Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “ZnSe”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 127 records · Page 7

Band Anticrossing in Highly Mismatched Compound Semiconductor Alloys

Compound semiconductor alloys in which metallic anions are partially replaced with more electronegative isoelectronic atoms have recently attracted significant attention. Group IIIN(sub x)V(sub 1-x) alloys with a small amount of the electronegative N substituting more metallic column V elements has been the most extensively studied class of such Highly Mismatched Alloys (HMAs). We have shown that many of the unusual properties of the IIIN(sub x)V(sub 1-x) alloys can be well explained by the Band Anticrossing (BAC) model that describes the electronic structure in terms of an interaction between highly localized levels of substitutional N and the extended states of the host semiconductor matrix. Most recently the BAC model has been also used to explain similar modifications of the electronic band structure observed in Te-rich ZnS(sub x)Te(sub 1-x) and ZnSe(sub y)Te(sub 1-y) alloys. To date studies of HMAs have been limited to materials with relatively small concentrations of highly electronegative atoms. Here we report investigations of the electronic structure of ZnSe(sub y)Te(sub 1-y) alloys in the entire composition range, y between 0 and 1. The samples used in this study are bulk ZnSe(sub y)Te(sub 1-y) crystals grown by either a modified Bridgman method or by physical vapor transport. Photomodulated reflection (PR) spectroscopy was used to measure the composition dependence of optical transitions from the valence band edge and from the spin-orbit split off band to the conduction band. The pressure dependence of the band gap was measured using optical absorption in a diamond anvil cell. We find that the energy of the spin-orbit split off valence band edge does not depend on composition and is located at about 3 eV below the conduction band edge of ZnSe. On the Te-rich side the pressure and the composition dependence of the optical transitions are well explained by the BAC model which describes the downward shift of the conduction band edge in terms of the interaction between localized Se states and the conduction band. On the other hand we show that the large band gap reduction observed on the Se-rich side of the alloy system is a result of an interaction between the localized Te level and the valence bands. This interaction leads to the formation of a Te-like valence band edge that strongly interacts with the light hole valence band. Calculations based on a modified k(sup dot)p model account for the reduction of the band gap and the large increase of the spin-orbit splitting observed in Se-rich ZnSe(sub y)Te(sub 1-y) alloys. We will also discuss the importance of these new results for understanding of the electronic structure and band offsets in other highly mismatched alloy systems.

Yu, Kin Man↗

Morphology and Luminescence Properties of Transition Metal Doped Zinc Selenide Crystals

Zinc selenide is an excellent matrix material to dope with rare-earth and transition metal to achieve mid-infrared luminescence to develop high power lasers. The luminescence, morphology and refractive index is significantly affected by the doping and defects generated due to size and valency of dopants, concentration, growth process and convection during the growth. The aim of the study is to investigate effect of point and line defects generated due to low doping of iron and chromium on the emission and morphology of the zinc selenide. Luminescence and morphological properties of large iron and chromium doped zinc selenide single crystals were studied to evaluate the effect of extremely low residual impurities and defects associated with the doping process. The emission properties following both short wavelength (i.e., ultraviolet; 350 – 370 nm) excitation and longer wavelength (i.e., near infrared; 850 – 870 nm) excitation were characterized. Luminescence emission bands were identified in both doped crystals. In addition to the primary emission bands, satellite peaks and intra-center transitions were also observed. Due to local population defects associated with the residual impurities (ppm to ppb) in the Fe-ZnSe and Cr-ZnSe crystals, peak emission wavelengths were observed to shift. Raman studies using 266 and 532 – nm excitation revealed different positions of longitudinal and transverse peaks for Fe-ZnSe and Cr-ZnSe crystals, associated with different levels of defects due to the different ion sizes. The emission bands were found to decrease in intensity due to recombination of residual impurity co-dopants and complex defects generated during growth and fabrication. Cryogenic temperature analyses revealed a very clean emission band due to freezing of some of the point and line defects. An emission band observed at 980 nm for both crystals at room temperature as well as cryogenic temperatures indicates a vibronic peak in ZnSe. The scanning electron microscopy (SEM) images of the local morphology support the conclusion that small crystallites in doped crystals are also present.

