Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “MAGNETRONS”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 1,279 records · Page 71

Novel hard, tough HfAlSiN multilayers, defined by alternating Si bond structure, deposited using modulated high-flux, low-energy ion irradiation of the growing film

Hf{sub 1−x−y}Al{sub x}Si{sub y}N (0 ≤ x ≤ 0.14, 0 ≤ y ≤ 0.12) single layer and multilayer films are grown on Si(001) at 250 °C using ultrahigh vacuum magnetically unbalanced reactive magnetron sputtering from a single Hf{sub 0.6}Al{sub 0.2}Si{sub 0.2} target in mixed 5%-N{sub 2}/Ar atmospheres at a total pressure of 20 mTorr (2.67 Pa). The composition and nanostructure of Hf{sub 1−x−y}Al{sub x}Si{sub y}N films are controlled by varying the energy E{sub i} of the ions incident at the film growth surface while maintaining the ion-to-metal flux ratio constant at eight. Switching E{sub i} between 10 and 40 eV allows the growth of Hf{sub 0.78}Al{sub 0.10}Si{sub 0.12}N/Hf{sub 0.78}Al{sub 0.14}Si{sub 0.08}N multilayers with similar layer compositions, but in which the Si bonding state changes from predominantly Si–Si/Si–Hf for films grown with E{sub i} = 10 eV, to primarily Si–N with E{sub i} = 40 eV. Multilayer hardness values, which vary inversely with bilayer period Λ, range from 20 GPa with Λ = 20 nm to 27 GPa with Λ = 2 nm, while fracture toughness increases directly with Λ. Multilayers with Λ = 10 nm combine relatively high hardness, H ∼ 24 GPa, with good fracture toughness.

36 MATERIALS SCIENCE↗

Tailoring the crystal structure of TiO{sub 2} thin films from the anatase to rutile phase

TiO{sub 2} films with various Sn concentrations were deposited on quartz substrates using rf reactive magnetron sputtering. The crystal structure was investigated by using x-ray diffraction, Raman spectroscopy, and transmission electron microscopy, and the chemical states of Ti and Sn were analyzed by x-ray absorption near edge structure (XANES) spectroscopy. Without Sn doping, TiO{sub 2} films change the crystal structure from rutile to anatase as the total gas pressure increases in the sputtering deposition. On the other hand, Sn doping induces the transformation of TiO{sub 2} crystalline structure from anatase to rutile phase, where the XANES spectra implied that Sn substitutes into Ti site of rutile TiO{sub 2}. Atomic force microscope analyses revealed that the Sn-doped TiO{sub 2} films exhibited a flat surface with the roughness of approximately 2 nm.

36 MATERIALS SCIENCE↗

Local structure study of (In{sub 0.95−x}Fe{sub x}Cu{sub 0.05}){sub 2}O{sub 3} thin films using x-ray absorption spectroscopy

The (In{sub 0.95−x}Fe{sub x}Cu{sub 0.05}){sub 2}O{sub 3} (x = 0.06, 0.08, 0.15, and 0.20) films prepared by RF-magnetron sputtering were investigated by the combination of x-ray absorption spectroscopy (XAS) at Fe, Cu, and O K-edge. Although the Fe and O K-edge XAS spectra show that the Fe atoms substitute for the In sites of In{sub 2}O{sub 3} lattice for all the films, the Cu K-edge XAS spectra reveal that the codoped Cu atoms are separated to form the Cu metal clusters. After being annealed in air, the Fe atoms are still substitutionally incorporated into the In{sub 2}O{sub 3} lattice, while the Cu atoms form the CuO secondary phases. With the increase of Fe concentration, the bond length R{sub Fe-O} shortens and the Debye–Waller factor σ{sup 2}{sub Fe-O} increases in the first coordination shell of Fe, which are attributed to the relaxation of oxygen environment around the substitutional Fe ions. The forming of Cu relating secondary phases in the films is due to high ionization energy of Cu atoms, leading that the Cu atoms are energetically much harder to be oxidized to substitute for the In sites of In{sub 2}O{sub 3} lattice than Fe atoms. These results provide new experimental guidance in the preparation of the codoped In{sub 2}O{sub 3} based dilute magnetic oxides.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Composition gradient effects on strain relaxation in Sr-doped LaMnO{sub 3} epitaxial thin films

