Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “etching”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 1,279 records · Page 71

Patterning graphene nanoribbons using copper oxide nanowires

We present a fabrication technique for graphene nanoribbons (GNRs) that employs copper oxide nanowires as the etch masks. We demonstrate that these etch masks have numerous advantages: they can be synthesized simply by heating a copper foil in air, deposited on graphene from a solution, they are inert to oxygen plasma, and can be removed from the substrate by dissolution in mild acids. We fabricated GNRs in the device configuration and tested their electrical properties. Depending on the duration of the plasma etching, GNR devices exhibiting either standard ambipolar electric field effects or p-type transistor behaviors with ON-OFF ratios > 50 can be fabricated. The resulting devices based on narrow GNRs are demonstrated to exhibit promising electronic properties, which can be exploited in studies where GNR devices are required.

36 MATERIALS SCIENCE↗

Surface electronic structure for various surface preparations of Nb-doped SrTiO{sub 3} (001)

High-resolution angle-resolved photoemission spectroscopy (ARPES) was used to study the surface electronic structure of Nb-doped SrTiO{sub 3} (STO) single crystals prepared using a variety of surface preparations. ARPES measurements show that simple degreasing with subsequent anneal in vacuum is not an adequate surface preparation of STO, rather, preparations consisting of etching with buffered HF or HCl, and to a lesser extent, simple water leaching resulted in surfaces with much less disorder. A non-dispersing, mid-gap state was found ∼800 meV above the top of the valence band for samples which underwent etching. This mid-gap state is not present for vacuum-annealed and water-leached samples, as well as for STO thin films grown using molecular beam epitaxy. Theoretical modeling using density functional theory suggests that this mid-gap state is not related to the SrO- and TiO{sub 2}-terminated surfaces, but rather, is due to a partial hydrogenation of the STO surface that occurs during etching.

36 MATERIALS SCIENCE↗

Atomic state and characterization of nitrogen at the SiC/SiO{sub 2} interface

We report on the concentration, chemical bonding, and etching behavior of N at the SiC(0001)/SiO{sub 2} interface using photoemission, ion scattering, and computational modeling. For standard NO processing of a SiC MOSFET, a sub-monolayer of nitrogen is found in a thin inter-layer between the substrate and the gate oxide (SiO{sub 2}). Photoemission shows one main nitrogen related core-level peak with two broad, higher energy satellites. Comparison to theory indicates that the main peak is assigned to nitrogen bound with three silicon neighbors, with second nearest neighbors including carbon, nitrogen, and oxygen atoms. Surprisingly, N remains at the surface after the oxide was completely etched by a buffered HF solution. This is in striking contrast to the behavior of Si(100) undergoing the same etching process. We conclude that N is bound directly to the substrate SiC, or incorporated within the first layers of SiC, as opposed to bonding within the oxide network. These observations provide insights into the chemistry and function of N as an interface passivating additive in SiC MOSFETs.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Ellipsometry characterization of polycrystalline ZnO layers with the modeling of carrier concentration gradient: Effects of grain boundary, humidity, and surface texture

Spectroscopic ellipsometry (SE) has been applied to study the effects of grain boundary, humidity, and surface texture on the carrier transport properties of Al-doped ZnO layers fabricated by dc and rf magnetron sputtering. In the SE analysis, the variation in the free carrier absorption toward the growth direction, induced by the ZnO grain growth on foreign substrates, has been modeled explicitly by adopting a multilayer model in which the optical carrier concentration (N{sub opt}) varies continuously with a constant optical mobility (μ{sub opt}). The effect of the grain boundary has been studied by comparing μ{sub opt} with Hall mobility (μ{sub Hall}). The change in μ{sub Hall}/μ{sub opt} indicates a sharp structural transition of the ZnO polycrystalline layer at a thickness of d ∼ 500 nm, which correlates very well with the structure confirmed by transmission electron microscopy. In particular, below the transition thickness, the formation of the high density grain boundary leads to the reduction in the μ{sub Hall}/μ{sub opt} ratio as well as N{sub opt}. As a result, we find that the thickness dependence of the carrier transport properties is almost completely governed by the grain boundary formation. On the other hand, when the ZnO layer is exposed to wet air at 85 °C, μ{sub Hall} reduces drastically with a minor variation of μ{sub opt} due to the enhanced grain boundary scattering. We have also characterized textured ZnO:Al layers prepared by HCl wet etching by SE. The analysis revealed that the near-surface carrier concentration increases slightly after the etching. We demonstrate that the SE technique can be applied to distinguish various rough textured structures (size ∼ 1 μm) of the ZnO layers prepared by the HCl etching.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Chains of quantum dot molecules grown on Si surface pre-patterned by ion-assisted nanoimprint lithography