Zinc selenide↗

The criteria in above-bandgap photo-irradiation in molecular beam epitaxy growth of heterostructure of dissimilar growth temperature

Above-bandgap photo-irradiation is known to improve the low temperature growth of II-VI semiconductors, but the trade-offs in the substrate temperature and light source power density are not well known. We investigated these effects on the growth of ZnSe epilayers on GaAs. Here, we find that the above-bandgap photo-irradiation can improve the ZnSe epilayer without substantially negatively impacting the underlying GaAs epilayer only if the laser energy is below a threshold intensity. When the threshold is exceeded, the growth rate drops, the optical properties of ZnSe layer deteriorate and interface intermixing is enhanced. Together, cross-sectional transmission electron microscopy, energy dispersive spectroscopy and photoluminescence results suggest that photo-irradiation at moderate to high laser energies produces a trade-off in interface intermixing and planar defect formation. Most importantly, the damage produced by high laser energies does not start at the interface but instead in the bulk. Further flexibility for selecting the temperature and photo-irradiation intensities could be realized by turning on the laser irradiation after the ZnSe growth has been initiated, limiting the potential intermixing at the interface.

36 MATERIALS SCIENCE↗

Auger Dynamics in InP/ZnSe/ZnS Quantum Dots Having Pure and Doped Shells

In this study, we report the negative trion and biexciton Auger dynamics in very high-quality InP/ZnSe/ZnS quantum dots (QDs) having varying amounts of indium-based traps in the ZnSe shell. Negative trion times are determined by time-correlated photon-counting measurements on QDs that have been photoreduced with lithium triethylborohydride. We find that the Auger times vary from 280 to 425 ps and scale linearly with the total particle volume. Excess indium in the ZnSe shell gives rise to hole traps that are transiently populated following photoexcitation. Comparing stoichiometric and nonstoichiometric particles, we find that the negative trion lifetimes are independent of the presence of indium in the ZnSe shell. Biexciton dynamics are determined from transient absorption (TA) bleach recovery measurements. Absorption of two photons results in the formation of two types of biexcitons: those having both holes in the InP core (XX state) and those having one hole trapped in the ZnSe shell (XT state). XX state Auger times are measured in stoichiometric QDs, and for these particles, the Auger times are ~80 ps. Nonstoichiometric QDs show an additional long TA decay component, assigned to Auger recombination of the XT state. Here, a previous study (J. Phys. Chem. C 2021, 125, 4110–4118) found that hole trapping at indium-based shell traps results in a slow photoluminescence (PL) rise component. We find that the fraction of the XT state formed by the absorption of two photons correlates with the product of the fraction of slow PL rise and the rise time constant following one-photon excitation.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Photocatalytic Semiconductor–Metal Hybrid Nanoparticles: Single-Atom Catalyst Regime Surpasses Metal Tips

Semiconductor–metal hybrid nanoparticles (HNPs) are promising materials for photocatalytic applications, such as water splitting for green hydrogen generation. While most studies have focused on Cd containing HNPs, the realization of actual applications will require environmentally compatible systems. Using heavy-metal free ZnSe-Au HNPs as a model, we investigate the dependence of their functionality and efficiency on the cocatalyst metal domain characteristics ranging from the single-atom catalyst (SAC) regime to metal-tipped systems. The SAC regime was achieved via the deposition of individual atomic cocatalysts on the semiconductor nanocrystals in solution. Utilizing a combination of electron microscopy, X-ray absorption spectroscopy, and X-ray photoelectron spectroscopy, we established the presence of single Au atoms on the ZnSe nanorod surface. Upon increased Au concentration, this transitions to metal tip growth. Photocatalytic hydrogen generation measurements reveal a strong dependence on the cocatalyst loading with a sharp response maximum in the SAC regime. Ultrafast dynamics studies show similar electron decay kinetics for the pristine ZnSe nanorods and the ZnSe-Au HNPs in either SAC or tipped systems. This indicates that electron transfer is not the rate-limiting step for the photocatalytic process. Combined with the structural-chemical characterization, we conclude that the enhanced photocatalytic activity is due to the higher reactivity of the single-atom sites. This holistic view establishes the significance of SAC-HNPs, setting the stage for designing efficient and sustainable heavy-metal-free photocatalyst nanoparticles for numerous applications.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Nitrogen p-type doping in polycrystalline zinc selenide telluride films