The authors report on a novel method to fabricate Sr-doped composition gradient epitaxial La{sub 1−x}Sr{sub x}MnO{sub 3} thin films by radio frequency magnetron sputtering. Biaxially strained epitaxial La{sub 1−x}Sr{sub x}MnO{sub 3} thin films were grown on (001) LaAlO{sub 3} substrates by following a cosputtering procedure from LaMnO{sub 3} and La{sub 0.67}Sr{sub 0.33}MnO{sub 3} targets. Three depositions were conducted by varying the substrate temperature (750 and 850 °C) and controlling the relative deposition rate from the two targets by varying their power rate during sputtering. The thickness of the thin films was about 20 and 30 nm for the short and long duration deposition, respectively. The films were studied by symmetric θ–2θ x-ray diffraction, pole figure analysis, atomic force microscopy, and x-ray photoelectron spectroscopy. Fabrication of smooth, composition gradient films of high epitaxial quality was achieved at a substrate temperature of 850 °C and low sputtering rate. A novel strain relaxation mechanism is also found that decreases significantly the mismatch between the film and substrate as the Sr doping level increases. The reported deposition procedure can produce new possibilities of designing nanoscale structures with cross coupled properties that may result in new materials.

42 ENGINEERING↗

Epitaxial growth of tungsten layers on MgO(001)

Smooth single crystal W(001) layers were grown on MgO(001) substrates by magnetron sputtering at 900 °C. X-ray diffraction ω–2θ scans, ω-rocking curves, pole figures, and reciprocal space maps indicate a 45°-rotated epitaxial relationship: (001){sub W}‖(001){sub MgO} and [010]{sub W}‖[110]{sub MgO}, and a relaxed lattice constant of 3.167 ± 0.001 nm. A residual in-plane biaxial compressive strain is primarily attributed to differential thermal contraction after growth and decreases from −0.012 ± 0.001 to −0.001 ± 0.001 with increasing layer thickness d = 4.8–390 nm, suggesting relaxation during cooling by misfit dislocation growth through threading dislocation glide. The in-plane x-ray coherence length increases from 3.4 to 33.6 nm for d = 4.8–390 nm, while the out-of-plane x-ray coherence length is identical to the layer thickness for d ≤ 20 nm, but is smaller than d for d ≥ 49.7 nm, indicating local strain variations along the film growth direction. X-ray reflectivity analyses indicate that the root-mean-square surface roughness increases from 0.50 ± 0.05 to 0.95 ± 0.05 nm for d = 4.8–19.9 nm, suggesting a roughness exponent of 0.38, but remains relatively constant for d > 20 nm with a roughness of 1.00 ± 0.05 nm at d = 47.9 nm.

36 MATERIALS SCIENCE↗

Influence of Al{sub 2}O{sub 3} layer insertion on the electrical properties of Ga-In-Zn-O thin-film transistors

