Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “INTERMETALLICS”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 1,279 records · Page 71

Origin of deactivation of aqueous Na–CO 2 battery and mitigation for long-duration energy storage

Here, the development of long-duration energy storage technology is crucial to facilitate the efficient utilization of renewable energy sources while mitigating carbon dioxide production. In this study, we investigate the deactivation and reactivation mechanisms of the aqueous Na–CO 2 battery during extended cycling. We have designed the cathode to include non-precious intermetallic catalysts. As the cell undergoes repeated cycles, the voltage polarization during discharge progressively rises, eventually leading to the cell's deactivation and formation of decomposition products clogging the electrode surface. Results obtained from comprehensive characterization techniques, including conductive atomic force microscopy (cAFM), Raman spectroscopy, X-ray photoelectron spectroscopy, X-ray diffraction, and inductively coupled plasma-mass spectrometry provide insight into the decomposition products. We also showcase an electrochemical approach for regeneration of these aqueous cells. Our findings, along with the insights we have gained, provide a path toward creating long-duration systems with self-healing properties.

25 ENERGY STORAGE↗

Ti{sub 2}GaC, Ti{sub 4}GaC{sub 3} and Cr{sub 2}GaC-Synthesis, crystal growth and structure analysis of Ga-containing MAX-phases M{sub n+1}GaC{sub n} with M=Ti, Cr and n=1, 3

Single crystals of Ga-containing MAX-phases Ti{sub 2}GaC, Ti{sub 4}GaC{sub 3}, and Cr{sub 2}GaC were grown from a metallic melt generated by an excess of Ga. This technique allows the crystal growth at different temperatures to control the product distribution. Compounds developed were Ti{sub 2}GaC and TiC at 1500 deg. C, and Ti{sub 2}GaC and Ti{sub 4}GaC{sub 3} at 1300 deg. C. Crystal structures were refined from single crystal data. Ti{sub 2}GaC and Cr{sub 2}GaC were previously known, and belong to the Cr{sub 2}AlC type as well as the solid solutions V{sub 2}Ga{sub 1-x}Al{sub x}C and Cr{sub 2}Ga{sub 1-x}Al{sub x}C. Ti{sub 4}GaC{sub 3} is one of the few 413-phases (P6{sub 3}/mmc, a=3.0690(4) A, c=23.440(5) A) and the first Ga-containing representative. The crystal structures of MAX-phases are intergrowths of layers of an intermetallic MGa in a hexagonal stacking sequence with carbidic layers (MC){sub n} of the NaCl type. The thickness of the layer depends from the value of n. The results of the structure refinements also demonstrate that also the structural details follow this description. - Graphical abstract: Single crystals of Ga-containing MAX-Phases (TiC){sub n}(TiGa) (n=1, 3) were grown from a metallic melt including and characterised by X-ray diffraction. Ti{sub 4}GaC{sub 3} is one of the few 413-phase and the first containing Ga.

36 MATERIALS SCIENCE↗

Crystal growth and magnetic behavior of R{sub 6}T{sub 13-x}Al{sub x}M{sub y} phases (R=La, Nd; T=Mn, Fe; M=main group) grown from lanthanide-rich eutectic fluxes

Binary eutectic mixtures of early lanthanide metals and late transition metals have been explored as media for crystal growth of new intermetallic phases. A large family of R{sub 6}T{sub 13-x}Al{sub x}M{sub y} phases (R=La or Nd; T=Fe or Mn; M=main group elements) with the La{sub 6}Co{sub 11}Ga{sub 3} structure type can be crystallized from La/Ni and Nd/Fe eutectics. The tetragonal structure of these compounds features slabs of transition metal atoms capped with mixed T/Al sites and separated by layers of lanthanide ions. The growth of large crystals of the lanthanum analogs allows for the study of the anisotropic magnetic properties of the transition metal slabs. For La{sub 6}Fe{sub 13-x}Al{sub x}M{sub y} analogs, these order antiferromagnetically with T{sub N} strongly dependent on the Fe/Al ratio on the mixed sites. Growth of Mn analogs is reported for the first time; the transition metal slabs in La{sub 6}(Mn/Ni){sub 10}Al{sub 3} phases order ferromagnetically with a T{sub C} of 200 K. - Graphical abstract: R{sub 6}T{sub 13-x}Al{sub x}M{sub y} phases with the La{sub 6}Co{sub 11}Ga{sub 3} structure type crystallize from La/Ni and Nd/Fe eutectics. Transition metal slabs in La{sub 6}Fe{sub 13-x}Al{sub x}M{sub y} and La{sub 6}(Mn/Ni){sub 10}Al{sub 3} order antiferromagnetically (T{sub N} 150 K) and ferromagnetically (T{sub C} 200 K), respectively.

