Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “CORROSION CONTROL”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 1,315 records · Page 73

Consequence Analysis of Residual Water in a Storage Canister (Preliminary Report)

The objective of this work is to examine the consequences of a residual water on change in condition of cladding and SNF during dry storage. Small amounts of residual water may remain in SNF dry storage canisters after the fuel assemblies are transferred to the canister in the spent fuel pool (SFP), the canister is removed from the SFP and drained or pumped, vacuum dried in several pressure reducing steps, and backfilled with helium. This residual water from incomplete drying could degrade fuel rod cladding, oxidize exposed fuel pellets, and cause cladding failure resulting in SNF fines’ release in canister cavity. If residual water content is high enough, it could corrode internal components inside the canister, e.g., fuel basket, and neutron absorber plates, but CNWRA work indicated that corrosion of the internal component is expected to be negligible even with 55 moles of residual water. Considering this, focus of this work to determine partitioning of residual water towards fuel and cladding oxidation. Residual water will decompose by radiolysis and create reactive oxygen species, which, at sufficient high temperatures will oxidize cladding, and UO 2 exposed by clad breaches. If a significant fraction of UO 2 in a fuel rod is oxidized to U 3 O 8 , swelling of the fuel pellets will rupture the cladding and release fuel particles, contaminating the inside of the canister and complicating retrieval of fuel assemblies, transport and ultimate disposal. The report describes an evaluation of the potential cladding and exposed SNF pellets due to residual water. An integrated quantitative approach was used to estimate the effects. The approach consisted of (i) the evolution of environmental conditions, i.e., temperature and radiation field, in the cask, (ii) the physicochemical processes that affect degradation of the materials within the cask, and (iii) the potential damage states that may result from these conditions and processes. The assessment considers the following set of cask environmental conditions: (i) the quantity of residual water after drying, (ii) internal temperature fields and their intensity decrease over time, and (iii) the strength of the internal radiation field. The quantity of residual water will affect the mass of cladding, SNF, and other components that are degraded by oxidation. Temperature controls the rate of the oxidation reactions, the phase composition of water, and, to a lesser extent, the rate at which water vapor is radiolyzed. The strength of the radiation field controls the radiolysis rate of residual water. These processes, i.e., time evolution of temperature fields and their effects on radiolysis of residual water, fuel and cladding oxidations, were modeled using the integrated approach.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

FEASIBILITY EVALUATION AND RETROFIT PLAN FOR COLD CRUCIBLE INDUCTION MELTER DEPLOYMENT IN THE DEFENSE WASTE PROCESSING FACILITY AT SAVANNAH RIVER SITE - 8118

Cold crucible induction melters (CCIM) have been proposed as an alternative technology for waste glass melting at the Defense Waste Processing Facility (DWPF) at Savannah River Site (SRS) as well as for other waste vitrification facilities. Proponents of this technology cite high temperature operation, high tolerance for noble metals and aluminum, high waste loading, high throughput capacity, and low equipment cost as the advantages over existing Joule Heated Melter (JHM) technology. This paper describes the CCIM technology and identifies technical challenges that must be addressed in order to implement CCIMs in the DWPF. The CCIM uses induction heating to maintain molten glass at high temperature. A water-cooled helical induction coil is connected to an AC current supply, typically operating at frequencies from 100 KHz to 5 MHz. The oscillating magnetic field generated by the oscillating current flow through the coil induces eddy currents in conductive materials within the coil. Those oscillating eddy currents, in turn, generate heat in the material. In the CCIM, the induction coil surrounds a 'Cold Crucible' which is formed by metal tubes, typically copper or stainless steel. The tubes are constructed such that the magnetic field does not couple with the crucible. Therefore, the field generated by the induction coil couples primarily with the conductive medium (hot glass) within. The crucible tubes are water cooled to maintain their temperature between 100 C to 200 C so that a protective layer of molten glass and/or batch material, referred to as a 'skull', forms between them and the hot, corrosive melt. Because the protective skull is the only material directly in contact with the molten glass, the CCIM doesn't have the temperature limitations of traditional refractory lined Joule heated melters. It can be operated at melt temperatures in excess of 2000 C, allowing processing of high waste loading batches and difficult-to-melt compounds. The CCIM is poured through a bottom drain, typically through a water-cooled slide valve that starts and stops the pour stream. To promote uniform temperature distribution and increase heat transfer to the slurry fed High Level Waste (HLW) sludge, the CCIM may be equipped with bubblers and/or water cooled mechanical agitators. The DWPF could benefit from use of CCIM technology, especially in light of our latest projections of waste volume to be vitrified. Increased waste loading and increased throughput could result in substantial life cycle cost reduction. In order to significantly surpass the waste throughput capability of the currently installed Joule Heated Melter, it may be necessary to install two 950 mm CCIMs in the DWPF Melt Cell. A cursory evaluation of system design requirements and modifications to the facility that may be required to support installation and operation of two 950 mm CCIMs was performed. Based on this evaluation, it appears technically feasible to position two CCIMs in the Melt Cell of the DWPF within the existing footprint of the current melter. Interfaces with support systems and controls including Melter Feed, Power, Melter Cooling Water, Melter Off-gas, and Canister Operations must be designed to support dual CCIM operations.

