Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “SPUTTERING”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 1,261 records · Page 70

Effects of deposition parameters on tantalum films deposited by direct current magnetron sputtering

The structure, composition, and temperature coefficient of resistance of tantalum films were studied as a function of deposition parameters and substrate temperature. As the sputtering power increases from 25 to 100 W, tantalum films deposited at 300 deg. C consisting of the {beta} phase, the preferred-growth orientation changes from (200) to (202) and the temperature coefficient of resistance reduces from -289.79 to -116.65 ppm/ deg. C. The decrease in oxygen and other impurity content in the films was observed when the deposition power was increased. The O/Ta ratio decrease and grain size reduction, which were related to a change in electrical resistivity, were also observed as substrate temperature was varied from 300 to 500 deg. C. These results indicated that the electrical properties were related to the oxygen and other impurity content and grain size in the films rather than to growth orientation. At 650 deg. C, the metastable {beta}-Ta phase was partially transformed into the stable {alpha}-Ta phase which leads to a sharp decrease in the electrical resistivity and a significant change in the microstructure of the tantalum films.

36 MATERIALS SCIENCE↗

Capability of focused Ar ion beam sputtering for combinatorial synthesis of metal films

The authors examined the use of focused Ar ion beam sputtering (FAIS) for combinatorial synthesis. A Langmuir probe revealed that the electron temperature and density for FAIS of metal film deposition was lower than that of other major combinatorial thin film growth techniques such as pulsed laser deposition. Combining FAIS with the combinatorial method allowed the compositional fraction of the Pt-Ru binary alloy to be systematically controlled. Pt-Ru alloy metal film grew epitaxially on ZnO substrates, and crystal structures changed from the Pt phase (cubic structure) to the Ru phase (hexagonal structure) in the Pt-Ru alloy phase diagram. The alloy film has a smooth surface, with the Ru phase, in particular, showing a clear step-and-terrace structure. The combination of FAIS and the combinatorial method has major potential for the fabrication of high quality composition-spread metal film.

36 MATERIALS SCIENCE↗

Pitting corrosion protection of stainless steel by sputter deposited hafnia, alumina, and hafnia-alumina nanolaminate films

316L stainless steel coated with sputter deposited HfO{sub 2}, Al{sub 2}O{sub 3}, and HfO{sub 2}-Al{sub 2}O{sub 3} nanolaminate films were subjected to direct current cyclic potentiodynamic polarization (DCP) in Hanks' balanced salt solution electrolyte. Postexposure morphology was characterized by scanning electron microscopy (SEM) with in situ energy dispersive spectroscopy (EDS). SEM/EDS data show that bare steel and steel coated with single-layer HfO{sub 2} develop pits with perforated covers. These pits become autocatalytic, consistent with an observed positive DCP hysteresis. On the other hand, SEM/EDS data show that steel coated with Al{sub 2}O{sub 3} and HfO{sub 2}-Al{sub 2}O{sub 3} nanolaminate films does not develop autocatalytic pits, consistent with an observed negative DCP hysteresis. However, Al{sub 2}O{sub 3} splinters upon polarization whereas the HfO{sub 2}-Al{sub 2}O{sub 3} nanolaminate remains intact. The areas of worst damage in the nanolaminate correspond to pit cover rupture before autocatalysis, allowing pit and bulk electrolyte to mix and the newly exposed steel surface to repassivate. The films' diverse behavior is discussed in terms of a model for perforated pit growth that requires occlusion until an autocatalytic geometry is established. The authors conclude that the key property a film must have to arrest autocatalytic geometry development is the ability to rupture locally at an early stage of pit growth.

