Engineering PapersSearch

SEARCH · Engineering Papers

Results for “intermetallic”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 127 records · Page 7

Deformation behavior of a Ni-30Al-20Fe-0.05Zr intermetallic alloy in the temperature range 300 to 1300 K

The deformation properties of an extruded Ni-30Al-20Fe-0.05Zr (at. pct) alloy in the temperature range 300-1300 K were investigated under initial tensile strain rates that varied between 10 exp -6 and 10 exp -3/sec and in constant load compression creep between 1073 and 1300 K. Three deformation regimes were observed: region I, occurring between 400 and 673 K, which consisted of an athermal regime of less than 0.3 percent tensile ductility; region II, between 673 and 1073, where exponential creep was dominant; and region III, between 1073 and 1300 K, where a significant improvement in tensile ductility was observed.

Raj, S. V.

Advanced reinforcement systems for intermetallic applications

A 2-D axisymmetric model was employed to determine the magnitude of the radial, axial, and hoop stresses caused by the thermal expansion difference between fiber and matrix and which result from the fabrication temperature cycle. Finite element analysis was conducted for single fiber model systems based on SCS-6/Ti3Al+Nb and Al2O3/NiAl. The stress distribution due to the imposition of a graded intermediate layer for each system was determined and included variables of layer thickness and gradation in interlayer chemistry in order to vary the expansion gradient between fiber and matrix. Thermal cycling tests were conducted on sputter coated SCS-6 fibers selectively coated with Ti3Al+Nb, with and without an intermediate layer. Cracking of the Ti3Al+Nb layers was prevented by an interlayer based on Ti-TiN-Ti. The interlayer thickness appeared critical to its efficiency. Similarly, for the case of Al2O3/NiAl, an intermediate layer consisting of a Ni bond coat on the sapphire fiber followed by a graded Al2O3-NiAl layer did not crack when given a thermal excursion to 1100 C and then cooled to room temperature. Acoustic emission tests on single fiber specimens were unsuccessful in detecting load drops associated with the successive fracture of the fiber. For the SCS-6/Ti3Al system this was the result of several factors which included the matrix/fiber ratio and poor bonding of the matrix and fiber. In the case of the Al2O3/NiAl system brittle failure of the NiAl matrix precluded fiber breakdown during tensile loading.

Merrick, Howard F.

Technical note - Plasma-sprayed ceramic thermal barrier coatings for smooth intermetallic alloys

A new approach for plasma spray deposition of ceramic thermal barrier coatings directly to smooth substrates is described. Ceramic thermal barrier coatings were directly applied to substrates that had been coated with low-pressure plasma sprayed NiCrAlY bond coats and then centerless ground to simulate a smooth oxidation-resistant substrate. As the high-temperature oxidation behavior of NiAl+Zr is superior to that of MCrALY alloy, the bond coat is not required for oxidation resistance.

Miller, R. A.

Nozzle material requirements and the status of intermetallic matrix composites

The HSCT exhaust nozzle must manage high temperature exhaust gases and pressure gradients while meeting HSCT economic and noise goals. The important features and requirements for an HSCT exhaust nozzle are shown for a 2DCD (two-dimensional convergent-divergent) design. The same requirements would apply to an axisymmetric design. Exhaust nozzle weight has an adverse effect on the overall aircraft range, payload, and engine specific fuel consumption and is therefore the primary driver for advanced exhaust nozzle materials. Because of the large airflow and pressure gradients, exhaust nozzles are extremely large and heavy when made from current materials. The use of advanced materials with higher specific strength will reduce the weight of exhaust nozzle components. In addition to the flow of high-temperature exhaust gases into the exhaust nozzle, ambient air is entrained to reduce gas exit velocities and suppress sound. This leads to components exposed to extremely high temperature gradients and, hence, high thermal stresses. Further, exhaust gases are highly oxidizing; material environmental resistance will be an important factor for long life. Several viable concepts have been identified to reduce noise through the mixture of exhaust and ambient air. Sound can be further suppressed by acoustic panels that absorb high-frequency noise.

Johnson, Andrew M.

