Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “CORROSIVE”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 1,333 records · Page 74

Electrochemical Mitigation of Corrosion in Molten Chloride Salts During CSP Plant Operation

We are designing an electrochemical flow-cell for removal of corrosive impurities from molten chloride salt Gen3 Concentrating Solar Power (CSP) plants during plant operation. Corrosive impurities will inevitably form in molten chloride salts upon exposure to air and moisture. We previously showed that even small amounts of these impurities, especially MgOHCl, will be detrimental in Gen3 CSP plants, necessitating prohibitively expensive containment alloys and frequent replacement of corroded components. Pre-purification of salt with Mg metal at temperatures above 650 degrees C is the current method for removing corrosive impurities from chloride salts before they are introduced to CSP systems. However, this is not a suitable method for impurity removal during plant operation. First, this method will produce MgO particulates which will damage plant components. Second, Mg metal is solid at the low temperature point (500 degrees C), so the purification will not proceed at a fast rate. At the high temperature point, Mg is soluble. In this case, fast purification may proceed, but dissolved metal is likely to precipitate out in cold-temperature point components, causing damage. In contrast, our electrochemically driven method allows fast Mg-based purification to proceed at the low temperature point, without formation of harmful particulates and without the risk of Mg metal precipitation. This novel approach is inspired by electrorefining techniques that are widely employed in industrial metallurgy for removal of impurities from metals. Impurities in the incoming molten salt will be reduced to inert MgO at the cathode, which can be removed by periodically washing the cell with acid. Simultaneously, Mg dissolution at the anode will ensure salt composition is maintained, with no net removal of Mg2+. We have validated this electrochemical approach at lab scale under static conditions with batch rectors. Furthermore, we have performed analytical modeling and technoeconomic analysis to produce a preliminary engineering design for the purification flow cell.

CSP↗

Non-invasive, in situ diagnosis and monitoring of corrosion in high temperature systems

Techniques for non-invasive diagnosis and/or monitoring of corrosion in high temperature systems using specialized sensors that produce multi-mode acoustic signals in situ for accurate determination of wall loss and/or physical property changes for a vessel in contact with a high temperature, highly corrosive substance are disclosed. Sensitivity of a few microns (or about 0.1%) of wall loss, detection of changes in physical properties of vessel contents (e.g., approximately 1%), or both, at temperatures of 500° C., 600° C., or higher may be realized. Corrosion may be identified and/or monitored using time domain, frequency domain, or mixed time domain and frequency domain analysis of signal characteristics, signal delay, or both, for relatively short circumferential acoustic wave propagation (e.g., a few inches), as well as relatively long axial acoustic wave propagation (e.g., tens of feet).

Findikoglu, Alp Tugrul↗

Milestone 1.2.14: Surface Characterization of Irradiated Surrogate Non-Native Corrosion Plumes on Aluminum 6061-T6 Specimens

The United States Department of Energy is seeking to evaluate the feasibility of extended dry storage of aluminum-clad spent nuclear fuel (ASNF) in helium-backfilled cannisters. A significant research effort has been devoted to determining the amount of radiation-induced molecular hydrogen generation from corrosion layers that would be present on the fuel assembly surfaces. However, to date, no evidence of radiation-induced changes in the microstructure of the corroded aluminum surfaces have been reported. This report provides surface characterization, in terms of corrosion layer composition and morphology, for aluminum alloy 6061-T6 “plume” samples subjected to one of three potential ASNF drying techniques—“vacuum only”, “vacuum + 4 hours at 100 oC”, and “vacuum + 4 hours at 220 oC”—and gamma irradiated (= 53 MGy) in the presence of helium gas with ~0% added relative humidity. At these high absorbed gamma doses, for the first time ever, radiation-induced circular defects were found on the sample surface, regardless of the drying regime employed. Additionally, large cracks that penetrated through the corrosion layer to expose bare aluminum metal were observed in irradiated “plume” specimens subjected to drying conditions of “vacuum + 4 hours at 220 oC”. The nature and implications of these defects on the extended dry storage of ASNF is unclear, requiring further study.