36 MATERIALS SCIENCE↗

Thermal stability and tribological properties of CrZr-Si-N films synthesized by closed field unbalanced magnetron sputtering

In this work, CrZr-Si-N films with various Si contents ({<=}6.4 at. %) were synthesized by closed field unbalanced magnetron sputtering with vertical magnetron sources. The characteristics such as hardness, surface morphology, and friction coefficient of the films as a function of the Si content after annealing up to 500 degree sign C in air were evaluated. Results revealed that the as-deposited films showed very similar characteristics irrespective of the Si content. However, after annealing at 500 degree sign C, the film characteristics showed a strong dependency upon the Si content. After annealing at 500 degree sign C, the hardness of the Cr{sub 39.4}Zr{sub 12.3}N{sub 48.3} film decreased significantly to approximately 24 GPa and the surface roughness value increased approximately 3.5 times more than that of the as-deposited film. The Cr{sub 34.6}Zr{sub 10.6}-Si{sub 6.4}-N{sub 48.4} film, however, was observed to have a hardness of approximately 30 GPa, which is close to that of the as-deposited film, 32 GPa. In addition, as the wear test temperature increased from room temperature to 500 degree sign C, the average friction coefficient of the Cr{sub 39.4}Zr{sub 12.3}N{sub 48.3} film increased significantly from approximately 0.23 to 0.81, but the average friction coefficient of the Cr{sub 34.6}Zr{sub 10.6}-Si{sub 6.4}-N{sub 48.4} film was not changed extensively, measuring approximately 0.43. These results could be attributed to the improvement of the thermal stability by adding Si into the Cr-Zr-N films.

36 MATERIALS SCIENCE↗

Sputter-deposited (Pb,La)(Zr,Ti)O{sub 3} thin films: Effect of substrate and optical properties

Optically transparent (Pb,La)(Zr,Ti)O{sub 3} (PLZT) thin films were sputter-deposited on SrTiO{sub 3}(001) and MgO(001) substrates with a SrRuO{sub 3}(110) bottom electrode. X-ray diffraction analysis showed epitaxial growth of monocrystalline PLZT, with (001) rocking curve full width at half maxima of {approx}0.03 degree sign and {approx}0.3 degree sign for films deposited on SrTiO{sub 3} and MgO, respectively. In-plane epitaxial alignment of the SrRuO{sub 3} and PLZT epilayers was verified from {phi}-scans. It was established from atomic force microscopy measurements that the PLZT surface roughness meets the requirement for optical waveguide applications. Recorded P-E loops for films grown on both substrates showed a remanent polarization of {approx}36 {mu}C/cm{sup 2}. The refractive index of the PLZT layer was estimated from rutile prism coupling measurements at {approx}2.56 for {lambda}=633 nm, consistent with data obtained by spectroscopic ellipsometry. The ferroelectric and optical characteristics of the films, as well as their surface roughness, were not appreciably different for the two substrates. This makes MgO the preferred choice of substrate for optical waveguide devices due to its low refractive index compared to that of SrTiO{sub 3}.

36 MATERIALS SCIENCE↗

Vanadium oxide thin films for bolometric applications deposited by reactive pulsed dc sputtering

Vanadium oxide (VO{sub x}) thin films were deposited by reactive pulse dc magnetron sputtering process using a pure vanadium metal target. The structural, microstructure, and electrical properties were correlated as a function of processing parameters such as substrate temperature, Ar:O partial pressures ratios, and pulsed dc power to fabricate these films. The VO{sub x} films deposited at various substrate temperatures between 30 and 300 degree sign C using a range of oxygen to argon partial pressure ratios exhibited huge variation in their microstructure even though most of them are amorphous to x-ray diffraction technique. In addition, the electrical properties such as temperature coefficient of resistance (TCR), resistivity, and noise levels were influenced by film microstructure. The TCRs of the VO{sub x} films were in the range of -1.1% to -2.4% K{sup -1} having resistivity values of 0.1-100 {Omega} cm. In particular, films grown at lower substrate temperatures with higher oxygen partial pressures have shown finer columnar grain structure and exhibited larger TCR and resistivity.