Nitrogen-doped zinc selenide telluride (N:ZnSe x Te 1−x ) is of interest because it is one of the widest-gap II–VI semiconductors that can still be doped p-type with reasonably high hole concentrations. We sputter deposit N:ZnSe x Te 1−x films, varying Se/(Se + Te), or x, from 0 to 0.7, N 2 flow rate from 0.25 to 0.75 sccm, and substrate temperature from 250 to 370 °C. Increasing x from 0 to 0.39 at the optimal temperature of 370 °C and N 2 flow rate of 0.5 sccm leads to 1.3 atomic % nitrogen incorporation and wurtzite phase stabilization. Such doping and alloying increases hole concentration from 3 × 10 18 cm −3 to 3 × 10 19 cm −3 , although mobility drops from 0.4 to 0.02 cm 2 V −1 s −1 . Our sputtered N:ZnSe 0.38 Te 0.62 has an absorption onset 0.1 eV greater than the ZnTe value of 1.87 eV. Increasing x from 0 to 0.51 enhances transmittance by moving absorption onset from 1.87 to 2.11 eV with diminished band gap bowing likely due to disorder, and increases the work function from 5.12 to 5.42 eV. This combination of tunable properties makes sputtered N:ZnSe x Te 1−x desirable for transparent p-type contacts in polycrystalline Cd(Se,Te) optoelectronic devices.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Optical Characterization of Bulk ZnSeTe Solid Solutions

Optical characterization was performed on wafers sliced from crystals of ZnSe, ZnTe and ZnSe (sub 1-x) Te (sub x) (0 less than x less than 0.4) grown by physical vapor transport technique. The energy band gaps at room temperature were determined from optical transmission measurements on 11 wafers. The best fit to the band gap vs. composition, x, data gives a bowing parameter of 1.336 which is between the value of 1.23 determined previously on ZnSeTe bulk crystals by reflectivity and the value of 1.621 reported on epilayers by photoconductivity. Low-temperature photoluminescence (PL) spectra were measured on 6 samples. The spectra of ZnSe and ZnTe were dominated by near band edge emissions and no deep donor-acceptor pairs were observed. The PL spectrum exhibited a broad emission for each of the ZnSe (sub 1-x) Te (sub x) samples, 0.09 less than x less than 0.39. For x = 0.09, this emission energy is about 0.2eV lower than the band gap energy measured at low temperature. As x increases the energy discrepancy gradually decreases and reduces to almost zero at x = 0.4. The single broad PL emission spectra and the spectra measured as a function of temperature were interpreted to be associated with the exciton bound to Te clusters because of the high Te content in these samples.

Su, Ching-Hua↗

Optical Characterization of Bulk ZnSeTe Solid Solutions

Optical characterization was performed on wafers sliced from crystals of ZnSe, ZnTe, and ZnSe(1-x)Te(x)(0 less than x less than 0.4) grown by physical vapor transport. Energy band gaps at room temperature were determined from optical transmission measurements on 11 wafers. A best fit curve to the band gap versus composition x data gives a bowing parameter of 1.45. This number lies between the value of 1.23 determined previously on ZnSeTe bulk crystals and the value of 1.621 reported on ZnSeTe epilayers. Low-temperature photoluminescence (PL) spectra were measured on six samples. The spectra of ZnSe and ZnTe were dominated by near band edge emissions and no deep donor-acceptor pairs were observed. The PL spectrum exhibited a broad emission for each of the ZnSe(1-x)Te(x) samples, 0.09 less than x less than 0.39. For x=0.09, this emission energy is about 0.2 eV lower than the band gap energy measured at low temperature. As x increases the energy discrepancy gradually decreases and reduces to almost zero at x=0.4. The single broad PL emission spectra and the spectra measured as a function of temperature were interpreted as being associated with the exciton bound to Te clusters because of the high Te content in these samples.