36 MATERIALS SCIENCE↗

Synthesis, electronic transport and magnetic properties of Zr{sub 1-x}Y{sub x}NiSn, (x=0-0.25) solid solutions

The crystal structure of the Zr{sub 1-x}Y{sub x}NiSn half-Heusler solid solutions is synthesized and their crystal structure is determined. Electrical resistivity and thermoelectric Seebeck coefficient are measured in the 80-380 K temperature range, whereas magnetic susceptibility is measured at 290 K. It is established that substitution of Zr host atoms by Y in the ZrNiSn intermetallic semiconductor is equivalent to doping by acceptor impurities. Self-consistent ab initio calculations, based on the full potential local orbital (FPLO) minimum basis method, are performed to investigate the electronic and thermoelectric properties of these alloys. Spin polarized within the framework of the coherent potential approximation (CPA) are included. - Graphical abstract: Both approaches experimental and calculations point to the same conclusions. Resistivity and thermopower measurements assert that doping of ZrNiSn based compound by the Y as acceptor impurity induces the insulator-metal transition and leads the S value sign reverse.

36 MATERIALS SCIENCE↗

Structure, bonding, and magnetic response in two complex borides: Zr{sub 2}Fe{sub 1-{delta}}Ru{sub 5+{delta}}B2 and Zr{sub 2}Fe{sub 1-{delta}}(Ru{sub 1-x}Rh{sub x}){sub 5+{delta}}B2

Polycrystalline samples of two complex intermetallic borides Zr{sub 2}Fe{sub 1-{delta}}Ru{sub 5+{delta}}B2 and Zr{sub 2}Fe{sub 1-{delta}}(Ru{sub 1-x}Rh{sub x}){sub 5+{delta}}B2 ({delta}=ca. 0.10; x=0.20) were synthesized by high-temperature methods and characterized by single-crystal X-ray diffraction, energy dispersive spectroscopy, and magnetization measurements. Both structures are variants of Sc{sub 2}Fe(Ru{sub 1-x}Rh{sub x}){sub 5}B{sub 2} and crystallize in the space group P4/mbm (no. 127) with the Ti{sub 3}Co{sub 5}B{sub 2}-type structure. These structures contain single-atom, Fe-rich Fe/Ru or Fe/Ru/Rh chains along the c-axis with an interatomic metal-metal distance of 3.078(1) A, a feature which makes them viable for possible low-dimensional temperature-dependent magnetic behavior. Magnetization measurements indicated weak ferrimagnetic ordering with ordering temperatures ca. 230 K for both specimens. Tight-binding electronic structure calculations on a model 'Zr{sub 2}FeRu{sub 5}B{sub 2}' using LDA yielded a narrow peak at the Fermi level assigned to Fe-Fe antibonding interactions along the c-axis, a result that indicates an electronic instability toward ferromagnetic coupling along these chains. Spin-polarized calculations of various magnetic models were examined to identify possible magnetic ordering within and between the single-atom, Fe-rich chains. -- Graphical abstract: Zr{sub 2}FeRu{sub 5-x}Rh{sub x}B{sub 2} (x=0, 1) crystallizes with magnetic atoms forming chains which have been shown to order magnetically depending on the total valence electron count. Magnetic measurements and tight-binding electronic structure calculations are employed to investigate the ordering. Display Omitted

36 MATERIALS SCIENCE↗

Crystal, electronic structure and electronic transport properties of the Ti{sub 1-x}V{sub x}NiSn (x=0-0.10) solid solutions

The n-TiNiSn ternary intermetallic semiconductor is doped by the V donor impurity and the crystalline structure of the obtained Ti{sub 1-x}V{sub x}NiSn solid solutions (x=0-0.10) is determined by X-ray diffraction. Temperature and concentration dependences of the resistivity and thermopower are investigated in 80-380 K range. As main results, the TiNiSn conductivity type is revealed insensitive to V doping and the thermopower factor substantially increases versus V content. First principle calculations based on DFT using FPLO and KKR-CPA methods are performed as well. Experimental data and electronic structure calculations are compared and discussed in terms of thermopower improvements. -- Graphical abstract: Both approaches experimental and calculations point to the same conclusions. Resisitivity, power factor and thermopower estimations indicate that doping of TiNiSn based compound by the V induces insulator-metal transition without change of the negative sign of S thermopower. Vanadium is revealed as donor impurity.

