Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “metallization wear”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 127 records · Page 7

Performance of PTFE-lined composite journal bearings

Plain cylindrical journal bearings consisting of aramid fiber reinforced epoxy outer shells and glass fiber reinforced PTFE lubricating liners were evaluated. All materials in these bearings are electrically nonconductive; thus eliminating the problem of galvanic corrosion sometimes encountered with metal bearings installed in dissimilar metal mountings. Friction and wear characteristics were determined for loads, temperatures, and oscillating conditions that are typical of current airframe bearing applications. Friction and wear characteristics were found to be compatible with most airframe bearing requirements from -23 C to 121 C. Contamination with MIL H-5606 hydraulic fluid increased wear of the PTFE liners at 121 C, but did not affect the structural integrity of the aramid/epoxy composite.

Sliney, H. E.↗

Tribological properties and thermal stability of various types of polyimide films

Thermal exposure experiments at 315 and 350 C were conducted on seven different types of polyimide films to determine which was the most thermally stable and adherent. The polyimides were ranked according to the rate of which they lost weight and how well they adhered to the metallic substrate. Friction and wear experiments were conducted at 25 C (room temperature) on films bonded to 440C HT stainless steel. Friction, film wear rates, wear mechanisms, and transfer films of the seven films were investigated and compared. The polyimides were found to fall into two groups as far as friction and wear properties were concerned. Group I had lower friction but an order of magnitude higher film wear rate than did group II. The wear mechanism was predominately adhesive, but the size of the wear particles was larger for group I polyimides.

Fusaro, R. L.↗

Friction and metal transfer for single-crystal silicon carbide in contact with various metals in vacuum

Sliding friction experiments were conducted with single-crystal silicon carbide in contact with transition metals (tungsten, iron, rhodium, nickel, titanium, and cobalt), copper, and aluminum. Results indicate the coefficient of friction for a silicon carbide-metal system is related to the d bond character and relative chemical activity of the metal. The more active the metal, the higher the coefficient of friction. All the metals examined transferred to the surface of silicon carbide in sliding. The chemical activity of metal to silicon and carbon and shear modulus of the metal may play important roles in metal transfer and the form of the wear debris. The less active and greater resistance to shear the metal has, with the exception of rhodium and tungsten, the less transfer to silicon carbide.

Miyoshi, K.↗

High-Temperature Tribometer And Data-Acquisition System

New tribometer tests friction and wear properties of ceramic and metal materials at temperatures up to 1,200 degrees C in controlled atmospheres. Connected to data-acquisition system using computer programs to enhance productivity and convenience of testing facility. Friction and wear properties of new materials and lubricants ascertained accurately and conveniently. Information needed in development of materials for advanced aerospace and terrestrial applications.

Sliney, Harold E.↗

Tribocatalytically-activated formation of protective friction and wear reducing carbon coatings from alkane environment

Minimizing the wear of the surfaces exposed to mechanical shear stresses is a critical challenge for maximizing the lifespan of rotary mechanical parts. In this study, we have discovered the anti-wear capability of a series of metal nitride-copper nanocomposite coatings tested in a liquid hydrocarbon environment. The results indicate substantial reduction of the wear in comparison to the uncoated steel substrate. Analysis of the wear tracks indicates the formation of carbon-based protective films directly at the sliding interface during the tribological tests. Raman spectroscopy mapping of the wear track suggests the amorphous carbon (a-C) nature of the formed tribofilm. Further analysis of the tribocatalytic activity of the best coating candidate, MoN-Cu, as a function of load (0.25–1 N) and temperature (25 °C and 50 °C) was performed in three alkane solutions, decane, dodecane, and hexadecane. Results indicated that elevated temperature and high contact pressure lead to different tribological characteristics of the coating tested in different environments. The elemental energy dispersive x-ray spectroscopy analysis and Raman analysis revealed formation of the amorphous carbon film that facilitates easy shearing at the contact interface thus enabling more stable friction behavior and lower wear of the tribocatalytic coating. These findings provide new insights into the tribocatalysis mechanism that enables the formation of zero-wear coatings.

