Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “ceramic materials”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 127 records · Page 7

Identification and analysis of factors affecting thermal shock resistance of ceramic materials in solar receivers

An analysis was conducted of the possible modes of thermal stress failure of brittle ceramics for potential use in point-focussing solar receivers. The pertinent materials properties which control thermal stress resistance were identified for conditions of steady-state and transient heat flow, convective and radiative heat transfer, thermal buckling and thermal fatigue as well as catastrophic crack propagation. Selection rules for materials with optimum thermal stress resistance for a particular thermal environment were identified. Recommendations for materials for particular components were made. The general requirements for a thermal shock testing program quantitatively meaningful for point-focussing solar receivers were outlined. Recommendations for follow-on theoretical analyses were made.

Hasselman, D. P. H.↗

Statistical study of thermal fracture of ceramic materials in the water quench test

The Weibull statistical theory of fracture was applied to thermal shock of ceramics in the water quench test. Transient thermal stresses and probability of failure were calculated for a cylindrical specimen cooled by convection. The convective heat transfer coefficient was calibrated using the time to failure which was measured with an acoustic emission technique. Theoretical failure probability distributions as a function of time and quench temperature compare favorably with experimental results for three high-alumina ceramics and a glass.

Rogers, Wayne P.↗

Method for improving the performance of oxidizable ceramic materials in oxidizing environments

Improved adhesion of thermal barrier coatings to nonmetallic substrates using a dense layer of ceramic on an underlying nonmetallic substrate that includes at least one oxidizable component. The improved adhesion occurs because the application of the dense ceramic layer forms a diffusion barrier for oxygen. This diffusion barrier prevents the oxidizable component of the substrate from decomposing. The present invention applies ceramic by a process that deposits a relatively thick and dense ceramic layer on the underlying substrate. The formation of the dense layer of ceramic avoids the problem of void formation associated with ceramic formation by most prior art thermal decomposition processes. The formation of voids has been associated with premature spalling of thermal barrier layers and other protective layers applied to substrates.

Nagaraj, Bangalore A.↗

Characterization of Ceramic Material Produced From a Cold Crucible Induction Melter Test

This report summarizes the results from characterization of samples from a melt processed surrogate ceramic waste form. Completed in October of 2014, the first scaled proof of principle cold crucible induction melter (CCIM) test was conducted to process a Fe-hollandite-rich titanate ceramic for treatment of high level nuclear waste. X-ray diffraction, electron microscopy, inductively coupled plasma-atomic emission spectroscopy (and inductively coupled plasma-mass spectroscopy for Cs), and product consistency tests were used to characterize the CCIM material produced. Core samples at various radial locations from the center of the CCIM were taken. These samples were also sectioned and analyzed vertically. Together, the various samples were intended to provide an indication of the homogeneity throughout the CCIM with respect to phase assemblage, chemical composition, and chemical durability. Characterization analyses confirmed that a crystalline ceramic with desirable phase assemblage was produced from a melt using a CCIM. Hollandite and zirconolite were identified in addition to possible highly-substituted pyrochlore and perovskite. Minor phases rich in Fe, Al, or Cs were also identified. Remarkably only minor differences were observed vertically or radially in the CCIM material with respect to chemical composition, phase assemblage, and durability. This recent CCIM test and the resulting characterization in conjunction with demonstrated compositional improvements support continuation of CCIM testing with an improved feed composition and improved melter system.

36 MATERIALS SCIENCE↗

Elevated temperature durability of ceramic materials

Fast fracture, stress rupture, and cyclic high temperature durability characterizations have been conducted for advanced silicon carbide and silicon nitride ceramics applicable to gas turbine hot section components. The fast fracture and stress rupture tests were conducted in four-point flexure at temperatures of up to 1540 C; the durability tests involved cycling specimens to temperatures of 1370 C and air quenching at 200 C for up to 3500 hrs. Materials with further reliability improvements are noted to be required for gas turbine hot section component applications.

Lindberg, Laura J.↗

Advanced ceramic material for high temperature turbine tip seals

Forty-one material systems were evaluated for potential use in turbine blade tip seal applications at 1370 C. Both ceramic blade tip inserts and abradable ceramic tip shoes were tested. Hot gas erosion, impact resistance, thermal stability, and dynamic rub performance were the criteria used in rating the various materials. Silicon carbide and silicon nitride were used, both as blade tips and abradables. The blade tip inserts were fabricated by hot pressing while low density and honeycomb abradables were sintered or reaction bonded.

