Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “alloy solidification”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 1,279 records · Page 71

Real-Time X-Ray Microscopy of Al-Cu Eutectic Solidification

Recent improvements in the resolution of the X-ray Transmission Microscope (XTM) for Solidification Studies provide microstructure feature detectability down to 5 micrometers during solidification. This presentation will show the recent results from observations made in real-time of the solid-liquid interfacial morphologies of the Al-CuAI2 eutectic alloy. Lamellar dimensions and spacings, transitions of morphology caused by growth rate changes, and eutectic grain structures are open to measurements. A unique vantage point viewing the face of the interface isotherm is possible for the first time with the XTM due to its infinite depth of field. A video of the solid-liquid interfaces seen in-situ and in real-time will be shown.

Kaukler, William F.↗

Role of Cyclic Phase Transitions in Additive Manufacturing of Metals and Alloys - Lessons Learned from Welding Science

Additive manufacturing (also known as 3D printing) of metals is considered to be a disruptive technology, able to produce limited number of high value components with topologically optimized geometries and functionalities. Realization of the above potential for real-world applications is stifled by lack of standard computational design tools; component certifications, varied starting powder feed stock compositions, methods to probe thermomechanical processes, microstructural homogeneity, residual stress, as well as, anisotropic static- and dynamic-material properties. Detailed research of direct energy deposition, laser- and electron-powder bed additive manufacturing demonstrates that the underlying physics of these processes are very similar to welding, except for complex boundary conditions. This paper will review published literature and on-going research with reference to fundamental aspects of heat and mass transfer, solidification under large (103 to 105 K/m) thermal gradients and (10-3 to 100 m/s) liquid solid-interface velocities, as well as, solid->solid transformation under repeated thermal excursions. Case studies on model based qualification of Ni- and Ti- alloy builds made by additive manufacturing (AM), based on the above fundamental knowledge will be discussed.

Babu, Sudarsanam Suresh↗

Enhancing microsegregation during rapid directional solidification through ternary microalloying

The nano-cellular dendritic microstructure formed during rapid directional solidification in powder bed fusion additive manufacturing creates unique properties such as simultaneous improvement in strength and ductility. However, process control of microsegregation features remains challenging due to low sensitivity of critical solidification mechanisms to process parameters. This study leverages microalloying to achieve large changes in dendrite composition, microstructure, and interdendritic zone width during laser powder bed fusion without modifying process parameters. CALPHAD simulations predict that the addition of Zr significantly steepens the solidus line of the dilute Cu-Cr alloy system, leading to enhanced Cr rejection into the melt and greater than 95% reduction in solubility of Cr in the solidified Cu matrix. Experimental validation using time-of-flight secondary ion mass spectrometry and Kelvin probe force microscopy reveals that the ternary alloy containing 0.01 wt% Zr exhibited wider interdendritic regions compared to the binary, a significantly higher number of Cr-rich particles within interdendritic regions, near-complete ejection of oxygen impurities from the matrix, and greater nanoscale work function contrast. These features indicate more aggressive Cr segregation in the presence of Zr and a purer Cu matrix and provide a potentially robust method for engineering the nano-cellular dendritic solidification microstructure.

CALPHAD↗

Nanocrystalline Material (FINEMET) (Rev.01)

Nanocrystalline materials are emerging soft magnetic materials that possess grain sizes on the order of a billionth of a meter and possess extremely useful magnetic properties. These materials fi ll the gap between amorphous materials (without any long-range order) and conventional (coarse-grained) materials. Nanocrystalline alloys are materials on the basis of Fe (iron), Si (silicon), and B (boron), with additions of Nb (niobium) and Cu (copper). Typically, they are produced through a rapid solidification process as a thin, ductile ribbon. Initially the ribbon is in the amorphous state, then crystallized in a subsequent heat treatment to promote nano-crystallization (~10-20 nanometers). Once nano-crystallized, they exhibit low core loss and magnetostriction, while maintaining high saturation induction and permeability. A variety of forms can be manufactured, including toroidal, rectangular, racetrack and block cores.

