Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “composite cathode”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 1,279 records · Page 71

Nucleation-promoting and growth-limiting synthesis of disordered rock-salt Li-ion cathode materials

Disordered rock-salt oxides and oxyfluorides are promising positive electrode materials for high-performance lithium-ion batteries free of nickel and cobalt. However, conventional synthesis methods rely on post-synthesis pulverization to achieve cycling-appropriate particle sizes, offering limited control over particle microstructure and crystallinity. This accelerates degradation and complicates secondary particle processing. Here we present a synthesis strategy that enhances nucleation while suppressing particle growth and agglomeration across various disordered rock-salt compositions, including lithium–manganese–titanium oxide, lithium–manganese–niobium oxide, and lithium–nickel–titanium oxide systems. Applied to Li 1.2 Mn 0.4 Ti 0.4 O 2 , this method yields highly crystalline, well-dispersed sub-200 nm particles that form homogeneous electrode films with stable cycling behavior. Tested in cells with lithium metal as the counter electrode, these electrodes deliver ~200 mAh/g with 85% capacity retention relative to the first cycle after 100 cycles (20 mA/g, 1.5–4.8 V), and an average discharge voltage loss of 4.8 mV per cycle, compared to 38.6% retention and 7.5 mV loss per cycle for electrodes derived from pulverized solid-state particles. This approach suggests a route to enhance the performance and durability of disordered rock-salt electrodes for sustainable lithium-ion batteries.

Batteries↗

Todorokite-type manganese oxide nanowires as an intercalation cathode for Li-ion and Na-ion batteries

Extended hydrothermal treatment at an elevated temperature of 220 °C allowed high yield synthesis of manganese oxide nanowires with a todorokite crystal structure suitable for ions intercalation. The flexible, high aspect ratio nanowires are 50–100 nm in diameter and up to several microns long, with 3 × 3 structural tunnels running parallel to the nanowire longitudinal axis. Moreover, the tunnels are occupied by magnesium ions and water molecules, with the chemical composition found to be Mg 0.2 MnO 2 ·0.5H 2 O. The todorokite nanowires were, for the first time, electrochemically tested in both Li-ion and Na-ion cells. A first discharge capacity of 158 mA h g -1 was achieved in a Na-ion system, which was found to be greater than the first discharge capacity in a Li-ion system (133 mA h g -1 ). In spite of the large structural tunnel dimensions, todorokite showed a significant first cycle capacity loss in a Na-ion battery. After 20 cycles, the capacity was found to stabilize around 50 mA h g -1 and remained at this level for 100 cycles. In a Li-ion system, todorokite nanowires showed significantly better capacity retention with 78% of its initial capacity remaining after 100 cycles. Rate capability tests also showed superior performance of todorokite nanowires in Li-ion cells compared to Na-ion cells at higher current rates. Finally, these results highlight the difference in electrochemical cycling behavior of Li-ion and Na-ion batteries for a host material with spacious 3 × 3 tunnels tailored for large Na + ion intercalation.

25 ENERGY STORAGE↗

Visualizing Crystallization Dynamics and Transformation Pathways of Disordered Rocksalt Oxides During Thermally Activated Sol–Gel Synthesis

Sol–gel synthesis is a wet-chemical processing route for fabricating functional materials with control over composition and microstructure at relatively low temperatures compared to conventional solid-state synthesis. While sol–gel process initiates with intermixed molecular precursors, the early-stage nucleation pathways are insufficiently understood. Here, in this study, the chemical and structural transformation of ion disordered rocksalt (DRX) Li 1.2 Mn 0.4 Ti 0.4 O 2 (LMTO), a promising cathode material for lithium batteries, is studied by multiscale characterizations. In situ heating transmission electron microscopy (TEM) using a liquid cell visualizes and identifies crystallization pathways at the nanoscale. While some regions follow a classical multi-step transition through thermodynamically stable intermediates, others exhibit a kinetic shortcut via a localized amorphous matrix to directly form the DRX structure. Macroscale Fourier transform infrared spectroscopy corroborates the findings and reveals that transition metal ions are more strongly incorporated into the acetate-coordinated network than lithium. Although in situ heating TEM captures diverse local transformation pathways, in situ synchrotron X-ray diffraction indicates that the macroscopic transformation proceeds predominantly through spinel LMTO and lithium titanates toward DRX-LMTO. The findings uncover the spatiotemporal chemical and structural transformations in sol–gel derived DRX-LMTO materials, and call for fine-tuning of such sol–gel chemistries to manipulate the crystallization pathways and achieve target material homogeneity more efficiently.

