Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “TEM”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 1,297 records · Page 72

Electron Microscopy Approaches to Unraveling the Structure of Amorphous Materials

Determining atomic structures in crystalline materials—where atoms are arranged in rigid, periodic lattices—has been highly successful using probes such as electrons, X-rays, and neutrons. In contrast, amorphous materials, despite their ubiquity and technological importance, remain far more challenging to characterize with comparable accuracy and precision. This review highlights existing, emerging, and potential (scanning) transmission electron microscopy ((S)TEM) techniques for probing short- and medium-range order in amorphous materials. Approaches ranging from high-resolution (S)TEM imaging and selected electron diffraction pattern to four-dimensional STEM (4D-STEM) based pair distribution function, fluctuation electron microscopy, tomography, ptychography, and spectroscopic methods are discussed, emphasizing their ability to provide complementary insights across multiple length scales—from sub-angstrom local environments to nanometer-scale correlations. Here, we further explore the promise of multimodal and correlative strategies, as well as the growing role of machine learning and physics-informed AI in enabling real-time, quantitative interpretation of complex structural signatures. Together, these advances point toward a future where electron microscopy not only reveals the hidden order in amorphous systems but also establishes robust structure–property relationships, paving the way for materials innovation in disordered matter.

77 NANOSCIENCE AND NANOTECHNOLOGY↗

Large Scale Production of Magnetic Nanoparticles Using Bacterial Fermentation

Microbial production of nano-sized particles has a demonstrated capacity to make highly crystalline pure phase magnetite or with some substitution of Fe by Co, Ni, Cr, Mn, Zn or the rare earths. Microbial production of magnetic nanoparticles can be achieved in large quantities and at low cost. Over 1 kg (wet weight) of Zn-substituted magnetite (nominal composition of Zn0.6Fe2.4O4) has been recovered from 30 L fermentations. Transmission electron microscopy (TEM) was used to confirm that this mass produced extracellular magnetites exhibited good mono-dispersity. TEM results also showed a highly reproducible particle size and corroborated average crystallite size (ACS) of 13.1 0.8 nm determined through X-ray diffraction (N=7) at a 99 % confidence level. Based on scale-up experiments performed using a 35 L reactor, the increase in ACS reproducibility may be attributed to an increase of electron donor input, availability of divalent substitution metal ions and less ferrous ions in the case of substituted magnetite, increased reactor volume overcoming differences in each batch, or a combination of the above. While costs of commercial nanometer sized magnetite (25-50 nm) may cost $500/kg, microbial production is likely capable of producing 5-90 nm pure or substituted magnetites at a fraction of the cost of traditional chemical synthesis. While there are numerous approaches for the synthesis of nanoparticles, bacterial fermentation of magnetite or metal-substituted magnetite may represent an advantageous manufacturing technology with respect to yield, reproducibility and scalable synthesis with low costs at low energy input.

22 GENERAL STUDIES OF NUCLEAR REACTORS↗

Comparison of the Microstructure and Flux Pinning Properties of Polycrystalline YBa{sub 2}Cu{sub 3}O{sub 7-d} Containing Zn{sub 0.95}Mn{sub 0.05}O or Al{sub 2}O{sub 3} Nanoparticles

Here we compare the microstructure and flux pinning properties of polycrystalline YBa{sub 2}Cu{sub 3}O{sub 7-d} (Y-123 or YBCO) containing either Al{sub 2}O{sub 3} or Zn{sub 0.95}Mn{sub 0.05}O nanoparticles. Samples were prepared using a standard solid-state reaction process, and nanoparticles were added up to a concentration of 0.1 wt%. The crystal structure, microstructure, electrical and magnetic properties were analyzed using X-ray diffraction, scanning electron microscopy and transmission electron microscopy (TEM), and electrical resistivity and DC magnetization measurements, respectively. TEM observations showed that the addition of Zn{sub 0.95}Mn{sub 0.05}O resulted in a high density of fine twins and a variety of interacting microstructures, while Al{sub 2}O{sub 3} addition resulted in a high density of Al-rich nanoscale inhomogeneities embedded in the Y-123 matrix. Flux pinning forces were determined, and predominant pinning mechanisms in the prepared samples were proposed. We evaluated the superconducting properties of YBCO considering the effects of adding insulating or magnetic nanoparticles.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Investigation of Polypropylene-Montmorillonite Clay Nanocomposite Films Containing a Pro-degradant Additive