38 RADIATION CHEMISTRY, RADIOCHEMISTRY, AND NUCLEA↗

Multi-Parameter Optical Fiber Sensing of Humidity, CH4, CO2, and Corrosion

In this work, the previously demonstrated capability of the optical fiber sensor (OFS) for successful monitoring of humidity has been extended to monitor the humidity, CH4, and CO2 with different gas composition based on the strain produced along the single mode fiber (SMF) sensor. This is enabled by absorption of H2O/gases on to the commercially available polyacrylate coated jacketed portion of the fiber resulting a change in strain. Under equilibrium, a differential microstrain was observed along the jacketed portion of the SMF with N2, CH4, and CO2 at different humidity conditions, while the unjacketed portion of the fiber was used only for sensing pressure/temperature induced strain. In case of N2 at 800 psig pressure, the observed microstrain was approximately 80, 65, 50 and 35 µε at 100, 75.0, 46.8, and 23.4 RH% respectively. Comparatively, a microstrain of approximately 95 µε was observed with 100% RH CH4 which demonstrates that SMF produces a measurable CH4 response alongside water. Similarly, the observed microstrain with CO2 was approximately 105, 90, 85, 80, and 70 µε at 100, 75.0, 46.8, 23.4, and 0 RH% respectively. Linear regression and principal component analysis of these dataset provided deconvolution of the impact of strain from H2O, CH4, and CO2 enabling good cross sensitivity. Additionally, modified OFS comprising of Fe coated fiber section was employed to monitor corrosion, using Fe as corrosion proxy, under harsh corrosive environment.

Mainali, Badri↗

Determining Drying Conditions to Mitigate Hanford Transfer Line Corrosion

Radioactive waste is stored in underground, carbon-steel double-shell tanks at the Department of Energy Hanford site.1,2,3 The underground transfer lines are used to transfer the waste between the tanks and other assets at the Hanford tank farm facilities. The transfer lines constructed before 1990 are pipe-in-pipe design with most of the lines having carbon steel carrier pipe and carbon steel encasements. The lines constructed after 1990 have a stainless-steel carrier with a carbon steel encasement. The carrier lines, which are in contact with the waste, provide a critical confinement function, while the encasements provide secondary containment to reduce the risk of a release and contamination to the environment. In 2022, a visual inspection of the annulus between the encasement and the carrier for one of the pre-1990 transfer lines revealed standing liquid in contact with the carrier pipe. Additionally, a significant build-up of corrosion products on the exterior of the carrier pipe and the interior of the encasement pipe was observed. To assess the extent of condition, borescope inspections were performed in the encasement space of additional transfer lines in the facility to provide a baseline. The inspection revealed that of the lines inspected, 29 had either moisture present or evidence that moisture had been present in the past (e.g., waterline corrosion where the pipe had been exposed to standing water). Additional inspections indicated several instances of pitting corrosion on the interior of the encasement and exterior the carrier transfer lines. An image of the carrier pipe with several pits is presented in Figure 1(a) and the profiled image of the transfer line section along with the pit depths are presented Figure 1(b). As seen in the figure, the deepest pit was 73 mils on the pipe section. These lines were designated as “do-not-use” until further compensatory actions are implemented to return the lines to service.

Shukla, Pavan K. [Savannah River National Laborato↗

Corrosion Resistance and Mechanical Stability of Nickel Alloys in Molten-Salt Nuclear Reactors

Choosing structural materials for molten-salt nuclear reactors is a high-priority problem. The results making it possible to choose the basic structural material for a molten-salt nuclear reactor are colligated in the present article. Forced and natural circulation setups operating under reactor and laboratory conditions with molten metal-fluoride salts with different compositions have been developed at the National Research Center Kurchatov Institute: LiF–NaF–BeF{sub 2}–PuF{sub 3}, LiF–BeF{sub 2}–UF{sub 4}, and LiF–BeF{sub 2}–ThF{sub 4}–UF{sub 4}. Corrosion tests were conducted with domestically produced corrosion-resistant steel (12Kh18N10T, EP-164) and specially developed nickel-based alloys (KhN80M-VI, KhN80MTYu, KhN80MTV, et al.) as well as the alloy Hastelloy (USA), MONICR (Czechoslovakia) and EM-721 (France) in the working temperature range 600–800°C and mechanical loads up to 80 MPa on the samples.

21 SPECIFIC NUCLEAR REACTORS AND ASSOCIATED PLANTS↗

Corrosion and Fatigue Behavior of High-Strength Steel Treated with a Zn-Alloy Thermo-diffusion Coating

High and low cycle fatigue tests were conducted on high-strength steel using four-point bending. The materials tested were ASTM A723 steel in the as-machined condition, grit-blasted condition, MIL-DTL-16232 heavy manganese phosphate-coated condition, and ASTM A1059 Zn-alloy thermo-diffusion coated (Zn-TDC). The ASTM A723 steel base material exhibits a yield strength of ~1000 MPa. The effects of the surface treatments versus uncoated steel were examined. The fatigue life of the Zn-TDC specimens was generally reduced on as-coated specimens versus uncoated or phosphate-coated specimens. Several mechanisms are examined including the role of compressive residual stress relief with the Zn-TDC process as well as fatigue crack initiation from the hardened Zn-Fe alloy surface layer produced in the gas-metal reaction. Additionally, the effects of corrosion pitting on the fatigue life of coated specimens are explored as the Zn-TDC specimens exhibit significantly improved corrosion resistance over phosphate-coated and oiled specimens.