cathode material↗

Electrochemical lithium insertion in the solid solution Bi{sub 2}WO{sub 6}-Sb{sub 2}WO{sub 6} with Aurivillius framework

Following the structural evolution of the Aurivillius crystalline framework in the solid solution Bi{sub 2}WO{sub 6}-Sb{sub 2}WO{sub 6} we have carried out an electrochemical lithium insertion study in this system. A slight loss of the specific capacity of the electrochemical cell was observed as amount of Sb was increased. In general, the different compositions within solid solution Bi{sub 2-x}Sb{sub x}WO{sub 6} (0.25 {<=} x {<=} 0.75) exhibited a similar behaviour featured mainly by two semiconstant potential regions located at 1.7 and 0.8 V versus Li{sup +}/Li{sup o}. The oxide Sb{sub 2}WO{sub 6} with Autivillius structure but without Bi was tested as cathode too. The maximum amount of lithium inserted, 13.5 lithium atoms per formula, is the same amount inserted in its homologous bismuth oxide Bi{sub 2}WO{sub 6}.

36 MATERIALS SCIENCE↗

Unravelling structural ambiguities in lithium- and manganese-rich transition metal oxides

Although Li- and Mn-rich transition metal oxides have been extensively studied as high-capacity cathode materials for Li-ion batteries, the crystal structure of these materials in their pristine state is not yet fully understood. Here we apply complementary electron microscopy and spectroscopy techniques at multi-length scale on well-formed Li1.2(Ni0.13Mn0.54Co0.13)O2 crystals with two different morphologies as well as two commercially available materials with similar compositions, and unambiguously describe the structural make-up of these samples. Systematically observing the entire primary particles along multiple zone axes reveals that they are consistently made up of a single phase, save for rare localized defects and a thin surface layer on certain crystallographic facets. Finally and more specifically, we show the bulk of the oxides can be described as an aperiodic crystal consisting of randomly stacked domains that correspond to three variants of monoclinic structure, while the surface is composed of a Co- and/or Ni-rich spinel with antisite defects.

36 MATERIALS SCIENCE↗

Oxygen Transport Kinetics in Infiltrated SOFCs Cathode by Electrical Conductivity Relaxation Technique

Infiltration has attracted increasing attention as an effective technique to modify SOFC cathodes to improve cell electrochemical performance while maintaining material compatibility and long-term stability. However, the infiltrated material's effect on oxygen transport is still not clear and detailed knowledge of the oxygen reduction reaction in infiltrated cathodes is lacking. In this work, the technique of electrical conductivity relaxation (ECR) is used to evaluate oxygen exchange in two common infiltrated materials, Ce{sub 0.8}Sm{sub 0.2}O{sub 1.9} and La{sub 0.6}Sr{sub 0.4}CoO{sub 3-δ}. The ECR technique is also used to examine the transport processes in a composite material formed with a backbone of La{sub 0.6}Sr{sub 0.4}Co{sub 0.2}Fe{sub 0.8}O{sub 3-δ} and possessing a thin, dense surface layer composed of the representative infiltrate material. Both the surface oxygen exchange process and the oxygen exchange coefficient at infiltrate/LSCF interface are reported. ECR testing results indicate that the application of infiltrate under certain oxygen partial pressure conditions produces a measureable increase in the fitted oxygen exchange parameter. It is presently only possible to generate hypotheses to explain the observation. However the correlation between improved electrochemical performance and increased oxygen transport measured by ECR is reliably demonstrated. The simple and inexpensive ECR technique is utilized as a direct method to optimize the selection of specific infiltrate/backbone material systems for superior performance.

