Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “INTERMETALLIC COMPOUNDS”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 1,315 records · Page 73

Formation of Fe2Al5-xZnx intermetallic crystals at the Fe-Zn interface in hot-dip galvanizing

Highlights: • Interstitial-free steels were galvanized in Zn baths containing 0.14-0.28 wt% Al. • The Fe-Al layer formed in a 0.14 wt% Al bath is composed of equiaxed Fe{sub 2}Al{sub 5-x}Zn{sub x} crystals without preferred orientations. • The layers formed in baths containing 0.18 wt% Al or more are composed of orientated domains. • Each domain contains 4-12 Fe{sub 2}Al{sub 5-x}Zn{sub x} crystal variants of specific orientations. • A layer of a single variant crystal can grow epitaxially on the α-Fe grains as the Al content reaches 0.28 wt%. - Abstract: The formation of Fe{sub 2}Al{sub 5-x}Zn{sub x} inhibition layer at the Fe-Zn interface has been characterized by scanning electron microscopy/electron backscatter diffraction and transmission electron microscopy for interstitial-free steels galvanized in Zn baths containing 0.14–0.28 wt% Al. The inhibition layer formed in the 0.14 wt% Al bath is composed of fine, equiaxed Fe{sub 2}Al{sub 5-x}Zn{sub x} crystals without preferred orientations. The inhibition layers formed in the baths containing 0.18 wt% Al or more are composed of orientated domains and each domain contains 4–12 Fe{sub 2}Al{sub 5-x}Zn{sub x} crystal variants of specific orientations. All the variants follow the same Fe{sub 2}Al{sub 5-x}Zn{sub x}/Fe orientation relationship of [110]{sub Fe2Al5-xZnx}//[1 1-bar 1]{sub Fe} and (001){sub Fe2Al5-xZnx}//(110){sub Fe}. Therefore, each domain is formed on a single α-Fe grain and the number of variants in the domain is determined by the orientation of the α-Fe grain. The fraction of the area of epitaxial growth increases with increasing Al content in bath. When the Al content reaches 0.28 wt%, a layer of a single variant (SV) crystal can grow epitaxially on the α-Fe grains having orientations distributed from <110> to <113> parallel to the normal direction of the sheet surface. The formation of a dense SV inhibition layer is the major reason for the drastic reductions in both the Al-pickup rate and the inhibition layer thickness at high Al content baths.

36 MATERIALS SCIENCE↗

The influence of sintering temperature on microstructure and mechanical properties of Ni-Al intermetallics fabricated by SPS

In the present study PN85Yu15 was used as elemental powder to produce a sintered compound with Ni3Al as main phase. The Spark Plasma Sintering (SPS) technique is used to compact the powders. The powder was sintered in a temperature range between 1000°C and 1150°C to observe the influence of the sintering temperature on the microstructure and the mechanical properties. The microstructure was observed with optical microscope (OM), the phase composition was characterized by X-ray diffraction (XRD) technique. Density and microhardness were observed and compared the values with the results of other researchers. The compressive-, density- and microhardness tests show as clear result that with increasing the sintering temperature nearly all properties become better and also the microstructure studies show that porous places become less.

36 MATERIALS SCIENCE↗

X-ray diffraction study of the phase purity, order, and texture of ductile B2 intermetallics

Representatives (AgY, CuY, AgEr, CuDy, MgY and MgCe) of the newly discovered family of ductile stoichiometric B2 intermetallic (metal-rare-earth element, MR) compounds were characterized by X-ray diffraction, to determine if their anomalous ductility is related to an exceptional level of phase purity, lack of chemical ordering or a strong crystallographic texture. Brittle NiAl served as an anti-type in this study. We found that all of the rare-earth compounds, except MgY, have a significant volume fraction (-5-20vol.%) of second phases (M{sub 2}R intermetallics and R{sub 2}O{sub 3} oxides), which has not been reported in previous studies of these materials. The most ductile of observed MR compounds, AgY, is highly ordered. A moderate texture was observed in AgY, which may explain its higher ductility (using polycrystal modeling) as compared to other MR compounds. However, the intrinsic polycrystalline ductility of these compounds in the randomly textured state (like that observed in CuY) still has no specific, definitive explanation.