36 MATERIALS SCIENCE↗

Low temperature grown polycrystalline La{sub 0.7}Sr{sub 0.3}MnO{sub 3} thin films on amorphous SiO{sub 2} substrates by rf magnetron sputtering

The La{sub 0.7}Sr{sub 0.3}MnO{sub 3} thin films have been prepared on amorphous SiO{sub 2} substrates by a rf magnetron sputtering technique under various oxygen flow rates and rf powers at a relatively low substrate temperature of 350 deg. C. The effects of oxygen flow rate and rf power on their physical properties were systematically investigated. X-ray diffraction results show that the growth orientation and crystallinity of the films were affected by rf power and oxygen flow rate. The electrical resistivity of the films was reduced with increasing oxygen flow rate and rf power due to enhanced {l_brace}100{r_brace} growth plane orientation and enlarged grain size of the films. In addition, a relatively high temperature coefficient of resistance value of -2.4% was obtained in the present investigation even with low deposition temperature.

36 MATERIALS SCIENCE↗

Effect of cesium assistance on the electrical and structural properties of indium tin oxide films grown by magnetron sputtering

Indium tin oxide (ITO) thin films were deposited by cesium (Cs)-assisted dc magnetron sputtering in an attempt to achieve a high performance at low temperatures. The films were deposited on SiO{sub 2}/Si wafer and glass (Eagle 2000) substrates at a substrate temperature of 100 degree sign C with a Cs vapor flow during the deposition process. The ITO thin films deposited in the presence of Cs vapor showed better crystallinity than the control films grown under normal Ar/O{sub 2} plasma conditions. The resistivity of the films with the Cs assistance was lower than that of the control films. The lowest resistivity of 6.2x10{sup -4} {Omega} cm, which is {approx}20% lower than that of the control sample, was obtained without any postdeposition thermal annealing. The surface roughness increased slightly when Cs vapor was added. The optical transmittance was >80% at wavelengths ranging from 380 to 700 nm.

36 MATERIALS SCIENCE↗

Structural, electrical, and optical properties of antimony-doped tin oxide films prepared at room temperature by radio frequency magnetron sputtering for transparent electrodes

Antimony-doped tin oxide (ATO) films were prepared on 7059 Corning glass substrate by the radio frequency (rf) magnetron sputtering method using SnO{sub 2} target mixed with Sb of 6 wt % at room temperature. The working pressure was varied from 0.67 to 2 Pa in steps of 0.67 Pa, and the rf power was varied from 100 to 175 W in steps of 25 W at room temperature. The thickness of the deposited ATO films was about 150 nm. X-ray diffraction (XRD) measurements showed the ATO films to be crystallized with a strong (101) preferred orientation as the rf power is increased. The spectra revealed that the deposited films were polycrystalline, retaining the tetragonal structure. The grain size was estimated from the XRD spectra using the Scherrer equation and found to decrease with a decrease in the working pressure and an increase in the rf power, while the surface roughness was observed to be smoothened. The ATO film that was deposited at a working pressure of 0.67 Pa with rf power of 175 W showed the lowest resistivity of 8.6x10{sup -3} {Omega} cm, and the optical transmittance was 86.5% in the visible wavelength range from 400 to 800 nm.

36 MATERIALS SCIENCE↗

Thermal stability of sputter deposited nanomosaic rutile TiO{sub 2}

A domain structure based on the rutile lattice with a large density of (1/2)<011>{l_brace}011{r_brace}-type stacking faults is found in sputter deposited TiO{sub 2} films [J. Vac. Sci. Technol. A 24, 2054 (2006)]. The thermal stability of nanomosaic rutile at moderate temperature is reported here. Films are annealed at 973 K for 0.25-15 h, characterized by x-ray diffraction. A Johnson-Mehl-Avrami-Kolmogorov analysis indicates impeded crystallite growth. A dislocation-locking mechanism is proposed for this behavior. Partial dislocations with (1/2)<011> Burgers vectors that bound the stacking faults glide on intersecting {l_brace}011{r_brace} slip planes and react to produce sessile stair rod dislocations. Without the high temperature required for dislocation climb, (1/2)<011>{l_brace}011{r_brace}-type faults inherent to nanomosaic rutile provide thermal stability against massive crystallite growth.

