Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “electrolytes”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 1,279 records · Page 71

Locally developed electronic conduction in a yttria stabilized zirconia (YSZ) electrolyte for durable solid oxide fuel cells

In the present work, anode supported solid oxide fuel cells (SOFCs) based on a YSZ single layer electrolyte with locally developed electronic conduction near the anode side is fabricated to improve the cell durability under negative voltage conditions. A ceria added Ni/YSZ anode functional layer is utilized and co-sintered with the YSZ electrolyte at 1460 °C. Cerium ions are diffused into a limited region of the YSZ layer (~6 μm), establishing a ceria doped YSZ region. We successfully demonstrate that this YSZ single layer cell can operate stably for ~100 h without anode/electrolyte interface delamination, even under a negative voltage. The embedded probe technique and theoretical calculation reveal that the internal oxygen partial pressure (near the anode) is substantially reduced (stabilized) by means of local electronic conduction of ceria doped YSZ. Thus, we propose an SOFC electrolyte design comprising a YSZ single layer with a ceria added anode functional layer (locally formed ceria doped YSZ in the electrolyte) as a protection method against fuel cell stack degradation caused by negative voltage operation.

25 ENERGY STORAGE↗

Deconvoluting sources of failure in lithium metal batteries containing NMC and PEO-based electrolytes

Solid-state lithium metal batteries (SSLMBs) containing polyethylene oxide (PEO)-derived polymer electrolytes and high-voltage (> 4 V vs. Li/Li + ) cathode materials suffer from three sources of failure: (1) instability between the polymer electrolyte and cathode at high voltage, (2) instability of the polymer electrolyte with Li metal, and (3) poorly-designed cathodes. In this study, these three sources of failure are deconvoluted by studying Ni-rich LiNi x Mn y Co 1-x-y O 2 (NMC, x ≥ 0.6) cathodes and a gel polymer electrolyte (GPE) derived from PEO. Initial cycling data reveals that rapid capacity fade occurs regardless of whether soft short circuits form due to Li dendrites. Cyclic voltammetry scans on cells featuring a Li metal electrode, GPE, and a NMC811 electrode free of additives suggest that there are no runaway reactions between the GPE and NMC811 up to 4.5 V vs. Li/Li + . Cathode/cathode symmetric cell cycling demonstrates that Li metal reactivity is a prime source of failure, though a poorly-designed cathode leads to subpar performance. A cathode with single-crystal NMC particles was demonstrated to achieve better initial capacity and longer cycle life, indicating room for improvement in SSLMB cathode design. Therefore, the sources of failure as enumerated may be ranked as follows from most to least concerning: 2 > 3 > 1.

25 ENERGY STORAGE↗

Mastering the synergy between Na 3 V 2 (PO 4 ) 2 F 3 electrode and electrolyte: A must for Na-ion cells

Sodium-ion batteries are emerging as suitable energy storage devices for special applications such as high-power devices with the advantages of being cheaper and more sustainable than the Li-ion equivalents. The sodium ion cells consisting of polyanionic Na 3 V 2 (PO 4 ) 2 F 3 - hard carbon electrodes exhibit high power rate capabilities but limited cycle life, especially at high temperatures. To circumvent this drawback we herein conducted in-depth analyses of the origins of structural degradations occurring in Na 3 V 2 (PO 4 ) 2 F 3 electrodes upon long cycling. Vanadium dissolution with associated parasitic reactions is identified as one of the major reasons for cell failure. Its amount varies depending on the electrolyte, with NaTFSI-based electrolyte showing the least vanadium dissolution as the TFSI - anion decomposes without producing acidic impurities, in contrast to the NaPF 6 -based electrolyte. The dissolved vanadium species undergoes oxidation and reduction processes at the Na 3 V 2 (PO 4 ) 2 F 3 and HC electrodes, respectively, with the electrochemical signature of these processes being used as a fingerprint to identify state of health of the 18650 cells. Here, having found that surface reactivity is the primary cause of vanadium dissolution we provide methods to mitigate it by combining surface coating and optimized electrolyte formulation.