36 MATERIALS SCIENCE↗

Formation of Aluminide Coatings on Fe-Based Alloys by Chemical Vapor Deposition

Aluminide and Al-containing coatings were synthesized on commercial ferritic (P91) and austenitic (304L) alloys via a laboratory chemical vapor deposition (CVD) procedure for rigorous control over coating composition, purity and microstructure. The effect of the CVD aluminizing parameters such as temperature, Al activity, and post-aluminizing anneal on coating growth was investigated. Two procedures involving different Al activities were employed with and without including Cr-Al pellets in the CVD reactor to produce coatings with suitable thickness and composition for coating performance evaluation. The phase constitution of the as-synthesized coatings was assessed with the aid of a combination of X-ray diffraction, electron probe microanalysis, and existing phase diagrams. The mechanisms of formation of these CVD coatings on the Fe-based alloys are discussed, and compared with nickel aluminide coatings on Ni-base superalloys. In addition, Cr-Al pellets were replaced with Fe-Al metals in some aluminizing process runs and similar coatings were achieved.

36 MATERIALS SCIENCE↗

Overview of Quantum Sensing Materials and Techniques for Energy Sector Applications

The energy sector has become increasingly dependent upon highly sensitive sensing devices for a wide range of applications. Variables such as temperature, pH, electromagnetic fields, ions, and pressure must be measured with high precision, often in harsh conditions (e.g. highly corrosive environments due to high temperature, pressure and humidity). These sensors are deployed in infrastructure such as transformers, pipelines, mines, nuclear power plants, and other areas to ensure safe operating conditions and uninterrupted, optimized service. Moreover, new opportunities for sensors have emerged due to the expansion of smart grids/meters, driverless vehicles, and the discovery of new oil, gas, and critical mineral deposits. The continued maturation of quantum sensing technologies offers exciting opportunities for quantum-enhanced measurements within the energy sector that may provide significant improvements in sensitivity beyond the classical limit. Here, an overview of established and emerging quantum materials for sensing applications will be provided, from trapped ions to color centers in diamond and silicon carbide. Associated quantum sensing methods for these materials will be discussed, with an emphasis on platforms that are nearing commercial viability. Specific application opportunities within the energy sector for quantum sensors will then be analyzed, including oil/gas discovery, greenhouse gas emission monitoring, pH and ion sensing, current measurement in electric vehicle batteries, and quantum-enhanced spectroscopy. Remaining barriers, such as quantum sensor platform miniaturization and ruggedization, will also be analyzed. A specific project at the National Energy Technology Laboratory involving the functionalization of qubits using metal-organic frameworks for enhanced quantum sensing will also be highlighted. Here, nitrogen vacancy centers (NV) in nanodiamonds, a commercially available qubit with long coherence times and utilizable quantum properties at room temperature, are encapsulated in a controlled way using the metal-organic framework ZIF-8. The ZIF-8 provides a well-defined, porous scaffold that can be controlled to promote the selective uptake of specific target analytes, such as gas molecules or ions. The quantum sensing performance of this composite material is either preserved or enhanced following ZIF-8 encapsulation; the optically detected magnetic resonance response of the NV nanodiamonds with and without the ZIF-8 coating are identical, while the ZIF-8 coating increases the longitudinal spin relaxation lifetime (T1) of the NV centers, an important parameter for spin relaxometry-based quantum sensing experiments. Taken together, these results demonstrate the importance of qubit functionalization as a crucial step for rationally designing high performance quantum sensors.

Crawford, Scott↗

Quantification of Aerosol Transmission through Stress Corrosion Crack-Like Geometries

The formation of a stress corrosion crack (SCC) in the canister wall of a dry cask storage system (DCSS) has been identified as a potential issue for the long-term storage of spent nuclear fuel. The presence of an SCC in a storage system could represent a through-wall flow path from the canister interior to the environment. Modern, vertical DCSSs are of particular interest due to the commercial practice of using more significant backfill pressures in the canister, up to approximately 800 kPa. This pressure differential offers a relatively high driving potential for blowdown of any particulates that might be present in the canister. In this study, the rates of gas flow and aerosol transmission of a spent fuel surrogate through an engineered microchannel with dimensions representative of an SCC were evaluated experimentally using coupled mass flow and aerosol analyzers. The microchannel was formed by mating two gage blocks with a linearly tapering slot orifice nominally 13 μm (0.005 in.) tall on the upstream side and 25 μm (0.0010 in.) tall on the downstream side. The orifice is 12.7 mm (0.500 in.) wide by 8.86 mm (0.349 in.) long (flow length). Surrogate aerosols of cerium oxide, CeO 2 , were seeded and mixed with either helium or air inside a pressurized tank. The aerosol characteristics were measured immediately upstream and downstream of the simulated SCC at elevated and ambient pressures, respectively. These data sets are intended to add to previous testing that characterized SCCs under well-controlled boundary conditions through the inclusion of testing improvements that establish initial conditions in a more consistent way. These ongoing testing efforts are focused on understanding the evolution in both size and quantity of a hypothetical release of aerosolized spent fuel particles from failed fuel to the canister interior and ultimately through an SCC.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Testing of Microchannels and Lab-Grown Stress Corrosion Cracks for Quantification of Aerosol Transmission