This paper investigates the performance of polypropylene (PP) incorporated with montmorillonite (MMT) nanoclay, maleic anhydride grafted PP (PP-g-MAH), and pro-degradant additive (TDPA®), which provides additional benefits of increasing biodegradability. A twin-screw extruder was used to compound PP, MMT, PP-g-MAH, and TDPA, and the extruded nanocomposite films were collected for testing, and their mechanical, thermal, barrier, oxo-biodegradability, and morphological properties were evaluated. Tensile test, differential scanning calorimetry (DSC), thermogravimetric analysis (TGA), oxygen permeability test, soil burial test, X-ray diffraction (XRD), transmission electron microscopy (TEM), and scanning electron microscope (SEM) analysis were used to investigate these properties. Increasing MMT content from 1 to 3 phr increases tensile strength and Young’s modulus of the neat PP samples up to ca.45% and 27% respectively. Improvement of thermal properties for neat PP samples was observed by increasing MMT content from 1 to 3 phr. However, at 4 phr MMT content, both mechanical and thermal properties of nanocomposites dropped slightly. For soil buried samples, DSC and TGA results revealed significant changes in the thermal properties for PP samples containing TDPE additive compared to neat PP, clearly confirming the effectiveness of this TDPA additive in promoting oxo-biodegradation process of PP. Similarly weight loss evaluation result shows that about 4% weight loss for sample (PP/TD), which is PP and TDPA blend only, compared to neat PP. However, increasing MMT content from 1 to 4 phr slightly reduced weight loss of PP from 3.5 to 1.5%, respectively, for 6 month soil exposure period, which indicates that increasing MMT content was detrimental to the degradation process. For higher MMT content, the oxygen permeability of PP nanocomposites was decreased by 46% of the corresponding values for neat PP. The XRD and TEM results confirmed the exfoliation structure of the nanocomposites. The morphological change after soil burial test was studied using scanning electron microscopy (SEM).

77 NANOSCIENCE AND NANOTECHNOLOGY↗

Utilization of a Novel Chitosan/Clay/Biochar Nanobiocomposite for Immobilization of Heavy Metals in Acid Soil Environment

An organic–inorganic composite of chitosan, nanoclay, and biochar (named as MTCB) was chosen to develop a bionanocomposite to simultaneously immobilize Cu, Pb, and Zn metal ions within the contaminated soil and water environments. The composite material was structurally and chemically characterized with the XRD, TEM, SEM, BET, and FT-IR techniques. XRD and TEM results revealed that a mixed exfoliated/intercalated morphology was formed upon addition of small amounts of nanoclay (5% by weight). Batch adsorption experiments showed that the adsorption capacity of MTCB for Cu{sup 2+}, Pb{sup 2+}, and Zn{sup 2+} were much higher than that of the pristine biochar sample (121.5, 336, and 134.6 mg g{sup −1} for Cu{sup 2+}, Pb{sup 2+}, and Zn{sup 2+}, respectively). The adsorption isotherm for Cu{sup 2+} and Zn{sup 2+} fitted satisfactorily to a Freundlich model while the isotherm of Pb{sup 2+} was best represented by a Temkin model. That the adsorption capacity increased with increasing temperature is indicative of the endothermic nature of the adsorption process. According to the FTIR analysis, the main mechanism involved in immobilization of metals is binding with –NH{sub 2} groups. Results from this study indicated that modification of biochar by chitosan/clay nanocomposite enhances its potential capacity for immobilization of heavy metals, rendering the bionanocomposite into an efficient heavy metal sorbent in mine-impacted acidic waters and soils.

