite material. 8. The composite-overwrapped liner is cured in an oven. 9. The pressure is relieved and the shaft is removed. The tank is then ready for use. The process as described above accommodates variations: a) The mandrel could be made of a wax that melts at a higher temperature and not removed until the tank is cured in the oven. b) The tank need not be cylindrical or axisymmetric, as long as the filament-winding machine can accommodate the chosen shape. c) Shallow grooves could be formed on the surface of the mandrel to give the liner a bellows-like character for reinforcement and/or to accommodate expansion and contraction.

DeLay, Tom↗