36 MATERIALS SCIENCE↗

A study of reduced chromium content in a nickel-base superalloy via element substitution and rapid solidification processing

A study of reduced chromium content in a nickel base superalloy via element substitution and rapid solidification processing was performed. The two elements used as partial substitutes for chromium were Si and Zr. The microstructure of conventionally solidified materials was characterized using microscopy techniques. These alloys were rapidly solidified using the chill block melt spinning technique and the rapidly solidified microstructures were characterized using electron microscopy. The spinning technique and the rapidly solidified microstructures was assessed following heat treatments at 1033 and 1272 K. Rapidly solidified material of three alloys was reduced to particulate form and consolidated using hot isostatic pressing (HIP). The consolidated materials were also characterized using microscopy techniques. In order to evaluate the relative strengths of the consolidated alloys, compression tests were performed at room temperature and 1033 K on samples of as-HIPed and HIPed plus solution treated material. Yield strength, porosity, and oxidation resistance characteristics are given and compared.

Powers, William O.↗

Welding of gamma titanium aluminide alloys

An article made of a gamma titanium aluminide alloy is welded, as for example in the weld repair of surface cracks, by removing foreign matter from the area to be welded, first stress relieving the article, cooling the entire article to a welding temperature of from about 1000.degree. F. to about 1400.degree. F., welding a preselected region in an inert atmosphere at the welding temperature, and second stress relieving the article. Welding is preferably accomplished by striking an arc in the preselected region so as to locally melt the alloy in the preselected region, providing a filler metal having the same composition as the gamma titanium aluminide alloy of the article, and feeding the filler metal into the arc so that the filler metal is melted and fused with the article to form a weldment upon solidification.

Smashey, Russell W.↗

Microstructural Characteristics of U-Zr Ingot Slug and Atomized Powder for SFR metal Fuel

Rod-type fuel slugs and spherical powder of U- 10wt.%Zr alloy was also fabricated and characterized in microstructure by injection casting, gravity casting and centrifugal atomization process. U grains became finer from ∼30μm in conventionally ingot rod to ∼2μm in atomized powder. Laminar structure became so fine from ∼0.2μm in conventionally cast ingot rod to 0.05∼0.1μm in atomized powder. Metallic fuels such as U-Zr and U-Pu-Zr alloys have been considered as a nuclear fuel for a sodium-cooled fast reactor (SFR), related to the closed fuel cycle for managing minor actinides and reducing a high radioactivity levels since the 1980's. Metallic fuel slugs of U-Pu-Zr alloys for SFR have conventionally been fabricated by an injection casting method. U-Pu-Zr alloy melts are injected and cast into quartz tube molds during injection casting. Metallic fuel slugs are collected by fracturing quartz tubes from the molds. Demolded quartz tubes are treated with radioactive wastes. Recently, management of minor actinides (MA) became an important issue because direct disposal of the long-lived MA can be a long-term burden for a tentative repository up to several hundreds of thousand years. The metallic fuel for SFR should be remotely fabricated under a radiation shielded environment such as a hot cell, because it contains highly radioactive MA such as Np, Am and Cm. The addition of MA in the fuel composition introduces new challenges in the manufacturing of a metallic fuel slug. Am has a high vapor pressure under a vacuum atmosphere at above a melting temperature of U-Zr or U-Pu-Zr. Used graphite crucibles and quartz molds cannot be recycled easily because of difficult decontamination of radioactive residues on their surfaces. It is necessary to minimize the vaporization of Am and volume of radioactive wastes. Atomized metallic fuel does not need these quartz molds during fabrication, as uranium alloys are prepared as a particle form. It is possible to reduce the formation of radioactive wastes by applying the fabrication process of a particulate metallic fuel. Metallic fuel having a fine microstructure, which originates from a rapid solidification effect during atomization process, results in a higher FG release rate during irradiation. In the case of applying a new forming method such as vibrocompaction in Zr sheath, the sheath can act as a reliable FCCI (fuel/cladding chemical interaction) barrier and a re-constraint for external elongation. In addition, atomized fuel powder, dispersed in a Na liquid metal having a high thermal conductivity, may have a lower temperature distribution during irradiation. In order to develop an efficient fabrication process of metallic fuel for SFR, U-Zr ingot rods were fabricated in a lab-scale with various casting methods. Rod-type U-Zr fuel slugs were fabricated by gravity casting and injection casting. Spherical powder of U-Zr alloy was also fabricated by centrifugal atomization. And then, the microstructural characteristics were investigated by using electron microscopes and energy-dispersive electron X-ray spectroscopy. Atomized U-10Zr powder generally showed spherical morphology of below 200 μm in particle size. U grains became finer from ∼30 μm in conventionally ingot rod to ∼2 μm in atomized powder. Laminar structure became so fine from ∼0.2 μm in conventionally cast ingot rod to 0.05∼0.1 μm in atomized powder. Atomized particulate metallic fuel for SFR has a fine microstructure, resulting in a higher fission gas release rate during irradiation. (authors)