36 MATERIALS SCIENCE↗

Competing anisotropies on 3d sub-lattice of YNi{sub 4–x}Co{sub x}B compounds

The magnetic anisotropy of 3d sub-lattices has an important rule on the overall magnetic properties of hard magnets. Intermetallics alloys with boron (R-Co/Ni-B, for instance) belong to those hard magnets family and are useful objects to help to understand the magnetic behavior of 3d sub-lattice, specially when the rare earth ions R do not have magnetic nature, like YCo{sub 4}B ferromagnetic material. Interestingly, YNi{sub 4}B is a paramagnetic material and Ni ions do not contribute to the magnetic anisotropy. We focused therefore our attention to YNi{sub 4–x}Co{sub x}B series, with x = 0, 1, 2, 3, and 4. The magnetic anisotropy of these compounds is deeper described using statistical and preferential models of Co occupation among the possible Wyckoff positions into the CeCo{sub 4}B type hexagonal structure. We found that the preferential model is the most suitable to explain the magnetization experimental data.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Characterisation and modelling of defect formation in direct-chill cast AZ80 alloy

Wrought magnesium alloys for demanding structural applications require high quality defect free cast feedstock. The aim of this study was to first identify and characterise typical defects in direct chill cast magnesium–aluminium–zinc (AZ) alloy billet and then use modelling to understand the origins of these defects so they can be prevented. Defects were first located using ultrasonic inspection and were then characterised using X-ray computed tomography (XCT) and serial sectioning, establishing the presence of oxide films and intermetallic particles Al{sub 8}Mn{sub 5} in all defects. A model was developed to predict the flow patterns and growth kinetics of the intermetallic phases during casting, which influence the formation of defects. Simulation of the growth of the intermetallic particles demonstrated that precipitation from the liquid occurs in the mould. The combination of the entrained oxide films and intermetallic particles recirculates in the liquid metal and continues to grow, until large enough to settle, which is predicted to occur at the centre of the mould where the flow is the slowest. Based on these predictions, strategies to reduce the susceptibility to defect formation are suggested. - Highlights: • Casting defects in magnesium direct chill casting have been imaged and characterised in 3-dimensions. • The occurrences of co-located clusters of particles and oxide films have been characterised and explained. • A coupled model has been developed to help interpret the observed trend for defects located towards the centre of billets.

36 MATERIALS SCIENCE↗

Analysis of Microstructure and Sliding Wear Behavior of Co{sub 1.5}CrFeNi{sub 1.5}Ti{sub 0.5} High-Entropy Alloy

Α Co{sub 1.5}CrFeNi{sub 1.5}Ti{sub 0.5} high-entropy alloy (HEA) of the well-known family of CoCrFeNiTi has been designed using empirical parameters. The aim of this design was the production of a HEA with fcc structure that gives ductile behavior and also high strength because of the solid solution effect. The VEC calculations (8.1) supported the fcc structure while the δ factor calculations (4.97) not being out of the limit values, advised a significant lattice distortion. From the other hand, the ΔΗ{sub mix} calculations (− 9.64 kJ/mol) gave strong indications that no intermetallic would be formed. In order to investigate its potential application, the Co{sub 1.5}CrFeNi{sub 1.5}Ti{sub 0.5} HEA was prepared by vacuum arc melting and a primary assessment of its surface degradation response was conducted by means of sliding wear testing using different counterbody systems for a total sliding distance of 1000 m. An effort to correlate the alloy’s wear response with the microstructural characteristics was attempted. Finally, the wear behavior of the Co{sub 1.5}CrFeNi{sub 1.5}Ti{sub 0.5} HEA was compared with that of two commercially used wear-resistant alloys. The results obtained provided some first signs of the high-entropy alloys’ better wear performance when tested under sliding conditions against a steel ball.

