Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “polymer characterization”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 127 records · Page 7

Emerging polyheterocyclic films, coatings and resins - Thermoplastic polyquinolines

The processing and performance characteristics of a soluble, thermoplastic polyquinoline suggest its utility in a variety of high performance applications. The polymer is characterized by excellent thermal and oxidative stability, very low moisture absorption, good mechanical properties, very low dielectric constant, and an unusually low thermal expansion coefficient. This polymer, designated PQ-100 (TM), can be cast into strong, transparent, free standing films from common solvents. Coatings of variable thickness can be spin-coated on to silicon and other surfaces. After processing into films, PQ-100 (TM) can be rendered insoluble in a wide range of solvents using a proprietary process. The low CTE contributes to very low residual stress when the polymer is spin-coated onto silicon wafers. PQ-100 (TM) is currently under evaluation for use as an interlayer dielectric substrate in high-density interconnect applications, including multichip modules. Many of the characteristics of the polymer also suggest its utility as a high-performance film and as a matrix resin for specialty composite applications.

Hendricks, Neil H.↗

Biodegradable High-Molecular-Weight Poly(pentylene adipate- co -terephthalate): Synthesis, Thermo-Mechanical Properties, Microstructures, and Biodegradation

Poly(pentylene adipate-co-terephthalate) (PPAT) is a promising biobased and biodegradable polymer that can replace polyethylene in flexible packaging films where biodegradability is desired. High-molecular-weight (100K–145 KDa) aliphatic–aromatic polyester PPAT was successfully synthesized, and the effects of reaction conditions on molecular weight were reported. PPAT polyesters were characterized for polymer compositions, number-average unit length, thermal transitions, and rheological properties. PPAT compression-molded films were characterized for crystallinity and tensile properties to correlate micro- and macroproperties. PPAT compression-molded films exhibited up to a 76% higher tensile modulus than compression-molded films from poly(butylene adipate-co-terephthalate) (PBAT), making PPAT films potentially comparable with compression-molded films from linear low-density polyethylene (LLDPE). Finally, PPAT is biodegradable in soil and freshwater environments with estimated 90% biodegradation times of 504–580 and 604–845 days, respectively, while PBAT takes 971 days in soil and 395 days in freshwater.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Novel Ordered Crown Ether-Containing Polyimides for Ion Conduction

We report the synthesis and characterization of thermally-stable polyimides for use as battery and fuel cell electrolyte membranes. Dianhydrides used were 1,4,5,8- naphthalenetetracarboxylic dianhydride and/or 4,4'-(hexafluoroisopropylidene)diphthalic anhydride. Diamines used were anti-4,4-diaminodibenzo-l8-crown-6, 4,4'- diaminodibenzo-24-crown-8, 2,2-bis(4-aminophenyl)hexafluoropropane, and/or 2,5- diaminobenzenesulfonic acid. The polymers were characterized using electrochemical impedance spectroscopy (EIS), thermal analysis and X-ray diffraction. Polymers containing the hexafluoroisopropylidene (HFIP) group were soluble in common organic solvents, while polymers without the HFIP group were very poorly soluble. Sulfonation yields polymers that are sparingly soluble in aqueous base and/or methanol. Degree of sulfonation, determined by titration, was between one and three sulfonate groups per repeat unit. Proton conductivity was determined as a function of water content, with a maximum conductivity of l x 10(exp -2) per centimeter when fully hydrated. Crown ether-containing polymers exhibit a high degree of order that may be indicative of crown ether channel formation, which may facilitate Li(+) transport for use in battery membranes.

