Size effect characteristics and influences on fatigue behavior of laser powder bed fusion of thin wall GRCop-42 copper alloy

Size effects, influencing a material's strength, elongation, fatigue limit, and longevity, depend on the operative and dominant deformation and failure mechanisms. This study explores the size effects in additive manufactured (AM) GRCop-42 (Cu-4at%Cr-2at%Nb) thin wall structures fabricated via laser-powder bed fusion (L-PBF) and their impact on fatigue life. The influence of internal defects and surface topography on the fatigue life of specimens in both as-built and hot isostatic pressed (HIP) conditions across different thicknesses is investigated. Where micro-computed tomography (μCT) was used to quantify the internal porosity of as-built, pristine HIP'd, and fatigued HIP'd specimens, and laser microscopy was employed to quantify the surface topography of specimens prior to fatigue. Additionally, quasi-static tests were used to establish baseline mechanical properties (i.e. yield strength (YS), ultimate tensile strength (UTS), and elongation) to frame fatigue testing conditions. Results indicate a significant enhancement in fatigue life for HIP'd specimens for both thicknesses, with internal defects depicting a greater impact than surface topography. Furthermore, fractographic analysis suggests that thicker specimens exhibit higher resistance to crack propagation during fatigue testing in the absence of substantial porosity. Thus, the size effects observed on the fatigue life of L-PBF GRCop-42 appears to be dominated by internal defects.

36 MATERIALS SCIENCE↗

Revealing melt flow instabilities in laser powder bed fusion additive manufacturing of aluminum alloy via in-situ high-speed X-ray imaging

Laser metal additive manufacturing technologies enable the fabrication of geometrically and compositionally complex parts unachievable by conventional manufacturing methods. However, the certification and qualification of additively manufactured parts are greatly hindered by the stochastic melt flow instabilities intrinsic to the process, which has not been explicitly revealed by direct observation. Here, we report the mechanisms of the melt flow instabilities in laser powder bed fusion additive manufacturing process revealed by in-situ high-speed high-resolution synchrotron X-ray imaging. Here we identified powder/droplet impact, significant keyhole oscillation, and melting-mode switching as three major mechanisms for causing melt flow instabilities. We demonstrated the detrimental consequences of these instabilities brought to the process, and presented new understanding on the melt flow evolution and keyhole oscillation. This work provides critical insights into process instabilities during laser metal additive manufacturing, which may guide the development of instability mitigation approaches. The results reported here are also important for the development and validation of high-fidelity computational models.

36 MATERIALS SCIENCE↗

Simplification of the purification of heat stable recombinant low molecular weight proteins and peptides from GST-fusion products

The synthesis and purification of peptides of importance in the fields of research and medicine continue to be a challenging task. Chemical synthesis of oligopeptides, especially those greater than 25 amino acids, is cost prohibitive. On the other hand, several bottlenecks exist in the production of recombinant short peptides in heterologous expression hosts such as Escherichia coli (E. coli). In this paper, a rapid, cost-effective, and reliable method for the production and singlestep-purification of peptides and small proteins was developed. Five peptides and small proteins were overexpressed in E. coli as GST-fusion products in high yields. The recombinant peptides or proteins were successfully purified after enzymatic cleavage with selective heat-induced precipitation of the GST-affinity tag. Qualitative and quantitative analysis using SDS-PAGE and mass spectrometric methods suggest that the recombinant peptides/ proteins were purified to >95% homogeneity. Results of biophysical experiments, including multi-dimensional NMR spectroscopy, show that the purified proteins/ peptides retain their native conformation. Isothermal titration calorimetry studies indicate no significant change in the binding affinity of the heattreated purified product to their interacting partner(s) compared to the recombinant peptides purified by conventional chromatographic procedures without subjecting to heat treatment. In our opinion, the results reported render the purification of recombinant proteins/ peptides of biomedical relevance using our proposed method easy and reliable.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Characterization of fusion welded ceramics in the SiC-ZrB 2 -ZrC system