36 MATERIALS SCIENCE↗

Corrosion Protection of Phenolic-Epoxy/Tetraglycidyl Metaxylediamine Composite Coatings in a Temperature-Controlled Borax Environment

The failure behavior for two kinds of phenolic-epoxy/tetraglycidyl metaxylediamine composite coatings in 60 °C borax aqueous solution was evaluated using electrochemical methods (EIS) combined with scanning electron microscopy, confocal laser scanning microscope, water immersion test, and Raman spectrum. The main focus was on the effect of curing agent on the corrosion protection of coatings. Results revealed that the coating cured by phenolic modified aromatic amine possessed more compact cross-linked structure, better wet adhesion, lower water absorption (0.064 mg h{sup −1} cm{sup −2}) and its impedance values was closed to 10{sup 8} Ω cm{sup 2} after immersion for 576 h, while the coating cured by modified aromatic ring aliphatic amine was lower than 10{sup 5} Ω cm{sup 2}. The corrosion mechanism of the two coatings is discussed.

36 MATERIALS SCIENCE↗

The Effect of Multiple Shot Peening on the Corrosion Behavior of Duplex Stainless Steel

Various types of shot peening treatments were applied to duplex stainless steel. The effects of shot peening intensity and working procedures on the microstructure were investigated. The domain size and microstrain evolution in the surface layer were characterized utilizing the Rietveld method. As the shot peening intensity increased, the surface roughness increased in the surface layer; however, it decreased after multiple (dual and triple) shot peening. The mole fraction of strain-induced martensite as a function of the intensity of shot peening was evaluated by XRD measurements. Both potentiodynamic polarization curves and salt spray tests of shot-peened samples in NaCl solution were investigated. The results indicate that traditional shot peening has negative effects on corrosion resistance with increasing shot peening intensity; however, the corrosion rate can be reduced by means of multiple shot peening.

36 MATERIALS SCIENCE↗

An Investigation on the Wear and Corrosion Behavior of HVOF-Sprayed WC-12Co-Al{sub 2}O{sub 3} Cermet Coating

The aim of the present study is to develop thermally sprayable WC-12Co and WC-12Co-xAl{sub 2}O{sub 3} (x = 10 and 15 wt.%) cermet coatings on steel substrate (SS 304) by high-velocity oxy fuel (HVOF) method. Influence of Al{sub 2}O{sub 3} addition on the wear and corrosion behavior of WC-12Co coating has been studied. The microstructure and chemical composition of the coatings were analyzed using field emission scanning electron microscope (FESEM), and phase identification was carried out using x-ray diffraction (XRD) studies. The morphology of the coating appears as coarse granular structure. The XRD studies revealed the presence of hexagonal WC phase along with η-Co{sub 6}W{sub 6}C phase. It has been observed from the microhardness measurements, that the values gradually increase from 950 to 1300 HK with the addition of Al{sub 2}O{sub 3} from 0 to 15 wt.%. The wear rate of WC-12Co-15Al{sub 2}O{sub 3} (3.19 × 10{sup −6} mm{sup 3}/Nm) and WC-12Co-10Al{sub 2}O{sub 3} (5.26 × 10{sup −6} mm{sup 3}/Nm) coatings was seen to be one order of magnitude lower than that of WC-12Co (2.9 × 10{sup −5} mm{sup 3}/Nm) coating. The polarization studies revealed that WC-12Co-15Al{sub 2}O{sub 3} cermet coating showed superior corrosion protection than that of WC-12Co-10Al{sub 2}O{sub 3} and WC-12Co coatings. This has been attributed to the gradual decrease in the porosity levels with an increase in Al{sub 2}O{sub 3} content which is supported by morphology studies. The microhardness and wear behavior of WC-12Co-Al{sub 2}O{sub 3} coatings are equivalent to those of hard chrome suggesting the possibility of its replacement.

