Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “catalyst layers”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 127 records · Page 7

Modeling Planar Electrodes and Zero–Gap Membrane Electrode Assemblies for CO 2 Electrolysis

Multiphysics modeling enables probing of conditions inside a CO 2 electrolyzer that are difficult to measure, such as local concentrations and pH, as well as rapid testing of possible design changes. A one-dimensional model for a zero-gap membrane electrode assembly (MEA) CO 2 electrolyzer was developed with the assumption that catalyst layers interact with the membrane ionomer such that the ionomer affects the underlying kinetics. The kinetics for bicarbonate reacting to form hydrogen are fit using a planar electrode model for silver with an ionomer coating. The MEA model results are validated against experimental studies for current density and product selectivity. Flooding of the cathode is modeled using saturation curves, and results show that blocked pores in the microporous layer play a significant role in limiting the mass transport at high potentials (>2.8 V). Sensitivity studies showed that CO Faradaic efficiency can be increased by decreasing catalyst layer thickness and porosity, and decreasing KHCO 3 concentration.

30 DIRECT ENERGY CONVERSION↗

Durable Thin‐Film Porous Transport Electrodes for High Current Density PEM Water Electrolysis

Proton exchange membrane water electrolyzers rely on relatively expensive Ir-based catalysts for efficient and durable hydrogen production. To reduce system costs, Ir loadings can be reduced if performance and durability are maintained. Sputter deposition is a readily scalable method to synthesize uniform, low-loading catalyst layers with controlled composition. A catalyst applied directly to the porous transport layer can have advantages for performance, manufacturing simplicity, and catalyst recovery. Suitable porous transport layer porosity can minimize activity losses when reducing loadings. Here, methods are presented to deposit metallic Ir as well as amorphous and rutile Ir oxides. The activity and durability of these materials in the porous transport electrode architecture is evaluated. The metallic and amorphous forms have better initial activity, however, operation at 3 A cm −2 with 0.1 mg Ir cm −2 shows that only rutile IrO 2 maintains performance beyond 100 h with a 50 mV improvement after 700 h. A >10x reduced dissolution rate is shown for rutile IrO 2 . With a low-porosity transport layer and 0.4 mg Ir cm −2 , a steady-state voltage decay rate of 6 µV h −1 is achieved. The results demonstrate that sputter-deposited rutile IrO 2 porous transport electrodes with low Ir loading can be operated at high current density to reduce hydrogen production costs.

08 HYDROGEN↗

Pt Nanoparticles on Atomic-Metal-Rich Carbon for Heavy-Duty Fuel Cell Catalysts: Durability Enhancement and Degradation Behavior in Membrane Electrode Assemblies

Proton exchange membrane fuel cells (PEMFCs) are a promising zero-emission power source for heavy-duty vehicles (HDVs). However, long-term durability of up to 25,000 h is challenging because current carbon support, catalyst, membrane, and ionomer developed for traditional light-duty vehicles cannot meet the stringent requirement. Therefore, understanding catalyst degradation mechanisms under the HDV condition is crucial for rationally designing highly active and durable platinum group metal (PGM) catalysts for high-performance membrane electrode assemblies (MEAs). Herein, we report a PGM catalyst consisting of platinum nanoparticles with a high content (40 wt %) on atomic-metal-site (e.g., MnN 4 )-rich carbon support. MEAs with the Pt (40 wt %)/Mn–N–C cathode catalyst achieved significantly enhanced performance and durability, generating 1.41 A cm –2 at 0.7 V under HDV conditions (0.25 mgPt cm –2 and 250 kPa abs pressure) and retaining 1.20 A cm –2 after an extended and accelerated stress test up to 150,000 voltage cycles. Electron microscopy studies indicate that most fine Pt nanoparticles are retained on or/and in the carbon support covered with the ionomer throughout the catalyst layer at the end of life. During the long-term stability test, the observed electrochemical active surface area reduction and performance loss primarily result from Pt depletion in the catalyst layer due to Pt dissolution and redeposition at the interface of the cathode and membrane. Importantly, the first-principle density functional theory calculations further reveal a support entrapment effect of the Mn–N–C, in which the MnN 4 site can specifically adsorb the Pt atom and further retard the Pt dissolution and migration, therefore enhancing long-term MEA durability.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

