Effects of Intercritical Annealing Temperature on Mechanical Properties of Fe-7.9Mn-0.14Si-0.05Al-0.07C Steel

A medium Mn steel has been designed to achieve an excellent combination of strength and ductility based on the TRIP (Transformation Induced Plasticity) concept for automotive applications. Following six passes of hot rolling at 850 °C, the Fe-7.9Mn-0.14Si-0.05Al-0.07C (wt.%) steel was warm-rolled at 630 °C for seven passes and subsequently air cooled to room temperature. The sample was subsequently intercritically annealed at various temperatures for 30 min to promote the reverse transformation of martensite into austenite. The obtained results show that the highest volume fraction of austenite is 39% for the sample annealed at 600 °C. This specimen exhibits a yield stress of 910 MPa and a high ultimate tensile stress of 1600 MPa, with an elongation-to-failure of 0.29 at a strain rate of 1 × 10⁻³/s. The enhanced work-hardening ability of the investigated steel is closely related to martensitic transformation and the interaction of dislocations. Especially, the alternate arrangement of acicular ferrite (soft phase) and ultrafine austenite lamellae (50–200 nm, strong and ductile phase) is the key factor contributing to the excellent combination of strength and ductility. On the other hand, the as-warm-rolled sample also exhibits the excellent combination of strength and ductility, with elongation-to-failure much higher than those annealed at temperatures above 630 °C.

36 MATERIALS SCIENCE↗

Influence of Mo Content on the Precipitation Behavior of 13Ni Maraging Ultra-High Strength Steels

This study offers valuable insights into the precipitation behavior of 13Ni maraging steels, emphasizing the role of molybdenum content in their microstructure, strengthening, and precipitate evolution. Precipitate morphology and crystallography were examined using a combination of high-resolution transmission electron microscopy and selected area electron diffraction. Strengthening mechanisms were assessed through Vickers hardness measurements. All the examined samples exhibited a lath martensite microstructure and displayed an increasing hardness over the aging time. The molybdenum content not only influenced the presence of retained austenite in the initial microstructure but also affected the type of precipitates formed during the early aging stages. Initially, Ni 3 Mo precipitates were formed, succeeded by the formation of more stable Fe 2 (Mo,Ti) Laves precipitates. The ultra-high strength of 13Ni maraging steels arises from the combination of the precipitate type and size distribution. The base composition of 13Ni maraging steels achieved a peak hardness of 798 HV1 through the precipitation of Laves Fe 2 (Mo,Ti) phases ranging from 3 to 14 nm in diameter.

13Ni maraging steels↗

Deformation Behavior of a Double Soaked Medium Manganese Steel with Varied Martensite Strength

The effects of athermal martensite on yielding behavior and strain partitioning during deformation is explored using in situ neutron diffraction for a 0.14C–7.14Mn medium manganese steel. Utilizing a novel heat treatment, termed double soaking, samples with similar microstructural composition and varied athermal martensite strength and microstructural characteristics, which composed the bulk of the matrix phase, were characterized. It was found that the addition of either as-quenched or tempered athermal martensite led to an improvement in mechanical properties as compared to a ferrite plus austenite medium manganese steel, although the yielding and work hardening behavior were highly dependent upon the martensite characteristics. Specifically, athermal martensite was found to promote continuous yielding and improve the work hardening rate during deformation. The results of this study are particularly relevant when considering the effect of post-processing thermal heat treatments, such as tempering or elevated temperature service environments, on the mechanical properties of medium manganese steels containing athermal martensite.

36 MATERIALS SCIENCE↗

Corrosion Compatibility of Stainless Steels and Nickel in Pyrolysis Biomass-Derived Oil at Elevated Storage Temperatures

Corrosion compatibility of stainless steels and nickel (Ni200) was assessed in fast pyrolysis bio-oil produced from pyrolysis of high ash and high moisture forest residue biomass. Sample mass change, ICP-MS and post-exposure electron microscopy characterization was used to investigate the extent of corrosion. Among the tested samples, type 430F and type 316 stainless steels (SS430F and SS316) and Ni200 (~98.5% Ni) showed minimal mass changes (less than 2 mg∙cm−2) after the bio-oil exposures at 50 and 80 °C for up to 168 h. SS304 was also considered to be compatible in the bio-oil due to its relatively low mass change (1.6 mg∙cm−2 or lower). SS410 samples showed greater mass loss values even after exposures at a relatively low temperature of 35 °C. Fe/Cr values from ICP-MS data implied that Cr enrichment in stainless steels would result in a protective oxide layer associated with corrosion resistance against the bio-oil. Post exposure characterization showed continuous and uniform Cr distribution in the surface oxide layer of SS430F, which showed a minimal mass change, but no oxide layer on a SS430 sample, which exhibited a significant mass loss.