36 MATERIALS SCIENCE↗

Structure, optical, and magnetic properties of facing-target reactive sputtered Ti{sub 1-x}Fe{sub x}O{sub 2-{delta}} films

Structure, optical, and magnetic properties of the anatase Ti{sub 1-x}Fe{sub x}O{sub 2-{delta}} films fabricated by facing-target reactive sputtering were investigated. Structural analyses indicate that there are no impurity phases in the films and the grain size reaches maximum when Fe content x is 0.017. The optical band gap of the Ti{sub 1-x}Fe{sub x}O{sub 2-{delta}} films decreases with the increasing x. Photoluminescence (PL) spectra show that direct and indirect band-to-band transitions coexist, and the indirect radiative recombination can be regarded as a one photon and two phonon coupling courses. The PL intensity due to oxygen vacancies enhances and the refractive index of the fims increases with the increasing x. The Ti{sub 1-x}Fe{sub x}O{sub 2-{delta}} films exhibit room-temperature ferromagnetism due to the oxygen vacancies.

36 MATERIALS SCIENCE↗

Effect of magnetic field strength on deposition rate and energy flux in a dc magnetron sputtering system

Variations in the magnetic field strongly affect the plasma parameters in a magnetron sputtering system. This in turn affects the throughput as well as the energy flux to the substrate. The variation in the magnetic field in this study, for a dc magnetron process, is achieved by shifting the magnet assembly slightly away from the target. Measurements of the plasma parameters show that while the electron density at the substrate increases with decrease in magnetic field, the electron temperature decreases. The cooling of the electron temperature is consistent with results reported elsewhere. The deposition rate per input magnetron power is found to increase slightly with the decrease in magnetic field for the process conditions considered in this study. Results suggest that the energy flux to the substrate tends to show a general decrease with the shift in the magnet assembly.

36 MATERIALS SCIENCE↗

High power impulse magnetron sputtering using a rotating cylindrical magnetron

Both the industrially favorable deposition technique, high power impulse magnetron sputtering (HIPIMS), and the industrially popular rotating cylindrical magnetron have been successfully combined. A stable operation without arcing, leaks, or other complications for the rotatable magnetron was attained, with current densities around 11 A cm{sup -2}. For Ti and Al, a much higher degree in ionization in the plasma region was observed for the HIPIMS mode compared to the direct current mode.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Coexistence of epitaxial Ta(111) and Ta(110) oriented magnetron sputtered thin film on c-cut sapphire

Epitaxial Ta films were grown on c-cut and r-cut sapphire substrates using magnetron sputtering. X-ray diffraction measurements indicate that the Ta films grown on c-cut sapphire substrates have two different crystal orientations. Low vacuum base pressure produced films with the (111) plane parallel to the basal plane after an initial (110) plane growth phase, whereas high base pressure resulted in the growth of (110) plane parallel to the basal plane with three azimuthally oriented domains coexisting. The superconducting critical temperatures T{sub c} of the films grown on c-cut substrates were found to be slightly higher than those for the films grown on r-cut substrates. The x-ray photoelectron spectroscopic data show oxygen content in the high vacuum base pressure deposited films and a difference in the valance band with different Ta surface planes.