High-Current Density Durability of Pt/C and PtCo/C Catalysts at Similar Particle Sizes in PEMFCs

The durability of carbon supported PtCo-alloy based nanoparticle catalysts play a key role in the longevity of proton-exchange membrane fuel cells (PEMFC) in electric vehicle applications. To improve its durability, it is important to understand and mitigate the various factors that cause PtCo-based cathode catalyst layers (CCL) to lose performance over time. These factors include i) electrochemical surface area (ECSA) loss, ii) specific activity loss, iii) H + /O 2 -transport changes and iv) Co 2+ contamination effects. We use a catalyst-specific accelerated stress test (AST) voltage cycling protocol to compare the durability of Pt and PtCo catalysts at similar average nanoparticle size and distribution. Our studies indicate that while Pt and PtCo nanoparticle catalysts suffer from similar magnitudes of electrochemical surface area (ECSA) losses, PtCo catalyst shows a significantly larger cell voltage loss at high current densities upon durability testing. The distinctive factor causing the large cell voltage loss of PtCo catalyst appears to be the secondary effects of the leached Co 2+ cations that contaminate the electrode ionomer. A 1D performance model has been used to quantify the cell voltage losses arising from various factors causing degradation of the membrane electrode assembly (MEA).

08 HYDROGEN↗

Optimizing feed modulation for coupled methane and NO x conversion over Pd-Pt/Mn 0.5 Fe 2.5 O 4 /Al 2 O 3 monolith catalyst

Here the impacts of feed modulation (frequency, amplitude) and catalyst design (composition and architecture) parameters are reported for the conversion of methane and NO x over a dual-layer Pt+Pd/Al 2 O 3 + Mn 0.5 Fe 2.5 O 4 /Al 2 O 3 monolith. CH 4 and NO x conversion data show that the dual-layer catalyst outperforms single-layer samples having the same catalyst loadings, with and without spinel. Close proximity of the PGM and MFO functions in the mixed-layer catalyst lowers the CH 4 conversion at high temperature while separating the PGM and spinel layers with an intermediate Al 2 O 3 layer does not. Methane conversion enhancement is linked to its nonmonotonic dependence on O 2 . The performance gains are tied to a transient activity spike that occurs during the lean-to-rich feed transition when water is present in the feed. The transient spike is attributed to the removal of CO and H 2 products via reactions with stored O 2 in the spinel, eliminating inhibition of methane steam reforming.

03 NATURAL GAS↗

Influence of Pt-Metal Alloy Catalysts with Various Ionomers on Oxygen Reduction Reaction in Fuel Cell Application

Pt-M/C (M = Co, Ni, Mn, etc.) alloy catalysts exhibit superior oxygen reduction reaction (ORR) activity compared to pure Pt/C, leading to a high energy efficiency in hydrogen fuel cells. However, many Pt-M/C alloy catalysts were synthesized and evaluated at the lab scale in model test-bed systems like rotating disc electrodes, which don't always correlate to performance within a fuel cell system; there is a clear need to evaluate catalysts in electrodes that can be prepared at industrially relevant scales to evaluate how factors like ink formulation can greatly affect device-level of fuel cell performance. Herein, three commercial Pt-M/C alloy catalysts (two Pt-Co/C and one Pt-Ni/C) were comprehensively characterized by various techniques. The results show that the average particle sizes of the three catalysts are close to 5 nm; the atomic ratio of Pt/M is around 4; and the M was successfully embedded into Pt lattice, resulting in the positive shift of Pt 4f in XPS spectra and XRD patterns. These catalytic materials were incorporated into 9 different cathode catalyst layers (CCLs) with three kinds of ionomers (Nafion D2020, high oxygen permeability ionomer (HOPI), and Aquivion D79-25BS), and their performance in proton exchange membrane fuel cells (PEMFCs) were investigated. The results demonstrate that the Pt-Co/C catalysts possess a higher mass activity (MA) than Pt-Ni/C; the cathodes with Nafion ionomer provide the highest MA while electrodes with Aquivion ionomer showed the lowest activity, attributed to poor H+ conductivity resulting from suboptimal ionomer incorporation. Finally, these alloys were shown to exceed DOE targets for MA and H2/Air performance reported in the recent publications at beginning of life and after 90k cycle catalyst AST protocol. This study provides valuable performance benchmarks for these materials guiding future Pt-M/C catalyst design and material integration for heavy duty PEMFC applications.