An original approach based on the combination of nanoimprint lithography and ion irradiation through mask has been developed for fabrication of large-area periodical pattern on Si(100). Using the selective etching of regions amorphized by ion irradiation ordered structures with grooves and ridges were obtained. The shape and depth of the relief were governed by ion energy and by the number of etching stages as well. Laterally ordered chains of Ge quantum dots were fabricated by molecular beam epitaxy of Ge on the pre-patterned Si substrates. For small amount of Ge deposited chains contain separate quantum dot molecules. The increase of deposition amount leads to overlapping of quantum dot molecules with formation of dense homogeneous chains of quantum dots. It was shown that the residual irradiation-induced bulk defects underneath the grooves suppress nucleation of Ge islands at the bottom of grooves. On pre-patterned substrates with whole defect regions, etched quantum dots grow at the bottom of grooves. The observed location of Ge quantum dots is interpreted in terms of local strain-mediated surface chemical potential which controls the sites of islands nucleation. The local chemical potential is affected by additional strain formed by the residual defects. It was shown by molecular dynamics calculations that these defects form the compressive strain at the bottom of grooves.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Effect of low-damage inductively coupled plasma on shallow nitrogen-vacancy centers in diamond

Near-surface nitrogen-vacancy (NV) centers in diamond have been successfully employed as atomic-sized magnetic field sensors for external spins over the last years. A key challenge is still to develop a method to bring NV centers at nanometer proximity to the diamond surface while preserving their optical and spin properties. To that aim we present a method of controlled diamond etching with nanometric precision using an oxygen inductively coupled plasma process. Importantly, no traces of plasma-induced damages to the etched surface could be detected by X-ray photoelectron spectroscopy and confocal photoluminescence microscopy techniques. In addition, by profiling the depth of NV centers created by 5.0 keV of nitrogen implantation energy, no plasma-induced quenching in their fluorescence could be observed. Moreover, the developed etching process allowed even the channeling tail in their depth distribution to be resolved. Furthermore, treating a {sup 12}C isotopically purified diamond revealed a threefold increase in T{sub 2} times for NV centers with <4 nm of depth (measured by nuclear magnetic resonance signal from protons at the diamond surface) in comparison to the initial oxygen-terminated surface.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Image processing analysis of nuclear track parameters for CR-39 detector irradiated by thermal neutron

CR-39 detector which covered with boric acid (H{sub 3}Bo{sub 3}) pellet was irradiated by thermal neutrons from ({sup 241}Am - {sup 9}Be) source with activity 12Ci and neutron flux 10{sup 5} n. cm{sup −2}. s{sup −1}. The irradiation times -T{sub D} for detector were 4h, 8h, 16h and 24h. Chemical etching solution for detector was sodium hydroxide NaOH, 6.25N with 45 min etching time and 60 C° temperature. Images of CR-39 detector after chemical etching were taken from digital camera which connected from optical microscope. MATLAB software version 7.0 was used to image processing. The outputs of image processing of MATLAB software were analyzed and found the following relationships: (a) The irradiation time -T{sub D} has behavior linear relationships with following nuclear track parameters: i) total track number - N{sub T} ii) maximum track number - MRD (relative to track diameter - D{sub T}) at response region range 2.5 µm to 4 µm iii) maximum track number - M{sub D} (without depending on track diameter - D{sub T}). (b) The irradiation time -T{sub D} has behavior logarithmic relationship with maximum track number - M{sub A} (without depending on track area - A{sub T}). The image processing technique principally track diameter - D{sub T} can be take into account to classification of α-particle emitters, In addition to the contribution of these technique in preparation of nano- filters and nano-membrane in nanotechnology fields.