Su, Ching-Hua↗

The Crystal Structure of BaZn 2 Se 2 (OH) 2 Featuring Brownmillerite‐Type Layers

Abstract A bimetallic hydroxychalcogenide, BaZn 2 Se 2 (OH) 2 , was synthesized through hydrothermal pouch methods. The single crystal X‐ray diffraction and electron diffraction indicates that the phase crystallizes in the orthorhombic space group Pnma and is composed of anionic layers [ZnSe 3/3 (OH) 1/1 ] − that are separated and charged balanced by Ba 2+ cations. The [ZnSe 3/3 (OH) 1/1 ] – layer comprises two unique Zn sites, which form interpenetrating zigzag chains with an in‐plane dipole moment and adopts a brownmillerite‐type structural motif. The adjacent layers contain tetrahedrally coordinated Zn chains of opposite handedness related by an inversion center, which cancel the microscopic dipoles to minimize the macroscopic electric polarization. The adoption of a brownmillerite structural motif in BaZn 2 Se 2 (OH) 2 can be rationalized by the distinct charge difference between Se 2− and OH − anions, which creates a sufficient dipole moment in the ZnSe 3 (OH) tetrahedra to allow the occurrence of twisted chains. FTIR spectroscopy confirms the existence of OH − anions and DFT calculations indicate that BaZn 2 Se 2 (OH) 2 is a semiconductor with a direct band gap. This work expands the chemistry of the brownmillerite family from traditional homoanionic oxides to multianion hydroxychalcogenides, offering a new opportunity to explore tunable structural complexity for better design of functional materials.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Polytypic Zn–(In,Ga)–Se Nanocrystals with Tunable Emission

While the polymorphism of chalcopyrite semiconductors has been widely studied, the wurtzite analogues of defect-chalcopyrite II–III 2 –VI 4 compositions, such as Zn(In,Ga) 2 (S,Se) 4 , remain underexplored. Here, we report the synthesis of polytypic Zn–(In,Ga)–Se multipods via cation exchange using ZnSe as a template. With cubic cores and wurtzite arms elongated along the hexagonal c-axis, the multipods retain the structure and morphology of the ZnSe template. Optical characterization reveals composition-dependent absorption and photoluminescence, tunable from the visible to the near-infrared region, with spectral features distinct from those of previously reported defect-chalcopyrite structures. Temperature-dependent measurements demonstrate strong emission at cryogenic temperatures, which is quenched near room temperature due to thermally activated nonradiative processes. Here, we illustrate the use of ZnSe as a platform for cation exchange toward wurtzite multinary chalcogenides, unlocking access to novel structures with colorful optical properties.

cation exchange↗

Impact of window temperature variations on ITER toroidal interferometer and polarimeter (TIP) measurements

Abstract The toroidal interferometer and polarimeter (TIP) is one of the primary electron density diagnostics on ITER. To meet measurement requirements over several thousand seconds, environmental factors such as changes in the window temperature, air temperature, and humidity, which can cause uncompensated phase drifts, must be minimized. This paper reports measurements of the phase shift induced by ZnSe and BaF₂ windows as their temperature is varied utilizing the TIP prototype. To accomplish these measurements, test pieces of BaF₂ and ZnSe are placed in a small oven that is located in one leg of the 10.59/5.22 micron two-color interferometer TIP prototype. The oven temperature was varied from room temperature to ∼90 °C, which is slightly higher than the expected window temperatures on ITER. The vibration compensated phase shifts measured for these two materials are dϕᵥ꜀ /dT/L = 0.0121 and −0.275 deg. /°C/cm −1 for BaF₂ and ZnSe, respectively. From these measurements, it was concluded that temperature variations of the environmental/secondary confinement barrier window and primary vacuum window have to be suppressed within approximately 1°C and 2°C, respectively, in order to passively meet the electron density measurement requirements in ITER.

Akiyama, T (ORCID:0000000198469795)↗

Diamondlike carbon protective coatings for optical windows

Diamondlike carbon (DLC) films were deposited on infrared transmitting optical windows and were evaluated as protective coatings for these windows exposed to particle and rain erosion. The DLC films were deposited on zinc selenide (ZnSe) and zinc sulfide (ZnS) by three different ion beam methods: (1) sputter deposition from a carbon target using an 8-cm argon ion source; (2) direct deposition by a 30-cm hollow cathode ion source with hydrocarbon gas in argon; and (3) dual beam direct deposition by the 30-cm hollow cathode ion source and an 8-cm argon ion source. In an attempt to improve the adherence of the DLC films on ZnSc and ZnS, ion beam cleaning, ion implantation with helium and neon ions, or sputter deposition of a thin, ion beam intermediate coating was employed prior to deposition of the DLC film. The protection that the DLC films afforded the windows from particle and rain erosion was evaluated, along with the hydrogen content, adherence, intrinsic stress, and infrared transmittance of the films. Because of the elevated stress levels in the ion beam sputtered DLC films and in those ion beam deposited with butane, films thicker than 0.1 micron and with good adherence on ZnS and ZnSe could not be generated. An intermediate coating of germanium successfully allowed the DLC films to remain adherent to the optical windows and caused only negligible reduction in the specular transmittance of the ZnS and ZnSe at 10 microns.