Investigation of Strain Aging in the Ordered Intermetallic Compound beta-NiAl

The phenomenon of strain aging has been investigated in polycrystalline and single crystal NiAl alloys at temperatures between 300 and 1200 K. Static strain aging studies revealed that after annealing at 1100 K for 7200 s (i.e., 2h) followed by furnace cooling, high purity, nitrogen-doped and titanium-doped polycrystalline alloys exhibited continuous yielding, while conventional-purity and carbon-doped alloys exhibited distinct yield points and Luders strains. Prestraining by hydrostatic pressurization removed the yield points, but they could be reintroduced by further annealing treatments. Yield points could be reintroduced more rapidly if the specimens were prestrained uniaxially rather than hydrostatically, owing to the arrangement of dislocations into cell structures during uniaxial deformation. The time dependence of the strain aging events followed at t(exp 2/3) relationship suggesting that the yield points observed in polycrystalline NiAl were the result of the pinning of mobile dislocations by interstitials, specifically carbon. Between 700 and 800 K, yield stress plateaus, yield stress transients upon a ten-fold increase in strain rate, work hardening peaks, and dips in the strain rate sensitivity (SRS) have been observed in conventional-purity and carbon-doped polycrystals. In single crystals, similar behavior was observed; in conventional-purity single crystals, however, the strain rate sensitivity became negative resulting in serrated yielding, whereas, the strain rate sensitivity stayed positive in high purity and in molybdenum-doped NiAl. These observations are indicative of dynamic strain aging (DSA) and are discussed in terms of conventional strain aging theories. The impact of these phenomena on the composition-structure-property relations are discerned. Finally, a good correlation has been demonstrated between the properties of NiAl alloys and a recently developed model for strain aging in metals and alloys developed by Reed-Hill et al.

Weaver, Mark Lovell

BFS Method for Alloys Optimized and Verified for the Study of Ordered Intermetallic Material

The aerospace industry has a need for new metallic alloys that are lightweight and have high strength at elevated temperatures. The BFS (Bozzolo, Ferrante, and Smith) method is a new, computationally efficient and physically sound quantum semi-perturbative approach for describing metals and their defects. Based on a simple interpretation of the alloy formation process that identifies strain and chemical contributions to the energy of the alloy, the method provides an atom-by-atom description of an alloy. Its implementation requires little more than algebra and the solution of transcendental equations. At the NASA Lewis Research Center, we have demonstrated that BFS can investigate the properties of a large number of alloys with a minimum computational effort on low-level computers. This screening allows the selection of the best alloy candidates for a particular application and, therefore, promises large cost savings over current approaches.

Source record

Processing Issues for Preliminary Melts of the Intermetallic Compound 60-NITINOL

The effect of various high temperature heat treatments and cooling rates on the hardness of cast 60-NITINOL (60wt%Ni- 40wt%Ti) was studied. The hardness ranged from approximately 33 HRC for annealed specimens to 63 HRC for water quenched specimens. Aging did not have a further effect on the hardness of the heat-treated and quenched material. The issue of material contamination and its possible effect on quench cracking during heat treatment above 1000 C was explored. The Charpy impact energy of the material was found to be relatively low (ranging from 0.4 to 1.0 J) and comparable to that of cast magnesium. Selection of service environments and applications for this material based on these findings should consider the processing route by which it was produced.

Stanford, Malcolm K.

Addressing Machining Issues for the Intermetallic Compound 60-NITINOL

60-NITINOL (60 wt.% Ni - 40 wt.% Ti) is being studied as a material for advanced aerospace components. Frequent wire breakage during electrical-discharge machining of this material was investigated. The studied material was fabricated from hot isostatically pressed 60-NITINOL powder obtained through a commercial source. Bulk chemical analysis of the material showed that the composition was nominal but had relatively high levels of certain impurities, including Al and O. It was later determined that Al2O3 particles had contaminated the material during the hot isostatic pressing procedure and that these particles were the most likely cause of the wire breakage. The results of this investigation highlight the importance of material cleanliness to its further implementation.

Stanford, Malcolm K.