08 HYDROGEN↗

Regulating catalyst and ionomer interactions to promote oxygen transport in fuel cells

The cost of proton exchange membrane fuel cells (PEMFCs) has been a major impediment to their widespread commercialization. Reducing platinum (Pt) usage in PEMFC represents an essential step in lowering the cost. However, decreasing Pt loading in the cathode catalyst layer (CCL) often leads to a significant increase in the local oxygen transport resistance (R Local ), which not only slows the oxygen reduction reaction but also causes a higher polarization overpotential. The poisoning of Pt by perfluorosulfonic acid ionomers also becomes more predominant at low Pt loadings. Therefore, regulating catalyst and ionomer interactions by optimizing their interface in the CCL is crucial to improving PEMFC performance. Here, in this review, the strategies of improving oxygen transport by controlling Pt-ionomer interactions and interfaces through catalyst design, ionomer structure, and incorporation of additives are summarized. Finally, perspectives on future optimization of catalyst and ionomer interactions are proposed.

25 ENERGY STORAGE↗

Oxygen Reduction on Platinum-Nickel and Platinum-Cobalt Alloy Based Catalysts for High Temperature Proton Exchange Membrane Fuel Cells

Catalyst layers, with commercial PtNi/TKK (TECNiE52; platinum 46.5 wt%), PtCo/TKK (TEC36E52; platinum 45.8 wt%) catalysts, and an in-house catalyst PtNi-NC (platinum 38.4 wt%), synthesised using acoustic mixer and a tube furnace, are prepared using three different ionomers: 20 wt% Nafion®, 60 wt% polytetrafluoroethylene (PTFE), and an in-house 5 wt% ionomer (‘Ionomer X’). These inks are bar-coated onto carbon paper gas diffusion layers (GDLs), which are cut into 3 cm × 5 cm pieces. The coated layers are tested for oxygen reduction in a commercial gas diffusion electrode (GDE) test cell, FlexCell® (Gaskatel GmbH, Germany), using 85 wt% phosphoric acid at both room temperature and at 155°C. This study evaluates the polynorbornene (PNB)-based in-house ionomer performance as binder and in-house catalyst oxygen reduction reaction (ORR) activity in comparison to commercial products. The catalyst layers are characterised using X-ray diffraction (XRD) analysis, X-ray photoelectron spectroscopy (XPS), and high-angle annular dark-field scanning transmission electron microscopy (HAADF-STEM). Among the catalyst layers prepared with PTFE ionomer and tested at 155°C, the in-house catalyst demonstrates the highest ORR activity. Ionomer X proves to be a good candidate to be used as a per- and polyfluoroalkyl-free binder for high-temperature (HT) proton exchange membrane fuel cell (PEMFC) applications.

85 wt% phosphoric acid↗

Application of a temporal multiscale method for efficient simulation of degradation in PEM Water Electrolysis under dynamic operating conditions