30 DIRECT ENERGY CONVERSION↗

Examination of Hybrid Metal Coatings for Mitigation of Fission Product Release and Corrosion Protection of LWR SiC/SiC

There is a need to increase the safety margins of current and future light water reactors (LWRs) due to the unfortunate events at Fukushima Daiichi Nuclear Plant. Safety is crucial to restore public confidence in nuclear energy, acknowledged as an economical, high-­density energy solution to climate change. The development of accident-­tolerant fuel (ATF) concepts is crucial to this endeavor. The objective of ATF is to delay the consequences of accident progression, being inset in high temperature steam and maintaining high thermomechanical strength for radionuclide retention. The use of advanced SiCf-­SiC composite as a substitute for zircaloy-­based cladding is being considered. However, at normal operations, SiC is vulnerable to the reactor coolant and may corrode at an unacceptable rate. As a ceramic-­matrix composite material, it is likely to undergo microcracking operation, which may compromise the ability to contain gaseous fission products. A proposed solution to both issues is the application of mitigation coatings for use in normal operations. At Oak Ridge National Laboratory (ORNL), three coating technologies have been investigated with industry collaborators and vendors. These are electrochemical deposition, cathodic arc physical vapor deposition (PVD hereafter) and vacuum plasma spray (VPS). The objective of this document is to summarize these processing technologies, the resultant as-­processed microstructures and properties of the coatings. In all processes, substrate constraint resulted in substantial tensile stresses within the coating layer. Each technology must mitigate this tensile stress. Electrochemical coatings use chromium as the coolant facing material, and are deposited on a nickel or carbon “bond coat”. This is economical but suffers microcracking in the chromium layer. PVD-­based coatings use chromium and titanium in both metallic form and nitrides, and can be deposited defense-­in-­depth as multilayers. This vapor method eliminated tensile stress during processing and coatings were up to ~30 μm thick without microcracking. VPS produced coatings based on Zircaloy-2, which has a proven reactor-­compatibility. The tensile stresses appearred to be partially mitigated by annealing. Analysis showed that VPS coatings required further optimizations to prevent adverse reactions with the substrate and need a minimum thickness of ~50 μm. In addition, development of coatings are constrained by neutronic depletion analysis, which clearly indicated enrichment as an issue if the coating is too thick. Based on the present work, the cathodic arc PVD technology was considered ready for the extensive testing and evaluation on cladding materials due to their ability to mitigate the excessive tensile stresses and the reasonable coating quality achieved. The VPS Zircaloy-­2 coating technology required additional development toward mitigation of issues related to the substrate reaction and porosity. In the future, PVD and VPS will have be scaled upon successful development and demonstration. Electrochemical coatings, which are proven scalability, currently require development to mitigate issues related to the tensile stress after deposition.