36 MATERIALS SCIENCE↗

Crystal structure, magnetism and transport properties of Ce{sub 3}Ni{sub 25.75}Ru{sub 3.16}Al{sub 4.1}B{sub 10}

Single crystals of Ce{sub 3}Ni{sub 25.75}Ru{sub 3.16}Al{sub 4.1}B{sub 10} were obtained from a process in which a polycrystalline sample of CeRu{sub 2}Al{sub 2}B was annealed in an excess of a Ni–In flux. The initial phase, CeRu{sub 2}Al{sub 2}B, does not recrystallize, instead, crystals of a new phase, Ce{sub 3}Ni{sub 25.75}Ru{sub 3.16}Al{sub 4.1}B{sub 10}, could be isolated once the flux was removed. The title compound crystallizes in the tetragonal space group P4/nmm (No. 129) with a=1139.02(8), c=801.68(6) pm (c/a=0.70) in the Nd{sub 3}Ni{sub 29}Si{sub 4}B{sub 10} structure type. Electrical resistivity measurements reveal metallic behavior with a minimum of 700 µΩ cm and a small residual resistivity ratio of RRR=1.4 indicating a large amount of disorder scattering. The cerium atoms are either in the 4+ or an intermediate valence state with a valence fluctuation temperature far above room temperature. - Graphical abstract: Single crystals of Ce{sub 3}Ni{sub 25.75}Ru{sub 3.16}A{sub l4.1}B{sub 10} were obtained using a process in which a polycrystalline sample of CeRu{sub 2}Al{sub 2}B was annealed in an excess of a Ni–In flux. Electrical resistivity measurements reveal metallic behavior with a minimum of 700 μΩ cm and a small residual resistivity ratio of RRR=1.4 indicating a large amount of disorder scattering. The cerium atoms are either in the 4+ or an intermediate valence state with a valence fluctuation temperature far above room temperature. Display Omitted - Highlights: • Flux synthesis of high quality single crystals of Ce{sub 3}Ni{sub 25.75}Ru{sub 3.16}Al{sub 4.1}B{sub 10} is presented along with the crystal structure, magnetic and transport properties. • The compound is isostructural to Nd{sub 3}Ni{sub 29}Si{sub 4}B{sub 10} but is first of this structure type showing mixed occupancies of d-elements. • This is an intermetallic phase with Ce in either the 4+ or an intermediate valence state. • The fact that this structure with mixed occupied transition metal sites exists suggests that more compounds of this type should be accessible and the physical properties tuned.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Structural, magnetic, magneto-caloric and Mössbauer spectral study of Tb{sub 2}Fe{sub 17} compound synthesized by arc melting

We have synthesized the intermetallic Tb{sub 2}Fe{sub 17} compound in hexagonal crystal structure by arc-melting without annealing. X-ray diffraction pattern has been refined by Rietveld method. The crystal structure is hexagonal with P6{sub 3}/mmc space group (Th{sub 2}Ni{sub 17}-type). The Mössbauer spectrum of Tb{sub 2}Fe{sub 17} compound has been analyzed with seven magnetic sextets assigned to the inequivalent crystallographic sites. The temperature dependence of magnetization data revealed that Tb{sub 2}Fe{sub 17} exhibits a second-order ferromagnetic to paramagnetic phase transition in the vicinity of Curie temperature (T{sub C}=412 K). The relative cooling power around the magnetic transition and the Arrott plots are also reported. - Graphical abstract: A 3D surface showing the temperature and applied magnetic field dependencies of the magnetization for Tb{sub 2}Fe{sub 17} compound (left). Rietveld analysis of the XRD pattern (right). Crystal structure for the hexagonal P6{sub 3}/mmc Tb{sub 2}Fe{sub 17} (bottom). Display Omitted - Highlights: • Tb{sub 2}Fe{sub 17} single-phase synthesized by simple arc-melting without any heat treatment. • The crystal structure is hexagonal with P6{sub 3}/mmc space group. • The magnetic entropy change of the sample was determined by Maxwell relation. • Hyperfine parameters, magnetic and magnetocaloric properties were studied.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Characterization of phases in a Mg-6Gd-4Sm-0.4Zr (wt.%) alloy during solution treatment