46 INSTRUMENTATION RELATED TO NUCLEAR SCIENCE AND ↗

A method for determining average damage depth of sawn crystalline silicon wafers

The depth of surface damage (or simply, damage) in crystalline silicon wafers, caused by wire sawing of ingots, is determined by performing a series of minority carrier lifetime (MCLT) measurements. Samples are sequentially etched to remove thin layers from each surface and MCLT is measured after each etch step. The thickness-removed (δt) at which the lifetime reaches a peak value corresponds to the damage depth. This technique also allows the damage to be quantified in terms of effective surface recombination velocity (S eff ). To accomplish this, the MCLT data are converted into an S eff vs δt plot, which represents a quantitative distribution of the degree of damage within the surface layer. We describe a wafer preparation procedure to attain reproducible etching and MCLT measurement results. We also describe important characteristics of an etchant used for controllably removing thin layers from the wafer surfaces. Lastly, some typical results showing changes in the MCLT vs δt plots for different cutting parameters are given.

14 SOLAR ENERGY↗

In situ photoacoustic characterization for porous silicon growing: Detection principles

There are a few methodologies for monitoring the in-situ formation of Porous Silicon (PS). One of the methodologies is photoacoustic. Previous works that reported the use of photoacoustic to study the PS formation do not provide the physical explanation of the origin of the signal. In this paper, a physical explanation of the origin of the photoacoustic signal during the PS etching is provided. The incident modulated radiation and changes in the reflectance are taken as thermal sources. In this paper, a useful methodology is proposed to determine the etching rate, porosity, and refractive index of a PS film by the determination of the sample thickness, using scanning electron microscopy images. This method was developed by carrying out two different experiments using the same anodization conditions. The first experiment consisted of growth of the samples with different etching times to prove the periodicity of the photoacoustic signal, while the second one considered the growth samples using three different wavelengths that are correlated with the period of the photoacoustic signal. The last experiment showed that the period of the photoacoustic signal is proportional to the laser wavelength.

46 INSTRUMENTATION RELATED TO NUCLEAR SCIENCE AND ↗

The impact of interfacial Si contamination on GaN-on-GaN regrowth for high power vertical devices

The development of gallium nitride (GaN) power devices requires a reliable selective-area doping process, which is difficult to achieve because of ongoing challenges associated with the required etch-then-regrow process. The presence of silicon (Si) impurities of unclear physical origin at the GaN regrowth interface has proven to be a major bottleneck. Furthermore, this paper investigates the origin of Si contamination at the epitaxial GaN-on-GaN interface and demonstrates an approach that markedly reduces its impact on device performance. An optimized dry-etching approach combined with UV-ozone and chemical etching is shown to greatly reduce the Si concentration levels at the regrowth interface, and a significant improvement in a reverse leakage current in vertical GaN-based p–n diodes is achieved.

36 MATERIALS SCIENCE↗

Restored Passivation after Complete Removal of Front Poly-Si Between the Grid in Poly-Si/SiO2 Front/Back Cells

This work explores the use of wet chemical etching to completely remove the front poly-Si layer between grid lines of a front/back poly-Si/SiO2 passivated contact device. The purpose of the work is to provide excellent passivation under the metal grid, but to also maximize Jsc by eliminating optical absorption in the front poly-Si. We show that after a high temperature anneal to distribute carriers in the poly-Si/SiO2/c-Si interface all of the poly-Si can be removed selectively with TMAH, using the SiO2 as an etch-stop layer. The etched surface can be repassivated back to its original level with the addition of a SiNx/Al2O3 stack grown on the preserved tunnelling oxide layer followed by a short forming gas anneal. Using symmetric 100 - 200 nm intrinsically doped poly-Si/SiO2 on textured n-type wafer templates we show absolute device efficiency enhancement from 15% to 21% by increasing the Jsc by 12 mA/cm2 after removing the front poly-Si and repassivating while effectively preserving the Voc, and FF of the device. IQE values are similar to PERC devices in the short wavelength range.