36 MATERIALS SCIENCE↗

Fundamental tribological properties of ceramics

When a ceramic is brought into contact with itself, another ceramic, or a metal, strong bond forces can develop between the materials. Adhesion between a ceramic and itself or another solid are discussed from a theoretical consideration of the nature of the surfaces and experimentally by relating bond forces to the interface resulting from solid state contact. Elastic, plastic, and fracture behavior of ceramics in solid-state contact are discussed as they relate to friction and wear. The contact load necessary to initiate fracture in ceramics is shown to be appreciably reduced with tangential motion. Both friction and wear of ceramics are anisotropic and relate to crystal structure as with metals. Both free energy of oxide formation and the d valence bond character of metals are related to the friction and wear characteristics for metals in contact with ceramics. Lubrication is found to increase the critical load necessary to initiate fracture of ceramics with sliding or rubbing contact.

Buckley, D. H.↗

Fundamental tribological properties of ceramics

When a ceramic is brought into contact with itself, another ceramic, or a metal, strong bond forces can develop between the materials. Adhesion between a ceramic and itself or another solid are discussed from a theoretical consideration of the nature of the surfaces and experimentally by relating bond forces to the interface resulting from solid state contact. Elastic, plastic, and fracture behavior of ceramics in solid-state contact are discussed as they relate to friction and wear. The contact load necessary to initiate fracture in ceramics is shown to be appreciably reduced with tangential motion. Both friction and wear of ceramics are anisotropic and relate to crystal structure as with metals. Both free energy of oxide formation and the d valence bond character of metals are related to the friction and wear characteristics for metals in contact with ceramics. Lubrication is found to increase the critical load necessary to initiate fracture of ceramics with sliding or rubbing contact.

Buckley, D. H.↗

Composition optimization of chromium carbide based solid lubricant coatings for foil gas bearings at temperatures to 650 C

A test program to determine the optimum composition of chromium carbide based solid lubricant coatings for compliant gas bearings is described. The friction and wear properties of the coatings are evaluated using a foil gas bearing test apparatus. The various coatings were prepared by powder blending, then plasma sprayed onto Inconel 718 test journals and diamond ground to the desired coating thickness and surface finish. The journals were operated against preoxidized nickel-chromium alloy foils. The test bearings were subjected to repeated start/stop cycles under a 14 kPa (2 psi) bearing unit load. The bearings were tested for 9000 start/stop cycles or until the specimen wear reached a predetermined failure level. In general, the addition of silver and eutectic to the chromium carbide base stock significantly reduced foil wear and increased journal coating wear. The optimum coating composition, PS212 (70 wt% metal bonded Cr3C2, 15 wt% Ag, 15% BaF2/CaF2 eutectic), reduced foil wear by a factor of two and displayed coating wear well within acceptable limits. The load capacity of the bearing using the plasma-sprayed coating prior to and after a run-in period was ascertained and compared to polished Inconel 718 specimens.

Dellacorte, Christopher↗

Simulated studies of wear and friction in total hip prosthesis components with various ball sizes and surface finishes

Experiments were conducted on a newly designed total hip joint simulator. The apparatus closely simulates the complex motions and loads of the human hip in normal walking. The wear and friction of presently used appliance configurations and materials were determined. A surface treatment of the metal femoral ball specimens was applied to influence wear. The results of the investigation indicate that wear can be reduced by mechanical treatment of metal femoral ball surfaces. A metallographic examination and surface roughness measurements were made.

Swikert, M. A.↗

Mechanisms of lubrication and wear of a bonded solid-lubricant film

The tribological properties of polyimide-bonded graphite fluoride films were investigated. A pin-on-disk type of testing apparatus was used; in addition to sliding a hemispherically tipped rider, a rider with a 0.95-mm-diameter flat area was slid against the film so that a lower, less variable contact stress could be achieved. Two stages of lubrication occurred: in the first, the film supported the load and the lubricating mechanism consisted of the shear of a thin surface layer between the rider and the bulk of the film. The second occurred after the bonded film had worn to the substrate, and consisted of the shear of very thin lubricant films between the rider and flat plateaus generated on the metallic substrate asperities. The film wear mechanism was strongly dependent on contact stress.

Fusaro, R. L.↗

Lubricating and wear mechanisms for a hemisphere sliding on polyimide-bonded graphite fluoride film

Friction, wear life, rider wear, and film wear for a 440 C high-temperature-stainless-steel, hemispherically tipped rider sliding against polyimide-bonded graphite fluoride films were evaluated in a moist-air atmosphere at 25 C. Optical microscope and surface profilometry observations were made at various sliding intervals to determine how film thickness affected the lubricating and failure mechanisms of the films. Two lubrication regimes operated for the same load. In the first, the film supported the load and the lubricating mechanism consisted of the shear (plastic flow) of a thin layer of the lubricant between the metallic rider and the film surface. In the second, the film did not support the load (it was worn away) and the lubricating mechanism consisted of the shear of very thin lubricant films between flat areas generated on the rider and on sandblasted metallic asperities in the film wear track. Lubricant was supplied from the valleys between the asperities or from the sides of the wear track. With thicker films, wear life increased since a greater lubricant supply was available from the sides of the wear track.

