Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “STEELS”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 1,279 records · Page 71

Microstructure development of novel composite heating elements for steel decarbonization

The iron and steel industry is critical for the modern world but is also responsible for 7% of the total energy sector CO2 emissions. It is a difficult industry to decarbonize due to the high temperature heat required for the production of steel, such as reheating steel slabs to ~1250 °C for hot rolling. Electrification of this process using resistive heating is currently not possible due to the poor creep resistance of MoSi2 heating elements, which need to be operated well below their maximum temperatures when mounted horizontally. To solve this problem, novel MoSi2 composite heating elements with SiBCN ceramic reinforcements are being developed using high energy ball milling and electric field assisted sintering (EFAS). The microstructure and density of the composites after sintering depends on the sintering parameters chosen. Herein we present the effects of EFAS sintering parameters on the microstructure and density of the MoSi2-SiBCN composites.

36 - MATERIALS SCIENCE↗

A New Perspective on Fatigue Performance of Advanced High- Strength Steels (AHSS) GMAW Joints

Weld fatigue performance is a critical aspect for application of advanced high-strength steels (AHSS) in automotive body structures. A comparative study has been conducted to evaluate the fatigue life of AHSS welds. The material studied included seven AHSS of various strength levels - DP 600, DP 780, DP 980, M130, M220, solution annealed boron and fully hardened boron steels. Two conventional steels, HSLA 590 and DR 210, were also included for baseline comparison. Lap fillet welds were made on 2-mm nominal thick sheets by the gas metal arc welding process (GMAW). Fatigue test was conducted under a number of stress levels to obtain the S/N curves of the weld joints. It was found that, unlike in the static and impact loading conditions, the fatigue performance of AHSS is not influenced by the HAZ softening in AHSS. There are appreciable differences in the fatigue lives among different AHSS. Changes in weld parameters can influence the fatigue life of the weld joints, particularly of these of higher strength AHSS. A model is developed to predict the fatigue performance of AHSS welds. The validity of the model is benchmarked with the experimental results. This model is capable to capture the effects of weld geometry and weld microstructure and strength on the fatigue performance experimentally observed. The theoretical basis and application of the newly developed fatigue modeling methodology will be discussed.

36 MATERIALS SCIENCE↗

IAEA Coordinated Research Project on Master Curve Approach to Monitor Fracture Toughness of RPV Steels: Final Results of the Experimental Exercise to Support Constraint Effects

The precracked Charpy single-edge notched bend, SE(B), specimen (PCC) is the most likely specimen type to be used for determination of the reference temperature, T0, with reactor pressure vessel (RPV) surveillance specimens. Unfortunately, for many RPV steels, significant differences have been observed between the T0 temperature for the PCC specimen and that obtained from the 25-mm thick compact specimen [1TC(T)], generally considered the standard reference specimen for T0. This difference in T0 has often been designated a specimen bias effect, and the primary focus for explaining this effect is loss of constraint in the PCC specimen. The International Atomic Energy Agency (IAEA) has developed a coordinated research project (CRP) to evaluate various issues associated with the fracture toughness Master Curve for application to light-water RPVs. Topic Area 1 of the CRP is focused on the issue of test specimen geometry effects, with emphasis on determination of T0 with the PCC specimen and the bias effect. Topic Area 1 has an experimental part and an analytical part. Participating organizations for the experimental part of the CRP performed fracture toughness testing of various steels, including the reference steel JRQ (A533-B-1) often used for IAEA studies, with various types of specimens under various conditions. Additionally, many of the participants took part in a round robin exercise on finite element modeling of the PCVN specimen, discussed in a separate paper. Results from fracture toughness tests are compared with regard to effects of specimen size and type on the reference temperature T0. It is apparent from the results presented that the bias observed between the PCC specimen and larger specimens for Plate JRQ is not nearly as large as that obtained for Plate 13B (-11 C vs -37 C) and for some of the results in the literature (bias values as much as -45 C). This observation is consistent with observations in the literature that show significant variations in the bias that are dependent on the specific materials being tested. There are various methods for constraint adjustments and two methods were used that reduced the bias for Plate 13B from -37 C to -13 C in one case and to -11 C in the second case. Unfortunately, there is not a consensus methodology available that accounts for the differences observed with different materials. Increasing the Mlim value in the ASTM E-1921 to ensure no loss of constraint for the PCC specimen is not a practicable solution because the PCC specimen is derived from CVN specimens in RPV surveillance capsules and larger specimens are normally not available. Resolution of these differences are needed for application of the master curve procedure to operating RPVs, but the research needed for such resolution is beyond the scope of this CRP.