Phases in as-cast and solution-treated Mg-6Gd-4Sm-0.4Zr (wt.%) alloy have been characterized using transmission electron microscopy in this paper. The intermetallic phase in as-cast microstructure has a face centered cubic crystal structure (a = 2.2879 nm) with a composition of Mg{sub 6.2}(Sm{sub 0.56}Gd{sub 0.44}) and was dissolved after solution treatment. A particulate phase with a face centered cubic crystal structure (a = 0.5502 nm) was found in the solution-treated microstructure and suggested to already exist in as-cast sample as the nucleus for its further growth during solution treatment.

36 MATERIALS SCIENCE↗

Sigma phase morphologies in cast and aged super duplex stainless steel

Solution annealed and water quenched duplex and super duplex stainless steels are thermodynamically metastable systems at room temperature. These systems do not migrate spontaneously to a thermodynamically stable condition because an energy barrier separates the metastable and stable states. However, any heat input they receive, for example through isothermal treatment or through prolonged exposure to a voltaic arc in the welding process, cause them to reach a condition of stable equilibrium which, for super duplex stainless steels, means precipitation of intermetallic and carbide phases. These phases include the sigma phase, which is easily identified from its morphology, and its influence on the material's impact strength. The purpose of this work was to ascertain how 2-hour isothermal heat treatments at 920 deg. C and 980 deg. C affect the microstructure of ASTM A890/A890M GR 6A super duplex stainless steel. The sigma phase morphologies were found to be influenced by these two aging temperatures, with the material showing a predominantly lacy microstructure when heat treated at 920 deg. C and block-shaped when heat treated at 980 deg. C.

36 MATERIALS SCIENCE↗

Observation of high-temperature phase transformation in the Si-modified aluminide coating on mild steel using EBSD

Mild steel was coated by hot-dipping in a molten bath containing Al-10 wt.% Si. The phase transformation in the aluminide layer during diffusion at 750 deg. C in static air was analyzed by Electron Backscatter Diffraction. The results showed that the aluminide layer of the as-coated specimen consisted of an outer Al-Si eutectic topcoat and the inner Fe-Al-Si and Fe-Al intermetallic layers. The formation of {tau}{sub 5}-Al{sub 7}Fe{sub 2}Si and {tau}{sub 6}-Al{sub 4}FeSi was observed with increasing exposure time at 750 deg. C, while the {tau}{sub 1}-(Al,Si){sub 5}Fe{sub 3} phase precipitated into the Fe{sub 2}Al{sub 5} phase. After 60 min of exposure, the {tau}{sub 5}-Al{sub 7}Fe{sub 2}Si and {tau}{sub 6}-Al{sub 4}FeSi phases disappeared. The FeAl phase not only formed at the interface between Fe{sub 2}Al{sub 5} and the steel substrate, but also transformed from {tau}{sub 1}-(Al,Si){sub 5}Fe{sub 3} after diffusion for 10 h. With prolonged exposure, the growing FeAl phase decreased the thickness of Fe{sub 2}Al{sub 5} and forced the formation of FeAl{sub 2} phase. Finally, the aluminide layer comprised only FeAl{sub 2} and FeAl.

36 MATERIALS SCIENCE↗

EBSD characterization of high-temperature phase transformations in an Al-Si coating on Cr-Mo steel