The formation of a stress corrosion crack (SCC) in the canister wall of a dry cask storage system (DCSS) has been identified as a potential issue for the long-term storage of spent nuclear fuel. The presence of an SCC in a storage system could represent a through-wall flow path from the canister interior to the environment. Modern, vertical DCSSs are of particular interest due to the commercial practice of using higher backfill pressures in the canister, up to approximately 800 kPa, compared to their horizontal counterparts. This pressure differential offers a relatively high driving potential for blowdown of any particulates that might be present in the canister. In this study, the rates of gas flow and aerosol transmission of a spent fuel surrogate through an engineered microchannel with dimensions representative of an SCC were evaluated experimentally using coupled mass flow and aerosol analyzers. The microchannel was formed by mating two gage blocks with a linearly tapering slot orifice nominally 13 μm (0.005 in.) tall on the upstream side and 25 μm (0.0010 in.) tall on the downstream side. The orifice is 12.7 mm (0.500 in.) wide by 8.86 mm (0.349 in.) long (flow length). Surrogate aerosols of cerium oxide, CeO 2 , were seeded and mixed with either helium or air inside a pressurized tank. The aerosol characteristics were measured immediately upstream and downstream of the simulated SCC at elevated and ambient pressures, respectively. These data sets are intended to add to previous testing that characterized SCCs under well-controlled boundary conditions through the inclusion of testing improvements that establish initial conditions in a more consistent way. While the engineered microchannel has dimensions similar to actual SCCs, it does not reproduce the tortuous path the aerosol laden flow would have to traverse for eventual transmission. SCCs can be rapidly grown in a laboratory setting given the right conditions, and initial characterization and clean-flow testing has begun on lab grown crack samples provided to Sandia National Laboratories (SNL). Many such samples are required to produce statistically relevant transmission results, and SNL is developing a procedure to produce samples in welded steel plates. These ongoing testing efforts are focused on understanding the evolution in both size and quantity of a hypothetical release of aerosolized spent fuel particles from failed fuel to the canister interior and ultimately through an SCC.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Continued Investigations of Respirable Release Fractions for Stress Corrosion Crack-Like Geometries

The formation of a stress corrosion crack (SCC) in the canister wall of a dry cask storage system (DCSS) has been identified as a potential issue for the long-term storage of spent nuclear fuel. The presence of an SCC in a storage system could represent a through-wall flow path from the canister interior to the environment. Modern, vertical DCSSs are of particular interest due to the commercial practice of using relatively high backfill pressures (up to approximately 800 kPa) in the canister to enhance internal natural convection. This pressure differential offers a comparatively high driving potential for blowdown of any particulates that might be present in the canister. In this study, the rates of gas flow and aerosol transmission of a spent fuel surrogate through an engineered microchannel with dimensions representative of an SCC were evaluated experimentally using coupled mass flow and aerosol analyzers. The microchannel was formed by mating two gage blocks with a linearly tapering slot orifice nominally 13 μm (0.005 in.) tall on the upstream side and 25 μm (0.0010 in.) tall on the downstream side. The orifice is 12.7 mm (0.500 in.) wide by 8.89 mm (0.350 in.) long (flow length). Surrogate aerosols of cerium oxide, CeO 2 , were seeded and mixed with either helium or air inside a pressurized tank. The aerosol characteristics were measured immediately upstream and downstream of the simulated SCC at elevated and ambient pressures, respectively. These data sets are intended to demonstrate a new capability to characterize SCCs under well-controlled boundary conditions. Modeling efforts were also initiated that evaluate the depletion of aerosols in a commercial dry storage canister. These preliminary modeling and ongoing testing efforts are focused on understanding the evolution in both size and quantity of a hypothetical release of aerosolized spent fuel particles from failed fuel to the canister interior and ultimately through an SCC.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Modification of Ni-20Cr corrosion dealloying behavior in molten fluorides via cold work induced plastic deformation