Various SiC-ZrB 2 -ZrC ceramics were joined by fusion welding to determine the maximum silicon carbide content that could be joined. Commercial powders were hot pressed, machined, and preheated to 1450 °C before joining with a tungsten inert gas welding torch at 160–200 A. Resulting welds were cross-sectioned and analyzed to determine which compositions were weldable and to characterize microstructural evolution in welded samples. As compositions approached the ternary eutectic, the welds had smaller SiC grains and exhibited better weldability. Penetration depth of welds was controlled by a combination of current input and welding speed. Here, the ternary eutectic in the system was found at 36.9 ± 1.3 vol% SiC, 42.7 ± 1.5 vol% ZrB 2 , and 20.4 ± 1.9 vol% ZrC and its melting temperature was 2330 ± 23 °C. A ternary phase diagram for the SiC-ZrB 2 -ZrC was constructed and proposed via microstructural analysis of arc melted pellets on binary joins between each binary eutectic and the ternary eutectic in the system.

36 MATERIALS SCIENCE↗

Additively manufactured β-Ti5553 with laser powder bed fusion: Microstructures and mechanical properties of bulk and lattice parts

Ti5553 (Ti-5Al-5Mo-5V-3Cr wt%) is a titanium alloy widely used for its high strength-to-weight ratio and good formability at elevated temperatures. Unlike Ti-6Al-4V, Ti5553 does not undergo martensitic transformation, preventing cracking of brittle martensite upon rapid cooling. This makes it a strong candidate for additive manufacturing (AM), particularly laser powder bed fusion (L-PBF). L-PBF offers the unique opportunity to make fine lattice structures to reduce component weight. Despite the growing field of AM, there have been limited studies on L-PBF Ti5553 lattices and how their properties differ from the bulk. Here the present work addresses this knowledge gap by investigating microstructures and properties of L-PBF bulk and lattice parts and the effect of post L-PBF heat treatments. Electron microscopy and mechanical testing show that the high dislocation density formed during L-PBF increases bulk part’s yield strength by approximately 100 MPa compared to the conventional alloy. Digital image correlation during compression testing of octet truss lattices reveals a layer-by-layer failure mode. Compared to the bulk, the lattice contains copious ω nanoprecipitation, weaker <001> texture, smaller average grain sizes, and larger content of high-angle grain boundaries. These features elicit differences in Taylor factor distributions for the lattice depending on load direction, underlining challenges in predicting lattice mechanical response based on bulk properties. By examining the processing-structure-property relationships in the bulk and lattice, the present results delineate their microstructural and mechanical differences and establish a benchmark for the future design applications of L-PBF Ti5553.

36 MATERIALS SCIENCE↗

Variant selection in laser powder bed fusion of non-spherical Ti-6Al-4V powder

The presence of α/α' on prior β/β grain boundaries directly impacts the final mechanical properties of the titanium alloys. The β/β grain boundary variant selection of titanium alloys has been assumed to be unlikely owing to the high cooling rates in laser powder bed fusion (L-PBF). However, we hypothesize that powder characteristics such as morphology (non-spherical) and particle size (50–120 µm) could affect the initial variant selection in L-PBF processed Ti-6Al-4V alloy by locally altering the cooling rates. Despite the high cooling rate found in L-PBF, the results showed the presence of β/β grain boundary α' lath growth inside two adjacent prior β grains. Electron backscatter diffraction micrographs confirmed the presence of β/β grain boundary variant selection, and synchrotron X-ray high-speed imaging observation revealed the role of the “shadowing effect” on the locally decreased cooling rate because of keyhole depth reduction and the consequent β/β grain boundary α' lath growth. The self-accommodation mechanism was the main variant selection driving force, and the most abundant α/α boundary variant was type 4 (63.26°//[ $\bar{10}$ 5 5 $\bar{3}$ ]). The dominance of Category II α lath clusters associated with the type 4 α/α boundary variant was validated using the phenomenological theory of martensite transformations and analytical calculations, from which the stress needed for the β→α' transformation was calculated.