To investigate the influence of ionic/covalent interface of Al{sub 2}O{sub 3}/SiO{sub 2} gate insulator on the electrical properties of thin-film transistors (TFTs) with ionic Ga-In-Zn-O (GIZO) semiconducting channel layers, Al{sub 2}O{sub 3} layers of different thickness were introduced between SiO{sub 2} and GIZO using plasma-enhanced atomic layer deposition. The GIZO layers were obtained by DC magnetron sputtering using a GIZO target (Ga:In:Zn = 1:1:1 mol. %). The GIZO TFTs with an Al{sub 2}O{sub 3}/SiO{sub 2} gate insulator exhibited positive threshold voltage (V{sub th}) shift (about 1.1 V), V{sub th} hysteresis suppression (0.23 V), and electron mobility degradation (about 13%) compared with those of a GIZO TFT with SiO{sub 2} gate insulator by the influence of ionic/ionic and ionic/covalent interface at Al{sub 2}O{sub 3}/GIZO and Al{sub 2}O{sub 3}/SiO{sub 2}, respectively. To clarify the origin of the positive V{sub th} shift, the authors estimated the shifts of flatband voltage (0.4 V) due to the dipole and the fixed charge (−1.1 × 10{sup 11}/cm{sup 2}) at Al{sub 2}O{sub 3}/SiO{sub 2} interface, from capacitance–voltage data for Pt/Al{sub 2}O{sub 3}/SiO{sub 2}/p-Si capacitors. Based on these experimental data, the authors found that the positive V{sub th} shift (1.1 V) could be divided into three components: the dipole (−0.4 V) and fixed charge (0.15 V) at the SiO{sub 2}/Al{sub 2}O{sub 3} interface, and the fixed charge (1.35 V) at the Al{sub 2}O{sub 3}/GIZO interface. Finally, it is noted that heterointerface of SiO{sub 2}/Al{sub 2}O{sub 3}/GIZO stacks is important not only to recognize mechanism of V{sub th} shift but also to design future TFTs with high-k dielectrics and low operating voltage.

42 ENGINEERING↗

Effect of porous morphology on phase transition in vanadium dioxide thin films

Vanadium oxide (VO{sub 2}) thin films were prepared on Si (100) substrates by direct current magnetron sputtering at room temperature, and then, postannealing was conducted at 450 °C for 2 h in vacuum. Structural characterizations demonstrated that the thin films exhibited porous morphology upon thermal annealing and the porosity and pore size depended on the oxygen flow rate in the process of film fabrication. Raman spectra were measured in the temperature range of 303–343 K, and resistance measurement was conducted in the temperature range of 293–363 K, to study the influence of porous morphology on the phase transition in VO{sub 2} thin films. It was illustrated that the porous morphology could provide a free space to release the stress induced in the monoclinic-to-tetragonal phase transition of VO{sub 2}, and lower the transition temperature to a certain degree.

36 MATERIALS SCIENCE↗

Effect of intermetallic compounds on the thermal conductivity of Ti-Cu composites

Ti films were deposited by magnetron sputtering on polycrystalline Cu substrates. The samples were annealed at different temperatures and characterized by x-ray diffraction for phase identification, scanning electron microscopy, and energy dispersive spectrometry for microstructure and composition and transient thermoreflectance for thermal conductivity and interface thermal conductance. The results showed that the diffused layer of Ti in Cu contained intermetallic compounds and solid solution of Ti in Cu. The thermal conductivity of the diffused layer is reduced, and the thickness increased for higher annealing temperature. The interface thermal conductance also decreased for higher temperature of annealing. A stable Cu{sub 4}Ti phase was formed after annealing at 725 °C with thermal conductivity of 10 W m{sup −1} K{sup −1}. The interface thermal conductance between the intermetallic compound and the solid solution of Ti in Cu also was reduced to 30 MW m{sup −2} K{sup −1}. The effective thermal resistance of the diffused layer and the interface was found to increase for higher annealing temperature.

36 MATERIALS SCIENCE↗

Work functions of hafnium nitride thin films as emitter material for field emitter arrays

The work functions of hafnium nitride thin films prepared by radio-frequency magnetron sputtering were investigated in vacuum, before and after surface cleaning processes, with a view of improving the properties of as-fabricated field emitter arrays comprising hafnium nitride emitters. The measurement of the work function was first performed for the as-deposited films and then for films subjected to surface cleaning process, either thermal treatment or ion bombardment. Thermal treatment at a maximum temperature of 300 °C reduced the work function by 0.7 eV. Once the film was heated, the work function maintained the reduced value, even after cooling to room temperature. A little change in the work function was observed for the second and third thermal treatments. The ion bombardment was conducted by exposing the sample to a thin plasma for different sample bias conditions and processing times. When the sample was biased at −10 V, the work function decreased by 0.6 eV. The work function reduction became saturated in the early stage of the ion bombardment. When the sample was biased at −50 V, the work function exhibited different behaviors, that is, first it decreased rapidly and then increased in response to the increase in processing time. The lowest attainable work function was found to be 4.00 eV. It should be noted that none of the work function values reported in this paper were obtained using surfaces that were demonstrated to be free from oxygen contamination. The present results suggest that the current–voltage characteristics of a field emitter array can be improved by a factor of 25–50 by the examined postprocesses.