The corrosion dealloying behavior of cold-worked (CW) Ni20Cr alloy (wt%) was studied in molten LiF-NaF-KF (or FLiNaK) salts at 600 °C, equal to a homologous temperature (TH) of 0.52. Alloys were cold-rolled to achieve reductions of thickness of 10%, 30%, and 50% introducing plastic deformation and a high density of dislocations. Potentiostatic holds (Eapplied) were applied in two different electrode potential regimes. At 1.75VK+/K$${\text{V}}_{{\text{K}}^{+}/{\text{K}}}$$, Cr dealloying to Cr(II) and Cr(III) is predominant, while at 1.90 VK+/K$${\text{V}}_{{\text{K}}^{+}/{\text{K}}}$$, both Ni and Cr are oxidized in molten FLiNaK at 600 °C. In these potential regimes, dealloyed Ni20Cr displayed bicontinuous porosity within the grain interior and at grain boundaries, driven by the high driving force for Cr dissolution and sustained by defect mediated outward solid state diffusion of Cr in parallel with surface diffusion of Ni. The bicontinuous porous structure developed was observed to undergo further coarsening and densification of the Ni-rich ligaments at a higher electrode potential. The main effect of CW observed is the introduction of plastic deformation and dislocation substructures that serve as short-circuit paths for Cr solid state diffusion to surfaces exposed to FLiNaK. This modified the evolution of the bicontinuous porous structure which increased with CW substantially. Kinetic analysis reveals that the Cr dealloying at +1.75 VK+/K$${\text{V}}_{{\text{K}}^{+}/{\text{K}}}$$ and 1.90 VK+/K$${\text{V}}_{{\text{K}}^{+}/{\text{K}}}$$ is initially charge transfer controlled, except for the 50% CW condition at 1.90 VK+/K$${\text{V}}_{{\text{K}}^{+}/{\text{K}}}$$, where the process becomes limited by slow Cr defect mediated bulk diffusion. The rate determining factors are explored and compared to experimental results.

Chan, Ho Lun↗

SLUDGE BATCH 5 VARIABILITY STUDY WITH FRIT 418

The Defense Waste Processing Facility (DWPF) is preparing to initiate processing Sludge Batch 5 (SB5) in early FY 2009. In support of the upcoming processing, the Savannah River National Laboratory (SRNL) provided a recommendation to utilize Frit 418 as a transitional frit to initiate processing of SB5. This recommendation was based on the results of assessments on the compositional projections for SB5 available at that time from both the Liquid Waste Organization (LWO) and SRNL (using a model-based approach). To support qualification of the Frit 418-SB5 system, SRNL executed a variability study to assess the acceptability of the Frit 418-SB5 glasses with respect to durability and the applicability of the current durability models. Twenty one glasses were selected for the variability study based on the available SB5 projections primarily spanning a waste loading (WL) range of 25-37%. In order to account for the addition of caustic to Tank 40, which occurred in July 2008, 3 wt% Na2O was added to the original Tank 40 heel projections. The addition of the Actinide Removal Process (ARP) stream to the blend composition was also included. Two of the glasses were fabricated at 25% and 28% WL in order to challenge the homogeneity constraint of the Product Composition Control System (PCCS) for SB5 coupled operations. These twenty one glasses were fabricated and characterized using chemical composition analysis, X-ray Diffraction (XRD) and the Product Consistency Test (PCT). The results of this study indicate that Frit 418 is a viable option for sludge-only and coupled operations. The addition of ARP did not have any negative impacts on the acceptability and predictability of the variability study glasses. Based on the measured PCT response, all of the glasses were acceptable as compared to the Environmental Assessment (EA) reference glass regardless of the thermal history and were also predictable using the current PCCS model for durability. The homogeneity constraint can be ignored for SB5 for coupled operations (based on the Appendix J compositional information), as both of the glasses targeting lower WLs (SB5VS-18 and SB5VS-19) had durabilities that were acceptable with respect to the reference EA glass.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

An Electrochemical, Microtopographical and Ambient Pressure X-Ray Photoelectron Spectroscopic Investigation of Si/TiO 2 /Ni/Electrolyte Interfaces

The electrical and spectroscopic properties of the TiO 2 /Ni protection layer system, which enables stabilization of otherwise corroding photoanodes, have been investigated in contact with electrolyte solutions by scanning-probe microscopy, electrochemistry and in-situ ambient pressure X-ray photoelectron spectroscopy (AP-XPS). Specifically, the energy-band relations of the p + -Si/ALD-TiO 2 /Ni interface have been determined for a selected range of Ni thicknesses. AP-XPS measurements using tender X-rays were performed in a three-electrode electrochemical arrangement under potentiostatic control to obtain information from the semiconductor near-surface region, the electrochemical double layer (ECDL) and the electrolyte beyond the ECDL. The degree of conductivity depended on the chemical state of the Ni on the TiO 2 surface. At low loadings of Ni, the Ni was present primarily as an oxide layer and the samples were not conductive, although the TiO 2 XPS core levels nonetheless displayed behavior indicative of a metal-electrolyte junction. In contrast, as the Ni thickness increased, the Ni phase was primarily metallic and the electrochemical behavior became highly conductive, with the AP-XPS data indicative of a metal-electrolyte junction. Electrochemical and microtopographical methods have been employed to better define the nature of the TiO 2 /Ni electrodes and to contextualize the AP-XPS results.