36 MATERIALS SCIENCE↗

Relative Humidity and the Susceptibility of Austenitic Stainless Steel to Stress Corrosion Cracking in an impure Plutonium Oxide Environment

Laboratory tests to investigate the corrosivity of moist plutonium oxide/chloride salt mixtures on 304L and 316L stainless steel coupons showed that corrosion occurred in selected samples. The tests exposed flat coupons for pitting evaluation and 'teardrop' stressed coupons for stress corrosion cracking (SCC) evaluation at room temperature to various mixtures of PuO{sub 2} and chloride-bearing salts for periods up to 500 days. The exposures were conducted in sealed containers in which the oxide-salt mixtures were loaded with about 0.6 wt % water from a humidified helium atmosphere. Observations of corrosion ranged from superficial staining to pitting and SCC. The extent of corrosion depended on the total salt concentration, the composition of the salt and the moisture present in the test environment. The most significant corrosion was found in coupons that were exposed to 98 wt % PuO{sub 2}, 2 wt % chloride salt mixtures that contained calcium chloride and 0.6 wt% water. SCC was observed in two 304L stainless steel teardrop coupons exposed in solid contact to a mixture of 98 wt % PuO{sub 2}, 0.9 wt % NaCl, 0.9 wt % KCl, and 0.2 wt % CaCl{sub 2}. The cracking was associated with the heat-affected zone of an autogenous weld that ran across the center of the coupon. Cracking was not observed in coupons exposed to the headspace gas above the solid mixture, or in coupons exposed to other mixtures with either no CaCl{sub 2} or 0.92 wt% CaCl{sub 2}. SCC was present where the 0.6 wt % water content exceeded the value needed to fully hydrate the available CaCl{sub 2}, but was absent where the water content was insufficient. These results reveal the significance of the relative humidity in the austenitic stainless steels environment to their susceptibility to corrosion. The relative humidity in the test environment was controlled by the water loading and the concentration of the hydrating salts such as CaCl{sub 2}. For each salt or salt mixture there is a threshold relative humidity below which the necessary liquid electrolyte cannot exist, and therefore below which the SCC risk is very low. This threshold is a thermodynamic quantity known as the deliquescence relative humidity that is dependent on the identity of the salt but is independent of the quantity of salt. Below the deliquescence RH there should be low corrosion risk, and above it the corrosion risk increases rapidly as a liquid phase, which is initially saturated with salt, grows and becomes more widespread in the container.

36 MATERIALS SCIENCE↗

Ultrasonic Spot Welding of AZ31B to Galvanized Mild Steel

Ultrasonic spot welds were made between sheets of 0.8-mm-thick hot-dip-galvanized mild steel and 1.6-mm-thick AZ31B-H24. Lap-shear strengths of 3.0-4.2 kN were achieved with weld times of 0.3-1.2 s. Failure to achieve strong bonding of joints where the Zn coating was removed from the steel surface indicate that Zn is essential to the bonding mechanism. Microstructure characterization and microchemical analysis indicated temperatures at the AZ31-steel interfaces reached at least 344 C in less than 0.3 s. The elevated temperature conditions promoted annealing of the AZ31-H24 metal and chemical reactions between it and the Zn coating.

36 MATERIALS SCIENCE↗

Precipitate Evolution in Low-Nickel Austenitic Stainless Steels During Neutron Irradiation at Very Low Dose Rates

Neutron-induced microstructural evolution in response to long term irradiation at very low dose rates was studied for a Russian low-nickel austenitic stainless steel designated Х18Н9 that is analogous to AISI 304. The irradiated samples were obtained from an out-of-core support column for the pressure vessel of the BN-600 fast reactor with doses ranging from 1.7 to 20.5 dpa generated at 3.8x10-9 to 4.3x10-8 dpa/s. The irradiation temperatures were in a very narrow range of 370-375°С. Microstructural observation showed that in addition to voids and dislocations, an unexpectedly high density of small G-phase precipitates was formed that are not usually observed at higher dpa rates in this temperature range. A similar behavior was observed in a Western stainless steel, namely AISI 304 stainless steel, irradiated at similar temperatures and somewhat higher dpa rates in the EBR-II fast reactor, indicating that irradiation at low dpa rates for many years can lead to a different precipitate microstructure and therefore different associated changes in matrix composition than are generated at higher dpa rates. The contribution of such radiation-induced precipitation to changes in electrical resistivity was measured in the Х18Н9 specimens and was shown to cause significant deviation from predictions based only on void swelling.

