Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “sinter”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 127 records · Page 7

On the Arrhenius-like behavior of conductivity during flash sintering of 3 mol% yttria stabilized zirconia ceramics

Here, we discuss the Arrhenius behavior of electrical conductivity σ during flash sintering of 3 mol% yttria stabilized zirconia (3YSZ). In situ x-ray diffraction is used to determine sample temperature. Sintering contribution to σ is excluded by investigating the flash event on a dense ceramic. We show that total conductivity follows an Arrhenius-like equation in both dense and green samples, even during Stage II of flash. The non-linearity often verified during flash sintering of 3YSZ is therefore related to the furnace temperature instead of the sample temperature when building the ln(σ) vs. 1/T plots. Furthermore, we verified a change in the activation energy for conduction prior to the ignition of the flash event and discussed the possible mechanisms. For instance, the decrease in activation energy from Stage I to II in the dense sample is attributed to a contribution from electronic carriers.

36 MATERIALS SCIENCE↗

Ultrafast Reactive Laser Sintering of Highly Conductive Garnet-Type LLZTO Solid Electrolytes

Rapid and scalable fabrication of garnet-type solid electrolytes remains a major challenge for the practical deployment of lithium metal batteries. Here, we report reactive laser sintering (RLS) as an ultrafast and potentially scalable strategy for fabricating garnet-type Li 6.4 La 3 Zr 1.4 Ta 0.6 O 12 (LLZTO) solid electrolytes. RLS of LLZTO enables simultaneous reaction and densification, achieving ∼95% relative density while minimizing lithium loss and suppressing secondary phase formation. Compared to conventional furnace sintering, RLS promotes enhanced grain growth and improved densification, leading to improved ionic conductivity (0.36 ± 0.08 mS cm −1 ) while maintaining comparable activation energies for Li + transport. Structural characterization by X-ray diffraction (XRD), Raman spectroscopy, and solid-state 6 Li/ 7 Li NMR confirms the formation of cubic garnet LLZTO with homogeneous microscale elemental distribution. In addition, nanoindentation measurements demonstrate that RLS preserves the mechanical properties of the garnet framework despite ultrafast localized thermal processing. By integrating simultaneous reaction and densification with tunable microstructural control, reactive laser sintering provides a promising manufacturing pathway for high-performance garnet solid electrolytes toward next-generation solid-state batteries.

CO2 laser↗

Surface Self-Diffusion Induced Sintering of Nanoparticles

Despite the critical role of sintering phenomena in constraining the long-term durability of nanosized particles, a clear understanding of nanoparticle sintering has remained elusive due to the challenges in atomically tracking the neck initiation and discerning different mechanisms. Through the integration of in situ transmission electron microscopy and atomistic modeling, this study uncovers the atomic dynamics governing the neck initiation of Pt–Fe nanoparticles via a surface self-diffusion process, allowing for coalescence without significant particle movement. Real-time imaging reveals that thermally activated surface morphology changes in individual nanoparticles induce significant surface self-diffusion. Further, the kinetic entrapment of self-diffusing atoms in the gaps between closely spaced nanoparticles leads to the nucleation and growth of atomic layers for neck formation. This surface self-diffusion-driven sintering process is activated at a relatively lower temperature compared to the classic Ostwald ripening and particle migration and coalescence processes. The fundamental insights have practical implications for manipulating the morphology, size distribution, and stability of nanostructures by leveraging surface self-diffusion processes.

36 MATERIALS SCIENCE↗

Reliability Analysis of Large-Area, Low Pressure-Assisted Silver Sintering for Medium-Voltage Power Modules

Multi-layer insulating ceramic substrates can enable medium-voltage (MV) power modules with reduced peak electric field. This benefit is particularly important for MV silicon carbide (SiC) MOSFETs due to their higher operating voltages. Large-area, low-pressure assisted silver sintering is a potential solution for bonding substrates to create a multi-layer structure. The voiding content and defect density of the bond used to create the multi-layer substrate stack-up is critical to the reliability of the power module and the thermal performance, as this bond is in the primary path for heat dissipation in the power module structure. Here, samples of two-layer direct bonded aluminum (DBA) stacks have been fabricated and subjected to thermal cycling to analyze their reliability. Passive thermal cycling from -40 degrees C to 200 degrees C was performed. Cross-sections were cut at pre-determined intervals and imaged with Scanning Electron Microscopy (SEM). After 1000 thermal cycles, adhesive failures are observed between the sintered silver and the DBA surface. Cross-sections were cut and imaged via optical microscope and SEM. Thermal analyzer measurements are recorded on a 10-kV SiC power module utilizing the sintered DBA substrate stacks.