36 MATERIALS SCIENCE↗

Study on MoO{sub 3-x} films deposited by reactive sputtering for organic light-emitting diodes

The authors investigate the role of reduced molybdenum trioxide [MoO{sub 3-x} (x{<=}1)] films in organic light-emitting diodes, particularly from the viewpoint of the oxidation state of Mo. MoO{sub 3-x} films were deposited by reactive sputtering under a mixture of argon (Ar) and oxygen (O{sub 2}). The O{sub 2} gas-flow ratio (GFR) [O{sub 2}/(Ar+O{sub 2})] was adjusted between 10% and 100%. Mo with six, five, and four valence electrons was detected in MoO{sub 3-x} film deposited with an O{sub 2} GFR of 10% and 12.5%, whereas, under higher O{sub 2} GFRs, only six valence electrons for Mo in the MoO{sub 3-x} film were detected. N,N{sup '}-di(1-naphthyl)-N,N{sup '}-diphenylbenzidine ({alpha}-NPD) layer, hole-transport material, were deposited over the MoO{sub 3-x} layer by subsequent vacuum evaporation. At the {alpha}-NPD/MoO{sub 3-x} interface, it was found that {alpha}-NPD cations were generated and that MoO{sub 3-x} was reduced, which provided evidence of charge transfer across the interface by Raman spectroscopy and x-ray photoelectron spectroscopy.

46 INSTRUMENTATION RELATED TO NUCLEAR SCIENCE AND ↗

Spatial resistivity distribution of transparent conducting impurity-doped ZnO thin films deposited on substrates by dc magnetron sputtering

In transparent conducting impurity-doped ZnO thin films prepared by a conventional dc magnetron sputtering deposition (dc-MSD), the key factors in the deposition conditions that are necessary for practical use in transparent electrode applications were investigated. It was found that impurity-doped ZnO targets with a resistivity higher than approximately 3 m{Omega} cm are unsuitable for practical use in the preparation of transparent conducting Al-doped ZnO and Ga-doped ZnO thin films by conventional dc-MSD. Improvements of both the resulting resistivity distribution and resistivity can be sufficiently obtained only by using targets with a resistivity lower than about 0.5 m{Omega} cm. Using a low oxygen content target having a lower resistivity was found to reduce both the amount of oxygen in the chamber and the amount of oxygen reaching the substrate surface. As a result, it was demonstrated that sintered impurity-doped ZnO targets optimized for the preparation of thin films with lower resistivity as well as more uniform resistivity distribution on the substrate surface tended to exhibit a resistivity lower than about 0.5 m{Omega} cm.

36 MATERIALS SCIENCE↗

Morphology of TiN thin films grown on MgO(001) by reactive dc magnetron sputtering

Thin TiN films were grown by reactive dc magnetron sputtering on single-crystalline MgO(001) substrates at a range of temperatures from room temperature to 600 deg. C. Structural characterization was carried out using x-ray diffraction and reflection methods. TiN films grow epitaxially on the MgO substrates at growth temperatures of 200 deg. C and above. The crystal coherence length determined from Laue oscillations and the Scherrer method agrees with x-ray reflection thickness measurements to 6% and within 3% for growth temperatures of 200 and 600 deg. C, respectively. For lower growth temperatures the films are polycrystalline but highly textured and porous.

36 MATERIALS SCIENCE↗

Electrical and optical properties of Nb-doped TiO{sub 2} films deposited by dc magnetron sputtering using slightly reduced Nb-doped TiO{sub 2-x} ceramic targets

Nb-doped anatase TiO{sub 2} films were deposited on unheated glass by dc magnetron sputtering using slightly reduced Nb-doped TiO{sub 2-x} targets (Nb concentration: 3.7 and 9.5 at. %) with various hydrogen or oxygen flow ratios. After postannealing in a vacuum (6x10{sup -4} Pa) at 500 deg. C for 1 h, both films were crystallized into the polycrystalline anatase TiO{sub 2} structure. The resistivity decreased from 1.6x10{sup -3} to 6.3x10{sup -4} {Omega} cm with increasing Nb concentration from 2.8 to 8.0 at. %, where the carrier density increased from 5.4x10{sup 20} to 2.0x10{sup 21} cm{sup -3} and the Hall mobility was almost constant at 5-7 cm{sup 2} V{sup -1} s{sup -1}. The films exhibited a high transparency of over 60%-80% in the visible region.

36 MATERIALS SCIENCE↗