36 MATERIALS SCIENCE↗

Self-propagating reactions in Al/Zr multilayers: Anomalous dependence of reaction velocity on bilayer thickness

High temperature, self-propagating reactions are observed in vapor-deposited Al/Zr multilayered foils of overall atomic ratios 3 Al:1 Zr and 2 Al:1 Zr and nanoscale layer thicknesses; however, the reaction velocities do not exhibit the inverse dependence on bilayer thickness that is expected based on changes in the average diffusion distance. Instead, for bilayer thicknesses of 20-30 nm, the velocity is essentially constant at ∼7.7 m/s. We explore several possible explanations for this anomalous behavior, including microstructural factors, changes in the phase evolution, and phase transformations in the reactant layers, but find no conclusive explanations. We determine that the phase evolution during self-propagating reactions in foils with a 3 Al:1 Zr stoichiometry is a rapid transformation from Al/Zr multilayers to the equilibrium intermetallic Al{sub 3}Zr compound with no intermediate crystalline phases. This phase evolution is the same for foils of 90 nm bilayer thicknesses and foils of bilayer thicknesses in the range of 27 nm to 35 nm. Further, for foils with a bilayer thickness of 90 nm and a 3 Al:1 Zr overall chemistry, the propagation front is planar and steady, in contrast to unsteady reaction fronts in foils with 1 Al:1 Zr overall chemistry and similar bilayer thicknesses.

36 MATERIALS SCIENCE↗

Compression behavior of the forged Ll2 compounds Al67Ti25Cr8 and Al66Ti25Mn9

The paper presents the findings of a compression study as a function of temperature from cryogenic temperatures to 1373 K at a strain rate of about 0.0001/s on forged Al67Ti25Cr8 and Al66Ti25Mn9 compounds. The creep response of these alloys is analyzed at strain rates varying from 2 x 10 to the -4th to 2 x 10 to the -7th /s at 1000 K and 1100 K. It is shown that as-cast microstructures for both compounds are dendritic, while both intermetallics forged very well with no edge cracking, with the microstructures appearing fully recrystallized. True comprehensive stress-strain diagrams determined at 1100 K as a function of nominal strain rate reveal a range of behaviors in both materials.

Brown, S. A.↗

Microstructure, precipitates and hardness of selectively laser melted AlSi10Mg alloy before and after heat treatment

Highlights: • Microstructural characterization of SLM AlSi10Mg alloy and comparison with cast and powder AlSi10Mg • Effect of solution heat treatment and aging on the hardness change of SLM AlSi10Mg alloy • Evolution of strengthening precipitates and Fe-rich intermetallics in SLM AlSi10Mg during heat treatment - Abstract: The microstructure and precipitates within selectively laser melted (SLM) AlSi10Mg alloys in the as-built state and after T6 heat treatment were examined and correlated to the hardness evolution. The as-built alloy exhibited columnar patterns perpendicular to the build-direction and fish-scale pattern along the build-direction originating from the melt pool. The microstructure consisted of fine Al cells and eutectic structure with up to 4 μm in size. Tiny needle-like Si particles with highly faulted structure were identified within the Al cells and formed semi-coherent interface with the matrix. Nanoscale Si particles and π-Al{sub 8}Si{sub 6}Mg{sub 3}Fe phase were observed to segregate along the cell and grain boundary. Solution heat treatment (SHT) at 520 °C resulted in the dissolution of Al cellular microstructure. Precipitation and coarsening of the Si particles occurred, while the aspect ratio of Si particles remained nearly constant. The π-Al{sub 8}Si{sub 6}Mg{sub 3}Fe phase decomposed into plate-shaped β-Al{sub 5}SiFe. The artificial aging (AA) at 160 °C did not alter the microstructure but led to the formation of metastable Mg{sub 2}Si precipitates. The GP zones and β″ were identified through transmission electron microscopy after AA of 6 h, and β″ existed up to AA of 24 h. The hardness decreased after SHT due to the coarsening of the microstructure and reduced solid solution hardening. Hardness reached maximum magnitude after AA of 6–10 h due to the precipitation hardening, and remained relatively unchanged up to AA of 24 h. Microstructure and/or hardness of gas atomized powders and bulk cast AlSi10Mg alloys were also examined as references.