09 BIOMASS FUELS↗

Complex Nano-Scale Structures for Unprecedented Properties in Steels

Processing bulk nanoscrystalline materials for structural applications still poses a rather large challenge, particularly in achieving an industrially viable process. In this context, recent work has proved that complex nanoscale steel structures can be formed by solid reaction at low temperatures. These nanocrystalline bainitic steels present the highest strength ever recorded, unprecedented ductility, fatigue on par with commercial bearing steels and exceptional rolling-sliding wear performances. In this paper, a description of the characteristics and significance of these remarkable structures in the context of the atomic mechanism of transformation is provided.

36 MATERIALS SCIENCE↗

Combined Synchrotron X-ray Diffraction and Digital Image Correlation Technique for Measurement of Austenite Transformation with Strain in TRIP-assisted Steels

The strain-induced, diffusionless shear transformation of retained austenite to martensite during straining of transformation induced plasticity (TRIP) assisted steels increases strain hardening and delays necking and fracture leading to exceptional ductility and strength, which are attractive for automotive applications. A novel technique that provides the retained austenite volume fraction variation with strain in TRIP-assisted steels with improved precision is presented. Digital images of the gauge section of tensile specimens were first recorded up to selected plastic strains with a stereo digital image correlation (DIC) system. The austenite volume fraction was measured by synchrotron X-ray diffraction from small squares cut from the gage section. Strain fields in the squares were then computed by localizing the strain measurement to the corresponding region of a given square during DIC post-processing of the images recorded during tensile testing. Results obtained for a QP980 steel are used to study the influence of initial volume fraction of austenite and the austenite transformation with strain on tensile mechanical behavior.

Atom Probe Analysis↗

Effects of CO 2 and H 2 S on Corrosion of Martensitic Steels in Brines at Low Temperature

Corrosion studies were conducted for martensitic carbon steels in 5 wt% NaCl brine solutions at 4°C and 10 MPa (1,450 psi). These studies simulated different subsurface environments relevant to Arctic drilling. Here, two high-strength martensitic carbon steels, S-135 and UD-165, were studied in three different environments: (1) a CO 2 -NaCl-H 2 O solution with a CO 2 :H 2 O molar ratio of 0.312 in the whole system, (2) an H 2 S-NaCl-H 2 O solution with an H 2 S:H 2 O molar ratio of 3.12 × 10 –4 , and (3) a CO 2 -H 2 S-NaCl-H 2 O solution with the same acid gas to water ratios as environments 1 and 2. Results from the CO 2 +H 2 S mixed environment indicated that sour corrosion mechanism was dominant when the CO 2 :H 2 S molar ratio was 1,000. This impact of a small amount of H 2 S on the corrosion mechanism could be attributed to the specific adsorption of H 2 S on the steel surface. Electrochemical and mass loss measurements showed a distinct drop in the corrosion rate (CR) by more than one order of magnitude when transitioning from sweet to sour corrosion. This inhibiting effect on CR was attributed to the formation of a protective sulfide thin film. Tafel analyses of the anodic reaction showed that the Bockris mechanism was unlikely in the conditions tested. As a result, when comparisons were made between modeled and experimental CRs, good agreement was found in the CO 2 -only and H 2 S-only environments, but not in the CO 2 +H 2 S environment.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Iodine susceptibility of pseudomonads grown attached to stainless steel surfaces

Pseudomonads were adapted to grow in phosphate-buffered water and on stainless steel surfaces to study the iodine sensitivity of attached and planktonic cells. Cultures adapted to low nutrient growth were incubated at room temperature in a circulating reactor system with stainless steel coupons to allow biofilm formation on the metal surfaces. In some experiments, the reactor was partially emptied and refilled with buffer at each sampling time to simulate a "fill-and-draw" water system. Biofilms of attached bacteria, resuspended biofilm bacteria, and reactor suspension, were exposed to 1 mg l-1 iodine for 2 min. Attached bacterial populations which established on coupons within 3 to 5 days displayed a significant increase in resistance to iodine. Increased resistance was also observed for resuspended cells from the biofilm and planktonic bacteria in the system suspension. Generally, intact biofilms and resuspended biofilm cells were most resistant, followed by planktonic bacteria and phosphate buffer cultures. Thus, biofilm formation on stainless steel surfaces within water systems can result in significantly increased disinfection resistance of commonly-occurring water-borne bacteria that may enhance their ability to colonise water treatment and distribution systems.