36 MATERIALS SCIENCE↗

Structural, mechanical, and magnetic properties of GaFe{sub 3}N thin films

Using the density-functional theory, the structural, mechanical, and magnetic properties were investigated for different GaFe{sub 3}N configurations: ferromagnetic, ferrimagnetic, paramagnetic, and nonmagnetic. Ferrimagnetic and high-spin ferromagnetic states exhibit the lowest energy and are the competing ground states as the total energy difference is 0.3 meV/atom only. All theoretically predicted values could be fully confirmed by experiments. For this, the authors synthesized phase pure, homogeneous, and continuous GaFe{sub 3}N films by combinatorial reactive direct current magnetron sputtering. Despite the low melting point of gallium, the authors succeeded in the growth of GaFe{sub 3}N films at a temperature of 500 °C. Those thin films exhibit a lattice parameter of 3.794 Å and an elastic modulus of 226 ± 20 GPa. Magnetic susceptibility measurements evidence a magnetic phase transitions at 8.0 ± 0.1 K. The nearly saturated magnetic moment at ±5 T is about 1.6 μB/Fe and is close to the theoretically determined magnetic moment for a ferrimagnetic ordering (1.72 μB/Fe).

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Formation of homologous In{sub 2}O{sub 3}(ZnO){sub m} thin films and its thermoelectric properties

Homologous In{sub 2}O{sub 3}(ZnO){sub 5} thin films were produced on a synthetic quartz glass substrate by thermal annealing of magnetron sputtered In{sub 2}O{sub 3}-ZnO compound films. When the annealing temperature was increased to 700 °C, the sputtered In{sub 2}O{sub 3}-ZnO film with In{sub 2}O{sub 3} microcrystalline changed to a c-oriented homologous In{sub 2}O{sub 3}(ZnO){sub 5} structure, for which the crystallization is suggested to begin from the surface and proceed along with the film thickness. The annealing temperature of 700 °C to form the In{sub 2}O{sub 3}(ZnO){sub 5} structure was substantially lower than temperatures of conventional solid state synthesis from In{sub 2}O{sub 3} and ZnO powders, which is attributed to the rapid diffusional transport of In and Zn due to the mixing of In{sub 2}O{sub 3} and ZnO in the atomic level for sputtered In{sub 2}O{sub 3}-ZnO compound films. The homologous structure collapsed at temperatures above 900 °C, which is attributed to (1) zinc vaporization from the surface and (2) a gradual increase of zinc silicate phase at the interface. This c-oriented layer structure of homologous In{sub 2}O{sub 3}(ZnO){sub 5} thin films along the film thickness allowed the thin film to reach a power factor of 1.3 × 10{sup −4} W/m K{sup 2} at 670 °C, which is comparable with the reported maximum value for the textured In{sub 2}O{sub 3}(ZnO){sub 5} powder (about 1.6 × 10{sup −4} W/m K{sup 2} at 650 °C).

