Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “Ti”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 127 records · Page 7

Surface effects on hydrogen permeation through Ti-14Al-21Nb alloy

Hydrogen transport through Ti-14Al-21Nb (wt percent) alloy is measured using ultrahigh vacuum permeation techniques over the temperature range of 500 to 900 C and hydrogen pressure range of 0.25 to 10 torr. Hydrogen permeability through the alloy can be described through two different mechanisms depending on th temperature of exposure. In the 675 to 900 C range, the process is diffusion-limited: the permeability has a weak temperature dependence, but the diffusivity has a strong temperature dependence. Below 675 C, the permeation rate of hydrogen is very sensitive to surface controlled processes such as the formation of a barrier layer from contaminants. A physical model explaining the role of surface films on the transport of hydrogen through Ti-14Al-21Nb alloy was described.

Sankaran, Sandara N.↗

Tensile deformation damage in SiC reinforced Ti-15V-3Cr-3Al-3Sn

The damage mechanisms of a laminated, continuous SiC fiber reinforced Ti-15V-3Cr-3Al-3Sn (Ti-15-3) composite were investigated. Specimens consisting of unidirectional as well as cross-ply laminates were pulled in tension to failure at room temperature and 427 C and subsequently examined metallographically. Selected specimens were interrupted at various strain increments and examined to document the development of damage. When possible, a micromechanical stress analysis was performed to aid in the explanation of the observed damage. The analyses provide average constituent microstresses and laminate stresses and strains. It was found that the damage states were dependent upon the fiber architecture.

Lerch, Bradley A.↗

Low-threshold, CW, all-solid-state Ti:Al2O3 laser

A CW Ti:Al2O3 ring laser with a threshold power of 119 mW is demonstrated. It provides a tunable source of single-frequency, diffraction-limited radiation that is suitable for injection seeding. The Ti:Al2O3 laser is operated with a diode-laser-pumped, frequency-doubled, Nd:YAG laser as the sole pump source.

Harrison, James↗

Characteristics Of Superplastically Formed Ti-6242 Sheet

Near-alpha titanium alloy candidate for high-temperature structural airframe applications. Research characterizes selected mechanical properties of Ti-6242 sheets in superplastic forming (SPF) condition, both with and without heat treatment, and compares results with those obtained on as-received material. Information derived from research proves useful to aerospace community for designing and manufacturing Ti-6242 structures and structural components.

Royster, Dick M.↗

Amplified spontaneous emission measurement of a line-narrowed, tunable, Ti:Al2O3 amplifier using rubidium absorption

Amplified spontaneous emission, ASE, generated by a Ti:Al2O3 laser amplifier has been measured as a function of pump energy, and thus gain, using the atomic absorption of rubidium, Rb, gas at 0.780 micron. By tuning the Ti:Al2O3 laser, the Rb cell could selectively absorb the narrow spectral bandwidth laser radiation while transmitting the wide spectral bandwidth ASE. Transmission of laser amplifier pulses through a Rb absorption cell, measured at various temperatures, thus allows the measurement of the weak ASE in the vicinity of the strong laser pulse. A model for the transmission of Rb as a function of temperature and wavelength has been developed. The measured transmissions are in good agreement with the transmission model predictions.

Barnes, James C.↗

Injection Seeding of Ti:Al2O3 in an unstable resonator theory and experiment

Injection Seeding of a Ti:Al2O3 unstable resonator using both a pulsed single-mode Ti:Al2O3 laser and a continuous wave laser diode has been characterized. Results are compared with a theory which calculates injection seeding as function of seed and resonator alignment, beam profiles, and power.

Barnes, J. C.↗

Melting of cognetic depleted and enriched reservoirs and the production of high Ti Mare basalts

Implicit in current understanding of the location of terrestrial enriched and depleted reservoirs is the notion that they are spatially separated. The depleted reservoir on Earth is situated in the upper mantle, and the complementary enriched reservoir is located in the crust. However, Earth reservoirs are continually being modified by recycling driven by mantle convection. The Moon is demonstrably different from Earth in that its evolution was arrested relatively early - effectively with 1.5 Ga of its formation. It is possible that crystallized trapped liquids (from the late stages of a magma ocean) have been preserved as LILE-enriched portions of the lunar mantle. This would lead to depleted (cumulate) and enriched (magma ocean residual liquid) reservoirs in the lunar upper mantle. There is no evidence for significant recycling from the highland crust back into the mantle. Therefore, reservoirs created at the Moon's inception may have remained intact for over 4.0 Ga. The topics discussed include the following: (1) radiogenic isotopes in high-Ti mare basalts; (2) formation of cogenetic depleted and enriched reservoirs; and (3) melting of the source to achieve high-Ti mare basalts.