60NiTi Intermetallic Material Evaluation for Lightweight and Corrosion Resistant Spherical Sliding Bearings for Aerospace Applications

NASA Glenn Research Center and the Kamatics subsidiary of the Kaman Corporation conducted the experimental evaluation of spherical sliding bearings made with 60NiTi inner races. The goal of the project was to assess the feasibility of manufacturing lightweight, corrosion resistant bearings utilizing 60NiTi for aerospace and industrial applications. NASA produced the bearings in collaboration with Abbott Ball Corporation and Kamatics fabricated bearing assemblies utilizing their standard reinforced polymer liner material. The assembled bearings were tested in oscillatory motion at a load of 4.54kN (10,000 lb), according to the requirements of the plain bearing specification SAE AS81820. Several test bearings were exposed to hydraulic fluid or aircraft deicing fluid prior to and during testing. The results show that the 60NiTi bearings exhibit tribological performance comparable to conventional stainless steel (440C) bearings. Further, exposure of 60NiTi bearings to the contaminant fluids had no apparent performance effect. It is concluded that 60NiTi is a feasible bearing material for aerospace and industrial spherical bearing applications.

materials

Creepy (not KREEPy) Gold-Indium Intermetallic Compounds on Secondary Ion Mass Spectrometry Samples

A series of Secondary Ion Mass Spectrometry (SIMS) sessions to measure hydrogen (H) in Martian meteorite minerals was completed using the Cameca 6f SIMS and NanoSIMS 50L at Arizona State University (ASU). During these sessions, a “creeping” phenomenon has occurred, where the edges of samples pressed in indium are covered by a metal alloy. We summarize these observations herein, present a collection of preliminary data, and discuss explanations and concerns for future SIMS work. We conclude the report with a research plan for further study.

Dudley, J. M.

Melt Infiltration Studies of 2D Tyranno SA3(R) Ceramic Matrix Composite Preforms with CrSi2 Intermetallic Alloy

The present paper reports the results of melt infiltrating 2D Tyranno SA3@ fiber woven preforms with molten CrSi2 between 1768 and 1896 K under a vacuum of 1.3 x 10-4 Pa (10-6 torr). The infiltration times varied between 1800 and 7200 s, which did not have any significant effect on the volume fraction of voids filled with the metal. Optical and scanning electron microscopy, back scattered electron imaging, energy dispersion spectroscopy and Raman spectroscopy were used to characterize the infiltrated preforms. A plot of the volume fraction of open voids infiltrated against the absolute melt infiltration temperature showed a sharp peak at 1773 K with almost complete infiltration of the voids at this temperature. The extent of silicide infiltration of the preforms dropped steeply above 1773 K with increasing melt infiltration temperature irrespective of the amount of infiltration time. Above 1805 K, the volume fraction of voids infiltrated with the melt was nearly 0%. It is demonstrated that CrSi2 did not show evidence of a reaction with the SiC fibers. The possibility that a resisting force due to contact angle hysteresis (CAH) may have influenced the diminishing amount of voids filled with increasing temperature above 1773 K was examined. The resistance force was estimated to be extremely small to be consequential. Another possibility that the CrSi2 may have decomposed into Cr(g) and Si(g) in the vacuum melt infiltration furnace appeared to be more plausible based on thermodynamic analyses. An empirical equation is proposed to calculate the amount of remaining charge left to infiltrate the preforms at the infiltration temperature. It is shown that an initial charge of 10 g would rationalize the present observations. While the decomposition of the CrSi2 appeared to mostly explain the present results, some discrepancies were observed, which were inconsistent with the decomposition model.

CrSi2, chromium silicide, ceramic matrix composite

Vacuum Melt Infiltration of 2D Tyranno SA3® Ceramic Matrix Composites with Cr-25(wt.%)Si Intermetallic Alloy

The potential and limitations of vacuum melt infiltrating woven preforms of 2D Tyranno SA3 fibers with Cr-25(wt.%)Si alloy were investigated. Microstructural observations revealed that the volume fractions of open voids infiltrated by the molten metal varied between 3.7 and 10.0% irrespective of the magnitudes of the melt infiltration temperatures and hold times, which was attributed in part to substantial volatilization of the silicide charge based on computational thermodynamics. In the absence of experimental data, poor wettability of the melt could not be ruled out unambiguously. Other possible reasons are carefully examined and discarded. Ring microstructures were observed around the fibers mainly at the outer surfaces of the infiltrated preform, where the BN and chemical vapor infiltrated SiC coatings had vaporized in the high vacuum environment. In contrast, they were absent in the interior of the preform, where the coatings were still present with no evidence of molten metal attack of the coatings. Details of thermodynamic calculations are presented to confirm the volatilization of the BN and CVI SiC coatings thereby resulting in the ring microstructures due to the filling of voids by the molten silicide. It is concluded that successful melt infiltration of Tyranno SA3® with Cr-25%Si can be only achieved under sufficient positive pressure to prevent volatilization of the coatings and the molten silicide.