36 MATERIALS SCIENCE↗

Effect of the cadmium chloride treatment on RF sputtered Cd{sub 0.6}Zn{sub 0.4}Te films for application in multijunction solar cells

Single phase Cd{sub 0.6}Zn{sub 0.4}Te (CdZnTe) films of 1 μm thickness were deposited by radio frequency planar magnetron sputter deposition on commercial soda lime glass samples coated with fluorine-doped tin oxide and cadmium sulphide (CdS). The stack was then treated with cadmium chloride (CdCl{sub 2}) at different temperatures using a constant treatment time. The effect of the CdCl{sub 2} treatment was studied using optical, materials, and electrical characterization of the samples and compared with the as-deposited CdZnTe film with the same stack configuration. The band gap deduced from Tauc plots on the as-deposited CdZnTe thin film was 1.72 eV. The deposited film had good crystalline quality with a preferred orientation along the {111} plane. After the CdCl{sub 2} treatment, the absorption edge shifted toward longer wavelength region and new peaks corresponding to cadmium telluride (CdTe) emerged in the x-ray diffraction pattern. This suggested loss of zinc after the CdCl{sub 2} treatment. The cross sectional transmission electron microscope images of the sample treated at 400 °C and the energy dispersive elemental maps revealed the absence of chlorine along the grain boundaries of CdZnTe and residual CdTe. The presence of chlorine in the CdTe devices plays a vital role in drastically improving the device performance which was not observed in CdZnTe samples treated with CdCl{sub 2}. The loss of zinc from the surface and incomplete recrystallization of the grains together with the presence of high densities of stacking faults were observed. The surface images using scanning electron microscopy showed that the morphology of the grains changed from small spherical shape to large grains formed due to the fusion of small grains with distinct grain boundaries visible at the higher CdCl{sub 2} treatment temperatures. The absence of chlorine along the grain boundaries, incomplete recrystallization and distinct grain boundaries is understood to cause the poor performance of the fabricated devices.

36 MATERIALS SCIENCE↗

Synthesis of model sodium sulfide films

We report the direct deposition of model sodium sulfide films by RF magnetron sputtering from Na 2 S and Na 2 S 2 deposition targets. Analytical characterization and electrochemical cycling indicate that the deposited films are amorphous with stoichiometries that correspond to Na 2 S 3 and Na 2 S 2 formed from the Na 2 S and Na 2 S 2 targets, respectively. We propose that the loss of Na in the case of the Na 2 S target is due to preferential sputtering of Na resulting from the higher energy required to break the Na–S bonds in Na 2 S. Here, the development of thin film sodium sulfides opens a new route to understanding their fundamental properties, such as Na + transport, conductivity, and reactivity.

preferential sputtering↗

Deposition and characterization of α-Fe 2 O 3 /Pd thin films for neutron reflectometry studies

Here, we report deposition of hematite/Pd thin films on silicon wafers via radio frequency (RF) magnetron sputtering and subsequent characterization for future in situ neutron reflectometry studies. Following deposition, the hematite/Pd thin films were characterized as prepared and after annealing in air for 2h at 400, 500, and 600 °C, respectively. Raman spectroscopy, grazing incidence x-ray diffraction, and neutron reflectometry (NR) were used to characterize the structure and chemical compositions of the thin films. The results indicate that pure α-Fe 2 O 3 (hematite) films were produced, free from other iron oxide phases and impurities. NR data reveal that one intermediate layer between the Pd layer and the hematite layer was formed during sputtering deposition processes. The fitted scattering length density (SLD) of the as-deposited hematite layer is 70% of the theoretical SLD value, indicating that the grains are loosely packed in the RF-deposited hematite films. After annealing at elevated temperatures, the hematite films show increased SLD values but remain comparable to that of preannealed.

36 MATERIALS SCIENCE↗

Nb 3 Sn coating of SRF cavity by cosputtering from a composite target

Here, we deposited an Nb 3 Sn film on the inner surface of a 2.6 GHz Nb superconducting radio frequency cavity by cosputtering using a composite of Nb and Sn tube targets in a DC cylindrical magnetron sputtering system, followed by the thermal annealing of the coated cavity. An aluminum mockup cavity, replicating a 2.6 GHz Nb SRF cavity geometry, was utilized to optimize deposition parameters, resulting in cosputtered Nb–Sn films with an Sn content of 32–42 at. % on the beam tubes and equator positions. Several annealing conditions were investigated to improve the surface homogeneity of the Nb 3 Sn film. The best cosputtered Nb–Sn film was achieved after annealing at 600 °C for 6 h, followed by annealing at 950 °C for 1 h. The best process was applied to a Nb cavity, which was RF tested in a cryogenic dewar. RF testing of the Nb 3 Sn-coated cavity demonstrated a superconducting transition temperature of 17.78 K. The Nb 3 Sn cavity underwent light Sn recoating, followed by additional RF testing, resulting in the enhancement of the RF performance, primarily due to the improved surface homogeneity of the Nb 3 Sn coating.