Snyder, Gregory A.↗

Limited subsolidus diffusion in type B1 CAI: Evidence from Ti distribution in spinel

Most models of calcium aluminum-rich inclusions (CAI) have focused on early stages of formation by equilibrium crystallization of a homogeneous liquid. Less is known about the subsolidus cooling history of CAI. Chemical and isotopic heterogeneties on a scale of tens to hundreds of micrometers (e.g. MacPherson et al. (1989) and Podosek, et al. (1991)) suggest fairly rapid cooling with a minimum of subsolidus diffusion. However, transmission electron microscopy indicates that solid state diffusion may have been an important process at a smaller scale (Barber et al. 1984). If so, chemical evidence for diffusion could provide constraints on cooling times and temperatures. With this in mind, we have begun an investigation of the Ti distribution in spinels from two type B1 CAI from Allende to determine if post-crystallization diffusion was a significant process. The type B1 CAIs, 3529Z and 5241 have been described by Podosek et al. (1991) and by El Goresy et al. (1985) and MacPherson et al. (1989). We have analyzed spinels in these inclusions using the electron microprobe. These spinels are generally euhedral, range in size from less than 10 to 15 micron and are poikilitically enclosed by millimeter-sized pyroxene, melilite, and anorthite. Analyses were obtained from both the mantles and cores of the inclusions. Compositions of pyroxene in the vicinity of individual spinel grains were obtained by analyzing at least two points on opposite sides of the spinel and averaging the compositions. The pyroxene analyses were obtained within 15 microns of the spinel-pyroxene interface. No compositional gradients were observed within single spinel crystals. Ti concentrations in spinels included within pyroxene, melilite, and anorthite are presented.

Meeker, G. P.↗

Development of lasers optimized for pumping Ti:Al2O3 lasers

Laboratory demonstrations that were completed included: (1) an all-solid-state, broadly tunable, single-frequency, Ti:Al2O3 master oscillator, and (2) a technique for obtaining 'long' (nominally 100- to 200-ns FWHM) laser pulses from a Q-switched, Nd oscillator at energy levels commensurate with straightforward amplification to the joule level. A diode-laser-pumped, Nd:YLF laser with intracavity SHG was designed, constructed, and evaluated. With this laser greater than 0.9 W of CW, output power at 523.5 nm with 10 W of diode-laser pump power delivered to the Nd:YLF crystal was obtained. With this laser as a pump source, for the first time, to our knowledge, an all solid-state, single frequency, Ti:Al203 laser with sufficient output power to injection seed a high-energy oscillator over a 20-nm bandwidth was demonstrated. The pulsed laser work succeeded in demonstrating pulse-stretching in a Q-switched Nd:YAG oscillator. Pulse energies greater than 50-mJ were obtained in pulses with 100- to 200-ns pulsewidths (FWHM).

Rines, Glen A.↗

An investigation of the loss of ductility in hydrogen charged beta-Ti alloys

The high strength, low density, and good corrosion resistance of Ti-based alloys make them candidate materials for a number of applications in the aerospace industry. A major limitation in the use of these alloys in the advanced hypersonic flight vehicle program is their susceptibility to hydrogen embrittlement. This study focuses on the hydrogen sensitivity of TIMETAL 21S beta-Ti alloy. The material received was in the form of grip-ends of failed tensile test samples which had been exposed to different charging conditions (combinations of hydrogen pressure and temperature). The samples received, the charging conditions, and their fracture mode are discussed. It can be seen that the fracture behavior changes from ductile to brittle with increasing hydrogen content, but the transition in behavior occurs for a small increase in hydrogen concentration. The aim of this program was to assess the microstructural differences between the ductile and brittle alloys to ascertain the embrittlement mechanism. A range of tools which included x-ray diffraction, scanning electron microscopy (SEM) and transmission electron microscopy (TEM) were used.