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Characterization of complex carbide–silicide precipitates in a Ni–Cr–Mo–Fe–Si alloy modified by welding

Nickel based alloys of the type Hastelloy-N™ are ideal candidate materials for molten salt reactors, as well as for applications such as pressure vessels, due to their excellent resistance to creep, oxidation and corrosion. In this work, the authors have attempted to understand the effects of welding on the morphology, chemistry and crystal structure of the precipitates in the heat affected zone (HAZ) and the weld zone of a Ni–Cr–Mo–Fe–Si alloy similar to Hastelloy-N™ in composition, by using characterization techniques such as scanning and transmission electron microscopy. Two plates of a Ni–Cr–Mo–Fe–Si alloy GH-3535 were welded together using a TiG welding process without filler material to achieve a joint with a curved molten zone with dendritic structure. It is evident that the primary precipitates have melted in the HAZ and re-solidified in a eutectic-like morphology, with a chemistry and crystal structure only slightly different from the pre-existing precipitates, while the surrounding matrix grains remained unmelted, except for the zones immediately adjacent to the precipitates. In the molten zone, the primary precipitates were fully melted and dissolved in the matrix, and there was enrichment of Mo and Si in the dendrite boundaries after solidification, and re-precipitation of the complex carbides/silicides at some grain boundaries and triple points. The nature of the precipitates in the molten zone varied according to the local chemical composition. - Graphical abstract: Display Omitted - Highlights: • Ni-based alloy with Cr, Mo, Si, Fe and C was welded, examined with SEM, EBSD, and TEM. • Original Ni{sub 2}(Mo,Cr){sub 4}(Si,C) carbides changed from equiaxed to lamellar shape in HAZ. • Composition and crystal structure remained almost unchanged in HAZ. • Original carbides changed to lamellar Ni{sub 3}(Mo,Cr){sub 3}(Si,C) in some cases in weld metal. • Precipitates were mostly incoherent, but semi-coherent in some cases in weld metal.

36 MATERIALS SCIENCE↗

On the existence of orthorhombic martensite in a near-α titanium base alloy used for additive manufacturing

Additive manufacturing is a state-of-the-art production technology to produce tailor-made and highly complex parts. Among various other alloys, Ti base alloys are frequently used in this manufacturing technique due to their well-balanced properties and their wide range of applications. Allotropic phases and the occurrence of athermal phase transformations are the main reasons why these alloys hold a great development potential and are the basis of extensive use. High cooling rates during manufacturing lead to martensitic phases and the formation of nanometer-sized microstructures resulting in extraordinary strength. Simultaneously, such high cooling rates cause a high amount of lattice defects and the occurrence of residual stresses, which finally may result in delamination effects and cracks. Usually, a common approach to reduce residual stresses during additive manufacturing is to decrease thermal gradients by increasing the heat input or preheating the building platform. Instead of applying the typical approaches to lower thermal gradients, this study deals with the origin of the ‘softer’ orthorhombic martensite by accelerating the solidification process. The implementation of the orthorhombic phase in bulk components was inspired by a new phase transformation herein reported for the first time in the powder material, which also validates the possible occurrence of two martensitic phases in the same alloy. Various sophisticated characterization techniques like high energy and high-temperature X-ray diffraction, high-resolution transmission electron microscopy as well as atom probe tomography were applied to characterize this softer orthorhombic martensitic phase in detail aiming to highlight the opportunities accompanied by this new approach for additive manufacturing of titanium alloys.