5Cr-0.5Mo steel was coated by hot-dipping in a molten bath containing Al-10 wt.% Si. The phase transformation in the aluminide layer during diffusion at 750 Degree-Sign C in static air was analyzed by electron backscatter diffraction. The results show the aluminide layer of the as-coated specimen consisted of an outer Al-Si topcoat, a middle layer formed of scattered {tau}{sub 5(C)}-Al{sub 7}(Fe,Cr){sub 2}Si particles and minor plate-shaped {tau}{sub 4}-Al{sub 4}FeSi{sub 2} and {tau}{sub 6}-Al{sub 4}FeSi phases in the Al-Si matrix and an inner continuous {tau}{sub 5(H)}-Al{sub 7}Fe{sub 2}Si layer, respectively from the coating surface to the steel substrate. The formation of FeAl{sub 3} and Fe{sub 2}Al{sub 5} with {tau}{sub 1}-(Al,Si){sub 5}Fe{sub 3} precipitates can be observed with increasing exposure time at 750 Degree-Sign C. After 5 h of exposure, the Al-Si topcoat has been consumed, and the aluminide layer consisted of Fe{sub 2}Al{sub 5} and a few {tau}{sub 1}-(Al,Si){sub 5}Fe{sub 3} precipitates. The FeAl phase not only formed at the interface between Fe{sub 2}Al{sub 5} and the steel substrate, but also transformed from {tau}{sub 1}-(Al,Si){sub 5}Fe{sub 3} after diffusion for 10 h. With prolonged exposure, the aluminide layer comprised only FeAl{sub 2} and FeAl. - Highlights: Black-Right-Pointing-Pointer EBSD can differentiate phases in aluminide layer with similar chemical compositions. Black-Right-Pointing-Pointer Mapping and EBSPs functions in EBSD provide a reliable phase identification. Black-Right-Pointing-Pointer A phase transformation in the aluminide layer has been described in detail. Black-Right-Pointing-Pointer 5 Fe-Al-Si and 4 Fe-Al intermetallic phases are performed during the diffusion. Black-Right-Pointing-Pointer Cubic {tau}{sub 5(C)}-Al{sub 7} (Fe,Cr){sub 2}Si and hexagonal {tau}{sub 5(H)}-Al{sub 7}(Fe,Cr){sub 2}Si are identified.

36 MATERIALS SCIENCE↗

Microstructures and microhardness evolutions of melt-spun Al-8Ni-5Nd-4Si alloy

Al-Ni-Nd-Si alloy with nominal composition of Al-8 wt.%Ni-5 wt.%Nd-4 wt.%Si was rapidly solidified by using melt-spinning technique to examine the influence of the cooling rate/conditions on microstructure and mechanical properties. The resulting conventional cast (ingot) and melt-spun ribbons were characterized by X-ray diffraction, optical microscopy, scanning electron microscopy together with energy dispersive spectroscopy, differential scanning calorimetry, differential thermal analysis and Vickers microhardness tester. The ingot alloys consists of four phases namely {alpha}-Al, intermetallic Al{sub 3}Ni, Al{sub 11}Nd{sub 3} and fcc Si. Melt-spun ribbons are completely composed of {alpha}-Al phase. The optical microscopy and scanning electron microscopy results show that the microstructures of rapidly solidified ribbons are clearly different from their ingot alloy. The change in microhardness is discussed based on the microstructural observations. - Highlights: Black-Right-Pointing-Pointer Rapid solidification allows a reduction in grain size, extended solid solution ranges. Black-Right-Pointing-Pointer We observed the matrix lattice parameter increases with increasing wheel speed. Black-Right-Pointing-Pointer Melt-spun ribbons consist of partly amorphous phases embedded in crystalline phases. Black-Right-Pointing-Pointer The solidification rate is high enough to retain most of alloying elements in the Al matrix. Black-Right-Pointing-Pointer The rapid solidification has effect on the phase constitution.

36 MATERIALS SCIENCE↗

AFM study of the effects of laser surface remelting on the morphology of Al-Fe aerospace alloys

