Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “Electron diffraction”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 1,261 records · Page 70

Domain configuration changes under electric field-induced antiferroelectric-ferroelectric phase transitions in NaNbO{sub 3}-based ceramics

We recently developed a feasible crystal chemistry strategy to stabilize the antiferroelectricity in NaNbO{sub 3} through a chemical substitution to decrease the tolerance factor and increase the average electronegativity of the system [Shimizu et al., Dalton Trans. 44, 10763 (2015) and Guo et al., J. Appl. Phys. 117, 214103 (2015)]. Two novel lead-free antiferroelectric (AFE) solid solutions, (1-x)NaNbO{sub 3}-xCaZrO{sub 3} and (1-x)NaNbO{sub 3}-xSrZrO{sub 3}, have been found to exhibit the double polarization hysteresis typical of a reversible AFE ↔ ferroelectric (FE) phase transition. In this study, as demonstrated by (1-x)NaNbO{sub 3}-xCaZrO{sub 3} system, the influence of chemical modification and electrical poling on the AFE/FE phase stability was investigated, primarily focusing on the microstructural and crystallographic evolutions. Together with the macroscopic polarization hysteresis measurements, a well-demonstrated structure-property relationship was presented. It was found that the CaZrO{sub 3} substitution into NaNbO{sub 3} can effectively destabilize the FE Q phase and correspondingly lead to a spontaneous reverting to AFE P phase. In contrast to the reversible AFE ↔ FE phase transition, the domain morphology evolution exhibits irreversible nature with a growing process of the orientational domains after applying electric field. Moreover, a multiple-zone axes electron diffraction map of P and Q phases has been summarized and is believed to be an efficient diagram to determine the AFE/FE nature of the NaNbO{sub 3}-based systems.

36 MATERIALS SCIENCE↗

Interface-structure of the Si/SiC heterojunction grown on 6H-SiC

The Si/SiC heterojunctions were prepared on 6H-SiC (0001) C-face by low-pressure chemical vapour deposition at 850 ∼ 1050 °C. Transmission electron microscopy and selected area electron diffraction were employed to investigate the interface-structure of Si/SiC heterojunctions. The Si/6H-SiC heterostructure of large lattice-mismatch follows domain matching epitaxy mode, which releases most of the lattice-mismatch strain, and the coherent Si epilayers can be grown on 6H-SiC. Si(1-11)/6H-SiC(0001) heterostructure is obtained at 900 °C, and the in-plane orientation relationship of Si/6H-SiC heterostructure is (1–11)[1-1-2]{sub Si}//(0001)[-2110]{sub 6H-SiC}. The Si(1-11)/6H-SiC(0001) interface has the same 4:5 Si-to-SiC matching mode with a residual lattice-mismatch of 0.26% along both the Si[1-1-2] and Si[110] orientations. When the growth temperature increases up to 1000 °C, the 〈220〉 preferential orientation of the Si film appears. SAED patterns at the Si/6H-SiC interface show that the in-plane orientation relationship is (-220)[001]{sub Si}//(0001)[2-1-10]{sub 6H-SiC}. Along Si[110] orientation, the Si-to-SiC matching mode is still 4:5; along the vertical orientation Si[001], the Si-to-SiC mode change to approximate 1:2 and the residual mismatch is 1.84% correspondingly. The number of the atoms in one matching-period decreases with increasing residual lattice-mismatch in domain matching epitaxy and vice versa. The Si film grows epitaxially but with misfit dislocations at the interface between the Si film and the 6H-SiC substrate. And the misfit dislocation density of the Si(1-11)/6H-SiC(0001) and Si(-220)/6H-SiC(0001) obtained by experimental observations is as low as 0.487 × 10{sup 14 }cm{sup −2} and 1.217 × 10{sup 14 }cm{sup −2}, respectively, which is much smaller than the theoretical calculation results.

36 MATERIALS SCIENCE↗

Composition and Structure of Ga{sub 1–} {sub x}Na{sub x}As Nanolayers Produced near the GaAs Surface by Na{sup +} Implantation

The composition and structure of nanodimensional Ga{sub 1–} {sub x}Na{sub x}As phases produced by implantation of Na{sup +} ions into the near-surface area of GaAs have been studied by Auger electron spectroscopy and fast electron diffraction. It has been found that the thickness of the ternary epitaxial layer is 10–12 nm for ion energy E{sub 0} = 20 keV. The composition of the three-layer nanosystems is GaAs–Ga{sub 0.5}Na{sub 0.5}As–GaAs.