30 DIRECT ENERGY CONVERSION↗

Pressureless sintering of dual-phase, high-entropy boride–carbide ceramics

Here, dual-phase, high-entropy boride–carbide ceramics were densified by pressureless sintering. Relative densities up to approximately 96% were obtained for ceramics containing about 30 vol% high-entropy boride and 70 vol% high-entropy carbide. Isostatic pressing at 200 MPa resulted in higher relative densities of both the green bodies and final ceramics compared to uniaxial pressing. The highest relative density of 96.3% was achieved for a ceramic that was isostatically pressed at 200 MPa and sintered at 2300°C for 2 h. Grain sizes of the resulting ceramics were approximately 2 µm. This is the first report of pressureless sintering of dual-phase, high-entropy boride–carbide ceramics.

36 MATERIALS SCIENCE↗

Sintering Characteristics of Multilayered Thermal Barrier Coatings Under Thermal Gradient and Isothermal High Temperature Annealing Conditions

Pyrochlore oxides have most of the relevant attributes for use as next generation thermal barrier coatings such as phase stability, low sintering kinetics and low thermal conductivity. One of the issues with the pyrochlore oxides is their lower toughness and therefore higher erosion rate compared to the current state-of-the-art TBC material, yttria (6 to 8 wt%) stabilized zirconia (YSZ). In this work, sintering characteristics were investigated for novel multilayered coating consisted of alternating layers of pyrochlore oxide viz Gd2Zr2O7 and t' low k (rare earth oxide doped YSZ). Thermal gradient and isothermal high temperature (1316 C) annealing conditions were used to investigate sintering and cracking in these coatings. The results are then compared with that of relevant monolayered coatings and a baseline YSZ coating.

Thermal Barrier Coatings↗

Vacuum Sintering of Highland Simulant CSM-LHT-1G

Sintering of lunar regolith is a process of interest to consolidate the ubiquitous granular material in durable structures on the lunar surface such as platforms, landing/launch pads, roads, and foundations for long-term robotic and human activities. Many publications do not report quantitative assessment of the effects of processing conditions on the strength properties of the sintered products. The work presented is an investigation into such effects on a carefully selected simulant, CSM-LHT-1G prepared for high temperature processing to eliminate undesired components that would not be present from lunar materials. Careful experiments under vacuum were conducted to identify the relevant factors that dominate the properties and the quality of the sintered product. CSM-LHT-1G simulant is a variant of the CSM-LHT-1 lunar highland simulant produced by Colorado School of Mines. The original mineralogical composition of CSM-LHT-1 (70 wt.% Greenspar, 30 wt.% Merriam Crater basalt) was modified to obtain a 30 wt.% glass content with the addition of NU-LHT-5M glass balanced with pyroxene (augite) to yield CSM-LHT-1G.

Vacuum Sintering↗

Effects of Post-sintering Annealing on (NdLa)-(FeCo)-B Magnets

A common limitation of La substitutions into (Nd, La) 2 Fe 14 B magnets is the reduction of the anisotropy field (H a ), which decreases magnet coercivity (H cj ). In this study, adding a small amount of Pr-Cu to a La-containing neo magnet may modify the grain boundary (GB), which can help recover a fraction of the degraded H cj . An optimal GB modification requires a carefully designed post-sinter heat treatment, which is the focus of this work on characterizing the effects of multi-step post-sintering annealing on the evolutions of microstructure and magnetic properties. We find that Nd and Cu concentrations at GBs and triple junctions (TJs) increase when the annealing temperatures are lowered. Annealing temperatures of 580°C and 480°C (near rare-earth-rich eutectic temperatures) enabled the development of a thick and continuous GB phase, which helps to magnetically decouple the grains, and, thus, enhance H cj . For the alloy with 25% Nd replaced by La, and with the addition of 7.5 wt.% of Pr 68 Cu 32 as GB modifier, the optimized multi-step post-sinter annealing improved the H cj from 4.8 kOe to 9 kOe.