Laser beam welding has recently been incorporated into the fabrication process of aircraft and automobile structures. Surface roughness is an important parameter of product quality that strongly affects the performance of mechanical parts, as well as production costs. This parameter influences the mechanical properties such as fatigue behavior, corrosion resistance, creep life, etc., and other functional characteristics such as friction, wear, light reflection, heat transmission, lubrification, electrical conductivity, etc. The effects of laser surface remelting (LSR) on the morphology of Al-Fe aerospace alloys were examined before and after surface treatments, using optical microscopy (OM), scanning electron microscopy (SEM), low-angle X-ray diffraction (LA-XRD), atomic force microscopy (AFM), microhardness measurements (Vickers hardness), and cyclic voltammetry. This analysis was performed on both laser-treated and untreated sanded surfaces, revealing significant differences. The LA-XRD analysis revealed the presence of alumina, simple metals and metastable intermetallic phases, which considerably improved the microhardness of laser-remelted surfaces. The morphology produced by laser surface remelting enhanced the microstructure of the Al-Fe alloys by reducing their roughness and increasing their hardness. The treated surfaces showed passivity and stability characteristics in the electrolytic medium employed in this study. - Highlights: Black-Right-Pointing-Pointer The samples laser-treated and untreated showed significant differences. Black-Right-Pointing-Pointer The La-XRD revealed the presence of alumina in Al-1.5 wt.% Fe. Black-Right-Pointing-Pointer The laser-treated reducing the roughness and increasing the hardness. Black-Right-Pointing-Pointer The laser-treated surfaces showed characteristic passive in the electrolytic medium. Black-Right-Pointing-Pointer The laser-treated is a promising technique for applications technological.

36 MATERIALS SCIENCE↗

Effect of solution annealing temperature on precipitation in 2205 duplex stainless steel

In the present study, effect of solution annealing temperature (1050 Degree-Sign C and 1100 Degree-Sign C) and isothermal ageing (700 Degree-Sign C: 15 min to 6 h) on the microstructural changes in 2205 duplex stainless steel has been investigated systematically. Scanning electron microscopy and X-ray diffraction were adopted to follow the microstructural evolution, while an energy dispersive spectrometer attached to scanning electron microscope was used to obtain localised chemical information of various phases. The ferritic matrix of the two phase 2205 duplex stainless steel ({approx} 45% ferrite and {approx} 55% austenite) undergoes a series of metallurgical transformations during ageing-formation of secondary austenite ({gamma}{sub 2}) and precipitation of Cr and Mo rich intermetallic (chi-{chi} and sigma-{sigma}) phases. For solution annealing at 1050 Degree-Sign C, significant amount of carbides were observed in the ferrite grains after 1 h of ageing at 700 Degree-Sign C. {chi} Phase precipitated after the precipitation of carbides-preferentially at the ferrite-ferrite and also at the ferrite-austenite boundaries. {sigma} Phase was not observed in significant quantity even after 6 h of ageing. The sequence of precipitation in samples solution annealed at 1050 Degree-Sign C was found to be carbides {yields} {chi} {yields} {sigma}. On the contrary, for samples solution annealed at 1100 Degree-Sign C, the precipitation of {chi} phase was negligible. {chi} Phase precipitated before {sigma} phase, preferentially along the ferrite-ferrite grain boundaries and was later consumed in the {sigma} phase precipitation. The {sigma} phase precipitated via the eutectoid transformation of ferrite to yield secondary austenite {gamma}{sub 2} and {sigma} phase in the ferrite and along the ferrite-austenite grain boundaries. An increase in the volume fraction of {gamma}{sub 2} and {sigma} phase with simultaneous decrease in the ferrite was evidenced with ageing. - Highlights: Black-Right-Pointing-Pointer Effect of solution annealing temperature on microstructural evolution is studied. Black-Right-Pointing-Pointer {chi} Phase precipitated preferentially in the samples solution annealed at 1050 Degree-Sign C. Black-Right-Pointing-Pointer {sigma} Phase precipitated preferentially in the samples solution annealed at 1100 Degree-Sign C. Black-Right-Pointing-Pointer For SA at 1050 Degree-Sign C, the sequence of precipitation was carbides {yields} {chi} phase {yields} {sigma} phase. Black-Right-Pointing-Pointer For SA at 1100 Degree-Sign C, {sigma} phase precipitated via the eutectoid reaction: ferrite (F) {yields} {sigma} + {gamma}{sub 2}.