21 SPECIFIC NUCLEAR REACTORS AND ASSOCIATED PLANTS↗

Friction Drilling of Stainless Steels Pipes

This work describes the experimental study of the friction drilling process in stainless steel by means of an optimization of the machining conditions. For such purpose austenitic stainless steel with different thicknesses were analyzed through controlled tests at different rotation speeds and feed rates. On one hand, the torque and the thrust force were computed and monitorized. On the other hand, the dimensional tolerances of the holes were evaluated, mainly the accuracy of the hole diameter and the burr thickness at different depths. Another topic of interest inherent to this special technique is the temperature level reached during the friction process which is crucial when it comes to development of microstructural transformations.

36 MATERIALS SCIENCE↗

Effect of the Heat Treatment on the Corrosion Resistance of Duplex Stainless Steels

Duplex stainless steels (DSS) are biphasic austenitic-ferritic steels in which the best combination of mechanical and corrosion resistance properties is achieved for an almost equal volume fraction of the phases. In this work, the effect of secondary phases precipitation on the corrosion resistance of four DSS grades (2101, 2304, 2205 and 2507), after isothermal aging in the critical temperature range 750-900 °C, was studied. The corrosion resistance was investigated by potentiodynamic polarization tests in both 0.6 M NaCl solution (pH 7) and in an acid chlorinated solution (pH 3) at room temperature. Moreover, the critical pitting temperature was determined according to ASTM G150. The results showed that secondary phases precipitation mainly influenced the resistance to corrosion of the lean duplex grades.

36 MATERIALS SCIENCE↗

Influence of the grain size on deleterious phase precipitation in superduplex stainless steel UNS S32750

In the present work, the effect of grain size on deleterious phase precipitation in a superduplex stainless steel was investigated. The materials studied were heat treated isothermally at 800 deg. C, 850 deg. C and 900 deg. C for times up to 120 min. Hardness tests, light optical microscopy, scanning electron microscopy and X-ray diffraction were carried out to detect sigma and other harmful precipitate phases. The ferritic and austenitic grain sizes in the solution treated condition of the two steels analyzed were measured by electron backscattered diffraction (EBSD). Cyclic polarization corrosion tests were performed to evaluate the effect of grain size on the corrosion resistance. The results presented show that the precipitation of deleterious phases such as {chi}, {sigma} and {gamma}{sub 2}, which can occur during welding and forming operations, is retarded by grain growth.

36 MATERIALS SCIENCE↗

Structural characterization of “carbide-free” bainite in a Fe–0.2C–1.5Si–2.5Mn steel

Low-alloyed, low C containing carbide-free bainitic steels are attractive candidates for applications in the automotive industry due to their well-balanced combination of high strength and ductility achieved in an economic way. In this work, their complex microstructure consisting of a mixture of bainitic ferrite, austenite with different morphologies and stabilities, martensite, M/A constituent and a few carbides has been investigated with metallographic and high-resolution techniques. After specific isothermal heat treatments in a dilatometer, a combination of LePera and Nital etching was applied to distinguish between bainite and martensite. Site-specific atom probe tips were prepared by means of scanning electron microscopy, electron backscatter diffraction and focused ion beam, revealing that “carbide-free” bainite consists of C depleted bainitic ferrite, C enriched retained austenite and occasional ε-carbides. Furthermore, it was found that the M/A constituent is highly dislocated and mainly martensitic. Its C content is increased compared to the nominal composition, but below the values obtained for retained austenite, explaining the lower transformation resistance. - Highlights: • Detailed top-down characterization of low C “carbide-free” bainitic steel • APT of all constituents in “carbide-free” bainite • Identification of ε-carbide based on its C content determined by APT • M/A constituent is mainly martensitic with austenitic areas at the boundaries • Lower C content of M/A constituent explains its lower stability.

