Tribological properties of boron nitride synthesized by ion beam deposition

The adhesion and friction behavior of boron nitride films on 440 C bearing stainless steel substrates was examined. The thin films containing the boron nitride were synthesized using an ion beam extracted from a borazine plasma. Sliding friction experiments were conducted with BN in sliding contact with itself and various transition metals. It is indicated that the surfaces of atomically cleaned BN coating film contain a small amount of oxides and carbides, in addition to boron nitride. The coefficients of friction for the BN in contact with metals are related to the relative chemical activity of the metals. The more active the metal, the higher is the coefficient of friction. The adsorption of oxygen on clean metal and BN increases the shear strength of the metal - BN contact and increases the friction. The friction for BN-BN contact is a function of the shear strength of the elastic contacts. Clean BN surfaces exhibit relatively strong interfacial adhesion and high friction. The presence of adsorbates such as adventitious carbon contaminants on the BN surfaces reduces the shear strength of the contact area. In contrast, chemically adsorbed oxygen enhances the shear strength of the BN-BN contact and increases the friction.

Miyoshi, K.↗

Tribological properties of boron nitride synthesized by ion beam deposition

The adhesion and friction behavior of boron nitride films on 440 C bearing stainless steel substrates was examined. The thin films containing the boron nitride were synthesized using an ion beam extracted from a borazine plasma. Sliding friction experiments were conducted with BN in sliding contact with itself and various transition metals. It is indicated that the surfaces of atomically cleaned BN coating film contain a small amount of oxides and carbides, in addition to boron nitride. The coefficients of friction for the BN in contact with metals are related to the relative chemical activity of the metals. The more active the metal, the higher is the coefficient of friction. The adsorption of oxygen on clean metal and BN increases the shear strength of the metal - BN contact and increases the friction. The friction for BN-BN contact is a function of the shear strength of the elastic contacts. Clean BN surfaces exhibit relatively strong interfacial adhesion and high friction. The presence of adsorbates such as adventitious carbon contaminants on the BN surfaces reduces the shear strength of the contact area. In contrast, chemically adsorbed oxygen enhances the shear strength of the BN-BN contact and increases the friction.

Miyoshi, K.↗

Aluminum runway surface as possible aid to aircraft braking

Several concepts are described for use singly or in combination to improve aircraft braking. All involve a thin layer of aluminum covering all or part of the runway. Advantage would derive from faster heat conduction from the tire-runway interface. Heating of tread surface with consequent softening and loss of friction coefficient should be reduced. Equations are developed indicating that at least 99 percent of friction heat should flow into the aluminum. Preliminary test results indicate a coefficient of sliding friction of 1.4, with predictably slight heating of tread. Elimination of conventional brakes is at least a remote possibility.

Miller, C. D.↗

The friction and wear of metals and binary alloys in contact with an abrasive grit of single-crystal silicon carbide

Sliding friction experiments were conducted with various metals and iron-base binary alloys (alloying elements Ti, Cr, Mn, Ni, Rh and W) in contact with single crystal silicon carbide riders. Results indicate that the friction force in the plowing of metal and the groove height (corresponding to the wear volume of the groove) decrease linearly as the shear strength of the bulk metal increases. The coefficient of friction and groove height generally decrease, and the contact pressure increases with an increase in solute content of binary alloys. There appears to be very good correlation of the solute to iron atomic ratio with the decreasing rate of change of coefficient of friction, the decreasing rate of change of groove height and the increasing rate of change of contact pressure with increasing solute content. These rates of change increase as the solute to iron atomic radius ratio increases or decreases from unity.

Miyoshi, K.↗

The friction and wear of metals and binary alloys in contact with an abrasive grit of single-crystal silicon carbide

Sliding friction experiments were conducted with various metals and iron-base binary alloys (alloying elements Ti, Cr, Mn, Ni, Rh, and W) in contact with single-crystal silicon carbide riders. Results indicate that the coefficient of friction and groove height (corresponding to the wear volume) decrease linearly as the shear strength of the bulk metal increases. The coefficient of friction and groove height generally decrease with an increase in solute content of binary alloys. A separate correlation exists between the solute to iron atomic radius ratio and the decreasing rates of change of coefficient of friction and groove height with increasing solute content. These rates of change are minimum at a solute to iron radius ratio of unity. They increase as the atomic ratio increases or decreases linearly from unity. The correlations indicate that atomic size is an important parameter in controlling friction and wear of alloys.