36 MATERIALS SCIENCE↗

Joining Techniques for Novel Metal Polymer Hybrid Heat Exchangers

In the United States, over 50% of the unrecovered energy from industrial processes is in the form of low-grade heat (< 220°C). Materials and maintenance costs of common heat exchangers are typically too high to justify their usage. Polymers, though more affordable, are usually unsuitable for HX applications due to their low thermal conductivity (~0.2 W/mK). Here, we show that metal-polymer hybrids may be attractive from both performance and cost perspectives. The use of polymers further increases the resistance to corrosion by sulfuric and carbonic acids often present in flue gases. An ongoing work explores different configurations of layered polyimide-copper macroscale hybrids for heat exchanger applications using numerical simulations. This paper explores a manufacturing pathway for producing such layered hybrid tubes that involves directly rolling and bonding tapes made of polymer and copper foil into tubes. A critical problem in the fabrication process is the bonding of metal and polymers. We explore approaches involving adhesives (epoxy, acrylic and silicone) for metal/polymer interfaces and direct welding (ultrasonic) for metal/metal interfaces that can be integrated into the manufacturing process. We report characterizations of the thermomechanical properties of these joining processes. This work paves the way for realizing cost-effective manufacturing of heat exchangers for low grade waste heat recovery.

Kuntumalla, Gowtham↗

Dynamic Binary Complexes (DBC) as Super-Adjustable Viscosity Modifiers for Hydraulic Fracturing Fluids

In the preceding project year two, we refined three DBC formulations from a selection of over 50 different chemistries. The optimization study primarily encompassed testing for (i) reversibility extent, (ii) performance in the presence of chemical additives, (iii) adhesion and friction behavior during displacement in wellbores and pipelines, (iv) corrosion protection performance, and (v) injection performance with model fracture systems at the laboratory scale. Highly promising results obtained from all these tests signify the significant potential of DBCs in enhancing hydrocarbon recovery from unconventional reservoirs. The primary activities in the third project year included publishing experimental findings across multiple articles and conducting outreach initiatives. Throughout the year, we undertook tasks such as replicating experimental results, further optimizing various formulations and their associated experimental sets, and conducting additional tests to address missing components based on reviewer feedback and suggestions. We also explored the surfactant and friction-reduction aspects of selected formulations through drag reduction tests. In addition, we constructed an improved fracturing performance setup and performed flow injection tests. The specific DBC formulations focused on during this project period were A8/B1, A12/B5, and A10/B12. We also obtained results for additional DBC formulations and a select few commercial fracturing fluids for the purpose of comparison. Within the project's scope, we aim to enhance the experimental findings with the development of various models. The first two years focused on two key aspects: (i) the creation of a high-fidelity hydraulic fracturing model for non-Newtonian fluids to gain insights into the implementation of DBC fluids in fracking environments, and (ii) the development of a multiphase flow simulator for estimating total production, fluid saturation in the reservoir, and the creation of a fracture propagation model and kinetic Monte Carlo (kMC) models for diverse applications. In the third year, we delved into the fundamental nanostructural properties of DBCs, exploring aspects such as material chemistry, pH tunability, and control of DBC formation and stability. Subsequently, in the extension year, we conducted a systematic investigation of various building blocks containing primary, secondary, and tertiary amine functional groups to understand their impact on rheological and viscoelastic properties. Furthermore, we explored a Dissipative Particle Dynamics (DPD) model to simulate self-assembly processes with precision, creating a high-fidelity representation of relevant nanostructures. The tasks performed this year with the significant results obtained have been discussed in Section 2.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Mechanistic Studies Of Combustion And Structure Formation During Combustion Synthesis Of Advanced Materials: Phase Separation Mechanism For Bio-Alloys

Among all implant materials, Co-Cr-Mo alloys demonstrate perhaps the most useful balance of resistance to corrosion, fatigue and wear, along with strength and biocompatibility [1]. Currently, these widely used alloys are produced by conventional furnace technology. Owing to high melting points of the main alloy elements (e.g. Tm.p.(Co) ~1768 K), high-temperature furnaces and long process times (several hours) are required. Therefore, attempts to develop more efficient and flexible methods for production of such alloys with superior properties are of great interest. The synthesis of materials using combustion phenomena is an advanced approach in powder metallurgy [2]. The process is characterized by unique conditions involving extremely fast heating rates (up to 10(exp 6 K/s), high temperatures (up to 3500 K), and short reaction times (on the order of seconds). As a result, combustion synthesis (CS) offers several attractive advantages over conventional metallurgical processing and alloy development technologies. The foremost is that solely the heat of chemical reaction (instead of an external source) supplies the energy for the synthesis. Also, simple equipment, rather than energy-intensive high-temperature furnaces, is sufficient. This work was devoted to experiments on CS of Co-based alloys by utilizing thermite (metal oxide-reducing metal) reactions, where phase separation subsequently produces materials with tailored compositions and properties. Owing to high reaction exothermicity, the CS process results in a significant increase of temperature (up to 3000 C), which is higher than melting points of all products. Since the products differ in density, phase separation may be a gravitydriven process: the heavy (metallic phase) settles while the light (slag) phase floats. The goal was to determine if buoyancy is indeed the major mechanism that controls phase segregation.