Nb3Sn film↗

Feasibility of producing a short, high energy s-band linear accelerator using a klystron power source

Purpose: To use a finite-element method (FEM) model to study the feasibility of producing a short s-band (2.9985 GHz) waveguide capable of producing x-rays energies up to 10 MV, for applications in a linac-MR, as well as conventional radiotherapy. Methods: An existing waveguide FEM model developed by the authors' group is used to simulate replacing the magnetron power source with a klystron. Peak fields within the waveguide are compared with a published experimental threshold for electric breakdown. The RF fields in the first accelerating cavity are scaled, approximating the effect of modifications to the first coupling cavity. Electron trajectories are calculated within the RF fields, and the energy spectrum, beam current, and focal spot of the electron beam are analyzed. One electron spectrum is selected for Monte Carlo simulations and the resulting PDD compared to measurement. Results: When the first cavity fields are scaled by a factor of 0.475, the peak magnitude of the electric fields within the waveguide are calculated to be 223.1 MV/m, 29% lower than the published threshold for breakdown at this operating frequency. Maximum electron energy increased from 6.2 to 10.4 MeV, and beam current increased from 134 to 170 mA. The focal spot FWHM is decreased slightly from 0.07 to 0.05 mm, and the width of the energy spectrum increased slightly from 0.44 to 0.70 MeV. Monte Carlo results show d{sub max} is at 2.15 cm for a 10 Multiplication-Sign 10 cm{sup 2} field, compared with 2.3 cm for a Varian 10 MV linac, while the penumbral widths are 4.8 and 5.6 mm, respectively. Conclusions: The authors' simulation results show that a short, high-energy, s-band accelerator is feasible and electric breakdown is not expected to interfere with operation at these field strengths. With minor modifications to the first coupling cavity, all electron beam parameters are improved.

60 APPLIED LIFE SCIENCES↗

Poster — Thur Eve — 15: Improvements in the stability of the tomotherapy imaging beam

Use of helical TomoTherapy based MVCT imaging for adaptive planning requires the image values (HU) to remain stable over the course of treatment. In the past, the image value stability was suboptimal, which required frequent change to the image value to density calibration curve to avoid dose errors on the order of 2–4%. The stability of the image values at our center was recently improved by stabilizing the dose rate of the machine (dose control servo) and performing daily MVCT calibration corrections. In this work, we quantify the stability of the image values over treatment time by comparing patient treatment image density derived using MVCT and KVCT. The analysis includes 1) MVCT - KVCT density difference histogram, 2) MVCT vs KVCT density spectrum, 3) multiple average profile density comparison and 4) density difference in homogeneous locations. Over two months, the imaging beam stability was compromised several times due to a combination of target wobbling, spectral calibration, target change and magnetron issues. The stability of the image values were analyzed over the same period. Results show that the impact on the patient dose calculation is 0.7% +− 0.6%.

60 APPLIED LIFE SCIENCES↗

Electron microscopy of phase and structural transformations in soft magnetic nanocrystalline Fe-Zr-N films

The effect of deposition conditions (film thickness) on the structure of soft magnetic Fe{sub 80-78}Zr{sub 10}N{sub 10-12} films formed by reactive magnetron deposition on a heat-resistant glass substrate has been investigated by analytical transmission electron microscopy, high-resolution electron microscopy, and diffraction analysis. The processes of evolution of the phase and structural state of films and the film-substrate interface upon annealing in the temperature range of 200-650 Degree-Sign C have been analyzed taking into account the thermodynamic, kinetic, and structural factors and the specific features of the nanocrystalline state.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