CISCC Countermeasures for Spent Fuel Canisters in Concrete Casks
Aging management of spent fuel is an important issue worldwide. Chloride-induced stress corrosion cracking (CISCC) of welded canisters is particularly important for concrete casks, where it occurs in response to a combination of environmental, material, and residual stress factors. In this paper, we introduce a countermeasure to prevent the occurrence of CISCC by adjusting the flow rate of the cooling air into the concrete cask so that the canister surface temperature does not decrease below 100°C, which is a conservative deliquesce temperature threshold for CISCC occurrence. The flow adjustment device was installed in a cask model, and two tests were conducted under the heat rate conditions corresponding to those of an actual canister. In the first test, the device was operated under a condition where the canister surface temperature was below 100°C to verify whether it could increase the canister surface temperature to above 100°C. In the second test, the heat rate was decreased from a state where the canister surface temperature was above 100°C, to verify whether the device could maintain the canister surface temperature above 100°C. Good results were obtained in both cases. However, in the case of a low decay heat rate of spent fuel after extended dry storage, the temperature of the canister surface may decrease below 100°C even if no air supply is provided. Therefore, in this case, it may be necessary to take measures such as blocking air outlets.