36 MATERIALS SCIENCE↗

Removal of the long-lived {sup 222}Rn daughters from steel and germanium surfaces

Removal of the long-lived {sup 222}Rn daughters ({sup 210}Pb, {sup 210}Bi and {sup 210}Po) from stainless steel and germanium surfaces was investigated. As cleaning technique etching was applied to samples in a form of discs exposed earlier to a strong radon source. Reduction of the {sup 210}Pb activity was tested using a HPGe spectrometer, for {sup 210}Bi a beta spectrometer and for {sup 210}Po an alpha spectrometer was used. According to the conducted measurements all the isotopes were removed very efficiently from germanium. Results obtained for stainless steel were worse but still better than those achieved for copper.

07 ISOTOPE AND RADIATION SOURCES↗

A Hierarchical Upscaling Method for Predicting Strength of Materials under Thermal, Radiation and Mechanical loading - Irradiation Strengthening Mechanisms in Stainless Steels

Stainless steels based on Fe-Cr-Ni alloys are the most popular structural materials used in reactors. High energy particle irradiation of in this kind of polycrystalline structural materials usually produces irradiation hardening and embrittlement. The development of predictive capability for the influence of irradiation on mechanical behavior is very important in materials design for next-generation reactors. Irradiation hardening is related to structural information crossing different length scale, such as composition, dislocation, crystal orientation distribution and so on. To predict the effective hardening, the influence factors along different length scales should be considered. A multiscale approach was implemented in this work to predict irradiation hardening of iron based structural materials. Three length scales are involved in this multiscale model: nanometer, micrometer and millimeter. In the microscale, molecular dynamics (MD) was utilized to predict on the edge dislocation mobility in body centered cubic (bcc) Fe and its Ni and Cr alloys. On the mesoscale, dislocation dynamics (DD) models were used to predict the critical resolved shear stress from the evolution of local dislocation and defects. In the macroscale, a viscoplastic self-consistent (VPSC) model was applied to predict the irradiation hardening in samples with changes in texture. The effects of defect density and texture were investigated. Simulated evolution of yield strength with irradiation agrees well with the experimental data of irradiation strengthening of stainless steel 304L, 316L and T91. This multiscale model we developed in this project can provide a guidance tool in performance evaluation of structural materials for next-generation nuclear reactors. Combining with other tools developed in the Nuclear Energy Advanced Modeling and Simulation (NEAMS) program, the models developed will have more impact in improving the reliability of current reactors and affordability of new reactors.

22 GENERAL STUDIES OF NUCLEAR REACTORS↗

Multiscale Modeling of the Deformation of Advanced Ferritic Steels for Generation IV Nuclear Energy

The objective of this project is to use the multi-scale modeling of materials (MMM) approach to develop an improved understanding of the effects of neutron irradiation on the mechanical properties of high-temperature structural materials that are being developed or proposed for Gen IV applications. In particular, the research focuses on advanced ferritic/ martensitic steels to enable operation up to 650-700°C, compared to the current 550°C limit on high-temperature steels.

29 ENERGY PLANNING, POLICY, AND ECONOMY↗

Improvements in Low-Frequency, Ultrasonic Phased-Array Evaluation for Thick Section Cast Austenitic Stainless Steel Piping Components

Research is being conducted for the U.S. Nuclear Regulatory Commission (NRC) at the Pacific Northwest National Laboratory (PNNL) to assess the effectiveness and reliability of advanced nondestructive examination (NDE) methods for the inspection of light water reactor (LWR) components. A primary objective of this work is to evaluate various NDE methods to assess their ability to detect, localize, and size cracks in coarse-grained steel components. This particular study focused on the evaluation of custom-designed, low-frequency (500 kHz) phased-array (PA) probes for examining welds in thick-section cast austenitic stainless steel (CASS) piping. In addition, research was conducted to observe ultrasonic sound field propagation effects from known coarse-grained microstructures found in parent CASS material. The study was conducted on a variety of thick-wall, coarse-grained CASS specimens that were previously inspected by an older generation 500-kHz PA-UT probe and acquisition instrument configuration. This comparative study describes the impact of the new PA probe design on flaw detection and sizing in a low signal-to-noise environment. The set of Pressurized Water Reactor Owners Group (PWROG) CASS specimens examined in this study are greater than 50.8-mm (2.0-in.) thick with documented flaws and microstructures. These specimens are on loan to PNNL from the Electric Power Research Institute (EPRI) NDE Center in Charlotte, North Carolina. The flaws contained within these specimens are thermal fatigue cracks (TFC) or mechanical fatigue cracks (MFC) and range from 13% to 42% in through-wall extent. In addition, ultrasonic signal continuity was evaluated on two CASS parent material ring sections by examining the edge-of-pipe response (corner geometry) for regions of signal loss.