Varma, A.↗

PREPARATION AND TESTING OF CORROSIONAND SPALLATION-RESISTANT COATINGS

This Energy & Environmental Research Center (EERC) project is designed to determine if plating APMT®, a specific highly oxidation-resistant oxide dispersion-strengthened FeCrAl alloy made by Kanthal, onto nickel-based superalloy turbine parts is a viable method for substantially improving the lifetimes and maximum use temperatures of the parts. The method for joining the APMT plate to the superalloys is called evaporative metal bonding and involves placing a thin foil of zinc (Zn) between the plate and the superalloy, clamping them together, and heating in an atmosphere-controlled furnace. Upon heating, the Zn melts and dissolves the oxide skins of the alloys at the bond line, allowing the two alloys to diffuse into each other. The Zn then diffuses through the alloys and evaporates from their surfaces. Laboratory testing to determine the diffusion rate of Zn through the alloys has been completed. However, an analytical solution does not exist to model the diffusion of zinc through the alloys. For this reason, a finite difference algorithm using MATLAB was developed. It makes use of the hopscotch algorithm. The model allows the user to specify the dimensions of the metal parts, the Zn concentration at the bondline, the mesh size, time step, and Zn diffusivity. The experimentally measured values of diffusivity for Zn in APMT and Rene 80/CM 247LC are approximately 2.7 × 10-12 and 4 × 10-14 m2/s, respectively. While the qualitative behavior of the model appears correct, a comparison of the diffusion predictions with the experimental results from earlier in the project indicates that the expected Zn concentration is significantly higher than that measured experimentally. The difference depends on the assumed initial concentration, which is difficult to quantify exactly under experimental conditions for t = 0. In addition to the diffusion work, the coefficients of thermal expansions were determined for each of the alloys as a function of temperature. This information has been entered into a finite element model using ANSYS so that appropriate force-applying structures can be designed for use in joining structures composed of APMT and the nickel alloys. Finite element modeling has been performed to finalize the fabrication geometry for the corrosion-testing phase. The addition of another bolt increases stress uniformity away from the region where the clamping is applied. It appears that a bolt spacing of approximately 25 mm in each jig is appropriate. This will allow the fabrication of 50-mm-wide sections of joints for the corrosion-testing task. Gasifier sampling activities continue to determine what types of trace contaminants may occur in cleaned syngas that could lead to corrosion or deposition in turbines firing coal syngas. The EERC has several pilot-scale gasifiers that are continually used in a variety of test configurations as determined by the needs of the projects that are funding the tests. We are sampling both noncombusted and combusted syngas produced during some of the pilot-scale gasifier tests. This year sampling was performed of both syngas and combusted syngas while the entrained-flow gasifier (EFG) was firing subbituminous coal from the Antelope Mine in Wyoming. Results of scanning electron microscope analyses of the syngas before combustion showed no submicron particles, only flakes of iron oxide that had likely formed on steel surfaces inside the combustor. As shown in the 2013 annual report, soot was also collected from the syngas when the much-lower-temperature fluid-bed gasifier (FBG) was fired, indicating that the much higher temperature of the EFG prevented soot formation. However, particles collected from the combusted syngas consist almost entirely of submicron soot, and little to no vaporized metals made it past the warm-gas filters and scrubbers in the high-temperature EFG system which could then deposit in a turbine system burning a higher hydrogen syngas. These results are consistent with the analyses of the particulates collected from combusted syngas when the lowertemperature FBG system is used.