36 MATERIALS SCIENCE↗

The Effect of SiC Addition on Microstructure and Mechanical Properties of Gas Tungsten Arc-Welded Ti-6Al-4V Alloy

In the present study, SiC powder was added in situ for bead-on-plate weldments and fusion butt joints to modify the microstructure and the corresponding mechanical properties. Cross sections of bead-on-plate welds demonstrated that the SiC addition resulted in significant changes of the titanium microstructure. Specifically, a fine lamellar structure of α-phase with a small amount of intergranular β-titanium within the fusion zone could be established. Moreover, the size of prior β-grains was significantly reduced. After welding, no intermetallic silicides were observed. In the fusion zone of the SiC-enhanced samples, a small increase in hardness resulted, and the samples showed an increase in tensile strength, yield strength and elongation.

36 MATERIALS SCIENCE↗

Corrosion Behavior of Fe-40at.%Al-Based Intermetallic in 0.25 M H{sub 2}SO{sub 4} Solution

The electrochemical behavior of Fe-40at.%Al-based intermetallic microalloyed with 3 and 5 at.% Cu additions in 0.25 M H{sub 2}SO{sub 4} solution over time was studied. A complementary study to characterize the surface morphology and semiquantitative chemical analysis of the corrosion products after 24 h of immersion was performed using scanning electron microscopy and x-ray energy dispersion spectrum. By means of electrochemical techniques, it was shown that Cu addition has a positive effect on corrosion resistance of Fe-40at.%Al-based intermetallic alloy. Additionally, the relatively high concentration of Cu consolidated the passive film of corrosion products and its stability.

36 MATERIALS SCIENCE↗

The grain refinement mechanisms of various phases in shot-peened Nickel-Aluminum bronze (NAB) alloy

Highlights: • There exist two grain refinement mechanisms at the same time in the α phase. • The refinement of β' phase is attributed to the formation of dense and ordered nano twins. • The brittle strip-shape κ{sub iii} phases are fragmented after large deformation. • The κ{sub iv} and κ{sub ii} phases exhibit the twinning and dislocation deformation modes, separately. • The microhardness increases significantly owing to work hardening effect and grain refinement. - Abstract: In this study, coarse-grained Nickel-Aluminum bronze (NAB) alloy is subjected to shot-peening (SP) treatment, and the grain refinement mechanisms of various phases in shot-peened NAB alloy are investigated separately. The results show that severe deformation layers are produced on the surface. Meanwhile, refined grains with the average size below 100 nm are induced through SP treatment indicated by the results of X-ray diffraction (XRD) patterns. Various phases in NAB alloy including α, β' and three intermetallic phases (κ{sub ii}, κ{sub iii} and κ{sub iv}) display different grain refinement mechanisms. The grain refinement in the α phase involves dislocation segmentation in the precipitation-free zone and the twinning intersection in the precipitation zone. The formation of nanotwins by emitting partial dislocations at the grain boundary is found to be responsible for the grain refinement in the β' phase. As for the κ phases, the strip-shaped κ{sub iii} phases are fragmented after severe deformation, and the κ{sub iv} and κ{sub ii} phases exhibit the twinning and dislocation deformation modes, respectively. Also, the microhardness is significantly enhanced after SP treatment, which is mainly attributed to the work hardening effect and grain refinement.