NASA Program Environmental Health↗

A Five-year Performance Study of Low VOC Coatings over Zinc Thermal Spray for the Protection of Carbon Steel at the Kennedy Space Center

The launch facilities at the Kennedy Space Center (KSC) are located approximately 1000 feet from the Atlantic Ocean where they are exposed to salt deposits, high humidity, high UV degradation, and acidic exhaust from solid rocket boosters. These assets are constructed from carbon steel, which requires a suitable coating to provide long-term protection to reduce corrosion and its associated costs. While currently used coating systems provide excellent corrosion control performance, they are subject to occupational, safety, and environmental regulations at the Federal and State levels that limit their use. Many contain high volatile organic compounds (VOCs), hazardous air pollutants, and other hazardous materials. Hazardous waste from coating operations include vacuum filters, zinc dust, hazardous paint related material, and solid paint. There are also worker safety issues such as exposure to solvents and isocyanates. To address these issues, top-coated thermal spray zinc coating systems were investigated as a promising environmentally friendly corrosion protection for carbon steel in an acidic launch environment. Additional benefits of the combined coating system include a long service life, cathodic protection to the substrate, no volatile contaminants, and high service temperatures. This paper reports the results of a performance based study to evaluate low VOC topcoats (for thermal spray zinc coatings) on carbon steel for use in a space launch environment.

Zinc Thermal Spray↗

Structural Performance Evaluation of Composite-To-Steel Weld Bonded Joint

The Automotive Composites Consortium (ACC), a collaboration of Chrysler, Ford, General Motors, and the US Department of Energy is conducting a focal project to demonstrate the use of composite materials in high volume structural applications such as an underbody capable of carrying crash loads. One of the critical challenges is to attach the composite part to the steel structure in a high-volume automotive manufacturing environment and meet the complex requirements for crash. Weld-bonding, a combination of adhesive bonding and spot welding, was selected as the primary joining method. A novel concept of bonding doubler steel strips to composite enabled the spot welding to the steel structure, ensuring the compability with the OEM assembly processes. The structural performance of the joint, including durability, was assessed via analytical and physical testing under quasi-static loading at various temperatures. This paper discusses the results of the experiments designed to generate key modeling parameters for Finite Element Analysis of the joint.

36 MATERIALS SCIENCE↗

PERFORMANCE OF RC AND FRC WALL PANELS REINFORCED WITH MILD STEEL AND GFRP COMPOSITES IN BLAST EVENTS

The structural integrity of reinforced concrete structures in blast events is important for critical facilities. This paper presents experimental data generated for calibrating detailed finite element models that predict the performance of reinforced concrete wall panels with a wide range of construction details under blast loading. The test specimens were 1.2 m square wall panels constructed using Normal Weight Concrete (NWC) or Fiber Reinforced Concrete (FRC). FRC consists of macro-synthetic fibers dispersed in NWC. Five types of panels were tested: NWC panels with steel bar reinforcement (Type A); FRC panels without additional reinforcement (Type B); FRC panels with steel bar reinforcement (Type C); NWC panels with glass fiber reinforced polymer (GFRP) bar reinforcement (Type D); and NWC panels reinforced with steel bar reinforcement and external bidirectional GFRP overlays on both faces (Type E). An additional three Type C panels were used as control specimens (CON). Each panel type was constructed with three thicknesses: 152 mm, 254 mm, and 356 mm. The panels were instrumented with strain gauges, and accelerometers; in addition, pressure sensors and high speed videos were employed during the blast events. Panel types C and E had the best performance, whereas panel type B did not perform well. Preliminary dynamic simulations show crack patterns similar to the experimental results.

36 MATERIALS SCIENCE↗

Compatibility Assessment of Advanced Stainless Steels in Sodium

Type 316L stainless steel capsules containing commercially pure sodium and miniature tensile specimens of HT-UPS (austenitic, 14Cr-16Ni), NF-616 (ferritic/martensitic, 9Cr-2W-0.5Mo), or 316L (austenitic, 17Cr-10Ni-2Mo) stainless steel were exposed at 600 or 700 C for 100 and 400 h as a screening test for compatibility. Using weight change, tensile testing, and metallographic analysis, HT-UPS and 316L were found to be largely immune to changes resulting from sodium exposure, but NF-616 was found susceptible to substantial decarburization at 700 C. Subsequently, two thermal convection loops (TCLs) constructed of 316L and loaded with commercially pure sodium and miniature tensile specimens of HT-UPS and 316L were operated for 2000 h each one between 500 and 650 C, the other between 565 and 725 C at a flow rate of about 1.5 cm/s. Changes in specimen appearance, weight, and tensile properties were observed to be very minor in all cases, and there was no metallographic evidence of microstructure changes, composition gradients, or mass transfer resulting from prolonged exposure in a TCL. Thus, it appears that HT-UPS and 316L stainless steels are similarly compatible with commercially pure sodium under these exposure conditions.