25 ENERGY STORAGE↗

Thermodynamic modeling of aqueous lithium salt solutions with association electrolyte nonrandom two-liquid activity coefficient model

The high charge density of lithium ion and the resulting strong association phenomena make thermodynamic modeling of aqueous lithium electrolyte solutions extremely challenging. In this study, the association electrolyte nonrandom two-liquid activity coefficient model of Lin et al. (AIChE J. 2022, 68(2), e17422) is utilized to correlate and predict thermodynamic properties and solubility behavior of aqueous single electrolyte solutions of LiCl, LiBr, LiI, and LiNO 3 , and their mixed electrolyte solutions. Capturing self-association of water, cross-association of ion and water for hydration, and cross-association of cation and anion for ion-pairing, the association model accurately represents the literature experimental data up to saturation concentrations and at the temperature ranging from 263 K to 523 K. Here, this study further investigated the effect of anions of the lithium salts, and re-confirmed that the order of solution non-ideality as LiI > LiBr > LiCl > LiNO 3 because the anions with stronger association strengths are more likely to form ion pairs and thus lower the mean ionic activity coefficients.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Modeling the performance and faradaic efficiency of solid oxide electrolysis cells using doped barium zirconate perovskite electrolytes

Y-doped BaZrO 3 (BaZr 1 x Y x O 3 δ , or “BZY”), a proton-conducting ceramic featuring high bulk conductivity and good chemical stability, is a promising electrolyte material for solid oxide electrolysis cells. Further doping with Ce and/or Yb (creating materials “BCZY” and “BCZYYb”) can improve conductivity and sintering properties, but at significant penalty to cells’ faradaic efficiency (FE). Studies have proposed that reduction of lattice Ce can occur in the hydrogen electrode, which consumes some hydrogen produced by the hydrogen evolution reaction, leading to decreased FE. Despite studies suggesting this phenomenon, the mechanism is largely unknown. In this work, we developed a multiphysics model to study the transport of multiple defect species and the performance of BZY, BCZY, and BCZYYb, capturing the tradeoff between enhanced performance at the cost of FE for BCZY and BCZYYb electrolytes compared to BZY. We also found that increasing the water content of the anode gas supply lowers the current output of the cell but results in better FE. The model, which uses several parameters previously unavailable in the literature, was validated to experiments varying temperature, steam water content, and electrolyte material, as well as two performance metrics (performance curves and FE). Results verify and explain observed trends, informing future work on Ce-doped BZY electrolytes.

08 HYDROGEN↗

Investigation of the Rechargeability of Li-O2 Batteries in Non-aqueous Electrolyte

In order to understand the nature of the limited cycle life and poor energy efficiency associated with the secondary Li-O¬2 batteries the discharge products of primary Li-O2 cells at different depth of discharge (DOD) are systematically analyzed in this work. It is revealed that if discharged to 2.0 V a small amount of Li2O2 coexist with Li2CO3 and RO-(C=O)-OLi) in alkyl carbonate-based electrolyte. Further discharging the air electrodes to below 2.0 V the amount of Li2CO3 and LiRCO3 increases significantly due to the severe electrolyte decomposition. There is no Li2O detected in this alkyl carbonate electrolyte regardless of DOD. It is also found that the alkyl carbonate based electrolyte begins to decompose at 4.0 V during charging under the combined influences from the high surface area carbon, the nickel metal current collector and the oxygen atmosphere. Accordingly the impedance of the Li-O2 cell continues to increase after each discharge and recharge process indicating a repeated plating of insoluble lithium salts on the carbon surface. Therefore the whole carbon electrode becomes completely insulated only after a few cycles and loses the function of providing active tri-phase regions for the Li-oxygen batteries.