36 MATERIALS SCIENCE↗

Review of Solid State Consolidation Processing Techniques of ODS Steels (Hot Extrusion, Hot Isostatic Pressing, Spark Plasma Sintering, and Stir Friction Consolidation): Resulting Microstructures and Mechanical Properties

This paper reviews the solid-state consolidation processing techniques for Oxide Dispersion Strengthened steels and compares them in terms of the resulting microstructure and reported mechanical properties. Synthesis techniques include hot extrusion, hot isostatic pressing, spark plasma sintering and friction consolidation. The effects of process parameters on the resulting microstructures and performance are discussed for each technique. Average oxide size, average grain size, and porosity are compared across techniques, as well as mechanical strength and ductility. Across consolidation techniques where temperature can be controlled, a low sintering temperature with a high sintering pressure is favorable for keeping oxide sizes, grain sizes, and porosity low. The use of yttrium and titanium for oxide formation has been evidenced to reduce oxide sizes, and tungsten additions have been shown to improve strength. Current literature suggests that the more mature hot extrusion technique produces stronger steel with consistently fine oxides, while other alternative solid-state consolidation, while promising, offer margin for improvement.

36 MATERIALS SCIENCE↗

Combined DSC/TGA Analysis to Rationalize the As-Sintered Microstructure in Binder Jet Additively Manufactured H13 Tool Steel

In this study, a combined DSC/TGA analysis has been used to rationalize the constant liquid channel width at higher sintering temperatures in H13 tool steel manufactured by binder jet additive manufacturing. Using enthalpy conservation along with coupled DSC + TGA analysis, the phase fractions of liquid and austenite phases during heating and cooling respectively were estimated. The estimates from the DSC/TGA analysis were compared with equilibrium phase fraction predictions from ThermoCalc. The resulting phase evolution was correlated to the as-sintered microstructure to rationalize the unexpected lack of change in liquid channel width at higher sintering temperatures.

Kannan, Rangasayee↗

Perovskite evolution on La modified Mn 1.5 Co 1.5 O 4 spinel through thermal ageing with enhanced oxidation activity: Is sintering always an issue?

Non-precious metal oxides have great potential in catalytic deep oxidation of emitted hydrocarbons to help address various environmental pollution concerns. However, sintering issue is a stumbling block in practical application upon long-term high-temperature operation or thermal shock experience. Herein, La was applied to modify Mn 1.5 Co 1.5 O 4 spinel to get a highly active oxidation catalyst with exceptional stability against high-temperature thermal ageing treatment. With thermal ageing at 750 °C for 100 h, the La modified Mn–Co composite reached 90 % conversion in toluene oxidation at 265 °C under the high WHSV of 120,000 mL g -1 h -1 , while this value increased to 312 °C over blank Mn–Co spinel. The addition of La not only inhibited the growth of spinel nanocrystals, but also brought about perovskite formation through sintering, generating perovskite-spinel interfaces, thus enhancing both activity and stability. Meanwhile, the La modified Mn–Co spinel exhibited superior performance in presence of water or sulfur dioxide after thermal ageing treatment. In conclusion, this work offers a versatile strategy to design anti-sintering and active oxidation nanocatalysts based on non-precious metal oxides for industrial applications.

36 MATERIALS SCIENCE↗

Investigation of UO 2 doped with Fe 2 O 3 sintered under a reducing atmosphere

Nuclear fuel produced with trace amounts of transition metal additives is of potential interest for introducing intentional signatures for accelerating nuclear forensics. In this work, we investigate the effects on microstructure, grain size, crystal structure, and stoichiometry when trace amounts of Fe in the form of Fe 2 O 3 are added to UO 2 . Sintering of compacts with different concentrations, from 250 to 3000 ppmw, was performed under a reducing atmosphere at 1773 K. The persistence of the taggant during the fuel fabrication process as well as its impact on grain size, crystal lattice, and first-neighbor chemistry was evaluated using inductively coupled plasma–optical emission spectroscopy, powder X-ray diffraction (pXRD), Raman spectroscopy, scanning electron microscopy–backscatter electron spectroscopy, energy dispersive spectroscopy, and thermogravimetric analysis. We observed that a negligible amount of Fe was lost during sintering. Our results indicate that the feedstock, Fe 2 O 3 transforms into Fe and FeO under the test sintering conditions. For all compositions, metallic Fe precipitate was found in grain boundaries as a secondary phase. In conclusion, the potential incorporation of ionic Fe into the UO 2 unit cell was determined by pXRD and Raman spectra.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Rheology improvement for silicon nitride and resin slurries for vat photopolymerization printing and sintering

This work presents the formulation, rheological characterization, and sintering of silicon nitride (Si₃N₄) slurries for vat photopolymerization (VPP) using digital light processing (DLP). Bimodal Si₃N₄ powder was dispersed into commercial photopolymer resin using two different dispersants with opposing effects on surface charge, resulting in varied slurry stability and flow behavior. Slurries were engineered to exhibit shear-thinning behavior suitable for VPP, and their flow properties were quantified using a power-law fluid model. The formulations achieved cure depths of approximately 40 µm and enabled printing of green bodies. Post-processing included thermal debinding and liquid-phase sintering, yielding primarily β-Si₃N₄ with a minor Y-Si-Al-O-N glass phase. The sintered parts reached ~85% of theoretical density and demonstrated a flexural strength of ~330 MPa. Microstructural analysis revealed closed porosity along with some defects related to powder agglomeration and interlayer adhesion. These findings provide insights into slurry formulation strategies for additive manufacturing of high-performance non-oxide ceramics.