36 MATERIALS SCIENCE↗

Friction Stir Spot Welding of Advanced High Strength Steels

Experiments are continuing to evaluate the feasibility of friction stir spot welding advanced high-strength steels including, DP780, martensitic hot-stamp boron steel, and TRIP steels. Spot weld lap-shear strengths can exceed those required by industry standards such as AWS D8.1.

AHSS↗

The Prediction of Long-Term Thermal Aging in Cast Austenitic Stainless Steel

Cast austenitic stainless steel (CASS) materials are extensively used for many massive primary coolant system components of light water reactors (LWRs) including coolant piping, valve bodies, pump casings, and piping elbows. Many of these components are operated in complex and persistently damaging environments of elevated temperature, high pressure, corrosive environment, and sometimes radiation for long periods of time. Since a large number of CASS components are installed in every nuclear power plant and replacing such massive components is prohibitively expensive, any significant degradation in mechanical properties that affects structural integrity, cracking resistance in particular, of CASS components will raise a serious concern on the performance of entire power plant. The CASS materials for nuclear components are highly corrosion-resistant Fe-Cr-Ni alloys with 300 series stainless steel compositions and mostly austenite (γ)–ferrite (δ) duplex structures, which result from the casting processes consisting of alloy melting and pouring or injecting liquid metal into a static or spinning mold. Although the commonly used static and centrifugal casting processes enable the fabrication of massive components with proper resistance to environmental attacks, the alloying and microstructural conditions are not highly controllable in actual fabrication, especially in the casting processes of massive components. In the corrosion-resistant Fe-Cr-Ni alloy system, the minor phase (i.e., the δ-ferrite phase) is inevitably formed during the casting process, and is in a non-equilibrium state subject to detrimental changes during exposure to elevated temperature and/or radiation. In general, relatively few critical degradation modes are expected within the current design lifetime of 40 years, given that the CASS components have been processed properly. It has been well known, however, that both the thermal aging and the neutron irradiation can cause degradation of static and impact toughness in the cast stainless steels, and if combined with any flaws formed during the fabrication process or in service, the thermal degradation in CASS components can be a serious concern for the integrity of the power plant. On the integrity of the CASS components during the extended lifetime of 60 years or longer, no conclusive prediction has been possible, primarily because no direct experience with these materials currently exists, and the aging behavior of CASS alloys still remains largely uncertain. The ongoing research for CASS aging, as part of the LWRS Program/Materials Aging and Degradation Pathway, is an integrated research using holistic experimental and modeling means to provide both the scientific understanding on the aging and failure phenomena and the practical models to predict the degree of property degradation.

cast stainless steels↗

Effects of Strain Rate and Temperature on the Mechanical Properties of Medium Manganese Steels

The effects of temperature (-60 to 100 °C) and strain rate (0.002 to 0.2 s-1) on the properties of Al-alloyed 7 and 10 wt-% Mn steels containing 34.8 and 57.3 vol-% austenite respectively were evaluated by tensile tests in isothermal liquid baths. The tensile strengths of both medium Mn steels increased with a decrease in temperature owing to the decreased austenite stability with a decrease in temperature. At lower temperatures the strength of the 10MnAl steel was highest, a consequence of the higher strain hardening rate caused by more austenite transformation to martensite with deformation. The resulting properties are assessed with a consideration of the effects of strain rate and deformation on adiabatic heating which was observed to be as high as 95o C.

36 MATERIALS SCIENCE↗

Effect of radiogenic helium on stainless steel 12Cr18Ni10Ti mechanical properties and hydrogen permeability

Samples of stainless steel 12Cr18Ni10Ti with radiogenic helium were subjected to mechanical tests with a constant extension rate. The presence of {sup 3}He does not markedly affect the strength characteristic, but significantly decreases plasticity of steel. The presence of hydrogen enhances the embrittlement of steel, containing {sup 3}He. The diffusion coefficient of hydrogen does not change significantly in the presence of helium, but the traps for hydrogen, which occur due to the presence of helium, delay the kinetics of a steady state flux onset at helium concentration of 50 appm. (authors)

36 MATERIALS SCIENCE↗

Corrosion Testing of Carbon Steel Exposed to Sludge Heel Chemical Cleaning Solutions - 16109