36 MATERIALS SCIENCE↗

Effect of Exchanging Advancing and Retreating Side Materials on Mechanical Properties and Electrochemical Corrosion Resistance of Dissimilar 6013-T4 and 7003 Aluminum Alloys FSW Joints

Friction stir welding (FSW) was used to weld dissimilar joints between Al 6013-T4 and Al7003 alloys in this work. The effect of exchanging advancing (AS) and retreating (RS) side material on microstructure, mechanical behaviors and electrochemical corrosion resistance was discussed. Results showed that different joint cross sections were obtained when exchanging AS and RS materials. The material on the AS would be more deformed during the welding process. When the Al6013 placed on the AS, the plastic flow of weld is more sufficient. Whether on the AS or RS, the Al6013-T4 side is the weak region for both tensile specimens and hardness samples. The fracture position corresponds to the minimum hardness position. Also, more strengthening phase can be retained in the joint, and the joint of A6R7 has better corrosion resistance.

36 MATERIALS SCIENCE↗

Effect of Immersion Time on Corrosion Behavior of Single-Phase Alloy and Nanocomposite Bismuth Telluride-Based Thermoelectrics in NaCl Solution

The corrosiveness of bismuth telluride-based thermoelectric materials (n-type single-phase alloy and a nanocomposite with MoS{sub 2} nanoinclusions), in 0.1 molar solution of sodium chloride (NaCl), was investigated. The electrochemical impedance spectroscopy curves obtained after 1, 24, 48 and 72 h immersion time revealed the enhancement of the corrosion resistance of the nanocomposite specimen in a 0.1 molar NaCl solution in comparison with the single-phase bismuth telluride-based alloys, and the passivity increased by immersion time up to 72 h. The nanocomposite sample with submicron grains provided suitable nucleation sites for passive film nucleation that led to higher protective behavior.

77 NANOSCIENCE AND NANOTECHNOLOGY↗

Effect of Thiourea on the Corrosion Behavior of Aluminum Anode Foil of Aluminum Electrolytic Capacitor

The specific capacitance is a key performing factor for the aluminum anode foil of aluminum electrolytic capacitor. In order to increase the specific capacitance, the effect of thiourea (TU) as corrosion inhibitor on the aluminum anode foil was investigated in this paper. Electrochemical impedance spectroscopy (EIS), polarization curves and weight loss measurements were used to investigate the effect of corrosion inhibitor TU added to nitric acid. EIS and inductance–capacitance–resistance (LCR) meter were also used to measure the specific capacitance of the aluminum anode foil, which was etched in nitric acid containing different contents of TU, and then formed in boric acid solution (100 g L{sup −1}) at 540 V. The results showed that the TU could be used as an inhibitor for Al in an acid solution. When the concentration of TU was 0.10%, the specific capacitance reached up to 0.661 μF cm{sup −2}, which increased by nearly 24% compared to that without TU. The data for the specific capacitance of Al anode foil corresponding to different TU concentrations obtained by EIS coincided well with the one obtained using LCR meter; thus, EIS could be effectively used for the preliminary selection of the type and ideal concentration of inhibitor.

36 MATERIALS SCIENCE↗

Synthesis and Characterization of Zeolites for Anti-corrosion Application: The Effect of Precursor and Hydrothermal Treatment

Four different hydrothermal processes were used to synthesize NaX zeolites. The effect of the precursor, hydrothermal time and temperature on the zeolite structure was investigated in this research. The results of XRD and FESEM/EDX analysis indicated the key role of aluminum sources in the amorphous content and the structure of zeolite from non-zeolite sodium aluminum silicate hydrate to favorable NaX-faujasite. Moreover, the irregular shape of agglomerated hydrogel was changed from micro- to nano-zeolite structure via the hydrothermal process of different aluminum sources. It was found that the nano-zeolites could be formed by sodium aluminate source. In addition, the synthesized zeolite particles were examined as corrosion inhibitor reservoir, considering the effect of Si/Al ratio, particle size, and amorphous content. It was shown that there is a direct relation between crystallization and ion exchange capacity. Through monitoring the behavior of bare mild steel in sodium chloride solution containing zinc cations released from the zeolite particles, it was found that the nano-zeolite particles with low Si/Al ratio can offer the most effective corrosion inhibition.