77 NANOSCIENCE AND NANOTECHNOLOGY↗

Green Synthesis and Antioxidant Study of Silver Nanoparticles of Root Extract of Sageretia thea and Its Role in Oxidation Protection Technology

Development of environmentally friendly synthesis of nanoparticles is one of the important areas of research in nanotechnology. In present study silver naopartticles (AgNPs) of root extract of Sageretia thea (S. thea) were synthesized at room temperature. The synthesized AgNPs were characterized by UV. Visible spectroscopy (UV), scanning electron microscopy (SEM), X-ray diffraction (XRD), energy dispersive spectroscopy (EDX), transmission electron microscopy (TEM), dynamic light scattering (DLS) and Fourier transform infrared (FT-IR) spectroscopy. Formation of AgNPs was confirmed by visual examination the colour change from yellow to brick red due to surface Plasmon resonance band at 435 nm. SEM and TEM analysis of synthesized AgNPs revealed spherical morphology with average particle size 25 nm. Crystalline nature of the AgNPs in face centered cubic structure is evident from the selected area electron diffraction (SAED) and XRD pattern. The presence of elemental Ag was confirmed by EDX analysis at 3kv. Different functional groups which responsible for reduction and stabilization of reaction medium was confirmed by FTIR spectroscopy. The biosynthesized AgNPs showed strong DPPH and dye protection radical scavenging assay while modest hydrogen peroxide radical scavenging assay as compare to crude extract. The present investigations suggest that biosynthesized nanoparticles have a high potential for use in the preparation of drugs used against various diseases and also a promising candidate for many medical applications.

77 NANOSCIENCE AND NANOTECHNOLOGY↗

Effect of Silver Doped Zinc Oxide as Nanofiller for the Development of Biopolymer Nanocomposites from Chitin and Cashew Gum

Nanocomposites based on chitin (CT) and cashew gum (CG) with different concentrations of silver doped zinc oxide nanoparticles (Ag–ZnO) were prepared and characterized by FTIR, UV, XRD, TEM, SEM, DSC, TGA, electrical conductivity measurements. FTIR spectra showed that the characteristic absorption band of the blend was shifted to a higher frequency in nanocomposites, indicating the intermolecular interaction between the blend and nanoparticles. The change in the UV absorption of nanocomposites relative to that of pure blend indicated the successful encapsulation of crystalline metal oxide nanoparticles in the blend matrix. XRD patterns showed that the diffraction peak of the composites were shifted near to the metal oxide peak which indicated that the surface of Ag–ZnO was perpendicular to CT/CG and changed from a semi-crystalline nature to a crystalline structure. The morphological analysis using SEM and TEM showed a uniform attachment of nanoparticles within the CT/CG blend. DSC analysis showed the increased glass transition temperature by the addition of nanoparticles. Thermal stability of nanocomposites was higher than the blend and thermal stability increased with an increase in the content of nanoparticles. The different electrical properties such as AC conductivity and dielectric behaviour of the composites were increased with an increased loading of nanoparticles.

77 NANOSCIENCE AND NANOTECHNOLOGY↗

Fabrication of Engineered Silica-Functionalized-Polyanilines Nanocomposites for Water Decontamination of Cadmium and Lead

In this study, two novel functionalized silica nanocomposites were synthesized via covalent bonding with nanopolyaniline (NPANI) and crosslinked nanopolyaniline (CrossNPANI) to produce [NSi-NPANI] and [NSi-CrossNPANI], respectively. The two nanocomposites were portrayed by SEM, FT-IR, HR-TEM, BET-surface and TGA. The HR-TEM images of [NSi-NPANI] and [NSi-CrossNPANI] confirmed the particle size in the range 14.28–21.43 and 26.19–35.71 nm, respectively and these two nanocomposites were successfully applied to remove divalent cadmium and lead from solutions. As compared to nanosilica [NSi] sorbent, the maximum capacity values of the two nanocomposites for divalent cadmium and lead were identified to increase from 100–250 µmole g{sup −1} (pH 1.0) to 750–800 µmole g{sup −1} (pH 7.0) and from 400–1050 µmole g{sup −1} (pH 1.0) to 650–1350 µmole g{sup −1} (pH 6.0), at the optimum conditions. The adsorption data were compared using two and three parameter equations based on Langmuir, Freundlich, Temkin, Dubinin-Radushkevich, Redlish-Peterson and sips models. The kinetic study of [NSi-NPANI] and [NSi-CrossNPANI] revealed that the pseudo-second order kinetic was the best model to explain the kinetic data for cadmium(II) and lead(II). The free energy of sorption (ΔG{sup o}), enthalpy (ΔH{sup o}), and entropy (ΔS{sup o}) changes were calculated to portend the nature of adsorption. Adsorptive extraction of toxic lead and cadmium from tap water and wastewater was successfully accomplished with the range of percentage recovery values 98.5–100.0 and 91.9–93.0%, respectively.