25 ENERGY STORAGE↗

1 kW/1 kWh advanced vanadium redox flow battery utilizing mixed acid electrolytes

This paper explores demonstration of an advanced vanadium redox flow battery (VRFB) using a mixed acid (sulfuric and hydrochloric acid) supporting electrolyte in a kW scale. The prototype VRFB is capable of delivering more than 1.1 kW in the whole operation range (15~85% state of charge) at 80 mA/cm2 with high energy efficiency of 82% and energy content of 1.4 kWh. The system has been operated stably without any precipitation even at elevated electrolyte temperatures of > 45°C, while the control tests with the conventional sulfuric acid electrolyte suffered from precipitation after 80 cycles. The mixed acid system enabled operation at elevated temperature (> 40°C), providing unique advantages over the conventional pure sulfate system; 1) high stack energy efficiency due to better kinetics and low electrolyte resistance, 2) low viscosity, resulting in reduced pumping loss, 3) elimination of additional heat exchanger, 4) high system efficiency and 5) simple system design and operation.

advanced vanadium redox flow battery↗

Bis(trimethylsilyl) 2-fluoromalonate derivatives as electrolyte additives for high voltage lithium ion batteries

Three trimethylsilyl based malonate esters, bis(trimethylsilyl) 2-methyl-2-fluoromalonate (BTMSMFM), bis(trimethylsilyl) 2-ethyl-2-fluoromalonate (BTMSEFM) and bis(trimethylsilyl) 2-propyl-2-fluoromalonate (BTMSPFM), have been used as additives in 1.0 M LiPF 6 /ethylene carbonate (EC)-dimethyl carbonate (DMC)-diethyl carbonate (DEC) (1-1-1, by v) baseline electrolyte for LiNi 0.80 Co 0.15 Al 0.05 O 2 (NCA) based high voltage lithium ion batteries. The NCA half-cells with 5 wt% BTMSMFM exhibit higher capacity retention than that in the baseline electrolyte at different upper cut off voltages, that is, 4.2, 4.3, 4.4 and 4.5 V vs. Li/Li + . Scanning electron microscope (SEM) show that the additive successfully prevents the formation of thick solid electrolyte interphase (SEI) films on the surface of the NCA electrodes. X-ray diffraction (XRD) further reveals that the crystal structure of NCA is also maintained in the electrolyte with 5 wt% BTMSMFM at high cut off voltages. Finally, besides beneficial to NCA cathode, the BTMSMFM additive also ensures better cycling performance of the graphite based half-cells and NCA/graphite full-cells, and thus is a promising additive for application in rechargeable lithium ion batteries.

25 ENERGY STORAGE↗

Direct observation of MgO formation at cathode electrolyte interface of a spinel MgCo 2 O 4 cathode upon electrochemical Mg removal and insertion

Identifying a Mg 2+ insertion mechanism into Mg cathode is one crucial challenge of designing Mg batteries that own comparable specific energy to the lithium ion systems. Spinel Mg cathodes are attractive candidates mainly attributed to its high intercalation voltage and theoretical capacity, however, electrochemically removing Mg from its solid structure with identified capacity dedicated to actual reversible Mg intercalation introduce complications. Work presented here applies Scanning/Transmission Electron Microscopy with Energy Loss Spectroscopy and diffraction method to investigate the cathode electrolyte interface for a spinel MgCo 2 O 4 material electrochemically cycled in the presence of a non-aqueous, low water content Mg electrolyte. Findings at an atomic scale suggest a complete de-magnesiation is occurring for thin MgCo 2 O 4 particles upon electrochemical charging, but a vast majority of MgCo 2 O 4 shows formation of an amorphous MgO layer with a thickness of similar to ~10 nm at the cathode electrolyte interface. The amorphous MgO layer is directly jointed with the crystalline MgCo 2 O 4 at the outer edge of the cathode. Formation of MgO at the cathode electrolyte interface is believed to be the detrimental factor preventing further electrochemical cell cycling of MgCo 2 O 4 . A possible reaction pathway of intercalation-initiated surface conversion is proposed to explain reversible Mg insertion with MgCo 2 O 4 .