Miyoshi, K.↗

Solid Lubricant For Alumina

Outer layer of silver lubricates, while intermediate layer of titanium ensures adhesion. Lubricating outer films of silver deposited on thin intermediate films of titanium on alumina substrates found to reduce sliding friction and wear. Films provide effective lubrication for ceramic seals, bearings, and other hot sliding components in advanced high-temperature engines.

Dellacorte, Christopher↗

Friction and Wear Properties of Selected Solid Lubricating Films

To evaluate commercially developed solid film lubricants for aerospace bearing applications, we investigated the friction and wear behavior of bonded molybdenum disulfide (MoS2), magnetron-sputtered MoS2 and ion-plated silver films in sliding contact with 6-mm-diameter American Iron and Steel Institute (AISI) 440 C stainless steel balls. Unidirectional sliding friction experiments were conducted with a load of 5.9 N (600 g), a mean Herizian contact pressure of 0.79 GPa maximum 1.19 GPa), and a sliding velocity of 0.2 m/s at room temperature in three environments: ultrahigh vacuum (7x10 (exp -7Pa)), humid air (approx. 20 percent humidity), and dry nitrogen (less than 1 percent humidity). The resultant films were characterized by scanning electron microscopy, energy-dispersive x-ray spectroscopy, and surface profilometry. Marked differences in friction and wear resulted front the environmental conditions and the film materials. The main criteria for judging the performance were coefficient of friction and wear rate, which had to be less than 0.3 and on the order of 10 (exp -6mm exp 3/Nm or less), respectively. The bonded MoS2 and magnetron-sputtered MoS2 films met the criteria in all three environments. Also, the wear rates of the counterpart AISI 440 C stainless steel balls met that criterion in all three environments. The ion-plated silver films met the criteria only in ultrahigh vacuum. In ultrahigh vacuum the bonded MoS2 films were superior. In humid air the bonded MoS2 films had higher coefficient of friction and shorter wear life than did the magnetron-sputtered MoS2 films. The ion-plated silver films had a high coefficient of friction in humid air but relatively low coefficients of friction in the nonoxidative environments. Adhesion and plastic deformation played important roles in all three environments. All sliding involved adhesive transfer of materials.

Miyoshi, Kazuhisa↗

Friction and wear of metals with a single-crystal abrasive grit of silicon carbide: Effect of shear strength of metal

Sliding friction experiments were conducted with spherical, single-crystal silicon carbide riders in contact with various metals and with metal riders in contact with silicon carbide flats. Results indicate that: (1) the friction force in the plowing of metal and (2) the groove height (corresponding to the volume of the groove) are related to the shear strength of the metal. That is, they decrease linearly as the shear strength of the bulk metal increases. Grooves are formed in metals primarily from plastic deformation, with occasional metal removal. The relation between the groove width D and the load W can be expressed by W = kD, superscript n which satisfies Meyer's law.

Miyoshi, K.↗

Solid Lubrication by Multiwalled Carbon Nanotubes in Air and in Vacuum for Space and Aeronautics Applications

To evaluate recently developed aligned multiwalled carbon nanotubes (MWNTs) and dispersed MWNTs for solid lubrication applications, unidirectional sliding friction experiments were conducted with 440 C stainless steel balls and hemispherical alumina-yttria stabilized zirconia pins in sliding contact with the MWNTs deposited on quartz disks in air and in vacuum. The results indicate that MWNTs have superior solid lubrication friction properties and endurance lives in air and vacuum under dry conditions. The coefficient of friction of the dispersed MWNTs is close to 0.05 and 0.009 in air and in vacuum, respectively, showing good dry lubricating ability. The wear life of MWNTs exceeds 1 million passes in both air and vacuum showing good durability. In general, the low coefficient of friction can be attributed to the combination of the transferred, agglomerated patches of MWNTs on the counterpart ball or pin surfaces and the presence of tubular MWNTs at interfaces.

Miyoshi, Kazuhisa↗

Low-Friction Joint for Robot Fingers

Mechanical linkage allows adjacent parts to move relative to each other with low friction and with no chatter, slipping, or backlash. Low-friction joint of two surfaces in rolling contact, held in alinement by taut flexible bands. No sliding friction or "stick-slip" motion: Only rolling-contact and bending friction within bands. Proposed linkage intended for finger joints in mechanical hands for robots and manipulators.