77 NANOSCIENCE AND NANOTECHNOLOGY↗

Optimal Design of Ozone Bleaching Parameters to Approach Cellulose Nanofibers Extraction from Sugarcane Bagasse Fibers

Cellulose nanofibers (CNFs) were isolated from sugarcane bagasse (SCB) through the combination of bio-refinery, sulfur-free, and totally chlorine free (TCF) chemo-mechanical pretreatments, with a focus on the optimal design of ozone bleaching parameters based on a response surface methodology (RSM). For this purpose, the most effective parameters in ozone bleaching (temperature, time, and pulp consistency) were set between 40 and 85 °C, 60 and 360 min, and 1–5 wt%, respectively. High-performance liquid chromatography (HPLC), Fourier transform infrared spectroscopy (FTIR), Kappa number, and scanning electron microscopy (SEM) were used to chemically and morphologically characterize the SCB fibers. The size distribution and morphology of CNFs were also evaluated by dynamic light scattering (DLS) and transmission electron microscopy (TEM). HPLC analysis revealed that percentage of cellulose increased from 41.5 to 91.39% after chemical pretreatments. FTIR and Kappa number analyses also confirmed the successful isolation of cellulose fibers from the SCB fibers after chemical pretreatments. Furthermore, DLS results showed that the hydrodynamic diameter of the isolated cellulose fibers reduced to 268 nm by dint of ultrasonication. Additionally, TEM images confirmed the isolation of CNFs: the average diameter of cellulose fibers decreased to about 28 nm after mechanical steps and the yield of fibrillation was found to be around 99%. According to the obtained results, the applied chemo-mechanical treatment appears to be promising for green and facile isolation of CNFs.

77 NANOSCIENCE AND NANOTECHNOLOGY↗

Electrospun ZnO Nanoparticles Doped Core–Sheath Nanofibers: Characterization and Antimicrobial Properties

Coaxial electrospinning technique was used to fabricate the core–sheath composite nanofibers of ZnO nanoparticle (Nps) (10%, 20% w/w) doped polymethyl methacrylate (PMMA) (as sheath) and polyvinyl alcohol (PVA) (as core). Fourier transform infrared (FT-IR) spectra were confirmed the weak forces arise between ZnO Nps, PMMA and PVA matrixes. The hexagonal (wurtzite) structure of ZnO Nps with ~ 30.8 nm of diameter was confirmed from the X-ray diffraction pattern. The morphology and microstructure of core–sheath composite nanofibers were confirmed from the scanning electron microscopy (SEM) and transmission electron microscopy (TEM). It is clearly seen from the TEM images that the PMMA encapsulate the PVA core. Core–sheath composite nanofibers were assessed against Escherichia coli (E. coli) and Bacillus subtilis (B. subtilis) bacteria through quantitative, disk diffusion and viable cell count methods. It was found that ZnO Nps doped core–sheath nanofibers were effectively inhibit the growth of gram positive bacteria, B. subtilis.