36 MATERIALS SCIENCE↗

Inhibitory effect of Ti and La on Fe dissolution in Al–Zn–Si bath by in-situ SXRD, SXRF, TEM and DFT calculation

Highlights: • In-situ synchrotron X-rays diffraction was used to study the solid-liquid reaction. • The addition of Ti and La suppresses the dissolution of Fe in the reaction. • A new quaternary phase was found in the hot-dip coated sheets. • The formation of the quaternary phase needed an enrichment of Si from bath. • The continuous formation of dross probably caused by the initial dissolution - Abstract: During the hot-dipping process, there is always a desire to restrain the mutual diffusion between steel and alloy bath for suppressing the formation of bath dross. However, the dissolution of steel sheets is difficult to quantify by the traditional methods. In this work, in-situ X-ray diffraction was used to investigate the solid-liquid reaction between solid Fe and Al–Zn–Si liquid alloy for quantitatively analyzing the consumption of Fe and the formation of Fe–Al compounds. The results indicated that the addition of trace Ti or La could suppress the mutual diffusion. We also observed the microstructures of the Fe–Al intermetallic multilayers and the distribution of Ti or La in the multilayers. A new quaternary phase was identified. The inhibitory effects of Ti and La were also explained by calculating the diffusion barrier energies with density functional theory.

36 MATERIALS SCIENCE↗

On visualizing material flow and precipitate evolution during probeless friction stir spot welding of an Al-Li alloy

Highlights: • Severe thermal cycle and deformation refined grains and intermetallic particles in SZ. • T{sub 1} phases fully dissolved in SZ followed by re-precipitation of GP zone and δ′ phases. • The predominant flow direction remained in spiral-like pattern during P-FSSW. • Local abrasion existed in the lap-weld interface due to flow difference, forming joining. - Abstract: The precipitate evolution and material flow visualization during probeless friction stir spot welding (P-FSSW) of an Al-Li alloy has been investigated experimentally and numerically in this work. Due to severe heat input during welding, the main strengthening phases of T{sub 1} fully dissolved in the stir zone followed by the re-precipitation of GP zone and δ′ phases, assisted with the refinement of the intermetallic particles and grains. The history of material flow was three-dimensionally visualized with a tracer, studied with X-ray tomography. The experiments and the simulation results provided a consistent interpretation of a circumferential material flow which moved inwards radially near the top surface. Upward flow in the bottom sheet improved with dwell time, causing the interface to bend. Local abrasion between the two sheets due to flow difference led to the disruption of oxide layer, and formed a connection at the interface.

36 MATERIALS SCIENCE↗

Formation and Toughening Mechanisms of Dispersions in Interfacial Intermetallics of Dissimilar Laser Al/Steel Joints

The key to improve the strength of Al/steel dissimilar joint is to toughen the hard and brittle interfacial intermetallics. Introducing soft and tough dispersions into the interfacial intermetallics would be a promising method. In the present study, Zn-Al alloy (Zn-22Al) was used as the filler metal to generate dispersions in the interfacial intermetallics matrix of dissimilar laser Al/steel joint. The results have shown that soft and tough dispersions, i.e., FeZn{sub 10,} Al-rich amorphous phase, and Zn solid solution, were successfully introduced into the hard and brittle Fe{sub 2}Al{sub 5−x}Zn{sub x} matrix. The formation of these dispersions was resulted from diffusion of elements Fe and Al and infiltration of liquid Zn along the grain boundaries of Fe{sub 2}Al{sub 5−x}Zn{sub x} matrix and the subsequent chemical reaction and solidification. With this kind of interfacial microstructure, the joint exhibited a stable peak fracture load of 1200 N even though the interfacial layer thickness increased from 20 to 45 μm. This was because the interfacial layer was toughened by the soft and tough dispersions. Using this example, introduction of soft and tough dispersions into hard and brittle intermetallics matrix to toughen interfacial layer and then strengthening of dissimilar joints will be highlighted.