21 SPECIFIC NUCLEAR REACTORS AND ASSOCIATED PLANTS↗

Effects of Inclusions in HSLA Carbon Steel on Pitting Corrosion in CaCl2

Susceptibility of high strength low alloy steel to localized corrosion was studied in 6.7 M CaCl{sub 2} for oil and natural gas drilling applications. Results of the immersion and electrochemical experiments showed that the steel is susceptible to pitting corrosion. Optical microscopy investigations of the polished samples revealed that 10% of the surface area was occupied by defects in the form of pits. The energy dispersive X-ray (EDX) and wavelength dispersive X-ray (WDX) chemical analyses revealed higher concentrations of Mn and S compared to the metal matrix in defected areas. These areas served as the sites for development of corrosion pits during both immersion and electrochemical experiments. The fatigue results of the corroded samples indicate that if the pit was the most significant defect, the fatigue crack initiated and propagated at this site.

03 NATURAL GAS↗

Materials performance of ferritic steel in combustion gases for heat exchanger applications in solid oxide fuel cell systems

Ferritic steels have been recognized as candidates for their applications in heat exchangers used in Solid Oxide Fuel Cells’ balance of plant. Combustion gases flowing through those heat exchangers can be very corrosive. Therefore, the National Energy Technology Laboratory determined materials performance of commercial S43000 stainless steel exposed to a simulated combustion gas at 800 °C. The exposure experiments were conducted on flat samples in the simulated combustion gas: 19vol% O2+6vol% H2O + 4vol% CO2 +71vol% N2 under isothermal conditions. After the experiment, the surface of a corroded sample was characterized by X-ray diffraction (XRD) to identify possible phases present in the scale, scanning electron microscopy (SEM) to determine microstructure of the oxide scales, and energy dispersive X-ray (EDX) or wavelength dispersive energy X-ray (WDX) spectroscopy to determine chemical composition in the scale and the metal substrate.

36 MATERIALS SCIENCE↗

Review and construction of interatomic potentials for molecular dynamics studies of hydrogen embrittlement in Fe─C based steels

Abstract Reducing hydrogen embrittlement in the low‐cost Fe─C based steels have the potential to significantly impact the development of hydrogen energy technologies. Molecular dynamics studies of hydrogen interactions with Fe─C steels provide fundamental information about the behavior of hydrogen at microstructural length scales, although such studies have not been performed due to the lack of an Fe─C─H ternary interatomic potential. In this work, the literature on interatomic potentials related to the Fe─C─H systems are reviewed with the aim of constructing an Fe─C─H potential from the published binary potentials. We found that Fe─C, Fe─H, and C─H bond order potentials exist and can be combined to construct an Fe─C─H ternary potential. Therefore, we constructed two such Fe─C─H potentials and demonstrate that these ternary potentials can reasonably capture hydrogen effects on deformation characteristics and deformation mechanisms for a variety of microstructural variations of the Fe─C steels, including martensite that results from γ to α phase transformation, and pearlite that results from the eutectic formation of the Fe 3 C cementite compound.

Zhou, Xiaowang↗

A comparison of adiabatic shear bands in wrought and additively manufactured 316L stainless steel using nanoindentation and electron backscatter diffraction

The resistance of stainless steels to shear localization is dependent on processing and microstructure. The amount of research evaluating the shear response of additively manufactured (AM) stainless steels compared to traditionally manufactured ones is limited. To address this gap, experiments were performed on directed energy deposition AM as-built and wrought 316L stainless steel using a forced shear technique with a hat-shaped specimen and a Split-Hopkinson pressure bar. The resulting adiabatic shear bands were characterized with electron backscatter diffraction (EBSD) and nanoindentation to quantify the changes in microstructure and deformation hardening across shear band regions and between the wrought and AM materials. Despite significant differences between the wrought and AM materials including the forced shear response, the postmortem states of work hardening due to the shear band deformation are nearly the same. The maximum nanoindentation stresses occurred in the shear band center with similar magnitudes and only minor differences away from the shear band. Although EBSD data cannot be resolved in the shear band center, misorientation trends, particularly grain reference orientation deviation, were found to closely resemble nanoindentation trends. In conclusion, the combination of EBSD misorientation and nanoindentation, which are linked through changes in dislocation density, is a viable protocol to quantify local changes to macroscopically applied deformation.

36 MATERIALS SCIENCE↗