77 NANOSCIENCE AND NANOTECHNOLOGY↗

Intercalation of Nanopolyaniline with Nanobentonite and Manganese Oxide Nanoparticles as a Novel Nanocomposite to Remediate Cobalt/Zinc and Their Radioactive Nuclides {sup 60}Co/{sup 65}Zn

A novel nanocomposite based on the combination of nanobentonite with nanopolyaniline and nanomanganese oxide (N-Bent–NPANI–NMn{sub 3}O{sub 4}) was synthesized and investigated to extract Co/Zn ions from water using batch technique and {sup 60}Co/{sup 65}Zn radionuclides from radioactive wastewater using column techniques. Characterization was established by High resolution-transmission electron microscopy (HR-TEM), Scanning electron microscope, X-ray diffraction (XRD), thermal gravimetric analysis (TGA) and Fourier transform infrared spectrophotometer. The image of HR-TEM indicated that the produced nanocomposite was ranged from 59.07 to 83.38 nm. Solution pH, time of reaction, amount of solid and metal concentration, all of these parameters were inspected and optimized as fundamental factors during the extraction process. The obtained results implied that the ideal conditions for extraction were pH 6 and 7, reaction time 10 and 20 min, for Co and Zn ions, respectively. The highest removal capacities were found 255.28 and 202.22 mg g{sup −1} for Co and Zn, respectively by using 5 mg nanocomposite. Excellent recoveries were obtained as 94.0–94.5% and 92.0–93.0% for removal of Co–{sup 60}Co and of Zn–{sup 65}Zn ions, respectively from the examined samples. Graphical Abstract: .

77 NANOSCIENCE AND NANOTECHNOLOGY↗

Polymer Based Palladium Nanocatalyst for the Degradation of Nitrate and Congo Red

In this study, the Pd catalyst based on chitosan-tannin (CT) framework as support was prepared and characterized. The CT support and Pd catalyst were characterized by attenuated total reflection (ATR) spectroscopy and Raman spectroscopy, Scanning electron microscopy-energy dispersive X-ray analyzer (SEM–EDX) and transmission electron microscopy (TEM) and X-ray diffractometry (XRD). Attenuated total reflection (ATR) spectra revealed the coordination of Pd via hydroxyl and amino functional groups. Raman spectral analysis was carried out to give information about the structural defect of the catalyst compared to CT support. The SEM–EDX results revealed regular surface morphology and presence of Pd in the catalyst as compared to CT support. TEM analysis revealed that the deposition of Pd on organic support with a spherical shape possessing size in the range of 6.01 nm–20.7 nm (average particle size = 12.65 ± 3.14 nm). The XRD results revealed the amorphous nature of the catalyst compared to CT support. TGA analysis revealed that the catalyst is highly thermally-stable compared to CT support. The catalytic activity of Pd catalyst was investigated for the reduction of nitrate and Congo red in the presence and absence of H{sub 2}. The catalytic activities exhibited 71.11% and 23% removal of nitrate and Congo red in 20 and 60 min, respectively. Thus, results suggested that Pd catalyst has a potential of catalytic activity toward reduction of nitrate and Congo red in presence H{sub 2}.

36 MATERIALS SCIENCE↗

Synthesis and characterization of porous TiO2 with wormhole-like framework structure

A fast and reliable synthetic route for preparing contaminant-free porous TiO2 with a wormhole-like framework and close packed macropores is demonstrated based on a sol-gel process involving acid hydrolysis of an alkoxide in the presence of a cationic surfactant. Powder X-ray diffraction (XRD) and transmission electron microscopy (TEM) measurements have been used to characterize the porous structure and the crystallinity. The XRD patterns, TEM and scanning electron microscopy (SEM) images confirm that these materials have disordered wormhole-like topology with close-packed nearly hexagonal macropores. The mesopore diameters and surface area of titanium dioxide, evaluated from the N2-sorption isotherms, indicate average pore diameters of about 7 and 6 nm and surface areas of about 100 and 335 m2/g, for as-prepared and calcined samples at 400 C.