21 SPECIFIC NUCLEAR REACTORS AND ASSOCIATED PLANTS↗

Electrochemical hydrogen Storage Systems

As the global need for energy increases, scientists and engineers have found a possible solution by using hydrogen to power our world. Although hydrogen can be combusted as a fuel, it is considered an energy carrier for use in fuel cells wherein it is consumed (oxidized) without the production of greenhouse gases and produces electrical energy with high efficiency. Chemical storage of hydrogen involves release of hydrogen in a controlled manner from materials in which the hydrogen is covalently bound. Sodium borohydride and aminoborane are two materials given consideration as chemical hydrogen storage materials by the US Department of Energy. A very significant barrier to adoption of these materials as hydrogen carriers is their regeneration from 'spent fuel,' i.e., the material remaining after discharge of hydrogen. The U.S. Department of Energy (DOE) formed a Center of Excellence for Chemical Hydrogen Storage, and this work stems from that project. The DOE has identified boron hydrides as being the main compounds of interest as hydrogen storage materials. The various boron hydrides are then oxidized to release their hydrogen, thereby forming a 'spent fuel' in the form of a lower boron hydride or even a boron oxide. The ultimate goal of this project is to take the oxidized boron hydrides as the spent fuel and hydrogenate them back to their original form so they can be used again as a fuel. Thus this research is essentially a boron hydride recycling project. In this report, research directed at regeneration of sodium borohydride and aminoborane is described. For sodium borohydride, electrochemical reduction of boric acid and sodium metaborate (representing spent fuel) in alkaline, aqueous solution has been investigated. Similarly to literature reports (primarily patents), a variety of cathode materials were tried in these experiments. Additionally, approaches directed at overcoming electrostatic repulsion of borate anion from the cathode, not described in the previous literature for electrochemical reduction of spent fuels, have been attempted. A quantitative analytical method for measuring the concentration of sodium borohydride in alkaline aqueous solution has been developed as part of this work and is described herein. Finally, findings from stability tests for sodium borohydride in aqueous solutions of several different compositions are reported. For aminoborane, other research institutes have developed regeneration schemes involving tributyltin hydride. In this report, electrochemical reduction experiments attempting to regenerate tributyltin hydride from tributyltin chloride (a representative by-product of the regeneration scheme) are described. These experiments were performed in the non-aqueous solvents acetonitrile and 1,2-dimethoxyethane. A non-aqueous reference electrode for electrolysis experiments in acetonitrile was developed and is described. One class of boron hydrides, called polyhedral boranes, became of interest to the DOE due to their ability to contain a sufficient amount of hydrogen to meet program goals and because of their physical and chemical safety attributes. Unfortunately, the research performed here has shown that polyhedral boranes do not react in such a way as to allow enough hydrogen to be released, nor do they appear to undergo hydrogenation from the spent fuel form back to the original hydride. After the polyhedral boranes were investigated, the project goals remained the same but the hydrogen storage material was switched by the DOE to ammonia borane. Ammonia borane was found to undergo an irreversible hydrogen release process, so a direct hydrogenation was not able to occur. To achieve the hydrogenation of the spent ammonia borane fuel, an indirect hydrogenation reaction is possible by using compounds called organotin hydrides. In this process, the organotin hydrides will hydrogenate the spent ammonia borane fuel at the cost of their own oxidation, which forms organotin halides. To enable a closed-loop cycle, our task was then to be able to hydrogenate the organotin halides back to their hydride form. In addition to this experimental work, a parallel project was carried out to develop a new model of electrochemical impedance spectroscopy (EIS) that could be used to define the mechanisms of the electrochemical hydrogenation reactions. The EIS technique is capable of probing complex chemical and electrochemical reactions, and our model was written into a computer code that allowed the input of experimental EIS data and the extraction of kinetic parameters based on a best-fit analysis of theoretical reaction schemes. Finally, electrochemical methods for hydrogenating organic and metallo-organic materials have been explored.