77 NANOSCIENCE AND NANOTECHNOLOGY↗

Microscopic Examination of the Silicon Surface Subjected to High-Dose Silver Implantation

Low-energy (E = 30 keV) Ag{sup +} ions have been implanted into single-crystalline Si wafers (c-Si) with an implantation dose varying from 1.25 × 10{sup 15} to 1.5 × 10{sup 17} ions cm{sup –2} and an ion beam current density varying from 2 to 15 μA/cm{sup 2}. The surface morphology of implanted wafers has been examined using scanning electron microscopy, transmission electron microscopy, and atomic force microscopy, and their structure has been studied by means of reflection high-energy electron diffraction and elemental microanalysis. It has been shown that for minimal irradiation doses used in experiments, the surface layer of c-Si experiences amorphization. It has been found that when the implantation dose is in excess of the threshold value (~3.1 × 10{sup 15} ions cm{sup –2}), Ag nanoparticles uniformly distributed over the Si surface arise in the irradiated Si layer. At a dose exceeding 10{sup 17} ions cm{sup –2}, a porous Si structure is observed. In this case, the Ag nanoparticle size distribution becomes bimodal with coarse particles localized at the walls of Si pores.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Suppression of planar defects in the molecular beam epitaxy of GaAs/ErAs/GaAs heterostructures

We present a growth method that overcomes the mismatch in rotational symmetry of ErAs and conventional III-V semiconductors, allowing for epitaxially integrated semimetal/semiconductor heterostructures. Transmission electron microscopy and reflection high-energy electron diffraction reveal defect-free overgrowth of ErAs layers, consisting of >2x the total amount of ErAs that can be embedded with conventional layer-by-layer growth methods. We utilize epitaxial ErAs nanoparticles, overgrown with GaAs, as a seed to grow full films of ErAs. Growth proceeds by diffusion of erbium atoms through the GaAs spacer, which remains registered to the underlying substrate, preventing planar defect formation during subsequent GaAs growth. This growth method is promising for metal/semiconductor heterostructures that serve as embedded Ohmic contacts to epitaxial layers and epitaxially integrated active plasmonic devices.

36 MATERIALS SCIENCE↗

Indium hydroxide to oxide decomposition observed in one nanocrystal during in situ transmission electron microscopy studies

The high-resolution transmission electron microscopy (HR-TEM) is used to study, in situ, spatially resolved decomposition in individual nanocrystals of metal hydroxides and oxyhydroxides. This case study reports on the decomposition of indium hydroxide (c-In(OH){sub 3}) to bixbyite-type indium oxide (c-In{sub 2}O{sub 3}). The electron beam is focused onto a single cube-shaped In(OH){sub 3} crystal of {l_brace}100{r_brace} morphology with ca. 35 nm edge length and a sequence of HR-TEM images was recorded during electron beam irradiation. The frame-by-frame analysis of video sequences allows for the in situ, time-resolved observation of the shape and orientation of the transformed crystals, which in turn enables the evaluation of the kinetics of c-In{sub 2}O{sub 3} crystallization. Supplementary material (video of the transformation) related to this article can be found online at (10.1016/j.jssc.2012.09.022). After irradiation the shape of the parent cube-shaped crystal is preserved, however, its linear dimension (edge) is reduced by the factor 1.20. The corresponding spotted selected area electron diffraction (SAED) pattern representing zone [001] of c-In(OH){sub 3} is transformed to a diffuse strongly textured ring-like pattern of c-In{sub 2}O{sub 3} that indicates the transformed cube is no longer a single crystal but is disintegrated into individual c-In{sub 2}O{sub 3} domains with the size of about 5-10 nm. The induction time of approximately 15 s is estimated from the time-resolved Fourier transforms. The volume fraction of the transformed phase (c-In{sub 2}O{sub 3}), calculated from the shrinkage of the parent c-In(OH){sub 3} crystal in the recorded HR-TEM images, is used as a measure of the kinetics of c-In{sub 2}O{sub 3} crystallization within the framework of Avrami-Erofeev formalism. The Avrami exponent of {approx}3 is characteristic for a reaction mechanism with fast nucleation at the beginning of the reaction and subsequent three-dimensional growth of nuclei with a constant growth rate. The structural transformation path in reconstructive decomposition of c-In(OH){sub 3} to c-In{sub 2}O{sub 3} is discussed in terms of (i) the displacement of hydrogen atoms that lead to breaking the hydrogen bond between OH groups of [In(OH){sub 6}] octahedra and finally to their destabilization and (ii) transformation of the vertices-shared indium-oxygen octahedra in c-In(OH){sub 3} to vertices- and edge-shared octahedra in c-In{sub 2}O{sub 3}. - Graphical abstract: Frame-by-frame analysis of video sequences recorded of HR-TEM images reveals that a single cube-shaped In(OH){sub 3} nanocrystal with {l_brace}100{r_brace} morphology decomposes into bixbyite-type In{sub 2}O{sub 3} domains while being imaged. The mechanism of this decomposition is evaluated through the analysis of the structural relationship between initial (c-In(OH){sub 3}) and transformed (c-In{sub 2}O{sub 3}) phases and though the kinetics of the decomposition followed via the time-resolved shrinkage of the initial crystal of indium hydroxide. Highlights: Black-Right-Pointing-Pointer In-situ time-resolved High Resolution Transmission Electron Microscopy. Black-Right-Pointing-Pointer Crystallographic transformation path. Black-Right-Pointing-Pointer Kinetics of the decomposition in one nanocrystal.