Irvin, Jennifer A.↗

Initial Results of the MISSE-Flight Facility Polymers and Composites Experiment 1-4 (PCE 1-4)

Spacecraft in low Earth orbit (LEO) are subjected to harsh environmental conditions, including radiation (cosmic rays, ultraviolet (UV), x-ray and charged particle radiation), micrometeoroids and orbital debris, temperature extremes, thermal cycling, and atomic oxygen (AO). These environmental exposures can result in erosion, embrittlement and optical property degradation of susceptible materials threatening spacecraft performance and durability. To increase our understanding of effects such as AO erosion and radiation induced embrittlement of spacecraft materials, NASA Glenn Research Center has developed a series of experiments that are flown as part of the Materials International Space Station Experiment (MISSE) missions on the exterior of the International Space Station (ISS). These experiments have provided critical space environmental durability data such as AO erosion data of polymers and composites, and radiation induced mechanical property degradation of spacecraft insulation materials, after long term space exposure. In continuing these studies, four Glenn experiments with 365 flight samples have been flown on ISS’s external MISSE-Flight Facility (MISSE-FF). These experiments are the Polymers and Composites Experiment-1 (PCE-1) flown as part of the inaugural MISSE-9 mission, the PCE-2 flown as part of the MISSE-10 mission, the PCE-3 flown as part of the MISSE-12 and MISSE-15 missions, and the PCE-4 flown as part of the MISSE-13 mission. The primary objective of the PCE 1-4 experiments is to determine the AO and radiation durability of spacecraft polymers and composites. In addition, each experiment has a wide variety of spacecraft materials and hence they each have numerous additional sample objectives. Each of the PCE 1-4 is designed to examine the consequences of AO interactions including AO erosion yield (Ey) and optical and thermal property characterization. Several polymers were flown in both ram and zenith flight orientations to determine the effect of varying solar to AO ratios on Ey. Common spacecraft materials including Teflon FEP, white Tedlar and Upilex-S were included on multiple MISSE missions so erosion dependence on environment exposure can be determined. The PCE-1 includes epoxy composite samples with varying ZnO levels to determine the effect of inorganic filler level on AO durability. And, a variety of samples were flown to characterize AO scattering and AO undercutting processes. All four PCE experiments include samples to provide better insight into radiation durability of polymers and composites. The MISSE-9 PCE-1 includes Teflon FEP tensile samples flown in the wake and zenith direction so variations in radiation exposure from the different flight directions can provide insight into radiation induced embrittlement of Teflon FEP. Teflon FEP tensile samples were also flown in the wake direction as part of the MISSE-13 PCE-4. In addition, shape memory alloys, shape memory composites, melanin based composites, stressed and unstressed gossamer sun shield materials, coated and uncoated docking seal samples, and new solar cell cover slides were flown for space radiation durability and/or shielding assessment. This paper provides an overview of Glenn’s PCE 1-4 MISSE-FF experiments and provides initial post-flight observations and results.

atomic oxygen↗

Rational sub-nanometer manipulation of polymer morphology for efficient chemical separations

The ability to control polymer morphology on the sub-nanometer length scale has broad implications for chemical separations. To achieve such control on easily processable systems, this proposal focuses on the synthesis and characterization of polymers containing appended labile moieties that are easily detached by thermolysis or UV irradiation deep within the glassy state. Once liberated, these moieties can diffuse from the polymer matrix as gaseous products, leaving behind templated pathways for selective diffusion and sorption of small molecules. With a specific target of creating polymeric membrane materials with unprecedented diffusion and (ad)sorption characteristics for chemical separations, synthesis of new materials will be complemented with advanced metrologies, simulations, and evaluation of thermodynamic and transport theory.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Fire- and heat-resistant laminating resins based on maleimido-substituted aromatic cyclotriphosphazenes

A novel class of flame- and heat-resistant polymers has been synthesized by the thermal polymerization of maleimido-substituted aromatic cyclotriphosphazenes. The polymer obtained from tris-(aminophenoxy)tris(maleimidophenoxy)cyclotriphosphazene has good thermal stability and is noteworthy for its high char yield, viz., 82 percent at 800 C in nitrogen and 81 percent at 700 C in air. Graphite-fabric laminates prepared with this polymer did not burn in pure oxygen, even at 300 C, and were tested for mechanical properties. Hexakis(4-maleimidophenoxy)cyclotriphosphazene and some fluorine-containing monomers have also been synthesized. The structures of these cyclic phosphazene precursors and polymers were characterized by FT IR spectrophotometry, H-1 NMR, F-19 NMR, and P-31 solid-state magic angle spinning NMR spectroscopy, and mass spectrometry. The curing behavior of the polymer precursors and the thermal stabilities of the polymers were evaluated by differential scanning calorimetry (DSC) and thermogravimetric analyses (TGA).