Vogan, J. W.↗

On the sol-gel synthesis and characterization of strontium ferrite ceramic material

Highlights: Black-Right-Pointing-Pointer Successful sol-gel preparation of cubic perovskite SrFeO{sub 3-{xi}} ({xi} {approx} 0.13) with a{sub o} = 3.862 Angstrom-Sign . Black-Right-Pointing-Pointer Reduces to orthorhombic SrFeO{sub 2.5} via Fe{sup 4+} {yields} Fe{sup 3+}conversion with a {approx} a{sub o}{radical}2, b {approx} 4a{sub o}, c {approx} a{sub o}{radical}2. Black-Right-Pointing-Pointer High stability and good oxygen permeation characteristics at 1000 Degree-Sign C. Black-Right-Pointing-Pointer Phase reversibility upon heating in oxygen ambient at elevated temperatures. -- Abstract: A simple oxalate based sol-gel process has been described to produce a highly stable anion deficient strontium ferrite for separation of oxygen from air. The method involves metal nitrates and oxalic acid precursors with ethanol and water as solvents, gel formation, digestion for 4 h, drying at 150 Degree-Sign C for 24 h, and finally decomposition at 800 Degree-Sign C in air. The resulting material (i) exhibits a single perovskite-type cubic (SrFeO{sub 3-{xi}}; {xi} {approx} 0.13) phase with a{sub o} = 3.862 {+-} 0.002 Angstrom-Sign , (ii) contains both the Fe{sup 4+} and Fe{sup 3+} species in 2.8:1 ratio, (iii) undergoes Fe{sup 4+} {yields} Fe{sup 3+} reduction upon heating at 650 Degree-Sign C in rare gas ambient and transition to an orthorhombic phase with a {approx} a{sub o}{radical}2, b {approx} 4a{sub o}, c {approx} a{sub o}{radical}2, which reverts back to cubic phase with oxygen uptake at elevated temperatures, and (iv) acts as filter for air with excellent oxygen permeation, typical flux density value being 2.45 ml/cm{sup 2} min at 1000 Degree-Sign C.

36 MATERIALS SCIENCE↗

Characterization and thermal behavior of PrMO{sub 3} (M = Co or Ni) ceramic materials obtained from gelatin

Graphical abstract: The micrograph in figure shows sample calcined at temperature 900 °C. The sample exhibits morphology with considerable porosity and the formation of agglomerated nanometric particles. Gelatin provides the system with a large amount of organic matter, which is then removed during calcinations, favoring the appearance of pores in the material. Highlights: ► Oxides with PrNiO{sub 3} and PrCoO{sub 3} were prepared by new method synthesis. ► The gelatin, through its carboxylate groups and amine, is an efficient director. ► The obtained materials have magnetic properties and application in catalysis. ► The decomposition kinetic study of bonding groups of gelatin with metallic ions that takes part in the synthesis of PrMO{sub 3}. -- Abstract: Metal oxides with perovskite-type structure have attracted considerable interest in recent years due to their magnetic and electrical properties, as well as their catalytic activity. In this study, oxides with PrNiO{sub 3} and PrCoO{sub 3} composition were prepared by using gelatin powder as a precursor agent for its use as a catalyst. The powders obtained were calcined at 700 °C and 900 °C and characterized using the X-ray diffraction, thermal analysis (thermogravimetry and differential thermal analysis), infrared spectroscopy, temperature programed reduction and scanning electron microscopy techniques. Thermogravimetric data using the non-isothermal kinetic models of Flynn and Wall and “Model-free Kinetics” were used to determine the activation energy to study the decomposition kinetics of the ligand groups with system's metallic ions that takes part in the synthesis of PrMO{sub 3} (M = Ni or Co).

36 MATERIALS SCIENCE↗

Phonon spectroscopy of submicron ceramic materials based on Ce{sub 1-x}Gd{sub x}O{sub 2-y} solid solutions

The specific features of the kinetic characteristics of subterahertz phonons in ceramic samples based on Ce{sub 1-x} Gd{sub x}O{sub 2-y} electrolyte solid solutions have been investigated in the range of liquid-helium temperatures. It has been demonstrated that the observed anomalies of the transport characteristics of thermal phonons in this system are caused by the formation of structural defects associated with the position of vacancies in the anion sublattice with respect to impurity cations. The activation energy of the two-level system {Delta} = 8.53 K has been determined from an analysis of the experimental results.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Chemical and Microstructural Changes in Metallic and Ceramic Materials Exposed to Venusian Surface Conditions