08 HYDROGEN↗

Extending Ion Engine Technology to NEXT and Beyond

Extending ion engine technology beyond the current state-of-the art primary interplanetary electric propulsion system, the 2.3-kW NASA Solar Electric Propulsion Technology and Applications Readiness (NSTAR) system, will require thrusters with improved propellant throughput and total impulse capability. Many of the design choices that culminated in the NSTAR thrusters must be revisited, and their application to next generation ion engine technology must be evaluated. The concept of derating, which was successfully employed in NSTAR, has been applied to the 40 cm NASA Evolutionary Xenon Thruster (NEXT) currently under development at NASA Glenn Research Center (GRC). At 5-kW, NEXT operates with the same average beam current density as NSTAR, and at 10-kW, the peak beam current density is only ten percent greater than NSTAR. The result is that similar Ion optics technology is expected to yield comparable lifetime. Thick-accelerator- grid ion optics are also being tested to realize additional lifetime benefits. A 40-A discharge cathode is being developed for NEXT based on scaling the NSTAR design. Nevertheless, the experiences of the NSTAR ground tests and the thruster on the Deep Space One spacecraft indicate that the discharge cathode wear must be studied experimentally and theoretically to ensure that it meets the lifetime requirements. Although NEXT is in its infancy, investigations have already begun to examine possible modifications to engine design for even higher-power and higher-specific impulse engines. Ion optics using alternate materials such as titanium, graphite, or carbon-carbon composite are currently being investigated due to their low sputter yields at high voltage. To avoid the difficulties encountered using electrodes at high-currents, the use of a microwave-based ion thruster is under investigation for potential high-power ion thruster systems requiring long lifetimes. Additionally, alternative propellants are being considered for applications requiring high-specific impulse (>> 5000 s) and extremely long-life (>> 15,000 hr). Testing requirements make condensable propellants attractive for high-power engines. Although the NSTAR ion engine demonstrated the flight maturity of ion thruster technology, many challenges remain for the development of thrusters with improved propellant throughput and power handling capabilities.

Domonkos, Matthew T.↗

Activity and Evolution of Vapor Deposited Pt-Pd Oxygen Reduction Catalysts for Solid Acid Fuel Cells

The performance of hydrogen fuel cells based on the crystalline solid proton conductor CsH2PO4 is circumscribed by the mass activity of platinum oxygen reduction catalysts in the cathode. Here we report on the first application of an alloy catalyst in a solid acid fuel cell, and demonstrate an activity 4.5 times greater than Pt at 0.8 V. These activity enhancements were obtained with platinum-palladium alloys that were vapor-deposited directly on CsH2PO4 at 210 C. Catalyst mass activity peaks at a composition of 84 at% Pd, though smaller activity enhancements are observed for catalyst compositions exceeding 50 at% Pd. Prior to fuel cell testing, Pd-rich catalysts display lattice parameter expansions of up to 2% due to the presence of interstitial carbon. After fuel cell testing, a Pt-Pd solid solution absent of lattice dilatation and depleted in carbon is recovered. The structural evolution of the catalysts is correlated with catalyst de-activation.

Papandrew, Alexander B↗

Lithium-air batteries, method for making lithium-air batteries

The invention provides a method for generating Li.sub.2O.sub.2 or composites of it, the method uses mixing lithium ions with oxygen ions in the presence of a catalyst. The catalyst comprises a plurality of metal clusters, their alloys and mixtures, each cluster consisting of between 3 and 18 metal atoms. The invention also describes a lithium-air battery which uses a lithium metal anode, and a cathode opposing the anode. The cathode supports metal clusters, each cluster consisting of size selected clusters, taken from a range of between approximately 3 and approximately 18 metal atoms, and an electrolyte positioned between the anode and the cathode.

25 ENERGY STORAGE↗

Defect Chemistry in High‐Voltage Cathode Materials for Lithium‐Ion Batteries

High-voltage cathodes (HVCs) have emerged as a paramount role for the next-generation high-energy-density lithium-ion batteries (LIBs). However, the pursuit of HVCs comes with inherent challenges related to defective structures, which significantly impact the electrochemical performance of LIBs. The current obstacle lies in the lack of a comprehensive understanding of defects and their precise effects. This perspective aims to provide insights into defect chemistry for governing HVCs. The classifications, formation mechanisms, and evolution of defects are outlined to explore the intricate relationship between defects and electrochemical behavior. The pressing need for cutting-edge characterization techniques that comprehensively investigate defects across various temporal and spatial scales is emphasized. Building on these fundamental understandings, engineering strategies such as composition tailoring, morphology design, interface modification, and structural control to mitigate or utilize defects are thoroughly discussed for enhanced HVCs performance. Furthermore, these insights are expected to provide vital guidelines for developing high-performance HVCs for next-generation high-energy lithium-ion batteries.