25 ENERGY STORAGE↗

Evaluating the effect of membrane-ionomer combinations and supporting electrolytes on the performance of cobalt nanoparticle anodes in anion exchange membrane electrolyzers

In low temperature polymer electrolyte membrane electrolyzers, component choices and membrane electrode assembly (MEA) fabrication have pivotal roles in determining cell performance. Here, cobalt anodes were used in combination with different ionomers, membranes, and supporting electrolytes to delineate their effect on MEA performance in anion exchange membrane (AEM) based electrolyzers. Changes to the ionomer type suppress or enhance catalyst redox and were found to alter the resulting exchange current densities and Tafel slopes. Changes in membrane conductivity account for large differences in performance and overpotential losses among the different MEAs, with higher conductivity minimizing ohmic losses. Within supporting electrolytes, lower concentration results in lower conductivity and lower MEA performance; the performance, however, is higher in potassium hydroxide than bicarbonate. These experiments address the influence of individual components and their integration on cell-level performance, to help develop a pathway to an electrolyte free system while providing a foundation for studying electrode composition and component incorporation into MEAs.

25 ENERGY STORAGE↗

Effects of lithium salt concentration on graphited carbon microbead anodes in the piperidinium-based hybrid electrolytes

Graphical abstract: “Lithium aggregates” usually cause a significant decrease in Li{sup +} mobility and transfer efficiency. Therefore, as important as the problem of SEI, the content of lithium salt and the interaction between Li{sup +} and ILs’ anions should be taken into consideration in the optimization of ILs-based electrolytes for Li-ion batteries. - Highlights: • “Lithium aggregates” in piperidinium-based electrolytes are evidenced by IR and NMR. • High LiPF{sub 6} content could decrease Li{sup +} mobility due to “ionic aggregates”. • Lithium salt concentration is an important factor affecting graphite performances. - Abstract: The variations in LiPF{sub 6} concentration lead to the very different electrochemical performances of carbon microbeads anodes in the piperidinium-based hybrid electrolytes. The “two peaks” behaviors of lithium plating observed in cyclic voltammetry tests, and some detailed changes in infrared spectra and nuclear magnetic resonance indicates that the formation of “ionic aggregates” related to lithium ions”. Therefore, the excessive lithium salts in the piperidinium-based hybrid electrolytes, usually cause a significant decrease in Li{sup +} mobility and transfer efficiency. The main behaviors are that, when LiPF{sub 6} concentrations increased from 0.2 to 1.2 mol kg{sup −1}, the apparent migration energies (E{sub a}) increase largely from 8.83 to 21.16 kJ mol{sup −1}, while the lithium transference numbers (t{sub Li{sup +}}) drop markedly from 0.538 to 0.292.

36 MATERIALS SCIENCE↗

Unraveling local structures of Salt-in-Water and Water-in-Salt electrolytes via ab initio molecular dynamics

Water-in-salt electrolytes (WiSE) are attractive for electrochemical energy storage applications owing to their wide electrochemical stability windows and inherent safety. The high concentration of salts is widely known to suppress the decomposition of water, which otherwise limits the stability of conventional aqueous salt-in-water electrolytes (SiWE). Nevertheless, the microstructural features of WiSE that lead to this enhanced stability have not yet been fully elucidated. In this work, ab initio molecular dynamics simulations were performed to study the energetic, structural, and spectroscopic properties of LiTFSI SiWE and WiSE solutions. A detailed mapping of water-water and water-anion hydrogen bonding and cation–anion electrostatic interactions is reported for both electrolytes. Structural features are presented in terms of both radial and spatial distribution functions. Analysis of IR and vibrational power spectra reveal key differences in the intermolecular interactions in SiWE and WiSE that arise from modified solvation shell structures. Finally, the results obtained herein reveal the most important structural and spectroscopic differences between the electrolytes in normal and superconcentrated concentrations.