Swec, Diane M.↗

Diamondlike carbon protective coatings for optical windows

Diamondlike carbon (DLC) films were deposited on infrared transmitting optical windows and were evaluated as protective coatings for these windows exposed to particle and rain erosion. The DLC films were deposited on zinc selenide (ZnSe) and zinc sulfide (ZnS) by three different ion beam methods: (1) sputter deposition from a carbon target using an 8-cm argon ion source; (2) direct deposition by a 30-cm hollow cathode ion source with hydrocarbon gas in argon; and (3) dual beam direct deposition by the 30-cm hollow cathode ion source and an 8-cm argon ion source. In an attempt to improve the adherence of the DLC films on ZnSc and ZnS, ion beam cleaning, ion implantation with helium and neon ions, or sputter deposition of a thin, ion beam intermediate coating was employed prior to deposition of the DLC film. The protection that the DLC films afforded the windows from particle and rain erosion was evaluated, along with the hydrogen content, adherence, intrinsic stress, and infrared transmittance of the films. Because of the elevated stress levels in the ion beam sputtered DLC films and in those ion beam deposited with butane, films thicker than 0.1 micron and with good adherence on ZnS and ZnSe could not be generated. An intermediate coating of germanium successfully allowed the DLC films to remain adherent to the optical windows and caused only negligible reduction in the specular transmittance of the ZnS and ZnSe at 10 microns.

Swec, Diane M.↗

Crystal Growth of Ternary Compound Semiconductors in Low Gravity Environment

A low gravity material experiment will be performed in the Material Science Research Rack (MSRR) on International Space Station (ISS). There are two sections of the flight experiment: (I) crystal growth of ZnSe and related ternary compounds, such as ZnSeS and ZnSeTe, by physical vapor transport (PVT) and (II) melt growth of CdZnTe by directional solidification. The main objective of the project is to determine the relative contributions of gravity-driven fluid flows to the compositional distribution, incorporation of impurities and defects, and deviation from stoichiometry observed in the grown crystals as results of buoyancy-driven convection and growth interface fluctuations caused by irregular fluid-flows on Earth. The investigation consists of extensive ground-based experimental and theoretical research efforts and concurrent flight experimentation. This talk will focus on the ground-based studies on the PVT crystal growth of ZnSe and related ternary compounds. The objectives of the ground-based studies are (1) obtain the experimental data and conduct the analyses required to define the optimum growth parameters for the flight experiments, (2) perfect various characterization techniques to establish the standard procedure for material characterization, (3) quantitatively establish the characteristics of the crystals grown on Earth as a basis for subsequent comparative evaluations of the crystals grown in a low-gravity environment and (4) develop theoretical and analytical methods required for such evaluations. ZnSe and related ternary compounds have been grown by vapor transport technique with real time in-situ non-invasive monitoring techniques. The grown crystals have been characterized extensively by various techniques to correlate the grown crystal properties with the growth conditions.

Su, Ching-Hua↗

A strategy to eliminate selenium oxide islands formed on the ZnSe/GaAs epilayer

Atomically clean and smooth surfaces are essential for semiconductor device fabrication and epitaxial regrowth. In this regard, spontaneously formed oxide islands or clusters on the surfaces of II-VI semiconductor exposures to air can disrupt interface formation. Using ZnSe/GaAs heterostructures grown by molecular beam epitaxy (MBE), we investigated the effect of surface treatments in eliminating oxide islands. The samples were probed with atomic force microscopy, low-temperature photoluminescence, and scanning electron microscopy. Here, it was found that ultra-high vacuum (UHV) annealing at 200°C, regardless of annealing duration, largely removed the islands while leaving the crystallinity of the ZnSe and GaAs epilayers unaffected. UHV annealing at higher temperatures of 300°C completely removed the islands, but the optical properties of ZnSe and/or GaAs epilayers deteriorated depending on the annealing duration. Our observations provide guidance to set thermal annealing strategies for removing oxide islands from the surfaces of II-VI/III-V semiconductor heterostructures depending on the desired properties.