Hydrogen is emerging as a vital energy carrier, driven by the need to reduce carbon emissions. Proton Electrolyte Membrane Water Electrolysis (PEMWE) enables hydrogen production under fluctuating renewable power conditions but requires improved understanding and stability of the anode catalyst layer under dynamic operating conditions, especially with low noble metal loadings. Long-term degradation experiments are both time-consuming and costly; therefore, a systematic, model-aided approach is essential. In the present work, a temporal multiscale method is applied to reduce the computational effort of simulating long-term degradation processes in PEMWE, with an exemplary focus on catalyst dissolution. A mechanistic model incorporating the oxygen evolution reaction, catalyst dissolution, and hydrogen permeation from the cathode to the anode was hypothesized and implemented. In this way, the local periodicity of transport and reaction processes in dynamic PEMWE operation, which influence the gradual degradation of the catalyst layer, is captured. The temporal multiscale method significantly reduces the computational effort of simulation, decreasing processing time from hours to mere minutes. This efficiency gain is attributed to the limited evolution of Slow-Scale variables during each period of time P of the Fast-Scale variables. Consequently, simulation is required only until local periodicity is achieved within each Slow-Scale time step. Hence, the fully resolved dynamic problem is decoupled into these two scales, employing a heterogeneous multiscale technique. The developed approach effectively accelerates parameter estimation and predictive simulations, supporting systematic modeling of PEMWE degradation under dynamic conditions.

08 HYDROGEN↗

Intermediate Sr 2 Co 1.5 Fe 0.5 O 6-δ Tetragonal Structure between Perovskite and Brownmillerite as a Model Catalyst with Layered Oxygen Deficiency for Enhanced Electrochemical Water Oxidation

The generation of hydrogen in an environmentally benign way is highly essential to meet future energy demands. However, in the process of splitting water electrochemically, sluggish kinetics of the oxygen evolution reaction (OER) curtails its applicability, as it drags energy input. Herein, we synthesized SrCo-Fe-O oxides to optimize their OER activity by varying the Co/Fe ratio. Among them, Sr 2 Co 1.5 Fe 0.5 O 6-δ exhibited the best OER catalytic activity in the series, with an overpotential of 318 mV at 10 mA cm -2 and Tafel slope of 44.8 mV dec -1 . High-resolution neutron powder diffraction analysis identified an intermediate structure between the perovskite and brownmillerite, with alternating layers of disorderly orientated oxygen-deficient tetrahedra and fully stoichiometric octahedra. The unique stacking of tetrahedral and octahedral units facilitates desired interactions between the electrode surface and electrolyte. Theoretical calculations revealed that increased covalency of Co 3d and O 2p in Sr 2 Co 1.5 Fe 0.5 O 6-δ oxide is another primary contributor to its augmented water oxidation ability. As a model for developing catalysts with such an intermediate structure, the synergetic effect of oxygen vacancy and hybridization between Co 3d and O 2p assured the Sr 2 Co 1.5 Fe 0.5 O 6-δ oxide as a better catalyst for its enhanced OER activity.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Revealing in-plane movement of platinum in polymer electrolyte fuel cells after heavy-duty vehicle lifetime

Fuel cell heavy-duty vehicles (HDVs) require increased durability of oxygen-reduction-reaction electrocatalysts, making knowledge of realistic degradation mechanisms critical. Here identical-location micro-X-ray fluorescence spectroscopy was performed on membrane electrode assemblies. The results exposed heavy in-plane movement of electrocatalyst after HDV lifetime, suggesting that electrochemical Ostwald ripening may not be a local effect. Development of local loading hotspots and preferential movement of electrocatalyst away from cathode catalyst layer cracks was observed. The heterogeneous degradation exhibited by a modified cathode gas diffusion layer membrane electrode assembly after HDV lifetime was successfully quantified by the identical-location approach. Further synchrotron micro-X-ray diffraction and micro-X-ray fluorescence experiments were performed to obtain the currently unknown correlation between electrocatalyst nanoparticle size increase and loading change. A direct correlation was discovered which developed only after HDV lifetime. Finally, the work provides a route to engineer immediate system-level mitigation strategies and to develop structured cathode catalyst layers with durable electrocatalysts.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Editors’ Choice—Ionomer Side Chain Length and Equivalent Weight Impact on High Current Density Transport Resistances in PEMFC Cathodes