Ruoff, C. F.↗

Experimental test program for evaluation of solid lubricant coating as applied to compliant foil gas bearings to 315 deg C

An experimental apparatus and test procedure was developed to compare the performance of two solid lubricant coatings for air lubricated compliant foil gas bearings in the temperature range of 25 to 315 C. Polyimide bonded additive (SBGC) were tested extensively for durability and frictional characteristics. A partial arc bearing constructed of Inconel X-750 was coated on the bore with one of these coatings. The foil was subjected to repeated start/stop cycles. Performance comparisons reveal that although both coatings survive thousands of start/stop cycles, only the PBGF coated bearing achieves the specified 9000 start/stops. There is enough wear on the SBGC coated bearing to warrant termination of the test prior to 9000 start/stop cycles due to coating failure. The frictional characteristics of the PBGF are better at the elevated temperatures than at lower temperatures; a marked increase in sliding friction occurs as the temperature decreases. The SBGC maintains relatively constant frictional characteristics independent of operating temperature.

Wagner, R. C.↗

Evaluation of Selected Solid Lubricating Films

An investigation was conducted to examine the friction and wear properties of bonded molybdenum disulfide (MoS2), magnetron-sputtered MoS2, ion-plated silver, ion-plated lead, magnetron-sputtered diamondlike carbon (MS DLC), and plasma-assisted, chemical-vapor-deposited DLC (PACVD DLC) films in sliding contact with 6-mm-diameter AISI 440C stainless steel balls. Unidirectional ball-on-disk sliding friction experiments were conducted with a load of 5.9 N and a sliding velocity of 0.2 m/s at room temperature in three environments: ultrahigh vacuum (vacuum pressure, 7 x 10(exp -7) Pa), humid air (relative humidity, approx. 20 percent), and dry nitrogen (relative humidity, less than 1 percent). The main criteria for judging the performance of the solid lubricating films were coefficient of friction and wear rate, which had to be less than 0.3 and on the order of 10(exp -6) cubic mm/N(dot)m or less, respectively. The bonded MoS2 and magnetron-sputtered MoS2 films met the criteria in all three environments. The ion-plated lead and silver films met the criteria only in ultrahigh vacuum but failed in humid air and in dry nitrogen. The MS DLC and PACVD DLC films met the requirements in humid air and dry nitrogen but failed in ultrahigh vacuum.

Miyoshi, Kazuhisa↗

Durability Evaluation of Selected Solid Lubricating Films

An investigation was conducted to examine the coefficients of friction, wear rates, and durability of bonded molybdenum disulfide (MoS2), magnetron-sputtered MoS2, ion-plated silver, ion-plated lead, magnetron-sputtered diamondlike carbon (MS DLC), and plasma-assisted, chemical-vapor-deposited DLC (PACVD DLC) films in sliding contact with 6-mm-diameter AISI 440C stainless steel balls. Unidirectional ball-on-disk sliding friction experiments were conducted with a load of 5.9 N and a sliding velocity of 0.2 m/s at room temperature in three environments: ultrahigh vacuum (vacuum pressure, 7 x 10(exp -7) Pa), humid air (relative humidity, approx. 20 percent), and dry nitrogen (relative humidity, less than 1 percent). The main criteria for judging the performance of the solid lubricating films were coefficient of friction and wear rate, which had to be less than 0.3 and on the order of 10(exp -6) cu mm/N.m or less, respectively. The bonded MoS2 and magnetron-sputtered MoS2 films met the criteria in all three environments. The ion-plated lead and silver films met the criteria only in ultrahigh vacuum but failed in humid air and in dry nitrogen. The MS DLC and PACVD DLC films met the requirements in humid air and dry nitrogen but failed in ultrahigh vacuum.

Miyoshi, Kazuhisa↗

Friction and wear with a single-crystal abrasive grit of silicon carbide in contact with iron base binary alloys in oil: Effects of alloying element and its content

Sliding friction experiments were conducted with various iron-base binary alloys (alloying elements were Ti, Cr, Mn, Ni, Rh, and W) in contact with a rider of 0.025-millimeter-radius, single-crystal silicon carbide in mineral oil. Results indicate that atomic size and content of alloying element play a dominant role in controlling the abrasive-wear and -friction properties of iron-base binary alloys. The coefficient of friction and groove height (wear volume) general alloy decrease, and the contact pressure increases in solute content. There appears to be very good correlation of the solute to iron atomic radius ratio with the decreasing rate of coefficient of friction, the decreasing rate of groove height (wear volume), and the increasing rate of contact pressure with increasing solute content C. Those rates increase as the solute to iron atomic radius ratio increases from unity.