36 MATERIALS SCIENCE↗

Extremely Slow Trap-Mediated Hole Relaxation in Room-Temperature InP/ZnSe/ZnS Quantum Dots

Time-resolved photoluminescence (PL) and transient absorption (TA) spectroscopy have been used to elucidate the hole relaxation dynamics in high-quality InP/ZnSe/ZnS quantum dots (QDs) at room temperature. In QDs having an In/P ratio close to 1:1, hole cooling is fast compared to the ~40 ps time-correlated photon-counting instrument response. However, in QDs that luminesce at wavelengths greater than around 600 nm and have excess indium, a significant fraction of the PL exhibits a slower rise time. In this case, the PL rises over a range of timescales varying from close to the instrument response to approximately 300–400 ps. The time constant of the slowest component increases with increasing InP core size and the fraction of the PL that has the slow rise time increases with excess indium in the particle. In all cases, a slow rise time and any spectral evolution on that timescale are absent in the TA results, indicating that the slow dynamics may be assigned to relaxation in the valence band. QDs emitting at wavelengths below 560 nm show very different dynamics, exhibiting a barely detectable <50 ps rise time. Based on these results and measured elemental compositions, the slow hole relaxation is assigned to the transient population of indium-based traps in the ZnSe shell that are above the valence band edge only for the larger, red-emitting QDs. Here, the relative trap to band edge relaxation rates can be understood in terms of effective mass approximation hole wave function calculations, which show that the relaxation rate is largely determined by the extent to which the hole wave function in the lowest exciton penetrates into the ZnSe shell, overlapping the trapped-hole wave functions.

77 NANOSCIENCE AND NANOTECHNOLOGY↗

Two-dimensional forms of robust CO 2 reduction photocatalysts

Photoelectrocatalysts that use sunlight to power the CO 2 reduction reaction will be crucial for carbon-neutral power and energy-efficient industrial processes. Scalable photoelectrocatalysts must satisfy a stringent set of criteria, such as stability under operating conditions, product selectivity, and efficient light absorption. Two-dimensional materials can offer high specific surface area, tunability, and potential for heterostructuring, providing a fresh landscape of candidate catalysts. From a set of promising bulk CO 2 reduction photoelectrocatalysts, we screen for candidate monolayers of these materials, then study their catalytic feasibility and suitability. For stable monolayer candidates, we verify the presence of visible-light band gaps, check that band edges can support CO 2 reduction, determine exciton binding energies, and compute surface reactivity. We find visible light absorption for SiAs, ZnTe, and ZnSe monolayers, and that due to a lack of binding, CO selectivity is possible. We thus identify SiAs, ZnTe, and ZnSe monolayers as targets for further investigation, expanding the chemical space for CO 2 photoreduction candidates.

36 MATERIALS SCIENCE↗

Spectral widths and Stokes shifts in InP-based quantum dots

InP-based quantum dots (QDs) have Stokes shifts and photoluminescence (PL) line widths that are larger than in II–VI semiconductor QDs with comparable exciton energies. The mechanisms responsible for these spectral characteristics are investigated in this paper. Upon comparing different semiconductors, we find the Stokes shift decreases in the following order: InP > CdTe > CdSe. We also find that the Stokes shift decreases with core size and decreases upon deposition of a ZnSe shell. We suggest that the Stokes shift is largely due to different absorption and luminescent states in the angular momentum fine structure. The energy difference between the fine structure levels, and hence the Stokes shifts, are controlled by the electron–hole exchange interaction. Luminescence polarization results are reported and are consistent with this assignment. Spectral widths are controlled by the extent of homogeneous and inhomogeneous broadening. Here, we report PL and PL excitation (PLE) spectra that facilitate assessing the roles of homogeneous and different inhomogeneous broadening mechanisms in the spectra of zinc-treated InP and InP/ZnSe/ZnS particles. There are two distinct types of inhomogeneous broadening: size inhomogeneity and core–shell interface inhomogeneity. The latter results in a distribution of core–shell band offsets and is caused by interfacial dipoles associated with In–Se or P–Zn bonding. Quantitative modeling of the spectra shows that the offset inhomogeneity is comparable to but somewhat smaller than the size inhomogeneity. The combination of these two types of inhomogeneity also explains several aspects of reversible hole trapping dynamics involving localized In 3+ /V Zn 2– impurity states in the ZnSe shells.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