36 MATERIALS SCIENCE↗

Electrochemical and Magnetic Properties of Electrospun SrTi{sub 1−x}Fe{sub x}O{sub 3} (x = 0, 0.05 and 0.10) Nanofibers for Anodes of Li-Ion Batteries

SrTi{sub 1−x}Fe{sub x}O{sub 3} (x = 0, 0.05 and 0.1) nanofibers (NFs) were fabricated by electrospinning technique. As prepared products were calcined at 800 {sup ∘} C in argon atmosphere for 3 h to obtain a perovskite phase. The crystal structure and morphology of samples were investigated using X-ray diffraction (XRD), transmission electron microscopy (TEM) and scanning electron microscopy (SEM). Electrochemical and magnetic properties of calcined NFs were studied using a potentiostat/galvanostat electrochemical cell system and vibrating sample magnetometer (VSM), respectively. XRD results showed the cubic perovskite structure of calcined samples with the diameter estimated by TEM in the range of 137.4–141.3 nm SEM micrographs revealed the linkage of crystalline grains in NFs of porous and rough surfaces. Electrochemical properties performed on coin-cell-type Li-ion batteries (LIBs) with calcined SrTi{sub 1−x}Fe{sub x}O{sub 3} (x = 0.05 and 0.10) NF-based anodes showed a significant increase of the specific capacity from 305 to 431 mAh/g for the first cycle with the reversible values of 100 and 130 mAh/g, respectively. VSM measurements at room temperature (RT) indicated that calcined SrTiO{sub 3} NFs exhibited paramagnetic (PM) behavior, while calcined SrTi{sub 1−x}Fe{sub x}O{sub 3} NFs displayed ferromagnetic (FM) behavior at RT with the increase of unsaturated magnetization at 10 kOe from 0.46 to 0.82 emu/g for samples with x = 0.05 and 0.10, respectively. The observed FM behavior in calcined SrTi{sub 1−x}Fe{sub x}O{sub 3} (x = 0.05 and 0.1) NFs was suggested to originate from the face center exchange (FCE) mechanism owing to Fe{sup 3+} –Vo–Fe{sup 3+} couplings.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

The Effect of Ba Doping on the Structural, Optical, Magnetic, and Dielectric Properties of BiFeO{sub 3} Nanoparticles

Nanoparticles (Nps) of Ba (0, 1 to 5 at.%)-doped BiFeO{sub 3} were synthesized by a sol-gel route at 100 °C using tartaric acid as a chelating agent. The obtained results were studied by using XRD, SEM with EDAX, TEM, UV-vis diffusion reflectance spectra, VSM, and impedance analyzer. EDAX spectra confirmed the presence of Bi, Ba, and Fe in the samples. X-ray diffraction studies showed that BiFeO{sub 3} and Bi{sub 1−x}Ba{sub x}FeO{sub 3} samples exhibited the expected rhombohedral perovskite structure up to a Ba concentration of 3%, whereas 4 and 5% of Ba concentration exhibited the tetragonal phase. TEM studies indicate the particle sizes in the range of 08–28 nm. Reflectance spectra measurements showed a decrease in band gap with increasing Ba concentration. Magnetic properties indicated that the undoped BiFeO{sub 3} and Ba-doped BiFeO{sub 3} samples were ferromagnetic at room temperature. The dielectric constant (ε{sup ′}) and loss (ε{sup ″}) show large dispersion behavior. The dielectric constant increases with an increase of dopant concentration, but a very high value of the dielectric constant was noticed for x = 0.05.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Tailoring the Structural, Optical and Magnetic Properties of NiFe{sub 2}O{sub 4} by Varying Annealing Temperature

Magnetic nanocrystalline NiFe{sub 2}O{sub 4} nanoparticles of size ranging between 13 and 19 nm were synthesized by the hydrothermal method using polyethylene glycol (PEG) as surfactant. The role of annealing on phase, crystallite size, and morphology was determined by X-ray diffraction (XRD) and transmission electron microscopy (TEM). Energy-dispersive X-ray spectroscopy (EDX) was used for qualitative analysis. X-ray diffraction confirmed the single phase of as-obtained particles. TEM revealed a spherical morphology having an average particle size of 13.73 nm at 523 K and rises to 14.89, 16.42, and 21.14 nm at 623, 723, and 823 K respectively, which is approximately the same as the crystallite size determined from XRD. EDX results confirmed that elemental ratios were in stoichiometry. Fourier transform infrared (FTIR) spectral analysis demonstrates the formation of M-O bond in NiFe{sub 2}O{sub 4} nanoparticles. The optical spectra obtained from UV-visible spectroscopy revealed that nanoparticles have direct allowed energy band gap of 2.34, 2.47, 2.70, and 2.20 eV at 523, 623, 723, and 823 K respectively. A vibrating sample magnetometer (VSM) was used at room temperature for magnetic measurements which further showed ferromagnetic behavior of as-synthesized material. In addition, it was found that saturation magnetization increases with an increase of annealing temperature while coercivity decreases with temperature.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Synthesis and Characterization of Er-Doped Nano ZnO Samples