36 MATERIALS SCIENCE↗

Thermally Driven Interfacial Degradation between Li 7 La 3 Zr 2 O 12 Electrolyte and LiNi 0.6 Mn 0.2 Co 0.2 O 2 Cathode

Solid-state batteries offer higher energy density and enhanced safety compared to the present lithium-ion batteries using liquid electrolytes. A challenge to implement them is the high resistances, especially at the solid electrolyte interface with the cathode. Sintering at elevated temperature is needed in order to get good contact between the ceramic solid electrolyte and oxide cathodes and thus to reduce contact resistances. Many solid electrolyte and cathode materials react to form secondary phases. It is necessary to find out which phases arise as a result of interface sintering and evaluate their effect on electrochemical properties. Herein, we assessed the interfacial reactions between LiNi 0.6 Mn 0.2 Co 0.2 O 2 (NMC622) and Li 7 La 3 Zr 2 O 12 (LLZO) as a function of temperature in air. We prepared model systems by depositing thin-film NMC622 cathode layers on LLZO pellets. The thin-film cathode approach enabled us to use interface-sensitive techniques such as X-ray absorption spectroscopy in the near-edge as well as the extended regimes and identify the onset of detrimental reactions. We found that the Ni and Co chemical environments change already at moderate temperatures, on-setting from 500 °C and becoming especially prominent at 700 °C. By analyzing spectroscopy results along with X-ray diffraction, we identified Li 2 CO 3 , La 2 Zr 2 O 7 , and La(Ni,Co)O 3 as the secondary phases that formed at 700 °C. The interfacial resistance for Li transfer, measured by electrochemical impedance spectroscopy, increases significantly upon the onset and evolution of the detected interface chemistry. Our findings suggest that limiting the bonding temperature and avoiding CO 2 in the sintering environment can help to remedy the interfacial degradation.

36 MATERIALS SCIENCE↗

Toward the Understanding of the Reaction Mechanism of Zn/MnO2 Batteries Using Non-alkaline Aqueous Electrolytes

Zn/MnO 2 systems using non-alkaline aqueous electrolytes have attracted tremendous interest as rechargeable aqueous Zn ion batteries due to their safety and high specific capacities. Despite their promising electrochemical performance, however, their reaction mechanism has remained elusive. Here in this paper, we examined the structural evolution of cryptomelane α-MnO 2 cathode by ex situ transmission electron microscopy after electrochemical testing using two different non-alkaline aqueous Zn electrolytes with acetate and triflate salts of different pH values. We have discovered that the systems tested in both electrolytes exhibit a dissolution–deposition reaction mechanism through dissolution–deposition of Mn 2+ ions from/on the cathodes with a display of similar discharge/charge product formation. We have also found that the cell tested using the acetate electrolyte shows evidence of structural irreversibility that might contribute to its rapid capacity degradation. This finding offers an important insight into optimizing the cathode design for enhanced electrochemical function of aqueous Zn/MnO 2 batteries.

25 ENERGY STORAGE↗

The Effect of Fluoroethylene Carbonate as an Additive on the Solid Electrolyte Interphase on Silicon Lithium-Ion Electrodes

Fluoroethylene carbonate (FEC) has become a standard electrolyte additive for use with silicon negative electrodes, but how FEC affects solid electrolyte interphase (SEI) formation on the silicon anode’s surface is still not well understood. Herein, SEI formed from LiPF6-based carbonate electrolytes, with and without FEC, were investigated on 50 nm thick amorphous silicon thin film electrodes to understand the role of FEC on silicon electrode surface reactions. In contrast to previous work, anhydrous and anoxic techniques were used to prevent air and moisture contamination of prepared SEI films. This allowed for accurate characterization of the SEI structure and composition by X-ray photoelectron spectroscopy and time-of-flight secondary ion mass spectrometry depth profiling. These results show that FEC reduction leads to fluoride ion and LiF formation, consistent with previous computational and experimental results. Surprisingly, we also find that these species decrease lithium-ion solubility and increase the reactivity of the silicon surface. We conclude that the effectiveness of FEC at improving the Coulombic efficiency and capacity retention is due to fluoride ion formation from reduction of the electrolyte, which leads to the chemical attack of any silicon-oxide surface passivation layers and the formation of a kinetically stable SEI comprising predominately lithium fluoride and lithium oxide.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Structure, Chemistry, and Charge Transfer Resistance of the Interface between Li 7 La 3 Zr 2 O 12 Electrolyte and LiCoO 2 Cathode