36 MATERIALS SCIENCE↗

Cost analysis of advanced turbine blade manufacturing processes

A rigorous analysis was conducted to estimate relative manufacturing costs for high technology gas turbine blades prepared by three candidate materials process systems. The manufacturing costs for the same turbine blade configuration of directionally solidified eutectic alloy, an oxide dispersion strengthened superalloy, and a fiber reinforced superalloy were compared on a relative basis to the costs of the same blade currently in production utilizing the directional solidification process. An analytical process cost model was developed to quantitatively perform the cost comparisons. The impact of individual process yield factors on costs was also assessed as well as effects of process parameters, raw materials, labor rates and consumable items.

Barth, C. F.↗

Quench Module Insert Capabilities and Development Test Results

The Quench Module Insert is a directional solidification furnace that will operate in the Materials Science Research Rack (MSRR) on the International Space Station. It will provide high thermal gradient and quench capabilities for processing metals and alloys in microgravity. Numerical analyses and breadboard testing conducted to date show that the QMI can produce an axial temperature gradient approaching 150 C per centimeter in a 1 centimeter diameter aluminum sample with a maximum molten sample temperature of 1100 C. Breadboard testing and analysis have also shown that the quench capabilities of the furnace are sufficient to rapidly solidify at least a 5mm axial portion of a 1 centimeter diameter molten aluminum sample in significantly less than the required 2 seconds and prevent significant backmelt. This paper presents the furnace requirements and capabilities and a status of the associated development testing and analyses.

Carswell, William E.↗

Solidification and Morphological Evolution of Al-Si Eutectics in Convector-Diffusive Conditions

The Al-Si material system is an important and has been studied for over half century with a focus on industrial applications in high strength and high conductivity alloys. A great deal of researches have been focused on controlling the morphology and hence performance through the addition of small impurities and by processing conditions. Most of the structure-property correlations are based on the post solidified micromorphology and growth conditions. This material system is unique and has been explored for heat spreader, controlling coefficient of expansion by adjusting composition of silicon and in designing composites. The Al-Si system is very interesting system for understanding the dendritic (Al-rich side) eutectic transition. Recently this system has been of great interest because of its applications in designing heat spreader, low temperature flux to grow SiC large substrates and in controlling the coefficient of expansion of Al-based alloys. We have performed extensive experiments to understand eutectic transition and to understand the morphological evolution in presence of impurities. We will discuss the results of dendritic transition into faceted long grains in convector-diffusive conditions. In this presentation we will present morphological transition in presence of carbon impurity and development of novel morphology.

Singh, N. B.↗

Structural evolution of low-temperature liquid GaIn eutectic alloy

Structural changes of liquid Galn eutectic alloy upon cooling from about 373 K to 242 K are studied by using in situ synchrotron radiation X-ray diffraction (XRD) combined with the ab initio molecular dynamics simulations (AIMD). The experimental and theoretical results show that no abnormal structural change is observed in the supercooled liquid region prior to crystallization. The XRD data exhibit that the liquid can crystallize into a mixture of orthorhombic Ga-I and body-centered tetragonal (bct)-In phases. Also, the AIMD calculations simulate the solidification process, forming a bct-like structure locally similar to bct-Ga-III and bct-In phases. The aggregation of In atoms forms In-rich zones, acting as the processor of crystallization. Our results provide an in-depth understanding of liquid Galn alloys and will trigger more interests to other metallic liquids. (C) 2019 Elsevier B.V. All rights reserved.

36 MATERIALS SCIENCE↗

Microstructural evolution during transient liquid phase bonding of Inconel 738LC using AMS 4777 filler alloy

IN-738LC nickel-based superalloy was joined by transient liquid phase diffusion bonding using AMS 4777 filler alloy. The bonding process was carried out at 1050 Degree-Sign C under vacuum atmosphere for various hold times. Microstructures of the joints were studied by optical and scanning electron microscopy. Continuous centerline eutectic phases, characterized as nickel-rich boride, chromium-rich boride and nickel-rich silicide were observed at the bonds with incomplete isothermal solidification. In addition to the centerline eutectic products, precipitation of boron-rich particles was observed in the diffusion affected zone. The results showed that, as the bonding time was increased to 75 min, the width of the eutectic zone was completely removed and the joint was isothermally solidified. Homogenization of isothermally solidified joints at 1120 Degree-Sign C for 300 min resulted in the elimination of intermetallic phases formed at the diffusion affected zone and the formation of significant {gamma} Prime precipitates in the joint region. - Highlights: Black-Right-Pointing-Pointer TLP bonding of IN-738LC superalloy was performed using AMS 4777 filler alloy. Black-Right-Pointing-Pointer Insufficient diffusion time resulted in the formation of eutectic product. Black-Right-Pointing-Pointer Precipitation of B-rich particles was observed within the DAZ. Black-Right-Pointing-Pointer The extent of isothermal solidification increased with increasing holding time. Black-Right-Pointing-Pointer Homogenizing of joints resulted in the dissolution of DAZ intermetallics.