Robertson, Ian M.↗

Microstructure/Oxidation/Microhardness Correlations in Gamma-Based and Tau-Based Al-Ti-Cr Alloys

The relationships between alloy microstructure and air oxidation kinetics and alloy microstructure and microhardness in the Al-Ti-Cr system for exposures at 800 C and 1000 C were investigated. The relevant phases were identified as tau (Ll2), gamma (LIO), r-Al2Ti, TiCrAl (laves), and Cr2AI. Protective alumina formation was associated with tau, Al-rich TiCrAl, and gamma/TiCrAl mixtures. Brittleness was associated with the TiCrAl phase and tau decomposition to A12Ti + Cr2AI. It was concluded that two-phase gamma + TiCrAl alloys offer the greatest potential for oxidation resistance and room temperature ductility in the Al-Ti-Cr system.

Brady, Michael P.↗

Elevated-Temperature Deformation Properties of a HfC Modified Ti-48Al-2Mn-2Nb Matrix Particulate Composite

Rapid solidification techniques in combination with HIPing have been used to produce Ti-48Al-2Mn-2Nb and a Ti-48Al-2Mn-2Nb+15 wt% HfC composite. While the composite does contain several second phases within the gamma + alpha(sub 2) matrix, none was identified to be HfC. The elevated-temperature properties were determined by constant velocity compression and constant load tensile testing in air between 1000 and 1173 K. Such testing indicated that the elevated temperature strengths of the HfC-modified aluminide was superior to those of the unreinforced matrix with the best 1100 K temperature slow strain rate properties for both materials being achieved after high-temperature annealing prior to testing. Examination of the microstructures after deformation in combination with the measured stress exponents and activation energies suggest that creep resistance of the HfC-modified form is due to solid-solution strengthening from carbon and hafnium rather than the presence of second phases.

Whittenberger, J. D.↗

Two Wavelength Ti:sapphire Laser for Ozone DIAL Measurements from Aircraft

Laser remote sensing of ozone from aircraft has proven to be a valuable technique for understanding the distribution and dynamics of ozone in the atmosphere. Presently the differential absorption lidar (DIAL) technique, using dual ND:YAG lasers that are doubled to pump dye lasers which in turn are doubled into the UV for the "on" and "off' line lasers, is used on either the NASA DC-8 or P-3 aircraft. Typically, the laser output for each line is 40-mJ and this is split into two beams, one looking up and the other downward, each beam having about 20-mJ. The residual ND:YAG (1.06 micron) and dye laser energies are also transmitted to obtain information on the atmospheric aerosols. While this system has operated well, there are several system characteristics that make the system less than ideal for aircraft operations. The system, which uses separate "on" and "off" line lasers, is quite large and massive requiring valuable aircraft volume and weight. The dye slowly degrades with time requiring replacement. The laser complexity requires a number of technical people to maintain the system performance. There is also the future interest in deploying an ozone DIAL system in an Unpiloted Atmospheric Vehicle (UAV) which would require a total payload mass of less than 150 kg and power requirement of less than 1500 W. A laser technology has emerged that could potentially provide significant enhancements over the present ozone DIAL system. The flashlamp pumped Ti:sapphire laser system is an emerging technology that could reduce the mass and volume over the present system and also provide a system with fewer conversion steps, reducing system complexity. This paper will discuss preliminary results from a flashlamp-pumped Ti:sapphire laser constructed as a radiation source for a UV DIAL system to measure ozone.

Situ, Wen↗

Atomistic Modeling of Quaternary Alloys: Ti and Cu in NiAl

The change in site preference in NiAl(Ti,Cu) alloys with concentration is examined experimentally via ALCHEMI and theoretically using the Bozzolo-Ferrante-Smith (BFS) method for alloys. Results for the site occupancy of Ti and Cu additions as a function of concentration are determined experimentally for five alloys. These results are reproduced with large-scale BFS-based Monte Carlo atomistic simulations. The original set of five alloys is extended to 25 concentrations, which are modeled by means of the BFS method for alloys, showing in more detail the compositional range over which major changes in behavior occur. A simple but powerful approach based on the definition of atomic local environments also is introduced to describe energetically the interactions between the various elements and therefore to explain the observed behavior.