36 MATERIALS SCIENCE↗

Coverage induced structural transformations of tetracene on Ag(110)

Self-assembly of tetracene on an anisotropic surface of Ag(110) has been investigated using scanning tunneling microscopy and low-energy electron diffraction. We observe multistage structural transformations of the self-assembled tetracene on Ag(110) as a function of molecular coverages, which are accompanied by the changes in molecular orientations. They are analyzed by a balance between multiple molecule-molecule and anisotropic substrate-molecule interactions.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Lattice relaxation studies in strained epitaxial Fe-Co-C films

Aiming at high magnetocrystalline anisotropies, small additions of carbon have been proposed to stabilize a tetragonal lattice distortion in Fe-Co. In the present work, the relaxation mechanisms of Fe-Co films containing 2 at. % C are examined in detail. Film growth on buffers with different lattice constants is compared by a combination of in situ reflection high energy electron diffraction and ex-situ X-ray diffraction measurements. It is shown that relaxation starts at a thickness around 2 nm and ends at a distortion of about 4%, which is independent from the chosen buffer. Integral XRD and magnetization measurements suggest that the relaxation occurs over the complete film thickness.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Conformational diversity of 1-phenylpiperidin-4-one in the gas phase

Conformational preferences of substituted, saturated cyclic ketones may deviate from those of their parent analogues. 1-Phenylpiperidin-4-one was found to exist in several forms differing by not only position (axial or equatorial) of the aryl-substituent but also by a configuration of the piperidine cycle itself: chair-Eq, chair-Ax and twist-Tw. Here, the ratios of the co-existing species contributions in gas phase predicted by various quantum chemical calculations were confirmed by synchronous gas-phase electron diffraction and mass spectrometric experiments carried out for the vapor at 337 K demonstrating a best fit with the B3LYP-D3/cc-pVTZ combination: Eq:Ax:Tw=55(13):22(9):23(10) vs. 40:35:25.

1-phenylpiperidin-4-one↗

Sharp chemical interface in epitaxial Fe{sub 3}O{sub 4} thin films

Chemically sharp interface was obtained on single phase single oriented Fe{sub 3}O{sub 4} (001) thin film (7 nm) grown on NiO (001) substrate using oxygen assisted molecular beam epitaxy. Refinement of the atomic structure, stoichiometry, and oxygen vacancies were determined by soft and hard x-ray photoelectron spectroscopy, low energy electron diffraction and synchrotron based X-ray reflectivity, and X-ray diffraction. Our results demonstrate an epitaxial growth of the magnetite layer, perfect iron stoichiometry, absence of oxygen vacancies, and the existence of an intermixing free interface. Consistent magnetic and electrical characterizations are also shown.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Properties of single crystal Fe{sub 1-x}Ga{sub x} thin films

Molecular beam epitaxy was used to deposit single crystal thin film Fe{sub 1-x}Ga{sub x} samples on ZnSe buffer layers grown on (001) and (110) single crystal GaAs substrates. The crystal quality of the GaAs surface and each deposited layer was monitored in situ by reflection high energy electron diffraction. The magnetic properties of the samples were characterized by vibrating sample magnetometry and ferromagnetic resonance (FMR). The FMR linewidth increases dramatically with Ga concentration while the cubic anisotropy term K{sub 1} switches sign.