36 MATERIALS SCIENCE↗

Effects of helium on irradiation response of reduced-activation ferritic-martensitic steels: Using nickel isotopes to simulate fusion neutron response

Understanding the effects of helium on microstructures and mechanical properties of reduced-activation ferritic-martensitic steels is important to use of these steels in fusion reactor structures. The 9Cr-2WVTa steels were doped with 58Ni and 60Ni isotopes at 2 weight percent to control the rate of transmutation helium generation. The samples were irradiated in the High Flux Isotope Reactor to ~24 displacements per atom at nominal temperatures of 300, 400, and 500°C, producing 228 and 7 atomic parts-per-million helium in the 58 Ni- and 60 Ni-doped samples, respectively. Transmission electron microscopy revealed a variety of precipitates and the radiation-induced dislocation loops and cavities (voids or helium bubbles). Tensile tests of the irradiated samples at the irradiation temperatures showed radiation-induced hardening at 300°C and radiation-induced softening at 400°C. Analysis indicates that the hardening primarily originated from the loops and cavities. The 58 Ni-doped samples had greater strengthening contributions from loops and cavities, leading to higher hardening with lower ductility than the 60 Ni-doped samples. The greater helium production of 58 Ni did not show pronounced reductions in ductility of the samples.

36 MATERIALS SCIENCE↗

Creep behavior of 316 L stainless steel manufactured by laser powder bed fusion

Additive manufacturing as a new processing technique can produce unique microstructure that is difficult to achieve using conventional techniques. Here, we have investigated the creep behavior of 316 L stainless steel produced by a laser powder bed fusion process at temperatures of 550, 600 and 650 °C and stresses between 175 and 300 MPa. We found that additively-manufactured 316 L stainless steel had a higher stress dependence of the minimum creep rate than conventionally-made Type 316 SS, which could be attributed to the dislocation cell structure resulting from the printing process. The dislocation cell structure was unstable under creep, evolving into a uniform dislocation structure under the test conditions. While internal porosity in AM 316 L SS may serve as nucleation sites of creep voids and may be responsible for a relatively lower creep life, additively-manufactured 316 SS did not show inferior creep ductility when compared with conventionally-made 316 SS. The creep life of AM 316 L SS could be improved by stabilizing dislocation cell structure and/or reducing internal porosity through an optimized additive manufacturing process.

316 L stainless steel↗

Deuterium permeation and retention in 316L Stainless Steel Manufactured by Laser Powder Bed Fusion

Deployment of additively manufactured materials into nuclear energy systems requires investigation of the full range of the unique environmental effects on these materials. Hydrogen isotopes are common gaseous species in nuclear reactors and exhibit ample high mobility in most materials. While hydrogen isotopes mobility in wrought stainless steel is well understood, this property is not thoroughly studied for its additively manufactured variants. In this study, we investigated the deuterium permeation and retention in 316L stainless steel manufactured by laser powder bed fusion. The results showed that the deuterium permeability in the as-built additively manufactured 316L stainless steel (AM SS316L) is greater than that of the reference wrought 316L stainless steel by a factor of 2.8. However, the stress-relieved and solution-annealed AM SS316L samples exhibit lower deuterium permeability in comparison with the as-built condition. Following the solution annealing, the deuterium permeability of AM SS316L is comparable with that of the reference wrought SS316L. Deuterium retention in the as-built AM SS316L is 45% higher than that of the wrought 316L stainless steel and slightly higher than that of the two thermally annealed AM SS316L materials. Finally, transmission electron microscopy and positron annihilation lifetime spectroscopy were used to obtain microstructural information used to determine deuterium permeation and retention behavior in the studied materials.