Bozzolo, Guillermo↗

Northwest Africa 773: Lunar Mare Breccia with a Shallow-formed Olivine-Cumulate Component, Very-Low-Ti Heritage, and a KREEP Connection

Northwest Africa 773 is one of the more unusual lunar meteorites found in recent years because it contains a prominent clast lithology, which appears to be an olivine-rich cumulate and because it is a very-low-Ti (VLT) mare breccia with relatively high incompatible-trace-element concentrations and LREE/HREE enrichment. A lunar origin was verified by Fagan and coworkers on the basis of noble-gas contents, oxygen isotopes, and mineral compositions. Fagan et al. described two lithologies: (1) heterolithic impact breccia with a regolith component and (2) cumulus olivine gabbronorite. Here, we refer to these as the breccia (Bx) lithology and the olivine-cumulate (OC) lithology. The impact breccia components are predominantly volcanic (basaltic), and, in this context, the occurrence of the cumulus lithology is especially significant: is it related to the volcanic components or does it represent a deep-seated rock entrained by the basaltic magma as it rose to the surface? Elevated incompatible-element concentrations with more or less KREEP-like inter-element ratios and very-low-Ti concentrations distinguish both lithologies of this meteorite from Apollo mare basalts. Here, we summarize key compositional information (bulk and mineral), especially related to the OC lithology, to show that it formed at shallow depth and comes from a VLT ultramafic precursor that mixed with a KREEP-like trace-element component deep in the crust or upper mantle.

Jolliff, B. L.↗

Elevated Temperature Creep Deformation in Solid Solution <001> NiAL-3.6Ti Single Crystals

The 1100 to 1500 K slow plastic strain rate compressive properties of <001> oriented NiAl-3.6Ti single crystals have been measured, and the results suggests that two deformation processes exist. While the intermediate temperature/faster strain rate mechanism is uncertain, plastic flow at elevated temperature/slower strain rates in NiAl-3.6Ti appears to be controlled by solute drag as described by the Cottrell-Jaswon solute drag model for gliding b = a(sub 0)<101> dislocations. While the calculated activation energy of deformation is much higher (approximately 480 kJ/mol) than the activation energy for diffusion (approximately 290 kJ/mol) used in the Cottrell-Jaswon creep model, a forced temperature compensated - power law fit using the activation energy for diffusion was able to adequately (greater than 90%) predict the observed creep properties. Thus we conclude that the rejection of a diffusion controlled mechanism can not be simply based on a large numerical difference between the activation energies for deformation and diffusion.

Whittenberger, J. Daniel↗

Petrography of Lunar Meteorite LAP 02205, a New Low-Ti Basalt Possibly Launch Paired with NWA 032

Lunar meteorite LAP 02205 is a 1.23 kg basalt collected during the 2002 field season in the La- Paz ice field, Antarctica [1]. We present a petrographic description including mineral modes and compositions, and the major-element composition of the bulk meteorite. LAP 02205 is an Fe-rich, moderately low-Ti mare basalt that is similar in composition, mineralogy, and mineral chemistry to the NWA 032 basaltic lunar meteorite. LAP 02205 is yet another of the moderately low- Ti basaltic meteorites that are underrepresented among Apollo and Luna samples but that appear from remote sensing to be the most common basalt type on the Moon.

Jolliff, B. L.↗

Development of Creep-Resistant NiAl(Ti,Hf) Single-Crystal Alloys

Nickel-base superalloys are the current choice for high-temperature jet engine applications such as turbine blades and vanes. However, after more than five decades of use, nickel-base superalloys have reached their limit, since the operating temperatures in gas turbine engines are now approaching the melting temperature of these alloys. Thus alternative materials, such as lightweight NiAl intermetallic alloys with superior properties, (e.g., high melting temperature, high thermal conductivity, and excellent chemical stability and oxidation resistance) are required for the next generation of high-temperature structural materials for more efficient 21st century civil transport systems. The two major disadvantages that have historically prevented the application of NiAl as a high-temperature structural material are its poor creep resistance and low room-temperature ductility. Alloying strategies similar to those used for nickel-base superalloys are being used to improve the high-temperature strength via solid-solution and precipitate-hardening effects. This study highlights the potent role of Ti and Hf as potential solid-solution strengtheners in NiAl and also the added effect of second-phase particles when Ti and Hf are both used.