Kumar, D.↗

Specific molecular design of polycarboxylate polymers exhibiting optimal compatibility with clay contaminants in concrete

Highlights: • Allyl ether-based PCEs with short side chain length and low side chain density presented superior clay resistance. • PCEs with medium side chain density exhibited best clay robustness when compared at the absolute dosed quantities. • The proportion of PCE being intercalated into the layered structure of clay was quantified. It is widely recognized that the dispersing ability of polycarboxylate superplasticizers (PCEs) could be hindered due to the presence of clay contaminants in concrete. In this study, a series of allyl ether-based polycarboxylate superplasticizers possessing short polyethylene glycol side chains was successfully synthesized and probed for their clay tolerance. The resulting PCE polymers were characterized via Size Exclusion Chromatography (SEC) to obtain their molecular properties. Thereafter, their dispersing ability was probed in the absence and presence of sodium bentonite. Allyl ether-based polycarboxylate (APEG) polymers possessing short side chains were found to exhibit enhanced clay resistance as compared to that of conventional MPEG PCEs holding long pendant chains. The mode of interaction between APEG PCEs and bentonite was investigated via sorption and XRD measurements. The data revealed that APEG PCEs possessing a lower side chain density intercalate less into the interlayer space of bentonite than those exhibiting higher side chain density.

36 MATERIALS SCIENCE↗

Semiconducting polymers for gas detection

Conjugated polyenes, and polyesters containing phthalocyanine in their backbone, were synthesized. These polymers were characterized by chemical analysis, thermogravimetric analysis, spectral analysis, and X-ray diffraction studies for crystallinity, as well as for their film-forming capability and gas/polymer interactions. Most of the polymers were relatively insensitive to water vapor up to 50 percent relative humidity, but the polyester/phthalocyanine (iron) polymer was relatively insensitive up to 100 percent RH. On the other hand, poly(p-dimethylaminophenylacetylene) was too conductive at 100 percent RH. Of the gases tested, the only ones that gave any evidence of interacting with the polymers were SO2, NOx, HCN and NH3. Poly(imidazole)/thiophene responded to each of these gases at all relative humidities, while the other polymers gave varying response, depending upon the RH. Thus, since most of these gases were electron-accepting, the electron-donating character of poly(imidazole)/thiophene substantiates the concept of electronegativity being the operating principle for interaction effects. Of the six polymers prepared, poly(imidazole)/thiophene first showed a very good response to smoldering cotton, but it later became nonresponsive; presumably due to oxidation effects.

Byrd, N. R.↗

Polyimides with pendant alkyl groups

The effect on selected polyimide properties when pendant alkyl groups were attached to the polymer backbone was investigated. A series of polymers were prepared using benzophenone tetracarboxylic acid dianhydride (BTDA) and seven different p-alkyl-m,p'-diaminobenzophenone monomers. The alkyl groups varied in length from C(1) (methyl) to C(9) (nonyl). The polyimide prepared from BTDA and m,p'-diaminobenzophenone was included as a control. All polymers were characterized by various chromatographic, spectroscopic, thermal, and mechanical techniques. Increasing the length of the pendant alkyl group resulted in a systematic decrease in glass transition temperature (Tg) for vacuum cured films. A 70 C decrease in Tg to 193 C was observed for the nonyl polymer compared to the Tg for the control. A corresponding systematic increase in Tg indicative of crosslinking, was observed for air cured films. Thermogravimetric analysis revealed a slight sacrifice in thermal stability with increasing alkyl length. No improvement in film toughness was observed.