36 MATERIALS SCIENCE↗

Influence of Heat Input and Cold Wire Feeding Rate on Pitting Corrosion Resistance of Submerged Arc Welding Duplex Stainless Steel Welds

Welding thermal cycles may severely impair duplex stainless steel (DSS) performance, especially local pitting resistance and toughness. The restricted welding energy between 0.5 and 2.5 kJ mm{sup −1} represents a limiting factor for productivity increase in DSS welding, and the addition of cold wire is an interesting alternative to increase the welding deposition rate without adding extra heat. The aim of this work is to evaluate the influence of the cold wire feeding rate (CW) and heat input (HI) on pitting corrosion behavior of DSS UNS S32304 bead-on-plate welds obtained by submerged arc welding (SAW). Cyclic potentiodynamic polarization was carried out in transverse weld sections using 1 mol L{sup −1} NaCl solution at room temperature. Most pitting corrosion spots were located on the heat-affected zone (HAZ), and the pitting potentials were lower than the base metal due to higher ferrite fractions and the presence of chromium nitrides. Considering the same CW, the HI increasing reduced E{sub pit} for 1.6, 1.9, 2.2 kJ mm{sup −1}, but increased E{sub pit} for 2.7 kJ mm{sup −1}, due to a balance between the HAZ width and the austenite fraction.

36 MATERIALS SCIENCE↗

Stress Corrosion Cracking of AZ91 + xCe Alloy Using Proof Ring Test in ASTM D1384 and NaCl-K{sub 2}CrO{sub 4} Solutions

The effect of cerium addition on AZ91 magnesium alloy and its influence on stress corrosion cracking (SCC) were studied using constant load proof ring testing NaCl-K{sub 2}CrO{sub 4} and ASTM D1384 solutions at 70 and 80% of yield stress, respectively. The investigation revealed that the optimum grain refinement of desired phases occurred with 0.5% addition of cerium. The addition levels of cerium above 1.5 wt.% to AZ91 alloy resulted in premature failures due to poor SCC resistance in both solutions (K{sub 2}CrO{sub 4} and ASTM D1384 solutions). The microstructural studies of the experimental alloys were characterized by using optical and scanning electron microscopy. The elemental compositions of cerium-added AZ91 magnesium alloys were studied by energy-dispersive spectroscopy. The results indicate that the mode of SCC failure was found to be transgranular in nature along with secondary cracks containing cleavages which resulted from the hydrogen embrittlement and anodic dissolution phenomena. The AZ91 alloy with 0.5 wt.% cerium exhibits better mechanical properties and high stress corrosion resistance.

36 MATERIALS SCIENCE↗

Effect of Cobalt on the Microstructure and Corrosion Behavior of Martensitic Age-Hardened Stainless Steel

To evaluate the influence of cobalt on the microstructure and pitting behavior of martensitic age-hardened stainless steel (MASS), the microstructures and electrochemical behaviors were characterized by optical microscopy, scanning electron microscopy, transmission electron microscopy, x-ray photoelectron spectroscopy, potentiodynamic curve, electrochemical impedance spectroscopy, and Mott–Schottky analysis. Results indicated that adding cobalt reduced the grain size of the original austenite, refined the lath martensite, inhibited the precipitation of Cu-rich phases, and increased the content of reversed austenite. Compared with the cobalt-free steel, the cobalt-containing steel has a higher pitting potential, lower corrosion current density, and higher pitting resistance. The primary components of the passive film grown on the cobalt-free steel included (Cr, Fe) oxides, such as Cr{sub 2}O{sub 3}, Cr(OH){sub 3}, FeOOH, and Fe{sub 2}O{sub 3}. The cobalt-containing steel included the aforementioned components as well as Co, which was attributed to the formation of the passive film in the forms of CoFe{sub 2}O{sub 4}, Co(OH){sub 2}, and CoO. In addition, the synergy of the refined lath martensite and the precipitation of the Cu-rich phase induced an increase in corrosion resistance in MASS containing cobalt.

36 MATERIALS SCIENCE↗

Effect of Heat Input on Microstructure, Residual Stress, and Corrosion Resistance of UNS 32101 Lean Duplex Stainless Steel Weld Joints

In the present work, the influence of heat input on phase balance, residual stresses and corrosion resistance of UNS 32101 lean duplex stainless steel welds has been investigated. Three weldment types were obtained with different heat inputs by varying welding current, using gas tungsten arc welding process. The results revealed that increasing heat input caused a significant microstructural evolution with high austenite fraction in weld metals. The residual stresses were measured on the surface and through the sample’s thickness by x-ray diffraction technique based on Sin{sup 2}ψ method. The results showed an inversely proportional relationship between the heat input and the compressive residual stresses on the surface and through the thickness of the weld metal. Potentiodynamic polarization tests of the different welded joints evaluated in 3.5% NaCl solution exhibited high corrosion resistance of the weld metal produced with the low heat input.