36 MATERIALS SCIENCE↗

EuTZn (T=Pd, Pt, Au) with TiNiSi-type structure-Magnetic properties and {sup 151}Eu Moessbauer spectroscopy

The europium compounds EuTZn (T=Pd, Pt, Au) were synthesized from the elements in sealed tantalum tubes in an induction furnace. These intermetallics crystallize with the orthorhombic TiNiSi-type structure, space group Pnma. The structures were investigated by X-ray diffraction on powders and single crystals: a=732.3(2), b=448.5(2), c=787.7(2) pm, R{sub 1}/wR{sub 2}=0.0400/0.0594, 565 F{sup 2} values for EuPdZn, a=727.8(3), b=443.7(1), c=781.7(3) pm, R{sub 1}/wR{sub 2}=0.0605/0.0866, 573 F{sup 2} values for EuPtZn, and a=747.4(2), b=465.8(2), c=789.1(4) pm, R{sub 1}/wR{sub 2}=0.0351/0.0590, 658 F{sup 2} values for EuAuZn, with 20 variables per refinement. Together the T and zinc atoms build up three-dimensional [TZn] networks with short T-Zn distances. The EuTZn compounds show Curie-Weiss behavior in the temperature range from 75 to 300 K with mu{sub eff}=7.97(1), 7.70(1), and 7.94(1) mu{sub B}/Eu atom and theta{sub P}=18.6(1), 34.9(1), and 55.5(1) K for T=Pd, Pt, and Au, respectively, indicating divalent europium. Antiferromagntic ordering was detected at 15.1(3) K for EuPdZn and canted ferromagnetic ordering at 21.2(3) and 51.1(3) K for EuPtZn and EuAuZn. {sup 151}Eu Moessbauer spectroscopic measurements confirm the divalent nature of the europium atoms by isomer shift values ranging from -8.22(8) (EuPtZn) to -9.23(2) mm/s (EuAuZn). At 4.2 K full magnetic hyperfine field splitting is observed in all three compounds due to magnetic ordering of the europium magnetic moments. - Graphical abstract: Europium coordination in EuPdZn, EuPtZn, and EuAuZn.

36 MATERIALS SCIENCE↗

The relation between Mn additions, microstructure and corrosion behavior of new wrought Mg-5Al alloys

Highlights: • The influence of high Mn content (1.4 and 3.1 wt%) on Mg-5Al wrought alloys. • Core and shell Al-Mn particles formed when Mn content was 1.4 wt%. • 3.1 wt% Mn effectively mitigate the effect of Fe when it exceeds the tolerance limit. • Large Mn content stabilize the passive layer in long immersion periods. - Abstract: Three wrought Mg-5Al alloys with different Mn contents (0.5, 1.4, and 3.1 wt%) were examined and compared with a reference wrought Mg-5Al alloy. Additions of Mn decreased the grain size and caused precipitation of various Al-Mn intermetallide with different Al/Mn ratio. The corrosion resistance of the Mn-containing alloys significantly increased in comparison to the reference alloy. This contributed to a reduced harmful effect of the impurities, refined microstructure and formation of corrosion products layer. However, further increasing of Mn content caused greater precipitation of the Al-Mn intermetallics, which in its turn increased the galvanic micro-coupling. The alloy with 3.1 wt% Mn additions formed a relatively protective oxide film, which balances the increased number of cathodic particles, and its corrosion rate was very close to that of alloy with 1.4 wt% Mn content.

36 MATERIALS SCIENCE↗

Characterization of Laser-Welded Ti Alloy and Stainless Steel Joint Using Cu Interlayer

In this study, Cu was used as an interlayer to restrain the formation of brittle Ti-Fe intermetallics when joining Ti alloy to SS. Microstructures of the joint were analyzed using optical microscopy, scanning electron microscopy and x-ray diffraction. Besides, the tensile strength of the joint was also measured. The melting amount of base materials was controlled by changing thickness of Cu interlayer to control the melting proportion in weld. The melting amount of base materials in weld decreased with the thickness of Cu interlayer. The content of Cu solid solution in weld increased with the thickness of Cu interlayer. Ti-Cu compound layer was formed on the Ti alloy side. The width of the Ti-Cu compound layer increased with the increase in heat input. The tensile strength of joint was largely impacted by Ti-Cu compound layer. The tensile strength of joint first increased and then decreased with the increase in width of the Ti-Cu compound layer.

36 MATERIALS SCIENCE↗