36 MATERIALS SCIENCE↗

Implantation conditions for diamond nanocrystal formation in amorphous silica

We present a study of carbon ion implantation in amorphous silica, which, followed by annealing in a hydrogen-rich environment, leads to preferential formation of carbon nanocrystals with cubic diamond (c-diamond), face-centered cubic (n-diamond), or simple cubic (i-carbon) carbon crystal lattices. Two different annealing treatments were used: furnace annealing for 1 h and rapid thermal annealing for a brief period, which enables monitoring of early nucleation events. The influence of implanted dose and annealing type on carbon and hydrogen concentrations, clustering, and bonding were investigated. Rutherford backscattering, elastic recoil detection analysis, infrared spectroscopy, transmission electron microscopy, selected area electron diffraction, ultraviolet-visible absorption measurements, and Raman spectroscopy were used to study these carbon formations. These results, combined with the results of previous investigations on similar systems, show that preferential formation of different carbon phases (diamond, n-diamond, or i-carbon) depends on implantation energy, implantation dose, and annealing conditions. Diamond nanocrystals formed at a relatively low carbon volume density are achieved by deeper implantation and/or lower implanted dose. Higher volume densities led to n-diamond and finally to i-carbon crystal formation. This observed behavior is related to damage sites induced by implantation. The optical properties of different carbon nanocrystal phases were significantly different.

36 MATERIALS SCIENCE↗

Energy-loss magnetic chiral dichroism study of epitaxial MnAs film on GaAs(001)

The room-temperature ferromagnetic behavior of MnAs/GaAs(001) thin film has been locally explored by Transmission Electron Microscope (TEM). We first differentiated hexagonal α-MnAs and quasi-hexagonal β-MnAs which are very similar in atomic structure by electron diffraction. Local magnetic moment information of the identified α-MnAs was extracted from manganese-L{sub 2,3} edges using Energy-loss Magnetic Circular Dichroism technique and the ratio of orbital to spin magnetic moment was measured. In this experiment, atomic structure identification, chemical analysis, and magnetic moment measurement were simultaneously achieved at high spatial resolution in TEM, thus providing a potential method for in-situ study of local properties of multiphase magnetic materials.

71 CLASSICAL AND QUANTUM MECHANICS, GENERAL PHYSIC↗

Growth of high-quality SrTiO{sub 3} films using a hybrid molecular beam epitaxy approach

A hybrid molecular beam epitaxy approach for atomic-layer controlled growth of high-quality SrTiO{sub 3} films with scalable growth rates was developed. The approach uses an effusion cell for Sr, a plasma source for oxygen, and a metal-organic source (titanium tetra isopropoxide) for Ti. SrTiO{sub 3} films were investigated as a function of cation flux ratio on (001) SrTiO{sub 3} and (LaAlO{sub 3}){sub 0.3}(Sr{sub 2}AlTaO{sub 6}){sub 0.7} (LSAT) substrates. Growth conditions for stoichiometric insulating films were identified. Persistent (>180 oscillations) reflection high-energy electron diffraction oscillation characteristic of layer-by-layer growth were observed. The full widths at half maximum of x-ray diffraction rocking curves were similar to those of the substrates, i.e., 34 arc sec on LSAT. The film surfaces were nearly ideal with root mean square surface roughness values of less than 0.1 nm. The relationship between surface reconstructions, growth modes, and stoichiometry is discussed.