Aerospace engineering↗

Onset of selective laser flash sintering of AlN

Abstract Flash sintering uses a combination of heating and electric fields to rapidly densify ceramics. Previously, it has been shown that a scanning laser can be used to initiate flash sintering in localized regions on an yttria‐stabilized zirconia (YSZ) sample in a process known as selective laser flash sintering (SLFS). In this work, we show using a combination of measurements of electric current flowing through the sample and observations of necks formed between powder particles that aluminum nitride (AlN) can also undergo SLFS. Scan conditions required to initiate SLFS are characterized over a range of laser powers and laser scan speeds in a dry nitrogen environment. It is shown that initiation of SLFS in AlN is governed by both the local input energy density per scan and heat dissipation and a numerical model is developed to predict temperatures during SLFS. Assuming the minimum temperature along the conductive path determines the onset of SLFS, the minimum temperature and time required is 450–670 K in 2–0.25 s for the pressed AlN pellets used in this study for laser scan speeds of 33–300 m/s, laser powers of 10–30 W, and an applied electric field of 3000 V/cm.

Gouws, Andre↗

Embedding of Optical Fibers with Electric Field Assisted Sintering

The Electric Field Assisted Sintering (EFAS) technique was used for embedding the fibers, involving rapid heating via an electric current and pressure, reducing fiber exposure to high temperatures. Stainless steel guide tubes were inserted at the fiber-matrix junctions to prevent fiber breakage during the sintering process. The study varied key EFAS parameters—temperature (800°C to 980°C), pressure (40-50 MPa), and hold time (5-10 minutes)—to assess how they influenced fiber embedding. After embedding, the fibers were inspected using optical frequency domain reflectometry (OFDR) to evaluate optical losses and strain along the fiber length. The OFDR scans confirmed that the fibers remained intact, and subsequent transmission tests demonstrated no macroscopic fractures. The embedded samples were also analyzed using scanning electron microscopy (SEM) and X-ray computed tomography (CT) scans. These tests confirmed good bonding between the fiber and matrix with no cracking, though some porosity was present in samples fabricated at lower temperatures. At higher temperatures (980°C), the fiber-matrix bonding was continuous and defect-free, with metal coatings aiding in the bonding process. Elemental analysis showed interdiffusion between the fiber coatings and matrix materials, particularly between the gold coating and stainless steel. Helium leak tests revealed that lower sintering temperatures resulted in matrix porosity, causing leaks, but samples fabricated at 980°C were leak-tight.

46 - INSTRUMENTATION RELATED TO NUCLEAR SCIENCE AN↗

Activated sintering of ThO2 and ThO2-Y2O3 with NiO.

Scanning electron microscopy and isothermal shrinkage measurements were used to study the effects of additives on the sintering of Thoria-Yttria compacts and loose powders. Small amounts of the oxides of Ni, Zn, Co, and Cu were found to reduce the sintering temperature (which is normally above 2000 C). In particular, NiO, at a concentration of 0.8 wt %, was found to yield high-density bodies at temperatures below 1500 C. Densification occurs very rapidly, and is followed by a much slower sintering process typical of volume diffusion.

Halbfinger, G. P.↗

Sintering and hot pressing of Fra Mauro composition glass and the lithification of lunar breccias.

It is proposed that Apollo 14 type breccias lithify by sintering of particles of matrix glass under stress-free conditions. Meteorite impacts generate the heat necessary for sintering. Compacted angular particles of glass with the composition of an Apollo 14 rock were sintered experimentally. Loose clods of sub 37 micron grains form in several days at 700 C. Synthetic rocks, which texturally resemble the breccias, were produced at 795 C and above in 7.5 hours. Glass devitrified with increasing temperature. At 850 C, devitrification prevents much further densification of the synthetic breccias after 2 hours. Experiments compressing glass at 500 bars at 600 C produced dense vitreous masses which did not resemble lunar breccias. Confining pressure does not play a major role in lithifying the breccias. It is concluded that Apollo 14 type lunar breccias form at shallow depths at 800 C+ in a period of minutes to days.

Simonds, C. H.↗