As efforts continue to treat and dispose of millions of gallons of legacy radioactive materials from the production of nuclear weapons, non-compliant waste storage tanks will gradually be emptied of the bulk waste volume leaving heel materials requiring removal prior to tank closure. The waste heel slurries are distributed on the floor of large, million gallon tanks, which frequently contain numerous obstructions that limit the effectiveness of mechanical removal methods. As a result, chemical cleaning methods are needed for the effective removal of the heels as well as chemical scales that are present on the tank walls and other interior surfaces. Two tank cleaning technologies have already been implemented at the Savannah River Site (SRS): Low Temperature Aluminum Dissolution (LTAD) and Bulk Oxalic Acid Cleaning (BOAC). Recent chemical cleaning efforts on SRS Tank 12 were very successful with regard to bulk sludge heel (especially for Al, Fe, and U phases) and beta/gamma radionuclide removal. Although chemical cleaning using these technologies has been shown to be effective, no disposition path has been identified for oxalate added during BOAC, and insoluble oxalate salts are accumulating within the SRS tank farm and waste processing facilities (evaporators, etc.). Extensive sludge washing is also required to remove moderately soluble sodium oxalate salts prior to sludge vitrification in the SRS Defense Waste Processing Facility (DWPF). As a result, oxalate additions to the tank farm need to be minimized by the use of supplementary acids to assist sludge removal in OA or the use of other cleaning reagents or processing strategies. Previous SRNL testing revealed the importance of pH control for BOAC and recommended the use of a supplementary acid (dilute HNO{sub 3}) with OA to minimize oxalate additions. Primary drivers in SRS Tank Closure Performance Assessments, which evaluate the fate and impact of tank sludge residuals on a geological timescale, are the removal of alpha emitting radionuclides present at low concentrations such as Pu, Am, and Np, which are not highly soluble in currently utilized chemical cleaning reagents. Scoping studies conducted at SRNL revealed promising methods to dissolve the actinides within the HLW tank heels. Oxidation of the actinides with permanganate in either strong caustic (10 M NaOH) or dilute acidic (0.2 M HNO{sub 3}) solutions was shown to result in dissolution of oxy/hydroxide phases of these metals in the absence of major sludge phases. The waste tanks at SRS and Hanford are constructed of carbon steel. Carbon steel corrodes rapidly in most acidic and/or oxidizing environments. Previous electrochemical corrosion testing indicated that the corrosion rates in dilute HNO{sub 3} with OA may result in manageable corrosion rates, over short exposure periods. Additional corrosion testing was performed to provide data for the nitric acid/OA blend as well as the acid/permanganate and caustic permanganate based chemical cleaning solutions. Corrosion rates from the passive coupon tests for the nitric acid/oxalic acid blend were significantly greater than those observed previously with the electrochemical testing. This result may be due to simultaneous electrochemical and chemical dissolution of the steel. The corrosion rate data from the coupon tests in the nitric acid/oxalic acid blend were evaluated to determine the degree of potential structural damage. The corrosion rates, although relatively high, would not be expected to cause damage that would reduce the capacity of the tank primary wall if the process is completed within a month. The corrosivity of sodium permanganate in four proposed cleaning solutions, 1 nitric acid solution and 3 sodium hydroxide solutions, was studied by electrochemical methods at room temperature. The corrosion rates were significantly less aggressive than in the nitric acid/oxalic acid blend corrosion tests. Passive coupon tests needs to be performed in these solutions to ensure that chemical dissolution of the metal is not occurring simultaneously. (authors)

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Interactions of Chemical Contaminants to Steel and Concrete Via Spectroscopic and Computational Methods - 18398

There is limited understanding of the scientific interaction of the chemical contaminants to DOE facility materials which can alter the stability of the materials, and in turn, affecting the general safety. In addition, the materials themselves can be considered secondary waste and decontamination is necessary. Therefore, the overall goal of this project is to determine the physiochemical interactions of Hg and Cs to steel and concrete using spectroscopic, adsorption and computational studies. To achieve the overall goal, this proposal has the following objectives: 1) Evaluate the physicochemical interactions of Hg and Cs to steel and concrete using spectroscopic techniques under standard conditions and 2) Evaluate the impact of environmental conditions (temp., salt content, pH, and time) on the physicochemical interactions of Hg and Cs to steel and concrete using spectroscopic techniques. Less labor intensive than traditional wet chemical analyses, spectroscopic methods have the advantage of elucidating both structural and chemical changes at the micro to nano-scale. The potential impacts of the proposed work could lead to cost effective decontamination methods, minimize secondary waste, and reduce worker exposure. (authors)

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