Cr-25%Si

Variations in GARS powder microstructure as a function of powder chemistry and particle size

The properties of metal produced through powder metallurgy depends on the feedstock used. Powders produced via gas atomization reaction synthesis (GARS) are used to produce oxide dispersion strengthened alloys. The desired powder size range can vary for each consolidation technique. However, powder microstructure also can vary with powder particle size, which in turn can impact the microstructure and properties of the consolidated parts. In this study, GARS powders are characterized via inductively coupled plasma mass spectroscopy, inert gas fusion, and high-resolution x-ray diffraction to determine variations in elemental and phase compositions. Transmission electron microscopy was used to understand microstructure variations as a function of chemistry and size. Across the three batches tested intermetallic content was 0.73–1.35 wt% in the 0-20 μm powder batch and increased to 2.46–3.80 wt% in the coarse 45-106 μm batch. Across all batches, volume percent of surface oxidation decreased with powder diameter, with volume percents within the range of 0.75–1.2 % across 10 μm powder particles, and below 0.4 % across coarse powder particles approximately 100 μm in diameter. These observations were supported by inert gas fusion measurements. However, the oxide layer was thicker in coarse powder particles due to a slower cooling rate. Increasing oxygen content in atomization gas to 2000 ppm and adding yttrium increased both the surface oxidation content and yttrium intermetallic content. Lastly, intermetallic phases within the powder coarsened with powder size. Intermetallic morphology changed from fine spherical intermetallic and columnar dendritic growth to a cellular structure with finer spherical intermetallic, to coarse irregular intermetallic and intermetallic along grain boundaries as a result of slower cooling rate and solidification rate in coarse powder particles. Furthermore, the addition of zirconium does not appear to significantly change intermetallic morphology, but the composition changed from a Y-Fe rich intermetallic to a Y-Zr-Fe intermetallic.

42 ENGINEERING

Design Protocols and Analytical Strategies that Incorporate Structural Reliability Models

Ceramic matrix composites (CMC) and intermetallic materials (e.g., single crystal nickel aluminide) are high performance materials that exhibit attractive mechanical, thermal, and chemical properties. These materials are critically important in advancing certain performance aspects of gas turbine engines. From an aerospace engineers perspective the new generation of ceramic composites and intermetallics offers a significant potential for raising the thrust/weight ratio and reducing NO(sub x) emissions of gas turbine engines. These aspects have increased interest in utilizing these materials in the hot sections of turbine engines. However, as these materials evolve and their performance characteristics improve a persistent need exists for state-of-the-art analytical methods that predict the response of components fabricated from CMC and intermetallic material systems. This need provided the motivation for the technology developed under this research effort. Continuous ceramic fiber composites exhibit an increase in work of fracture, which allows for 'graceful' rather than catastrophic failure. When loaded in the fiber direction these composites retain substantial strength capacity beyond the initiation of transverse matrix cracking despite the fact that neither of its constituents would exhibit such behavior if tested alone. As additional load is applied beyond first matrix cracking, the matrix tends to break in a series of cracks bridged by the ceramic fibers. Any additional load is born increasingly by the fibers until the ultimate strength of the composite is reached. Thus modeling efforts supported under this research effort have focused on predicting this sort of behavior. For single crystal intermetallics the issues that motivated the technology development involved questions relating to material behavior and component design. Thus the research effort supported by this grant had to determine the statistical nature and source of fracture in a high strength, NiAl single crystal turbine blade material; map a simplistic future strength envelope of the material; develop a statistically based reliability computer algorithm; verify the reliability model and computer algorithm-, and model stator vanes for rig tests. Thus establishing design protocols that enable the engineer to analyze and predict the mechanical behavior of ceramic composites and intermetallics would mitigate the prototype (trial and error) approach currently used by the engineering community. The primary objective of the research effort supported by this short term grant is the continued creation of enabling technologies for the macro-analysis of components fabricated from ceramic composites and intermetallic material systems. The creation of enabling technologies aids in shortening the product development cycle of components fabricated from the new high technology materials.

Duffy, Stephen F.