Miyoshi, K.↗

Friction, wear, and thermal stability studies of some organotin and organosilicon compounds

Thermal decomposition temperatures were determined for a number of organotin and organosilicon compounds. A ball-on-disk sliding friction apparatus was used to determine the friction and wear characteristics of two representative compounds, (1) 3-tri-n-butylstannyl (diphenyl) and (2) 3-tri-n-butylsilyl (diphenyl). Friction and wear test conditions included a 1-kg load, 25 to 225 C disk temperatures, and a dry air atmosphere. The tin and silicon compounds yielded friction and wear results either lower than or similar to those obtained with a polyphenyl ether and a C-ether. The maximum thermal decomposition temperatures obtained in the silicon and tin series were 358 and 297 C, respectively. Increasing the steric hindrance around the silicon or tin atoms increased the thermal stability. Future work with these compounds will emphasize their use as antiwear additives rather than base fluids.

Jones, W. R., Jr.↗

Steady-state boundary lubrication with formulated C-ethers to 260 C

Steady state wear and friction studies were made at boundary lubrication conditions in a pin on disk (pure iron on rotating CVM M 50 steel) sliding friction apparatus with five C ether formulated fluids (modified polyphenyl ether containing phosphrous ester, organic acid, and other additives). Conditions included 20, 150, and 260 C disk temperatures, dry air test atmosphere, 1 kilogram load, 50 rpm disk speed, and test times to 130 minutes. Results were compared with those obtained with a formulated MIL L 27502 candidate ester and the C ether base fluid. Three of the C ether formulations gave better lubrication than both reference fluids under most conditions. The other two C ether formulations yielded higher wear rates and friction coefficients than the C ether base fluid for most of the temperature range. Only one C ether formulation showed consistently higher steady state wear rates than the ester.

Loomis, W. R.↗

Friction and Wear of Ion-Beam-Deposited Diamondlike Carbon on Chemical-Vapor-Deposited, Fine-Grain Diamond

Friction and wear behavior of ion-beam-deposited diamondlike carbon (DLC) films coated on chemical-vapor-deposited (CVD), fine-grain diamond coatings were examined in ultrahigh vacuum, dry nitrogen, and humid air environments. The DLC films were produced by the direct impact of an ion beam (composed of a 3:17 mixture of Ar and CH4) at ion energies of 1500 and 700 eV and an RF power of 99 W. Sliding friction experiments were conducted with hemispherical CVD diamond pins sliding on four different carbon-base coating systems: DLC films on CVD diamond; DLC films on silicon; as-deposited, fine-grain CVD diamond; and carbon-ion-implanted, fine-grain CVD diamond on silicon. Results indicate that in ultrahigh vacuum the ion-beam-deposited DLC films on fine-grain CVD diamond (similar to the ion-implanted CVD diamond) greatly decrease both the friction and wear of fine-grain CVD diamond films and provide solid lubrication. In dry nitrogen and in humid air, ion-beam-deposited DLC films on fine-grain CVD diamond films also had a low steady-state coefficient of friction and a low wear rate. These tribological performance benefits, coupled with a wider range of coating thicknesses, led to longer endurance life and improved wear resistance for the DLC deposited on fine-grain CVD diamond in comparison to the ion-implanted diamond films. Thus, DLC deposited on fine-grain CVD diamond films can be an effective wear-resistant, lubricating coating regardless of environment.

Miyoshi, Kazuhisa↗

Auger analysis of oxygen and sulfur interactions with various metals and the effect of sliding on these interactions

Various gases were adsorbed to copper, aluminum, and chromium surfaces. The gases included oxygen, hydrogen sulfide, methyl mercaptan, and sulfur dioxide. Chemisorption was conducted on static surfaces and during dynamic friction experiments. An Auger cyclindrical mirror analyzer was used to monitor surface films. The sulfur containing gases adsorbed readily to all surfaces. Exposures of as little as 0.000001 (torr)(sec) (1 langmuir) were sufficient to reduce friction. Sliding contact did not affect chemisorption of copper or aluminum but did affect chemisorption to chromium surfaces. Oxygen removed sulfur films from all surfaces at room temperature (23 C). Gaseous exposures were from 0.000001 to 0.01 (torr)(sec) (1 to 10,000 langmuirs).

Buckley, D. H.↗