Fusaro, R. L.↗

A percolation theory for designing corrosion-resistant alloys

Iron-chromium and nickel-chromium binary alloys containing sufficient quantities of chromium serve as the prototypical corrosion-resistant metals owing to the presence of a nanometre-thick protective passive oxide film. Should this film be compromised by a scratch or abrasive wear, it reforms with little accompanying metal dissolution, a key criterion for good passive behaviour. This is a principal reason that stainless steels and other chromium-containing alloys are used in critical applications ranging from biomedical implants to nuclear reactor components. Unravelling the compositional dependence of this electrochemical behaviour is a long-standing unanswered question in corrosion science. Herein, we develop a percolation theory of alloy passivation based on two-dimensional to three-dimensional crossover effects that accounts for selective dissolution and the quantity of metal dissolved during the initial stage of passive film formation. We validate this theory both experimentally and by kinetic Monte Carlo simulation. Our results reveal a path forward for the design of corrosion-resistant metallic alloys.

36 MATERIALS SCIENCE↗

Friction and wear behavior of glasses and ceramics

Adhesion, friction, and wear behavior of glasses and ionic solids are reviewed. These materials are shown to behave in a manner similar to other solids with respect to adhesion. Their friction characteristics are shown to be sensitive to environmental constituents and surface films. This sensitivity can be related to a reduction in adhesive bonding and the changes in surficial mechanical behavior associated with Rehbinder and Joffe effects. Both friction and wear properties of ionic crystalline solids are highly anisotropic. With metals in contact with ionic solids the fracture strength of the ionic solid and the shear strength in the metal and those properties that determine these will dictate which of the materials undergoes adhesive wear. The chemical activity of the metal plays an important role in the nature and strength of the adhesive interfacial bond that develops between the metal and a glass or ionic solid.

Buckley, D. H.↗

Mechanisms of lubrication and wear of a bonded solid lubricant film

To obtain a better understanding of how bonded solid lubricant films lubricate and wear (in general), the tribological properties of polyimide-bonded graphite fluoride films were studied (in specific). A pin-on-disk type of testing apparatus was used; but in addition to sliding a hemispherically tipped rider, a rider with a 0.95 mm diameter flat area was slid against the film. This was done so that a lower, less variable contact stress could be achieved. Two stages of lubrication occurred. In the first, the film supported the load. The lubricating mechanism consisted of the shear of a thin surface layer (of the film) between the rider and the bulk of the film. The second occurred after the bonded film had worn to the substrate, and consisted of the shear of very thin lubricant films between the rider and flat plateaus generated on the metallic substrate asperities. The film wear mechanism was strongly dependent on contact stress.

Fusaro, R. L.↗

Spray Application of Rapidly Solidified Metals

Fast and economical process now available. New process applies rapidly solidified (RS) metal coatings to substrates. RS metals made directly from molten material. Have amorphous or microcrystalline structures and yield coatings having superior wear and corrosion resistance. Mixture of RS metal powder and peening particles sprayed from nozzle against surface coated. Powder and peening particles strike surface simultaneously, and impact bonds powder to surface as uniform coating. New process, which employs shot peening, is safe, fast, and inexpensive.

Chu, H. P.↗

Changes Found on Run-In and Scuffed Surfaces of Steel Chrome Plate, and Cast Iron

A study was made of run-in and scuffed steel, chrome-plate, and cast-iron surfaces. X-ray and electron diffraction techniques, micro-hardness determinations, and microscopy were used. Surface changes varied and were found to include three classes: chemical reaction, hardening, and crystallite-size alteration. The principal chemical reactions were oxidation and carburization.

IRON, CAST - WEAR RESISTANCE↗

Environmental study of miniature slip rings

Investigation studied the long term operation of miniature slip ring assembles in high vacuum of space and included the influence of ring, brush, and insulator materials on electrical noise and mechanical wear. Results show that soft metal vapor plating and niobium diselenide miniature slip rings are beneficial.

Radnik, J. L.↗