Pure and erbium-doped ZnO nanoparticles (Zn{sub 1−x}Er{sub x}O), (0.00 ≤ x ≤ 0.10), were synthesized by wet chemical co-precipitation method. The structural, optical, and magnetic properties of the prepared samples were investigated using x-ray powder diffraction (XRD), transmission electron microscopy (TEM), ultraviolet-visible spectroscopy (UV), Fourier transform infrared spectroscopy (FTIR), M-H magnetic hysteresis, and electron paramagnetic resonance (EPR). XRD studies exhibit the presence of a single ZnO wurtzite hexagonal crystal structure for 0.00 ≤ x ≤ 0.06. A secondary phase of Er{sub 2}O{sub 3} appears for x > 0.06. This means that the solubility limit for doping Zn{sup 2+} ions by Er{sup 3+} ions is about x = 0.06 under our preparations condition. The lattice parameter a is not affected by the Erbium doping. On the other hand, the lattice parameter c and the unit cell volume V increase with the increase of x up to x = 0.06. This is attributed to the larger ionic size of Er{sup 3+} ions (0.88 Å) compared to Zn{sup 2+} ions (0.74 Å). Both c and V decrease for x > 0.06. TEM micrographs indicate that the shape and the size of the ZnO nanoparticles are modified by changing the doping level of Er. The UV measurements point out that band gap energy E{sub g} decreases with the increase of x up to x = 0.06. Then, it increases for both x = 0.08 and 0.10. FTIR spectra confirm the presence of O–H and Zn–O stretching modes at 3451.963 and 428.901 cm{sup − 1}, respectively, in pure and doped ZnO samples. The Zn–O stretching mode shifts toward a lower wavenumber for x = 0.06 and toward a higher wavenumber for x = 0.10. M-H hysteresis analysis, at room temperature, reveals that the pure ZnO has a ferromagnetic signal combined with diamagnetic and paramagnetic contributions. This ferromagnetism is reduced for the doped samples up to x = 0.02, and an antiferromagnetic alignment appears for 0.04 ≤ x ≤ 0.10. The saturation magnetization (M{sub s}), the coercivity (H{sub c}), the retentivity (M{sub r}), the anisotropy constant (K{sub a}), and the magnetic moment (μ{sub m}) were estimated and discussed in terms of erbium doping for the different samples. EPR spectra for Zn{sub 1−x}Er{sub x}O were measured at room temperature in order to study the effect of Er substitution on the g value, resonance field (H{sub r}), peak to peak line width (ΔH{sub pp}) and spin–spin relaxation time constant (T{sub 2}).

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Synthesis, Spectroscopy, and Magnetic Characterizations of PVP-Assisted Nanoscale Particle

Inverse spinel ferrite of nonmagnetic metal-doped ferro-ferric oxide was synthesized by co-precipitation technique, and its characterizations have been performed by XRD, FTIR, TEM, EDX, VSM, and EPR. XRD figures show the prepared samples in their cubic phase and that their crystallite faces vary from 5.57 to 18.47 nm. FTIR spectra of the as-synthesized samples were performed in the range of 400 and 4000 cm{sup −1} and annealed at 600 {sup ∘}C. The TEM revealed that the syllable construction of the nanoscale particles was agglomerated in their crystalline sample. From VSM study, the sample obtained has a doublet pattern, and ferromagnetic performance was observed from the samples. From EPR spectra, the line shape and the g values obtained for the samples conformed to superparamagnetic resonance due to Mg{sup + 2} ions with a stoichiometric composition. These typical magnetic hypnotic specifications are used for various sensing applications.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