Jensen, B. J.↗

Investigation of Polymer Liquid Crystals

The positron annihilation lifetime spectroscopy (PALS) using a low energy flux generator may provide a reasonably accurate technique for measuring molecular weights of linear polymers and characterization of thin polyimide films in terms of their dielectric constants and hydrophobity etc. Among the tested samples are glassy poly arylene Ether Ketone films, epoxy and other polyimide films. One of the proposed techniques relates the free volume cell size (V(sub f)) with sample molecular weight (M) in a manner remarkably similar to that obtained by Mark Houwink (M-H) between the inherent viscosity (eta) and molecular wieght of polymer solution. The PALS has also demonstrated that free-volume cell size in thermoset is a versatile, useful parameter that relates directly to the polymer segmental molecular weight, the cross-link density, and the coefficient of thermal expansion. Thus, a determination of free volume cell size provides a viable basis for complete microstructural characterization of thermoset polyimides and also gives direct information about the cross-link density and coefficient of expansion of the test samples. Seven areas of the research conducted are reported here.

Han, Kwang S.↗

Dynamic Implications of Noncovalent Interactions in Amphiphilic Single-Chain Polymer Nanoparticles

Single-chain polymer nanoparticles (SCNPs) combine the chemical diversity of synthetic polymers with the intricate structure of biopolymers, generating versatile biomimetic materials. The mobility of polymer chain segments at length scales similar to secondary structural elements in proteins is critical to SCNP structure and thus function. However, the influence of noncovalent interactions used to form SCNPs (e.g., hydrogen-bonding and biomimetic secondary-like structure) on these conformational dynamics is challenging to quantitatively assess. To isolate the effects of noncovalent interactions on SCNP structure and conformational dynamics, we synthesized a series of amphiphilic copolymers containing dimethylacrylamide and monomers capable of forming these different interactions: (1) di(phenylalanine) acrylamide that forms intramolecular β-sheet-like cross-links, (2) phenylalanine acrylamide that forms hydrogen-bonds but lacks a defined local structure, and (3) benzyl acrylamide that has the lowest propensity for hydrogen-bonding. Each SCNP formed folded structures comparable to those of intrinsically disordered proteins, as observed by size exclusion chromatography and small angle neutron scattering. The dynamics of these polymers, as characterized by a combination of dynamic light scattering and neutron spin echo spectroscopy, was well described using the Zimm with internal friction (ZIF) model, highlighting the role of each noncovalent interaction to additively restrict the internal relaxations of SCNPs. These results demonstrate the utility of local scale interactions to control SCNP polymer dynamics, guiding the design of functional biomimetic materials with refined binding sites and tunable kinetics.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Test method development for structural characterization of fiber composites at high temperatures

Test methods used for structural characterization of polymer matrix composites can be applied to glass and ceramic matrix composites only at low temperatures. New test methods are required for tensile, compressive, and shear properties of fiber composites at high temperatures. A tensile test which should be useful to at least 1000 C has been developed and used to characterize the properties of a Nicalon/glass composite up to the matrix limiting temperature of 600 C. Longitudinal and transverse unidirectional composite data are presented and discussed.

Mandell, J. F.↗

Evaluation of Oxygen Consumption as a Sensitive Measure of Electrical Cable Polymer Insulation Degradation

Polymers used as dielectric materials in nuclear grade electrical cables, such as cross-linked polyethylene (XLPE) and ethylene-propylene rubber (EPR), are long-lived and durable. Estimating the decades-long useful service life of polymers experimentally in a feasible timeframe of weeks or months requires greatly accelerated aging in the laboratory at elevated temperatures and/or gamma dose rates. Many limitations of accelerated aging, such as due to artefacts of the process including diffusion limited oxidation and dose rate effects, have been identified that can make accurate lifetime prediction at service conditions challenging. This can be due to differences in degradation mechanisms between rapid and extended aging or to the presence of induction periods during which early aging is undetectable using common metrics of polymer insulation characterization such as tensile elongation at break. Conceptually, an ideal measure of aging would track clearly and predictably with material changes throughout the lifecycle of the evolving material state from early aging through end of useful life. With such a metric accelerated aging could be performed at much milder conditions, conditions closer to those found in long term service, and end of life calculated from the early data. Oxygen consumption has previously been proposed as a sensitive measure of insulation polymer oxidation that might meet such desirable characteristics. In this work, nuclear cable insulation samples of the two most common types, XLPE and EPR, from two of the most sourced manufacturers, RSCC and The Okonite Company, were subjected to gamma irradiation at dose rates of 100, 200, and 300 Gy/hr for up to 42 days at 26°C. The aged samples were used to evaluate oxygen consumption as a sensitive measure of aging for these materials and these conditions. For comparison and validation, the aged samples were also characterized using the more conventional tests of mass change, density, carbonyl index, and yellowness index. For both materials, oxygen consumption during irradiation was found to track consistently with applied dose—oxygen consumption rate was linear with time. Mass change and carbonyl index were also clearly proportional to exposure dose. Yellowness index, a surface sensitive measure, was observed to increase linearly with dose at low exposure levels before plateauing. Sample density was not observed to change under the conditions explored. Oxygen consumption was found to be a particularly sensitive metric to measure the degradation of polymeric cable insulation exposed to radiation. Oxygen consumption was compared to Arrhenius and time-temperature-superposition methods for activation energy calculation using literature date and found to be a useful and viable alternative for lifetime prediction. The techniques developed in this work are anticipated to be valuable in the estimation of insulation aging rates under mild conditions approaching service conditions. Direction comparison of useful life prediction by oxygen consumption with prediction via Arrhenius methodology for thermal aging and existing methods for radiation and combined thermal/radiation aging would serve to further validate this promising approach and refine our understanding of material-specific aging rates.