Electric↗

Decarburization and Carburization Behavior of Grade 91 Steel in Sodium Environments

Two heats of G91 steel have been investigated in sodium at 550-650°C to understand its corrosion behaviour, microstructural evolution, and tensile properties. Sodium exposure tests of subsized tensile and coupon specimens of G91 base metal and weldment were conducted in Argonne’s forced convection sodium materials testing loops. Maximum exposure times of ~39,000 h at 550°C, ~37,000 h at 600°C, and ~20,000 h at 650°C have been achieved, respectively. Thermal aging experiments of G91 steel were conducted in parallel, and the data of the sodium-exposed specimens were compared with the thermal aging data of the same heat to isolate the thermal aging effect from the effect of sodium exposure. It was found that the tensile strength of G91 steel can be reduced by more than 50% after sodium exposures at 650°C. The effect of a sodium environment on tensile properties is largely dependent on the carburization/decarburization behavior of G91 steel exposed to sodium. The carbon concentrations in sodium in Argonne’s SMT-1 and SMT-2 loops were determined by the equilibration method. The carbon activity in sodium was established by equilibrating high-purity nickel in sodium, analyzing the material for carbon, and using the reported data on the carbon solubility for this material. The carbon activity results were combined with the carbon solubility data in sodium to establish the carbon concentration in sodium. The carbon concentrations in the SMT-1 and SMT-2 loop were estimated to be 1.23 and 0.25 ppm, respectively. With this initial success, we will continue to monitor the carbon contents in the two loops to correlate the microstructural and mechanical property changes with the sodium purity. Future experiments will also consider sodium exposure tests in controlled carbon activities. Online monitoring and control of carbon contents in sodium in nuclear reactors would also be of interest. Thermodynamic analysis was conducted to understand the carburization-decarburization behavior of G91 steel exposed to sodium in the SMT-1 and SMT-2 loops. The equilibrium carbon activity in the alloy was evaluated by the thermodynamics of M 23 C 6 carbides. The calculated carburization-decarburization boundary showed that G91 would undergo decarburization at 650°C in the SMT-1 loop and carburization at 600°C in the SMT-2 loop, which is consistent with our findings from the sodium exposure tests. Future work will include thermodynamic analysis of the carbon concentration – activity relationship including the effect of carbide-forming elements, vanadium and niobium in G91 steel. Kinetics of carbon diffusion and the effect on microstructure and mechanical performance under various service conditions will also be investigated. The ultimate goal is to understand the mechanisms and the kinetics of carbon transfer in the sodium-steel system and to provide a basis for predicting the effect of long-term decarburization-carburization process on the integrity of reactor components.

22 GENERAL STUDIES OF NUCLEAR REACTORS↗

High Toughness Cermets for Molten Salt Pumps

Concentrated Solar Power plants using nitrate salts used cantilevered pump designs to avoid use of bearings in the 565°C salt; however, this necessitated the use of a sump that added additional cost, complexity, and thermal losses. Sump systems had their own complications, including risk of flooding the sump due to control issues either with level indicators or failures in the control valve responsible for filling the sump. Long-shafted pumps were developed and tested, and they outline the need to develop journal sleeves and bearings for new salt systems. Based on reports, pumps will need to be a vertical single- or multi-stage type, mounted to the roof of the molten salt tanks. Design and service for molten salt pumps above 550°C is relatively limited, and at temperatures up to 750°C there is no available design or service experience. Long-shaft pumps that extend to the bottom of the thermal energy storage tank will require bearing materials that are suitable to the given salt chemistry. Lubricity of proposed salts is unclear and need to be determined, especially for cold-tank pumps that require multi-stages for lifting the salt to the top of the tower. Materials, design, and maintenance are all major unknowns.

14 SOLAR ENERGY↗

Colloid Rates of Radionuclides in Cooling Water of the 120-GeV Proton Accelerator Facilities at Fermilab - Paper 58

Cooling water systems for high-energy accelerators are typically equipped with a deionizer to keep water pure for accelerator materials and to remove radionuclides for radioactivity control. Although the deionizers are expected to collect the entire radionuclides, more radioactivity than expected remains in the cooling water in typical cooling water operations at J-PARC and the Tsukuba Campus of High Energy Accelerator Research Organization (KEK), Japan. For example, specific activity of {sup 7}Be in the cooling water for magnetic horns at the J-PARC Neutrino Experimental Facility was observed to be comparable to the limit of {sup 7}Be activity for drain (30 Bq/mL) after enough deionization duration. Removing this activity from the cooling water is an important problem that must be solved before the water can be released into the environment. In our previous study, it was found that some radionuclides had weak retention on ion-exchange resins in the cooling water deionizer system for the K2K target and magnetic horns at the 12-GeV proton accelerator in KEK, Japan. Incomplete adsorption in the deionizer was attributed to colloid formation. Therefore, understanding the colloid formation of radionuclides in cooling water is important for understanding the activity remaining in the cooling water. Colloid formation in water under high-intensity radiation fields has been investigated by previous irradiation experiments. Under 120-GeV proton irradiation of Cu foils in water, it was found that the colloid formation rates of Mg, Mn, Co, Ni, and Cu isotopes and those of {sup 7}Be, {sup 24}Na, {sup 42}K, and {sup 43}K were approximately 30% and 1.8-3.9%, respectively. Sc, Cr, and Fe isotopes were missing from the water. In the photon irradiation of water in a Cu tube using Bremsstrahlung from an electron linear accelerator and a {sup 60}Co γ-ray source at Kyoto University Research Reactor Institute, we observed Cu colloid formation in consequence of the corrosion of Cu. It is possible that radionuclides attach to the colloids formed by the corrosion of accelerator materials and pass through the deionizer. To enhance the understanding of the behavior of radionuclides in cooling water in a high-energy accelerator environment, we investigated the colloid formation of radionuclides in cooling waters at the 120-GeV proton accelerator facilities at Fermilab, USA. We have already reported the previous results of specific activities of γemitting radionuclides and {sup 3}H in water samples collected from eight cooling water systems. Following the previous study, this paper is concerned with the measurement of colloid formation rates of radionuclides in cooling waters. (authors)