36 MATERIALS SCIENCE↗

Development of multi-scale computational frameworks to solve fusion materials science challenges

Over the past two decades, the US-DOE has funded multiple projects that rely on high-performance computing and exascale computing platforms to accelerate scientific discoveries and address grand scientific challenges, such as harnessing fusion energy. In this article, we review in detail one of these efforts aimed at enhancing our capability to model plasma-facing materials subject to plasma and high-energy ion/neutron irradiation. The plasma surface interactions project has built a multi-scale modeling framework where many of the plasma- and high-energy ion/neutron irradiation-induced effects occurring in tungsten are explored. Here, this knowledge is used to develop atomistically-informed, high-fidelity continuum and meso-scale models that can be validated against experiments. We review the developments within this project, with attention to experimental validation efforts, and specifically highlight activities associated with: helium bubble bursting and equation of state, and hydrogen-helium interactions in tungsten; atomistically-informed model development for beryllium-tungsten material mixing; coupling of scrape-of-layer plasma, sheath and material models; and coupling of stochastic cluster-dynamics and crystal plasticity models to address radiation effects in tungsten under stress. Finally, we present how the project is preparing for future computational architectures, for instance through efforts to adapt atomistic methods to exascale computing.

36 MATERIALS SCIENCE↗

The role of cellular structure, non-equilibrium eutectic phases and precipitates on quasi-static strengthening mechanisms of as-built AlSi10Mg parts 3D printed via laser powder bed fusion

The quasi-static loading strengthening mechanism in the as-built state of an AlSi10Mg alloy 3D-printed via Laser Powder Bed Fusion (LPBF) was thoroughly identified and quantified using state-of-the-art electron microscopy and synchrotron X-ray diffraction techniques. The yield strength was comprehensively modelled through an in-depth characterization and quantification of the microstructural features as well as their effective volumes for strengthening. In particular, the non-equilibrium eutectic network was characterized with a two-fold structure: cell boundary particles as well as intracellular lamellar/fibrous networks, each consisting of discrete phases exhibiting a thru-thickness compositional gradient, a semi-coherent interface with the matrix and an abundance of crystal defects such as nano-sized sub-grains, microstrains and stacking faults. Further, these altogether made the eutectic phase the most potent contributor to the yield strength accounting for ~30–40% of the estimated value (i.e., cell boundary and eutectic network strengthening combined). Precipitates strengthening was identified as the second most potent mechanism via a shearing process only. Moreover, the presented methodology was able to capture the effect of LPBF processing variables on the individual strengthening contributions, e.g., the effect of a lower laser scanning speed on increasing the cell size as well as the mean precipitate size, which are shown to exhibit opposing impacts on strengthening.

36 MATERIALS SCIENCE↗

Understanding process-microstructure-property relationships in laser powder bed fusion of non-spherical Ti-6Al-4V powder

Powder feedstock is a major cost driver in metal additive manufacturing (AM). Replacing the spherical powder with the cost-efficient non-spherical one can reduce the feedstock cost up to 50% and attract more interest to adopt AM in production and new alloy development. Here, for this paper, a comprehensive study was conducted to understand process-microstructure-property relationships in laser powder bed fusion of hydride-dehydride Ti-6Al-4V powder. We demonstrated that variation of laser scan speed had a significant impact on the grain structure, pore evolution and properties compared to laser power. Dynamic X-ray radiography showed that with decreasing scan speed at a constant laser power, a transition from conduction to keyhole mode laser processing occurred, in which a deeper melt pool at lower scan speed intensified texture. In other words, an increase in laser scan speed resulted in formation of the refined prior β grains with shape factor of ~5, lowering the anisotropy. Furthermore, the degree of variant selection was evaluated based on the analyzed texture as a function of laser power and scan speed. With increasing laser scan speed, the dominant α/α boundary type was altered from type 2 to 4 and the degree of variant selection was noticeably decreased. On the other hand, increasing laser power left the morphology of prior β grains, their size, and the dominant α/α boundary (type 4) unchanged, while the texture and anisotropy were intensified, and the degree of variant selection was slightly decreased. Finally, dependency of surface roughness and microhardness were discussed as a function of laser processing parameters.

variant selection↗

The influence of chemical short-range order on the nanoindentation properties of high-entropy alloys prepared via laser powder bed fusion