Design Protocols and Analytical Strategies that Incorporate Structural Reliability Models

Ceramic matrix composites (CMC) and intermetallic materials (e.g., single crystal nickel aluminide) are high performance materials that exhibit attractive mechanical, thermal and chemical properties. These materials are critically important in advancing certain performance aspects of gas turbine engines. From an aerospace engineer's perspective the new generation of ceramic composites and intermetallics offers a significant potential for raising the thrust/weight ratio and reducing NO(x) emissions of gas turbine engines. These aspects have increased interest in utilizing these materials in the hot sections of turbine engines. However, as these materials evolve and their performance characteristics improve a persistent need exists for state-of-the-art analytical methods that predict the response of components fabricated from CMC and intermetallic material systems. This need provided the motivation for the technology developed under this research effort. Continuous ceramic fiber composites exhibit an increase in work of fracture, which allows for "graceful" rather than catastrophic failure. When loaded in the fiber direction, these composites retain substantial strength capacity beyond the initiation of transverse matrix cracking despite the fact that neither of its constituents would exhibit such behavior if tested alone. As additional load is applied beyond first matrix cracking, the matrix tends to break in a series of cracks bridged by the ceramic fibers. Any additional load is born increasingly by the fibers until the ultimate strength of the composite is reached. Thus modeling efforts supported under this research effort have focused on predicting this sort of behavior. For single crystal intermetallics the issues that motivated the technology development involved questions relating to material behavior and component design. Thus the research effort supported by this grant had to determine the statistical nature and source of fracture in a high strength, NiAl single crystal turbine blade material; map a simplistic failure strength envelope of the material; develop a statistically based reliability computer algorithm, verify the reliability model and computer algorithm, and model stator vanes for rig tests. Thus establishing design protocols that enable the engineer to analyze and predict the mechanical behavior of ceramic composites and intermetallics would mitigate the prototype (trial and error) approach currently used by the engineering community. The primary objective of the research effort supported by this short term grant is the continued creation of enabling technologies for the macroanalysis of components fabricated from ceramic composites and intermetallic material systems. The creation of enabling technologies aids in shortening the product development cycle of components fabricated from the new high technology materials.

Duffy, Stephen F.

Elucidating the factors controlling the methanol synthesis from CO 2 on ZnPd-ZnO/TiO 2 catalysts prepared by direct/inverse impregnation

The direct hydrogenation of CO 2 to methanol over supported ZnPd intermetallic catalysts remains a challenge due to the complex nature of the active sites, which are highly dependent on both the dispersion of ZnPd intermetallics and their proximity to ZnO. This study investigates the effect of the Pd and Zn incorporation order on methanol synthesis over TiO 2 -supported ZnPd catalysts. Catalysts were prepared via direct (Pd/Zn), inverse (Zn/Pd), and co-impregnation (Pd+Zn) methods using anatase TiO 2 as the support. Comprehensive characterization by XRD, HRTEM, CO-DRIFTS and XPS revealed that the formation of small and crystalline intermetallic β-ZnPd particles and their interaction with ZnO/ZnO x depends on the sequence of Pd and Zn incorporation. It was found that, under the reaction conditions, the ZnO x species plays a critical role in facilitating the formation of the intermetallic ZnPd through the interactions between Pd and ZnO x . In addition, ZnO x species have also been shown to modulate key catalytic properties, such as CO 2 activation and methanol selectivity. Specifically, the ZnPd/Pd surface ratio, determined by Pd dispersion and proximity to ZnO/ZnO x , was shown to determine the methanol production from CO 2 directly or via a CO intermediate. The Pd/Zn catalyst showed superior selectivity due to the in-situ formation of intermetallic species facilitated by Pd-ZnO x interactions.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH

Controlling microstructure and B2 ordering kinetics in Fe–Al system through additive manufacturing

Multi-material fabrication between steel and aluminum is challenging because of the formation of several intermetallic phases. Embrittling B2 ordered intermetallics form in the steel rich side and are stable till about 60% of Al dilution in steel. In this work by using multi-length scale characterization coupled with integrated computational process and thermokinetic modeling, we show that the ordered B2 intermetallics in the steel rich side of the Fe–Al system forms via a nucleation and growth mechanism. The extent of B2 ordered intermetallics can be controlled by modifying the directed energy deposition-additive manufacturing (DED-AM) process parameters. Our findings lay the foundation for enabling fabrication of crack-free functionally graded compositions between the two alloys.

36 MATERIALS SCIENCE