Subcritical crack growth in two titanium alloys.

Measurement of subcritical crack growth during static loading of precracked titanium alloys in salt water using samples too thin for plane strain loading to predominate was examined as a method for determining the critical stress intensity for crack propagation in salt water. Significant internal crack growth followed by arrest was found at quite low stress intensities, but crack growth rates were relatively low. Assuming these techniques provided a reliable measurement of the critical stress intensity, the value for annealed Ti-4Al-1.5Mo-0.5V alloy was apparently about 35 ksi-in. to the 1/2 power, while that for annealed Ti-4Al-3Mo-1V was below 45 ksi-in. to the 1/2 power. Crack growth was also observed in tests conducted in both alloys in an air environment. At 65 ksi-in. to the 1/2 power, the extent of crack growth was greater in air than in salt water. Ti-4Al-3Mo-1V showed arrested crack growth in air at a stress intensity of 45 ksi-in. to the 1/2 power.

Williams, D. N.↗

Titanium-alloy, metallic-fluid heat pipes for space service

Reactivities of titanium limit its long-term terrestrial use for unprotected heat-pipe envelopes to about 870 K (1100 F). But this external thermochemical limitation disappears when considerations shift to space applications. In such hard-vacuum utilization much higher operating temperatures are possible. Primary restrictions in space environment result from vaporization, thermal creep, and internal compatibilities. Unfortunately, a respected head-pipe reference indicates that titanium is compatible only with cesium from the alkali-metal working-fluid family. This problem and others are subjects of the present paper which advocates titanium-alloy, metallic-fluid heat pipes for long-lived, weight-effective space service between 500 and 1300 K (440 and 1880 F).

Morris, J. F.↗

Electroplating on titanium alloy

Activation process forms adherent electrodeposits of copper, nickel, and chromium on titanium alloy. Good adhesion of electroplated deposits is obtained by using acetic-hydrofluoric acid anodic activation process.

Lowery, J. R.↗

Nickel-Titanium Alloys: Corrosion "Proof" Alloys for Space Bearing, Components and Mechanism Applications

An intermetallic nickel-titanium alloy, 60NiTi (60 wt% Ni, 40 wt% Ti), is shown to be a promising candidate tribological material for space mechanisms. 60NiTi offers a broad combination of physical properties that make it unique among bearing materials. 60NiTi is hard, electrically conductive, highly corrosion resistant, readily machined prior to final heat treatment, and is non-magnetic. Despite its high Ti content, 60NiTi is non-galling even under dry sliding. No other bearing alloy, metallic or ceramic, encompasses all of these attributes. Since 60NiTi contains such a high proportion of Ti and possesses many metallic properties, it was expected to exhibit poor tribological performance typical of Ti alloys, namely galling type behavior and rapid lubricant degradation. In this poster-paper, the oil-lubricated behavior of 60NiTi is presented.

DellaCorte, Christopher↗