43 PARTICLE ACCELERATORS↗

Investigations of dual-purpose canister direct disposal feasibility - 15106

Direct disposal of commercial spent nuclear fuel (SNF) in dual-purpose canisters (DPCs) could avoid the cost and complexity of re-packaging spent fuel into smaller purpose-built containers, avoid disposing of the DPC hulls as low-level waste, and potentially decrease worker dose. Technical objectives for disposal are: 1) safety of workers and the public, 2) engineering feasibility; 3) thermal management; and 4) criticality control after permanent closure of a repository. The postclosure safety case for DPC direct disposal would resemble that for any repository-waste isolation would be enhanced by choosing host geology in which radionuclide transport is diffusion dominated, and for which transport properties and pathways are insensitive to the expected temperature history. Containment functions would be assigned to the disposal overpack, and published data show that suitable materials exist for most possible disposal environments. Earlier studies showed that DPC-based waste packages would be only slightly larger and heavier than those proposed for a repository in volcanic tuff. Engineered solutions are available for transporting and emplacing them underground, although some could be the largest of their kind. The cost of DPC direct disposal in various geologic settings has been compared to options involving a change to loading standardized multi-purpose canisters, or continuing to load DPCs and re-packaging all of them for disposal. In general DPC direct disposal would cost tens of billions of dollars less, in packaging and disposal costs. Calculations for emplacement in hard rock and sedimentary rock show that host rock peak temperature targets of 100 to 200 deg.C could be met by managing fuel age and burnup, with repository closure at up to 150 years from reactor discharge. For disposal in salt, DPC-based waste packages could be emplaced at only 50 to 100 years from discharge, depending on burnup. Sedimentary media such as shales pose special challenges especially if they have low thermal conductivity. If backfill is used around DPC-based packages its peak temperature could be 150 to 200 deg.C. Without flooding of waste packages with ground water, criticality can never occur. However, some small number of disposal overpacks could fail within the postclosure performance period due to corrosion or disruptive events. Once flooded, the aluminum-based neutron absorber materials used in most DPCs would readily degrade. Analysis has shown that even without neutron absorbers, virtually all DPCs could be subcritical if flooded with chloride brines such as would occur in a salt repository. The licensing basis for existing DPCs involves criticality analysis that may be conservative compared to fuel that is actually loaded, and the difference provides uncredited reactivity margin. Uncredited margin can offset increases in reactivity associated with flooding and basket degradation. For flooding with fresh water, with loss of neutron absorbers, many DPCs have been shown to be subcritical using uncredited margin. Significantly fewer are subcritical if the fuel basket also degrades. Thus, the materials of DPC basket construction (e.g., aluminum or carbon steel) could be deleterious if they fully corrode, along with the neutron absorbers, during the performance period. Logistical simulations are used to better understand the relationship between the needed DPC decay storage time for disposal, and the timing of future events such as the repository opening date, or a transition to loading multi-purpose (disposable) canisters at nuclear power plants. Results show that the maximum benefit from implementing a new canister design, with respect to shortening the cooling time for all SNF including that in DPCs, is associated with the earliest repository start date. As time passes more of the total SNF inventory will be in DPCs such that the value of a transition to multi-purpose canisters will decline, and the remaining options are DPC direct disposal and re-packaging in purpose-designed disposal canisters. Fuel age at emplacement is of interest to evaluate potential impacts from future changes in the fuel management system that could place fuel age limits on dry storage or transportation. The minimum fuel age at emplacement (best-case) is obtained by re-packaging all DPCs into smaller canisters for disposal, thus drastically decreasing the needed decay storage time for any geologic disposal setting. If the industry transitions to smaller, multi-purpose canisters, and without re-packaging, the fuel age at emplacement would be comparable to the best case if: 1) the emplacement power limit is high enough, or 2) both the transition and the repository start date occur early (e.g., 2036 was analyzed). Technical feasibility evaluation continues to show that direct disposal could be safe and cost effective, for some DPCs and in some geologic settings. Direct disposal of a substantial fraction of existing DPCs, limited mainly by thermal management, uncredited criticality margin, materials of DPC basket construction, and the salinity of ground water in the disposal environment, could be part of the overall waste management system. (authors)

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