All-solid-state batteries promise significant safety and energy density advantages over liquid-electrolyte batteries. The interface between the cathode and the solid electrolyte is an important contributor to charge transfer resistance. Strong bonding of solid oxide electrolytes and cathodes requires sintering at elevated temperatures. Knowledge of the temperature dependence of the composition and charge transfer properties of this interface is important for determining the ideal sintering conditions. To understand the interfacial decomposition processes and their onset temperatures, model systems of LiCoO 2 (LCO) thin films deposited on cubic Al-doped Li 7 La 3 Zr 2 O 12 (LLZO) pellets were studied as a function of temperature using interface-sensitive techniques. X-ray photoelectron spectroscopy, secondary ion mass spectroscopy, and energy-dispersive X-ray spectroscopy data indicated significant cation interdiffusion and structural changes starting at temperatures as low as 300 °C. La 2 Zr 2 O 7 and Li 2 CO 3 were identified as decomposition products after annealing at 500 °C by synchrotron X-ray diffraction. X-ray absorption spectroscopy results indicate the presence of also LaCoO 3 in addition to La 2 Zr 2 O 7 and Li 2 CO 3 . On the basis of electrochemical impedance spectroscopy and depth profiling of the Li distribution upon potentiostatic hold experiments on symmetric LCO|LLZO|LCO cells, the interfaces exhibited significantly increased impedance, up to 8 times that of the as-deposited samples after annealing at 500 °C. Here, our results indicate that lower-temperature processing conditions, shorter annealing time scales, and CO 2 -free environments are desirable for obtaining ceramic cathode|electrolyte interfaces that enable fast Li transfer and high capacity.

25 ENERGY STORAGE↗

Structures and Free Energies of Cerium Ions in Acidic Electrolytes

The Ce 3+ /Ce 4+ redox potential changes with the electrolyte, which could be due to unequal anion complexation free energies between Ce 3+ and Ce 4+ or a change in the solvent electrostatic screening. Ce complexation with anions and solvent screening also affect the solubility of Ce and charge transfer kinetics for electrochemical reactions involving waste remediation and energy storage. Here, we report the structures and free energies of cerium complexes n seven acidic electrolytes based on Extended X-ray Absorption Fine Structure, LTV vis, and Density Functional Theory calculations. Ce 3+ coordinates with nine water molecules as [Ce(H 2 O) 9 ] 3+ in all studied electrolytes. However, Ce 4+ complexes with anions in all electrolytes except HClO 4 . Thus, our results suggest that Ce 4+ anion complexation leads to the large shifts in standard redox potential. Long range screening effects are smaller than the anion complexation energies but could be responsible for changes in the Ce solubility with acid.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

The Chemistry of Electrolyte Reduction on Silicon Electrodes Revealed by in Situ ATR-FTIR Spectroscopy

While silicon is the most promising next-generation anode material for lithium-ion batteries (LIBs), silicon electrodes exhibit significant capacity fade with cycling. A common hypothesis is that the capacity loss is due to the solid electrolyte interphase (SEI) forming in the first cycle and becoming destabilized by large cyclic volume changes. A cell for in situ attenuated total reflection-Fourier transform infrared spectroscopy with controllable penetration depth was used to study the chemistry at the electrode–electrolyte interface. The SEI product precursors at the interface were successfully identified and differentiated from free or solvated solvent molecules in the bulk electrolyte. Intriguingly, for the most common electrolyte consisting of ethylene carbonate and diethyl carbonate, ethylene carbonate was found to directly reduce to lithium ethylene dicarbonate on the lithiated silicon surface and diethyl carbonate to selectively reduce to diethyl 2,5-dioxahexane dicarboxylate on the surface of the native silicon-oxide film. In conclusion, understanding this surface dependence of the SEI composition is critical to tuning the silicon electrode surface condition and, ultimately, enhancing the performance of future LIBs.

25 ENERGY STORAGE↗