Cell voltage at high current densities (HCD) of an operating proton-exchange membrane fuel cell (PEMFC) suffers from losses due to the local-O 2 and bulk-H + transport resistances in the cathode catalyst layer (CCL). Particularly, the interaction of perfluorosulfonic acid (PFSA) ionomer with the carbon supported platinum catalyst plays a critical role in controlling reactant transport to the active site. In this study, we perform a systematic analysis of the side chain length and equivalent weight (EW) of PFSA ionomers on the CCL transport resistances. Ex situ measurements were carried out to quantify the ionomer characteristics such as the molecular weight, proton conductivity and water uptake. Nanomorphology of ionomers cast as 60–120 nm thin-films is characterized using grazing-incidence X-ray scattering. In situ fuel cell electrochemical diagnostic measurements were carried out to quantify the reactant (H + /O 2 ) transport properties of the CCL. Ionomer EW was found to play a major role with decreasing EW yielding higher proton conductivity and water uptake that led to lower bulk-H + and local-O 2 transport resistances in the CCL. Finally, a 1D-semi-empirical performance model has been developed to quantify the impact of ionomer EW on cell voltage loss factors.

08 HYDROGEN↗

Understanding Platinum Ionomer Interface Properties of Polymer Electrolyte Fuel Cells

A well-designed cathode catalyst layer with optimal ionomer distribution is critical to minimizing amount of Platinum (Pt) content in polymer electrolyte fuel cells (PEFCs). The impact of Pt loading, ionomer content and carbon support types on the catalyst/ionomer interface were also investigated at dry and wet conditions. Higher Pt loadings resulted in higher double layer capacity (C dl ) and similar electrochemical surface area (ECSA) due to well dispersed ionic phase material. Higher ionomer content resulted in higher ionic conductivity but also showed similar SO 3 − group coverage. High surface area (HSA) carbon support had larger ECSA and C dl at both dry and wet conditions, as less agglomerated Pt was well dispersed in the meso-pores of the support. Lower SO 3 − group coverages were observed for HSA carbon than for Vulcan carbon due to Pt particles being buried within the porous HSA carbon support. The effect of cell conditioning and voltage recovery on the PEFC cathode catalyst layer was shown to have minimal impact on SO 3 − group coverage despite a decrease in C dl and ECSA due to the size increase of Pt particles. At dry condition, a significant increases in SO 3 − group coverage were observed for all MEAs due to higher adsorptivity of ionomer in dry conditions.

25 ENERGY STORAGE↗

High Performance non-PGM Transition Metal Oxide ORR Catalysts of PEMFCs

This project was designed to develop acid-stable PGM-free transition metal oxide oxygen reduction reaction (ORR) electrocatalysts to meet or exceed the performance and durability of the DOE 2020 Technical Targets for platinum-group metal (PGM) free electrocatalysts from first-principles to incorporation into membrane-electrode assemblies (MEAs) for polymer electrolyte membrane (PEM) fuel cells. The planned project was to accomplish this goal with a multi-step approach: 1) materials modeling and experimental screening to identify acid-stable oxides with high ORR activity, 2) optimization of catalyst particle size and catalyst/carbon/ionomer catalyst layer composition, 3) fabrication of MEAs for performance and durability testing. During the course of this project: 1) acid-stability descriptors were developed for manganese oxides; 2) a family of acid-stable multicomponent oxides based on antimony were developed; 3) a flexible synthesis for the formation of nanocrystalline nonstoichiometric oxides was developed; 4) limited ORR activity but modest and improving oxygen evolution reaction (OER) activity was measured for multicomponent antimony oxides. The project was programmed into five technical tasks: The development of acid-stable ORR electrocatalytic oxides through 1) identification and optimization of acid-stable oxide compositions, and 2) electrochemical characterization; 3) optimization of catalyst layer composition for MEAs using identified ORR electrocatalysts; 4) MEA fabrication and performance testing to result in performance of 44 mA-cm-2 at 0.9 V vs. RHE; and 5) accelerated-stress testing of optimized MEAs. Because no acid-stable oxide was identified with the requisite activity for ORR (4.4 µA-cm-2oxide intrinsic activity at 0.9 V vs. RHE) within the time and budget allotted in Tasks 1 and 2, the project was halted at the end of phase 1, with no activity in Tasks 3-5. The research output, while not succeeding in developing ORR electrocatalysts, advanced the development of acid-stable oxide materials, showing potential for further improvement as OER electrocatalysts.