The chemical and microstructural behavior of steels (304, 310, 316, and 1018), nickel-based alloys (beta-NiAl, G30, and 625), gold, coatings (4YSZ, SilcoNert(TradeMark) 1040 (SilcoTek Co.), Dursan(TradeMark) (SilcoTek Co.), and porcelain), and bulk ceramics (alpha-Al2O3, fused quartz, beta-SiC, and alpha-Si3N4) were probed after exposure to supercritical fluid with temperature, pressure, and composition mimicking the Venus lower atmosphere. Exposures were carried out in the Glenn Extreme Environments Rig (GEER) chamber with the Venusian gas mixture (96.5% CO2, 3.5% N2, 30 ppm H2O, 150 ppm SO2, 28 ppm CO, 15 ppm OCS, 3 ppm H2S, 0.5 ppm HCl, and 5 ppb HF) at 92 bar (1330 psi) and 467 C (873 F) for durations of 10 and 42 days. An additional 21-day exposure was done to stainless steel uncoated and coated with SilcoNert(TradeMark) and Dursan(TradeMark). Samples were characterized before and after the experiment by gravimetric analysis, X-ray diffraction, X-ray photoelectron and Auger electron spectroscopies, and cross section electron microscopy analysis. All steels exposed for 10 and 42 days formed double-layered scales consisting mainly of metal (Cr, Fe, Ni) oxides and sulfides showing different chemistry, microstructure, and crystalline phases. The alloys G30 and 625 formed double-layered scales consisting mainly of nickel sulfides. After 10 days, the beta-NiAl exhibited no detectable scale, suggesting only a very thin film was formed. The 304 and 316 stainless steels coated with 4YSZ that were exposed for 10 and 42 days exhibited no significant oxidation. Steel 1018 coated with 4YSZ exhibited a corrosion scale of iron and/or chromium oxide formed at the base of the alloy. The 304 steel coated with porcelain did not exhibit corrosion, although the coating exhibited recession. SilcoNert(TradeMark) exposed for 10 and 42 days exhibited recession, although no oxidation was found to occur at the base of the alloy. Stainless steel 316 coated with Dursan(TradeMark)  exhibited corrosion at the base of the alloy. All ceramics tested showed no clear evidence of reaction. The weight-gain-per-area performance of the materials exposed in the GEER for 10 and 42 days are reported from the lowest to the highest weight gain per area as follows: gold did not exhibit any weight change; nickel-based alloys: beta- NiAl < G30 < 625; steels: 304 < 310 < 316 < 1018; ceramics: considering the experimental uncertainties, no weight change was observed for all ceramics of this work (alpha-Al2O3, Si3N4, SiC, and amorphous SiO2).

Costa, Gustavo C. C.↗

Combined EDS and EBSD dataset from TiB2 ceramic material

This is supplemental information to a paper to be submitted, tentatively titled Cluster analysis of combined EDS and EBSD data to solve ambiguous phase identifications. Data was acquired from a TiB2 ceramic provided by Missouri University of Science and Technology. Simultaneous EDS and EBSD were acquired on a Tescan MIRA3 GMH field-emission SEM equipped with Oxford Instruments Symmetry CMOS-based EBSD detector and Oxford Instruments UltimMax 170 mm2 silicon-drift detector EDS. Data was acquired using Oxford Instruments AZtec 4.0 software. Data was acquired at 20 keV, 70° tilt, and ≈1 nA probe current. An 80×60 pixel, 40×30 μm map (500 nm pixel pitch) was acquired. EBSD indexing was performed using TiB2, space group 191 P6/mmm, and TiC, space group 225 Fm \bar{3}m, crystal cards.

36 MATERIALS SCIENCE↗

Ceramic material suitable for repair of a space vehicle component in a microgravity and vacuum environment, method of making same, and method of repairing a space vehicle component

A precursor of a ceramic adhesive suitable for use in a vacuum, thermal, and microgravity environment. The precursor of the ceramic adhesive includes a silicon-based, preceramic polymer and at least one ceramic powder selected from the group consisting of aluminum oxide, aluminum nitride, boron carbide, boron oxide, boron nitride, hafnium boride, hafnium carbide, hafnium oxide, lithium aluminate, molybdenum silicide, niobium carbide, niobium nitride, silicon boride, silicon carbide, silicon oxide, silicon nitride, tin oxide, tantalum boride, tantalum carbide, tantalum oxide, tantalum nitride, titanium boride, titanium carbide, titanium oxide, titanium nitride, yttrium oxide, zirconium diboride, zirconium carbide, zirconium oxide, and zirconium silicate. Methods of forming the ceramic adhesive and of repairing a substrate in a vacuum and microgravity environment are also disclosed, as is a substrate repaired with the ceramic adhesive.

Riedell, James A.↗

Ceramic material life prediction: A program to translate ANSYS results to CARES/LIFE reliability analysis

This manual describes the use of the ANSCARES program to prepare a neutral file of FEM stress results taken from ANSYS Release 5.0, in the format needed by CARES/LIFE ceramics reliability program. It is intended for use by experienced users of ANSYS and CARES. Knowledge of compiling and linking FORTRAN programs is also required. Maximum use is made of existing routines (from other CARES interface programs and ANSYS routines) to extract the finite element results and prepare the neutral file for input to the reliability analysis. FORTRAN and machine language routines as described are used to read the ANSYS results file. Sub-element stresses are computed and written to a neutral file using FORTRAN subroutines which are nearly identical to those used in the NASCARES (MSC/NASTRAN to CARES) interface.

Vonhermann, Pieter↗