cross-scale characterization↗

The preparation and characterization of iron fluorides polymorphs FeF{sub 3}·0.33H{sub 2}O and β-FeF{sub 3}∙3H{sub 2}O as cathode materials for lithium-ion batteries

Graphical abstract: Better rate capability and cycling performance were observed for β-FeF{sub 3}·3H{sub 2}O/C prepared by mechano-chemical synthesis. - Highlights: • A novel mechano-chemical preparation method. • The use of NH{sub 4}F as starting material. • Better electro-chemical performance in the case of β-FeF{sub 3}·3H{sub 2}O/C. - Abstract: Two kinds of iron fluorides, FeF{sub 3}·0.33H{sub 2}O and β-FeF{sub 3}∙3H{sub 2}O, have been synthesized by different chemical routes using Fe(NO{sub 3}){sub 3}·9H{sub 2}O and NH{sub 4}F as precursors and investigated as cathode materials for secondary lithium batteries. β-FeF{sub 3}·3H{sub 2}O was obtained via a mechano-chemical process and FeF{sub 3}·0.33H{sub 2}O was obtained by a precipitation reaction from ethanol solution. To further improve their electrochemical properties, a ball milling process with carbon has been used to form composites. The fluorides were characterized by X-ray diffraction (XRD), thermal analysis, FTIR spectroscopy, galvanostatic charge/discharge and cyclic voltammetry measurements. The results showed that the as-prepared β-FeF{sub 3}·3H{sub 2}O/C exhibited better rate performance and cycling stability. It exhibited an initial discharge capacity of 199.6 mA h g{sup −1} at a current density of 20 mA g{sup −1} in a voltage range of 1.8–4.5 V and still reserved a discharge capacity of about 146.5 mA h g{sup −1} after 10 cycles. Only a capacity loss of 15 mA h g{sup −1} and 7 mA h g{sup −1} was observed when the current density was at 40 mA g{sup −1} and 80 mA g{sup −1}, respectively.

36 MATERIALS SCIENCE↗

Technology development for phosphoric acid fuel cell powerplant, phase 2

The development of materials, cell components, and reformers for on site integrated energy systems is described. Progress includes: (1) heat-treatment of 25 sq cm, 350 sq cm and 1200 sq cm cell test hardware was accomplished. Performance of fuel cells is improved by using this material; (2) electrochemical and chemical corrosion rates of heat-treated and as-molded graphite/phenolic resin composites in phosphoric acid were determined; (3) three cell, 5 in. x 15 in. stacks operated for up to 10,000 hours and 12 in. x 17 in. five cell stacks were tested for 5,000 hours; (4) a three cell 5 in. x 15 in. stack with 0.12 mg Pt/sq cm anodes and 0.25 mg Pt/sq cm cathodes was operated for 4,500 hours; and (5) an ERC proprietary high bubble pressure matrix, MAT-1, was tested for up to 10,000 hours.

Christner, L.↗

Platinum nickel catalyst alloy

A Pt--Ni catalyst is provided which demonstrates an unusually high oxygen reduction mass activity. In some embodiments, the Pt--Ni catalyst is a Pt--Ni binary alloy. In some embodiments, the catalyst may be characterized as having a Pt fcc lattice parameter of less than 3.71 Angstroms or 0.371 nm. In some embodiments the catalyst has a Pt fcc lattice parameter of between 3.69 Angstroms (or 0.369 nm) and 3.73 Angstroms (or 0.373 nm). In some embodiments, the catalyst may be characterized as having a composition of close to Pt.sub.xNi.sub.(1-x), where x is between 0.2 and 0.4. In some embodiments the catalyst comprises nanostructured elements comprising microstructured support whiskers bearing a thin film of nanoscopic catalyst particles comprising a catalyst material described above. The catalyst may be particularly useful as a fuel cell catalyst and more specifically as a fuel cell cathode catalyst.