36 MATERIALS SCIENCE↗

High-Temperature Phase Change Materials (PCM) Candidates for Thermal Energy Storage (TES) Applications

It is clearly understood that lower overall costs are a key factor to make renewable energy technologies competitive with traditional energy sources. Energy storage technology is one path to increase the value and reduce the cost of all renewable energy supplies. Concentrating solar power (CSP) technologies have the ability to dispatch electrical output to match peak demand periods by employingthermal energy storage (TES). Energy storage technologies require efficient materials with high energy density. Latent heat TES systems using phase change material (PCM) are useful because of their ability to charge and discharge a large amount of heat from a small mass at constant temperature during a phase transformation like melting-solidification. PCM technology relies on the energyabsorption/liberation of the latent heat during a physical transformation. The main objective of this report is to provide an assessment of molten salts and metallic alloys proposed as candidate PCMs for TES applications, particularly in solar parabolic trough electrical power plants at a temperature range from 300..deg..C to 500..deg.. C. The physical properties most relevant for PCMs servicewere reviewed from the candidate selection list. Some of the PCM candidates were characterized for: chemical stability with some container materials; phase change transformation temperatures; and latent heats.

14 SOLAR ENERGY↗

Predictive modeling of reactive wetting and metal joining.

The performance, reproducibility and reliability of metal joints are complex functions of the detailed history of physical processes involved in their creation. Prediction and control of these processes constitutes an intrinsically challenging multi-physics problem involving heating and melting a metal alloy and reactive wetting. Understanding this process requires coupling strong molecularscale chemistry at the interface with microscopic (diffusion) and macroscopic mass transport (flow) inside the liquid followed by subsequent cooling and solidification of the new metal mixture. The final joint displays compositional heterogeneity and its resulting microstructure largely determines the success or failure of the entire component. At present there exists no computational tool at Sandia that can predict the formation and success of a braze joint, as current capabilities lack the ability to capture surface/interface reactions and their effect on interface properties. This situation precludes us from implementing a proactive strategy to deal with joining problems. Here, we describe what is needed to arrive at a predictive modeling and simulation capability for multicomponent metals with complicated phase diagrams for melting and solidification, incorporating dissolutive and composition-dependent wetting.

van Swol, Frank B.↗

Studies of directionally solidified eutectic Bi/MnBi at low growth velocities

The (lambda-squared)(V) deviation for diffusion-only rod eutectic growth, where lambda is the interrod spacing and V is the growth velocity, was studied at growth velocities less than 5 cm/h in directionally solidified eutectic Bi-Mn (Bi/MnBi). At lower growth velocities, (V less than 0.5 cm/h) morphological instability occurred which resulted in nonaligned, irregularly dispersed MnBi fibers. The (lambda-squared)(V) relation was experimentally determined over a range of growth velocities between 0.1 and 50 cm/h, thermal gradients in the liquid at the liquid-solid interface that varied from 40 to 120 C/cm and solidification orientation with respect to the direction of gravity. Naturally induced, convective instabilities are suggested as a possible growth velocity limit for cooperative growth in the Bi-Mn and related alloy systems.

Pirich, R. G.↗

The Impact of Ceramic Shell Strength on Hot Tearing during Investment Casting

The effect of ceramic shell strength on hot tearing susceptibility during solidification was inspected practicing investment casting of the cobalt-base superalloy samples with the same casting conditions, but different ceramic shell systems. Results showed that the lower the ceramic shell strength upon using polymer additives, the lower the hindered contraction rate, and the lower the hindered contraction rate, the smaller the hot tearing tendency. Optical microscopy and electron microscopy scanning revealed that the hot tear propagated along the last solidified interdendritic phase, and that the hot tear surface had two major modes: (1) the ductile region in the outer layer; and (2) the inner region of liquid embrittlement.

36 MATERIALS SCIENCE↗