36 MATERIALS SCIENCE↗

Microstructural evolution of P92 ferritic/martensitic steel under argon ion irradiation

Microstructural evolution of P92 ferritic/martensitic steel irradiated by Ar{sup +} ion beams at doses from 0.6 to 230 displacements per atom (dpa) at room temperature was investigated with conventional transmission electron microscope technique. Selected-area electron diffraction combined with bright-field and dark-field contrast image indicated that carbide/matrix interfaces were more easily damaged. The carbide peripheries became partly amorphous at irradiation dose of 2.3 dpa and were almost complete amorphous at the dose of 11.5 dpa. The small carbides would re-precipitate in matrices at 34.5 dpa. Energy dispersive X-ray analysis revealed that segregation of Cr and W and depletion of Fe in carbides occurred under irradiation. With the irradiation dose increasing, the irradiation induced segregation and depletion became more severe, which would influence mechanical properties of the steel. - Research Highlights: {yields} Carbide/matrix interfaces in P92 ferritic/martensitic steel were easily damaged. {yields} Small carbides re-precipitated in matrices after higher dose irradiation. {yields} Segregation of Cr and W and depletion of Fe in carbides occurred after irradiation.

36 MATERIALS SCIENCE↗

Nanostructural and electronic properties of polytypes in InN nanocolumns

Transmission electron microscopy techniques and density functional theory calculations were employed to investigate the nanostructural and electronic properties of InN polytypes observed in InN nanocolumns, grown on Si(111) by molecular beam epitaxy. Moiré fringes and alternating hexagonal and cubic lattice stacking sequences along the c-axis, observed among the wurtzite layers, implied the presence of different structures embedded in the basic 2H structure of the nanocolumns. Quantitative electron diffraction analysis and high-resolution image simulations verified the coexistence of the wurtzite structure with the 4H, 6H, and the 3C zinc-blende structural polytypes. Total energies calculations established the 2H wurtzite structure as the most stable polytype. The band gap of all polytypes was found direct with the energies and the band gaps of the 4H (E{sub g} = 0.64 eV) and 6H (E{sub g} = 0.60 eV) structures calculated between the corresponding values of the 2H (E{sub g} = 0.75 eV) and 3C (E{sub g} = 0.49 eV) basic structures. Theoretical and experimental analysis showed that at the initial stages of growth InN nanocolumns were under tensile strain along both the basal plane and growth direction. Structural polytypes were then introduced in the form of embedded inclusions to accommodate the excess tensile strain along the growth direction, allowing the entire process of polymorphism to be the dominant strain relaxation mechanism of InN nanocolumns. Moreover, the lattice and energetic properties and band gap values of InN polytypes showed a linear dependence on hexagonality, while the presence of polytypes led to a characteristic broadening of the photoluminescence emission peak toward lower emission energies.

36 MATERIALS SCIENCE↗

Microstructure evolution in TRIP-aided seamless steel tube during T-shape hydroforming process

Transformation-induced plasticity aided seamless steel tube comprising of ferrite, bainite, and metastable austenite was processed through forging, piercing, cold-drawing, and two-stage heat treatment. T-shape hydroforming is a classic forming method for experimental research and practical production. The current work studied austenite-to-martensite transformation and microcrack initiation and propagation of the tube during T-shape hydroforming using electron backscattering diffraction, scanning electron microscopy, and transmission electron microscopy. The strain distribution in the bcc-phase and fcc-phase was studied by evaluating changes in the average local misorientation. Compared to the compressive stress, metastable austenite with similar strain surrounding or inside the grains transformed easier under tensile loading conditions. The inclusions were responsible for microcrack initiation. The propagation of the cracks is hindered by martensite/austenite constituent due to transformation induced plasticity effect. The volume fraction of untransformed retained austenite decreased with increase in strain implying transformation-induced plasticity effect. - Highlights: • Hydroformed tubes processed via TRIP concept • EBSD provided estimate of micro local strain. • Retained austenite hinders propagation of microcracks.

36 MATERIALS SCIENCE↗

The Effect of the Ion Assistance Energy on the Electrical Resistivity of Carbon Films Prepared by Pulsed Plasma Deposition in a Nitrogen Atmosphere

Thin carbon films prepared by pulsed plasma ion-assisted deposition of graphite in an atmosphere of a mixture of argon and nitrogen are studied. The results of characteristic electron energy loss spectroscopy and electron diffraction indicate the increase in the graphite component with increasing ion assistance energy. The use of ion assistance during the film deposition makes it possible to control their resistivity by changing it from 10{sup 5} to 10{sup 2} Ω cm.