Debe, Mark K.↗

Sulfur Solutions: Advancing High Voltage and High Energy Lithium Batteries with Organosulfur Electrolytes

Achieving energy densities exceeding 350 Wh kg -1 while operating at elevated voltages (>4.5 V vs Li/Li + ) is attainable through judicious selection of electrochemical pairs at the cathode and anode. However, current state-of-the-art electrolytes exhibit limited stability when exposed to systems operating at or above 4.3 V. This limitation contributes to the degradation of electrode materials and raises critical safety concerns, impeding the commercialization of such systems. Consequently, there has been a notable surge in research efforts aimed at developing innovative electrolyte compositions capable of supporting high-voltage lithium-ion batteries (LIBs). A substantial portion of this research has focused on the family of organosulfur molecules, which possess high oxidative stability. Organosulfur salts also facilitate the formation of dense, ionically conductive solid electrolyte interfaces (SEI) and demonstrate excellent solubility. This article provides a comprehensive overview of the field of organosulfur electrolyte components for their applications in energy storage, encompassing solvents, alternative conducting salts, and additives. It emphasizes the idea that the deliberate design of electrolyte compositions is instrumental in controlling electrode passivation, with organosulfur-based structures historically proving advantageous in every aspect of the electrolyte. Crucially, it should be noted that many of these components are commercially available, holding significant implications for industrial applications.

25 ENERGY STORAGE↗

Correlating Catalyst Design and Discharged Product to Reduce Overpotential in Li-CO 2 Batteries

Li-CO 2 batteries with dual efficacy for greenhouse gas CO 2 sequestration and high energy output have been regarded as a promising electrochemical energy storage technology. However, battery feasibility has been hampered by inferior electrochemical performance due to large overpotentials and low cyclability primarily caused by the difficult decomposition of ultra-stable Li 2 CO 3 during charge. The use of cathode catalysts has been highlighted as a promising solution and catalyst properties, as well as the nature of discharge products, are closely correlated with electrochemical performance. Here, the catalyst design strategies that include active site enrichment, electrical transport enhancement, and mass transfer improvement are summarized. Catalyst effects on product decomposition are then subsequently introduced, while product geometry and chemical composition will be explored, with an emphasis on the formation/decomposition of Li 2 C 2 O 4 instead of Li 2 CO 3 . Building on previous research, future directions that facilitate improvements in catalyst design are put forward to reinforce the fundamental development of Li-CO 2 batteries.

25 ENERGY STORAGE↗

Direct reuse of graphite and lithium nickel manganese cobalt oxide (NMC) recovered from ultrafast-laser ablation debris in Li-ion battery electrodes

Here we demonstrate that debris collected from the ultrafast-laser ablation of graphite anodes can be directly reused in a lithium-ion battery with little to no negative effects on electrochemical performance. Further, we show that while post-ablation NMC (LiNi 0.33 Mn 0.33 Co 0.33 O) cathode debris will require additional processing before being incorporated into an electrode, its critical materials (nickel, manganese, and cobalt) are not lost during ablation and can be recovered for recycling. Pre- and post-ablation materials are characterized with a suite of diagnostics, including SEM, TEM, X-ray CT, EDS, and XRD, to study changes in material morphology, composition and crystal structure. Graphite exhibited little to no morphological or compositional changes and a slight annealing of its crystal structure. NMC underwent profound morphological and crystallographic changes, but retained its elemental composition. Finally, post-ablation materials were re-manufactured into electrodes and cycled vs lithium metal. Graphite showed equal or better capacity and Coulombic efficiency compared to pre-ablation electrodes, while the post-ablation NMC exhibited severely reduced electrochemical performance. Furthermore, we discuss the outlook for application of this work to advanced manufacturing lines that produce next-generation, laser-patterned electrodes.

25 ENERGY STORAGE↗