Chemical short-range order (CSRO) plays an instrumental role in determining the mechanical properties of high-entropy alloys (HEAs). Current methods for controlling CSRO mainly focus on cast HEAs, which can not solve the problem of grain coarsening caused by homogenization treatments. Laser Powder Bed Fusion (LPBF), which has extremely high cooling rates, can suppress compositional segregation, refine grain structures, and achieve low CSRO. This offers a promising avenue for quantitatively controlling CSRO without the need for homogenization treatments. In this study, we investigate the CSRO of HEAs fabricated via LPBF and elucidate their influence on nanoindentation behavior. The results show that, at the low cooling rate, the average size of CSRO is 0.66 nm and they occupy 2.8% of the cross-sectional area, while at high cooling rate, the corresponding values are 0.92 nm and 9.9%, respectively, both of which are significantly smaller than those of cast HEAs. Furthermore, by analyzing samples with different CSROs, we observe that the hardness increases and then decreases with the increase of CSRO, primarily due to the preferential formation of dislocations in regions enriched with Cr-Mn-Ni. With the improvement of CSRO, both the size and quantity of Cr-Mn-Ni rich region gradually increased; subsequently, as multiple Cr-Mn-Ni rich regions tend to merge into one during the CSRO improvement, the size of the Cr-Mn-Ni rich region continued to increase while the quantity gradually decreased; when the size of the Cr-Mn-Ni rich region is moderate and widely dispersed, the dislocation density is higher with much more uniform distributions, which favorably improves nanoindentation hardness.

36 MATERIALS SCIENCE↗

Chemistry effects on ODS steel consolidated via laser powder bed fusion from GARS powder

Oxide Dispersion Strengthened (ODS) steels are promising candidate alloys for structural and cladding applications in extreme environments. They contain a high density of nanoscale oxides for high temperature mechanical strength and radiation resistance. In this work, gas atomization reaction synthesis (GARS) was used to produce powders that were used for additive manufacturing (AM) Laser Powder Bed Fusion consolidation of ODS steels, in order to skip the traditional mechanical alloying of blended yttria and alloy powders. Powder containing iron, chromium, and tungsten with varying amounts of yttrium, titanium, oxygen and zirconium were used to produce ODS steel samples. AM consolidated specimens and powder samples were characterized with transmission electron microscopy. TEM imaging, diffraction patterns, and energy dispersive X-ray spectroscopy (EDS) was used to identify phases present before and after consolidation across chemistries. The effect of the controlled oxygen input (from GARS) and the oxide-forming additions (Y, Ti, Zr) on precipitate size distribution and composition is substantiated and discussed.

36 MATERIALS SCIENCE↗

Fracture characteristics and heat treatment of laser powder bed fusion additively manufactured GRCop-84 copper

Laser Powder Bed Fusion (LPBF) of Glenn Research Copper 84 (GRCop-84), a Cr 2 Nb (8 at. % Cr, 4 at. % Nb) precipitation hardened alloy, produces a fully dense high conductivity alloy with a yield strength of 500 MPa and ultimate tensile strength (UTS) of 740 MPa, superior to other competing copper alloys, and 20% elongation at fracture for material stressed perpendicular to the build direction. The high thermal stability of the Cr 2 Nb precipitate in the copper matrix reduces coarsening and maintains a 300 MPa yield, 520 MPa UTS and 26% elongation after a 900 °C, 5-h heat treatment, while a 3 h 450 °C heat treatment increases yield to 810 MPa, UTS to 970 MPa with 9% elongation at fracture, for samples stressed perpendicular to the build direction. Tensile strength anisotropy based on print direction was attributed to internal stress and columnar grain formation. Void nucleation during tensile fracture was initiated by brittle fracture of precipitate particles within the copper matrix. Fracture cusps contain matching precipitate fragment geometry on opposing sides located near the cusp center in at least 80% of fracture cusps. An optimal precipitate size of 100 nm is predicted for maximum tensile strength from precipitates on fracture surfaces, while tensile testing with varying heat treatments shows maximum strength with 100 nm and smaller precipitates. Cr2Nb precipitates are shown to transition between polycrystalline and monocrystalline structures at high temperature.