etching↗

Tin removal by an annular surface wave plasma antenna in an extreme ultraviolet lithography source

Tin contamination of the collector mirror surface remains one of the crucial issues of EUV (Extreme Ultraviolet) sources, directly impacting the availability of the tool. Hydrogen plasma-based tin removal processes employ hydrogen radicals and ions to interact with tin deposits to form gaseous tin hydride (SnH 4 ), which can be removed through pumping. An annular surface wave plasma (SWP) source developed at the University of Illinois—Urbana Champaign is integrated into the cone and perimeter of the collection mirror for in situ tin removal. The SWP is characterized by high ion and radical densities, low electron temperature, and local generation where etching is needed. This method has the potential to significantly reduce downtime and increase mirror lifetime. Radical probe measurements show hydrogen radical densities in the order of 10 19 m -3 , while Langmuir probe measurements show electron temperatures of up to 6 eV and plasma densities on the order of 10 17–18 m -3 . The generated ions are essential to the tin cleaning and have sufficiently low energy to cause no damage to the collector capping layer. Tin etch rates of up to 270 nm/min were observed in a variety of experimental conditions, including various powers, pressures, flowrates, and temperatures. In conclusion, the high etch rates demonstrated in this study exceed the expected contamination rate of the EUV source.

70 PLASMA PHYSICS AND FUSION TECHNOLOGY↗

Effect of fabrication processes on BaTiO 3 capacitor properties

There is an increasing desire to utilize complex functional electronic materials such as ferroelectrics in next-generation microelectronics. As new materials are considered or introduced in this capacity, an understanding of how we can process these materials into those devices must be developed. Here, the effect of different fabrication processes on the ferroelectric and related properties of prototypical metal oxide (SrRuO 3 )/ferroelectric (BaTiO 3 )/metal oxide (SrRuO 3 ) heterostructures is explored. Two different types of etching processes are studied, namely, wet etching of the top SrRuO 3 using a NaIO 4 solution and dry etching using an Ar + -ion beam (i.e., ion milling). Polarization-electric-field hysteresis loops for capacitors produced using both methods are compared. For the ion-milling process, it is found that the Ar + beam can introduce defects into the SrRuO 3 /BaTiO 3 /SrRuO 3 devices and that the milling depth strongly influences the defect level and can induce a voltage imprint on the function. Realizing that such processing approaches may be necessary, work is performed to ameliorate the imprint of the hysteresis loops via ex situ “healing” of the process-induced defects by annealing the ferroelectric material in a barium-and-oxygen-rich environment via a chemical-vapor-deposition-style process. This work provides a pathway for the nanoscale fabrication of these candidate materials for next-generation memory and logic applications.

36 MATERIALS SCIENCE↗

Point defect distribution in high-mobility conductive SrTiO{sub 3} crystals

We have carried out positron-annihilation spectroscopy to characterize the spatial distribution and the nature of vacancy defects in insulating as-received as well as in reduced SrTiO{sub 3} substrates exhibiting high-mobility conduction. The substrates were reduced either by ion etching the substrate surfaces or by doping with vacancies during thin-film deposition at low pressure and high temperature. We show that Ti vacancies are native defects homogeneously distributed in as-received substrates. In contrast, the dominant vacancy defects are the same both in ion etched crystals and substrates reduced during the film growth, and they consist of nonhomogeneous distributions of cation-oxygen vacancy complexes. Their spatial extension is tuned from a few microns in ion-etched samples to the whole substrate in specimens reduced during film deposition. Our results shed light on the transport mechanisms of conductive SrTiO{sub 3} crystals and on strategies for defect-engineered oxide quantum wells, wires, and dots.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Pyramidal pits created by single highly charged ions in BaF{sub 2} single crystals