36 MATERIALS SCIENCE↗

Brazing ZrO{sub 2} ceramic to Ti–6Al–4V alloy using NiCrSiB amorphous filler foil: Interfacial microstructure and joint properties

Reliable brazing of ZrO{sub 2} ceramic and Ti–6Al–4V alloy was achieved using NiCrSiB amorphous filler foil. The interfacial microstructure of ZrO{sub 2}/Ti–6Al–4V joints was characterized by scanning electron microscope, energy dispersive spectrometer and micro-focused X-ray diffractometer. The effects of brazing temperature on the interfacial microstructure and joining properties of brazed joints were investigated in detail. Active Ti of Ti–6Al–4V alloy dissolved into molten filler metal and reacted with ZrO{sub 2} ceramic to form a continuous TiO reaction layer, which played an important role in brazing. Various reaction phases including Ti{sub 2}Ni, Ti{sub 5}Si{sub 3} and β-Ti were formed in brazed joints. With an increasing of brazing temperature, the TiO layer thickened gradually while the Ti{sub 2}Ni amount reduced. Shear test indicated that brazed joints tend to fracture at the interface between ZrO{sub 2} ceramic and brazing seam or Ti{sub 2}Ni intermetallic layer. The maximum average shear strength reached 284.6 MPa when brazed at 1025 °C for 10 min. - Graphical Abstract: Interfacial microstructure of ZrO{sub 2}/TC4 joint brazed using NiCrSiB amorphous filler foil was: ZrO{sub 2}/TiO/Ti{sub 2}Ni + β-Ti + Ti{sub 5}Si{sub 3}/β-Ti/Widmanstätten structure/TC4. - Highlights: • Brazing of ZrO{sub 2} ceramic and Ti-6Al-4V alloy was achieved. • Interfacial microstructure was TiO/Ti{sub 2}Ni + β + Ti{sub 5}Si{sub 3}/β/Widmanstätten structure. • The formation of TiO produced the darkening effect of ZrO{sub 2} ceramic. • The highest joining strength of 284.6MPa was obtained.

36 MATERIALS SCIENCE↗

Microstructure, microstructural stability and mechanical properties of sand-cast Mg–4Al–4RE alloy

This paper presents a methodology for assessing the phase composition and the results of structural stability tests of the sand-cast Mg–4Al–4RE alloy after annealing it at 175 and 250 °C for 3000 h. The microstructure was analyzed with optical, scanning electron, and transmission electron microscopy. The phase composition was determined with X-ray diffraction. The structure of the Mg–4Al–4RE (AE44) alloy is composed of large grains of α-Mg solid solution, needle-shaped precipitates of the Al{sub 11}RE{sub 3}phase, polyhedral precipitates of the Al{sub 2}RE phase and Al{sub 10}RE{sub 2}Mn{sub 7} phase. After annealing at 175 °C for 3000 h, no changes in the alloy structure are observed, whereas after annealing at 250 °C the precipitates of the Al{sub 11}RE{sub 3} phase are found to be in the initial stages of spheroidization. The coarse-grained structure and unfavorable morphology of the intermetallic phases in the sand-cast AE44 alloy, which are caused by low solidification rates, result in low creep resistance up to 200 °C and low mechanical properties at ambient temperature and at 175 °C. - Highlights: • Complement the knowledge about the microstructure of Mg-Al-RE alloys. • Clarify the mechanism of formation of Mg17Al12 phase above 180 °C. • Applying a chemical dissolution of the α-Mg in order to phase identification. • Applying a statistical test to assess the spheroidization of precipitates. • Quantitative description of microstructure of Mg-Al-RE alloys.

36 MATERIALS SCIENCE↗

Precipitation process in a Mg–Gd–Y alloy grain-refined by Al addition

The precipitation process in Mg–10Gd–3Y (wt.%) alloy grain-refined by 0.8 wt.% Al addition has been investigated by transmission electron microscopy. The alloy was given a solution treatment at 520 °C for 6 h plus 550 °C for 7 h before ageing at 250 °C. Plate-shaped intermetallic particles with the 18R-type long-period stacking ordered structure were observed in the solution-treated state. Upon isothermal ageing at 250 °C, the following precipitation sequence was identified for the α-Mg supersaturated solution: β″ (D0{sub 19}) → β′ (bco) → β{sub 1} (fcc) → β (fcc). The observed precipitation process and age hardening response in the Al grain-refined Mg–10Gd–3Y alloy are compared with those reported in the Zr grain-refined counterpart. - Highlights: • The precipitation process in Mg–10Gd–3Y–0.8Al (wt.%) alloy has been investigated. • Particles with the 18R-type LPSO structure were observed in the solution state. • Upon ageing at 250 °C, the precipitation sequence is: β″ → β′ → β1 (fcc) → β. • The Al grain-refined alloy has a lower hardness than the Zr refined counterpart.

36 MATERIALS SCIENCE↗