36 MATERIALS SCIENCE↗

Degradation and crosslinking of perfluoroalkyl polyethers under X-ray irradiation in ultrahigh vacuum

Degradation of three types of commercially available perfluoroalkyl polyethers (PFPE)-Demnum S200, Fomblin Z25, and Krytox 16256-by X-ray irradiation was studied by using X-ray photoemission spectroscopy (XPS) and a mass spectrometer under ultra-high-vacuum conditions. The carbons in the polymers were characterized by chemical shifts of Cls binding energies. Gaseous products containing COF2 and low-molecular-weight fluorocarbons were formed. From Fomblin Z25, which has acetal linkages (-OCF2O-), a large quantity of COF2 gas was evolved. Liquid products became tacky after a long irradiation time, and some did not dissolve in Freon. High-pressure liquid chromatography (HPLC) showed that molecular weight distribution became broader and that higher molecular weight polymers were formed from Demnum and Krytox. We concluded from these results that degradation and cross-linking took place simultaneously. Demnum crosslinked more easily than the other fluids. The time dependence of both XPS spectra of Cls and mass spectra showed that C-O-bonded carbons in PFPE'S were removed faster than other carbons. There was no substrate effect on the degradation reaction because the first-order rate constants calculated from the change of gaseous products were similar when stainless steel (440C) and gold-coated surfaces were used. Metal fluorides were formed on stainless steel during the reaction. A mechanism for the degradation of PFPE'S is discussed on the basis of their molecular structures.

Mori, Shigeyuki↗

Addition polyimide end cap study

The characterization of addition polyimides with various end caps for adhesive applications at 120-250 C environments is discussed. Oligometric polyimides were prepared from 3,3',4,4'-benzophenone tetracarboxylic dianhydride and 3,3'-methylenedianiline which were end-capped with functionally reactive moities which cause crosslinking when the oligomers are heated to 200-400 C. The syntheses of the oligomers are outlined. The thermolysis of the oligomers was studied by differential scanning calorimetry and the resulting polymers were characterized by differential thermal analysis and adhesive performance. The adhesive data include lap shear strengths on titanium 6-4 adherends both before and after aging for 1000 hours at 121 C and/or 232 C.

St.clair, T. L.↗

Characterization of selected LDEF: Exposed polymer films and resins

The Long Duration Exposure Facility (LDEF) provided a unique environmental exposure of a wide variety of materials. The effects of 5 years and 10 months of Low-Earth Orbit (LEO) exposure of these materials to atomic oxygen, ultraviolet and particulate radiation, meteoroid and debris, vacuum, contamination, and thermal cycling is providing a data base unparalleled in the history of space environment research. Working though the Environmental Effects on Materials Special Investigation Group (MSIG), a number of polymeric materials in various processed forms have been assembled from LDEF investigators for analysis at the NASA Langley Research Center. This paper reports the status of on-going chemical characterization of these materials.

Young, Philip R.↗