08 HYDROGEN↗

Membrane Degradation in PEM Fuel Cells: Part I. Modeling Gas Crossover and the Pt Band

Understanding chemical degradation of the proton-exchange membrane in fuel cells is crucial for extending their lifetimes. Herein, various degradation reactions reported in literature are organized and analyzed, including direct radical generation and an indirect (Fenton) pathway. To understand the transport of dissolved H 2 and O 2 crossover gases as they relate to membrane degradation, an agglomerate-scale model is introduced, treating gas, ionomer, and catalyst as discrete phases. The model reveals a key phenomenon: at working potentials, dissolved gases are mostly consumed at the interface between the catalyst layer and the membrane, leaving little gas to cross the membrane. Under open-circuit conditions, dissolved gases are not consumed and can then cross the membrane. This explains high H 2 O 2 concentrations and degradation rates seen in experiments but not captured in previous models. Following mixed-potential theory, crossover gases supply the hydrogen-oxidation and oxygen-reduction reactions, which occur simultaneously on individual Pt particles comprising the Pt band in the membrane, forming reactive species (H 2 O 2 , OH·). Results show crossover gas almost entirely reacts on the Pt band, allowing little to reach the opposite electrode. Furthermore, the micro-scale geometry of the catalyst-layer/membrane interface impacts the gas crossover at working potentials, indicating that cell construction affects membrane durability.

Johnson, Evan F. [Lawrence Berkeley National Labor↗

Aging gracefully? Investigating iridium oxide ink's impact on microstructure, catalyst/ionomer interface, and PEMWE performance

Here, in this study, we conducted a thorough investigation of the impact of aging iridium oxide (IrO 2 ) perfluorosulfonic acid ionomer ink for up to 14 days on the properties of the ink and the resulting catalyst layers. We examined ink properties, such as zeta potential, dynamic light scattering (DLS), density, surface tension, and rheology, as functions of ink aging time. To evaluate the microstructure and catalyst/ionomer interface, we employed transmission electron microscopy (TEM), X-ray scattering, and X-ray photoelectron spectroscopy (XPS) techniques. Furthermore, we assessed the effect of ink aging on the performance of proton exchange membrane water electrolyzers (PEMWEs). Our findings reveal that most ink properties remain stable for 14 days. The variations in PEMWE cell performance are minimal, and no clear trend is observed in relation to ink aging time. This study demonstrates that the effects of aging the inks for 14 days on ink properties, catalyst layer structure, catalyst/ionomer interface, and PEMWE performance are negligible, indicating a substantial time window after ink preparation without any significant changes in its properties. These insights provide crucial guidance for the commercial production and coating processes of ink, which is necessary for scaling up PEM technologies to meet future demand.

30 DIRECT ENERGY CONVERSION↗

A Direct Ammonia Fuel Cell with a KOH-Free Anode Feed Generating 180 mW cm −2 at 120 °C

The motivations to operate the direct ammonia fuel cell (DAFC) with no addition of aqueous base, include facilitated fuel management and prevention of corrosion and shunt currents in the DAFC stack. We describe here a polymer electrolyte DAFC, operating at a cell temperature (T cell ) of 120 °C on ammonia and water alone as anode feed, that demonstrated peak power of 180 mW cm −2 —a record for this type of fuel cell. We offer a detailed analysis of polarization curves recorded for PE-DAFCs in the T cell range of 60 °C–120 °C, allowing to estimate the effects of KOH-free operation on the ionic and faradaic resistances, R i and R F , that determine together the value of R app , CL – an , the apparent resistance of the anode catalyst layer. The latter resistance drops ten times between 60 °C and 120 °C as result mainly of the drop in R F . Consequently, DAFC performance at T cell > 100 °C improves substantially, including the cell performance on a KOH-free anode feed. The demsontrated performance levels reported here for KOH-free DAFCs support further development of this type of ammonia/air fuel cells.

Achrai, Ben↗