36 MATERIALS SCIENCE↗

Characterization of multi-material 316L-Hastelloy X fabricated via laser powder-bed fusion

The aim of this work is to provide firsthand knowledge of 316 L stainless steel (316 L) and Hastelloy X (HX) multi-material processing via laser powder bed fusion (PBF). Specifically, microstructure of the interface is studied using scanning electron microscopy (SEM), energy-dispersive X-ray spectroscopy (EDS), and X-ray diffraction (XRD). Surface metrology is performed to characterize the resulting surface roughness at the interface followed by tensile and flexural testing of multi-material samples to characterize the mechanical properties of the interfaces. Results showed that use of proper process parameters for each individual material led to formation of a compositional gradient at the interface that stretched for 240 μm (10–12 layers) with no evidence of cracking or porosity. The interface exhibited higher surface roughness compared to 316 L or HX as measured by arithmetic mean height, Sa, and maximum valley depth, Sv, parameters. During tensile testing, samples failed in the 316 L region away from the interface, with comparable yield strength, ultimate strength, and ductility. Finally, it was concluded that the “naturally” formed interface created a compositional gradient which was defect free due to similar values of coefficient of thermal expansion, input energy density, and different Marangoni numbers of the materials.

316L stainless Steel↗

Interplay of strain and phase evolution of laser powder bed fusion Ti–6Al–4V

While additive manufacturing (AM) provides a method of producing geometrically complex and highly detailed structures, the generation of residual strain in AM processes like laser powder bed fusion (L-PBF) can negatively impact performance-enabling properties. In applications such as orthopedic implants, specific performance windows require optimized microstructures in order to obtain desirable properties from multi-phase alloys like Ti–6Al–4V. This research aims to quantify the microscale origins of strain in L-PBF manufactured Ti–6Al–4V by understanding how strain is distributed at the grain and sub-grain scale, the interplay between phase evolution and strain, and examining post-processing strain relief strategies to control these features. Model spinal cage implants were manufactured from Ti–6Al–4V powder via L-PBF and then subjected to strain relieving heat treatment cycles above and below the Ti–6Al–4V β transus as a function of time and cooling rate. Residual strain was then studied via high resolution electron backscatter diffraction (HR-EBSD), and 2D strain maps with sub-micron resolution were generated for each post-processing state. It was found that macroscale thermal strains decreased with heat treatment time, but additional contributions from phase stabilizing residual strains retained primarily in the α' grains as lattice distortive strain remained. Additionally, the retention of β phase significantly changed the strain and dislocation distribution while reducing overall residual strain. In conclusion, these results were validated and reinforced with 3D mesoscopic micromechanical modeling of strain behavior across simulated microstructures, confirming that the local lattice dilation of α’ martensite is a primary contributor of microscale strain generation and retention in L-PBF Ti–6Al–4V.

36 MATERIALS SCIENCE↗

Influence of post deposition annealing on the microstructural evolution and tensile behavior of austenitic stainless-steel alloy 709 made by laser powder bed fusion

Structural materials used in the next generation nuclear reactors or other advanced energy systems are often required to withstand higher operating temperatures for a longer service life. Alloy 709 (A709), a Nb-containing and N-stabilized Fe-25Ni-20Cr austenitic stainless steel, has been recommended for high-temperature reactor constructions due to the better performance over the baseline Type 316H stainless steel. Here, in the current manuscript, for the first time, the microstructure evolution and tensile behavior of an A709 made by laser powder bed fusion (LPBF) is discussed. The as deposited and heat treated LPBF alloys are compared with a reference wrought alloy. Owing to the chemical segregation and a higher number of dislocations, the LPBF materials show a significantly higher density of precipitates formed during high temperature treatments when compared to the wrought samples. This is reflected when looking at the tensile properties, both at room and elevated temperatures, where LPBF samples show higher strengths compared to wrought materials.

36 MATERIALS SCIENCE↗