In various insulators, the impact of individual slow highly charged ions (eV-keV) creates surface nanostructures, whose size depends on the deposited potential energy. Here we report on the damage created on a cleaved BaF{sub 2} (111) surface by irradiation with 4.5xq keV highly charged xenon ions from a room-temperature electron-beam ion trap. Up to charge states q=36, no surface topographic changes on the BaF{sub 2} surface are observed by scanning force microscopy. The hidden stored damage, however, can be made visible using the technique of selective chemical etching. Each individual ion impact develops into a pyramidal etch pits, as can be concluded from a comparison of the areal density of observed etch pits with the applied ion fluence (typically 10{sup 8} ions/cm{sup 2}). The dimensional analysis of the measured pits reveals the significance of the deposited potential energy in the creation of lattice distortions/defects in BaF{sub 2}.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Molecular dynamics simulations of GaAs sputtering under low-energy argon ion bombardment

Results from molecular dynamics (MD) simulations of low-energy (50-200 eV) Ar{sup +} ion bombardment on (110) GaAs surfaces are reported. A new analytical bond-order potential, originally developed for molecular beam epitaxy studies, is used and tested in the context of etching to investigate the nature and effects of physical sputtering on GaAs compounds. It is found that a thermal desorption model, which accounts for long time scale phenomena between MD simulated impacts, is necessary to achieve steady state sputtering. An initial rapid etch of both atomic species is observed up to 4x10{sup 16} ions/cm{sup 2} fluence with preferential sputtering of Ga atoms. At high fluences, simulations show the formation of an As-rich layer on the top surface, a subsurface enrichment of Ga, and a return to stoichiometry deeper in the solid. More than 97% of sputtered or desorbed species appear to be Ga or As atoms; sputtering of GaAs molecules is negligible. All these observations are in agreement with published experimental results. Finally, a significant fraction of the atoms leave the surface with more than 10% of the incident ion energy, which could alter passivation layers on sidewalls during etching.

36 MATERIALS SCIENCE↗

Feedback control of plasma electron density and ion energy in an inductively coupled plasma etcher

Here the authors report the development of a fuzzy logic based feedback control of the plasma electron density and ion energy for high density plasma etch process. The plasma electron density was measured using their recently developed transmission line microstrip microwave interferometer mounted on the chamber wall, and the rf voltage was measured by a commercial impedance meter connected to the wafer stage. The actuators were two 13.56 MHz rf power generators which provided the inductively coupled plasma power and bias power, respectively. The control system adopted the fuzzy logic control algorithm to reduce frequent actuator action resulting from measurement noise. The experimental results show that the first wafer effect can be eliminated using closed-loop control for both poly-Si and HfO{sub 2} etching. In particular, for the HfO2 etch, the controlled variables in this work were much more effective than the previous one where ion current was controlled, instead of the electron density. However, the pressure disturbance effect cannot be reduced using plasma electron density feedback.

70 PLASMA PHYSICS AND FUSION TECHNOLOGY↗

Comparison endpoint study of process plasma and secondary electron beam exciter optical emission spectroscopy

Traditionally process plasmas are often studied and monitored by optical emission spectroscopy. Here, the authors compare experimental measurements from a secondary electron beam excitation and direct process plasma excitation to discuss and illustrate its distinctiveness in the study of process plasmas. They present results that show excitations of etch process effluents in a SF{sub 6} discharge and endpoint detection capabilities in dark plasma process conditions. In SF{sub 6} discharges, a band around 300 nm, not visible in process emission, is observed and it can serve as a good indicator of etch product emission during polysilicon etches. Based on prior work reported in literature the authors believe this band is due to SiF{sub 4} gas phase species.

46 INSTRUMENTATION RELATED TO NUCLEAR SCIENCE AND ↗