The Development of a Stabilized SEI Layer for Si‐Containing Lithium-Ion Battery Anodes
Explore the source record for details and available documents.
Recent progress in understanding solid electrolyte interphase on lithium metal anode
Lithium (Li) metal batteries (LMBs) are among the most promising candidates of next-generation high-energy-density rechargeable batteries. Solid electrolyte interphase (SEI) on Li metal anode plays a significant role which influences the Li deposition morphology and the cycle life of LMBs. Although SEI is the most important part, a thorough understanding of SEI is inadequate. In this review, we focus on the progresses of understanding on structures, properties and influencing factors of SEI as well as efficient strategies of tailoring SEI. First, the compositions, models and recent progresses on characterizing atomic structure of SEI are summarized. Second, the properties of SEI, including electronic conduction, ionic conduction, stability and mechanical properties are elucidated. Structures and properties of SEI are greatly influenced by multiple factors such as solvent, salt, additive, solvation structure, impurity, current density, temperature, pressure and capacity utilization. Thus, interactions between these factors and SEI are comprehensively discussed. Correlations of SEI with Li deposition morphology, rate capability and cycle life are further summarized. Moreover, efficient strategies of tailoring SEI with desired properties, including in-situ SEI and ex-situ SEI are also reviewed. Despite the significant progresses that have been achieved in the researches of SEI, better understanding of SEI is still highly demand. Finally, future directions especially in-operando techniques, multi-modality approaches for characterization of SEI and artificial intelligence assisted understanding of correlation between electrolyte components and SEI properties are proposed.
Mechanical studies of the solid electrolyte interphase on anodes in lithium and lithium ion batteries
A stable solid electrolyte interphase (SEI) layer is key to high performing lithium ion batteries for metrics such as calendar and cycle life. The SEI must be mechanically robust to withstand large volumetric changes in anode materials such as lithium and silicon, so understanding the mechanical properties and behavior of the SEI is essential for the rational design of artificial SEI and anode form factors. The mechanical properties and mechanical failure of the SEI are challenging to study, because the SEI is thin at only ~ 10 – 200 nm thick and is air sensitive. Furthermore, the SEI changes as a function of electrode material, electrolyte and additives, temperature, potential, and formation protocols. A variety of in situ and ex situ techniques have been used to study the mechanics of the SEI on a variety of lithium ion battery anode candidates; however, there hasn't been a succinct review of the findings thus far. Because of the difficultly of isolating the true SEI and its mechanical properties, there have been a limited number of studies that can fully de-convolute the SEI from the anode it forms on. A review of past research will be helpful for culminating current knowledge and helping to inspire new innovations to better quantify and understand the mechanical behavior of the SEI. This review will summarize the different experimental and theoretical techniques used to study the mechanics of SEI on common lithium ion battery anodes and their strengths and weaknesses.
Direct Prelithiation of Silicon-Based Composite Electrodes via Island-like Thermal Evaporation
Irreversible losses of Li during solid electrolyte interface (SEI) conditioning is a key contributor to the lower specific capacities observed in silicon-containing Li-ion batteries. Herein, thermal evaporation of between 1 and 20 µm of Li onto Si-based composite anodes has been investigated as a prelithiation method to account for such losses. To account for mechanical strain caused by Li-Si alloying during the deposition, a stainless-steel mesh is applied to the electrodes before prelithiation to form “island-like” deposition on the electrode surface. The open circuit potential was also found to decrease as a function of increased Li evaporation, consistent with the potentials of electrochemically prepared LixSi alloys. Prelithiating to account for irreversible Li losses to SEI formation resulted in full cells with a 15.8% increase in initial coulombic efficiency and a 47.8% reduction in irreversible capacity loss after SEI formation cycling. Subsequent C/3 cycling showed up to a 62.9% increase in specific capacity in prelithiated cells. X-ray photoelectron spectroscopy (XPS) revealed differences in the SEI composition that was formed by electrochemical cycling and reactively formed in prelithiated cells upon exposure to Gen2 + 3% FEC electrolyte. The reactively formed SEI from the spontaneous reaction with lithiated silicon was carbonate-rich while the electrochemical SEI formation showed significantly more LiPFx species, which could play a role in overall cycling performance.
Unraveling the convoluted and dynamic interphasial mechanisms on Li metal anode
Accurate understanding of the chemistry of solid-electrolyte interphase (SEI) is key to developing new electrolytes for high-energy batteries using lithium metal (Li-0) anodes(1). SEI is generally believed to be formed by the reactions between Li-0 and electrolyte(2,3). However, our new study shows this is not the whole story. Through synchrotron-based X-ray diffraction and pair distribution function analysis, we reveal a much more convoluted formation mechanism of SEI, which receives considerable contributions from electrolyte, cathode, moisture and native surface species on Li-0, with highly dynamic nature during cycling. Using isotope labelling, we traced the origin of LiH to electrolyte solvent, moisture and a new source: the native surface species (LiOH) on pristine Li-0. When lithium accessibility is very limited as in the case of anode-free cells, LiOH develops into plate-shaped large crystals during cycling. Alternatively, when the lithium source is abundant, as in the case of Li||NMC811 cells, LiOH reacts with Li-0 to form LiH and Li2O. While the desired anion-derived LiF-rich SEI is typically found in the concentrated electrolytes or their derivatives, we found it can also be formed in low-concentration electrolyte via the crosstalk effect, emphasizing the importance of formation cycle protocol and opening up opportunities for low-cost electrolyte development.
Unraveling Morphology and Chemistry Dynamics in Fluoroethylene Carbonate Generated Silicon Anode Solid Electrolyte Interphase Across Delithiated and Lithiated States: Relative Cycling Stability Enabled by an Elastomeric Polymer Matrix
The silicon solid electrolyte interphase (SEI) faces cyclical cracking and reconstruction due to the ∼350% volume expansion. Understanding the SEI dynamic morphology and chemistry evolution from delithiated to lithiated states is thereby paramount to engineering a stable Si anode. Fluoroethylene carbonate (FEC) is a preferred additive with widely demonstrated enhancement of the Si cycling. Thus, insights into the dynamics of the FEC-SEI may provide hints toward engineering the Si interface. Herein, complementary ATR-FTIR, AFM, tip IR, and XPS probing reveal the presence of an elastomeric polycarbonate-like matrix in the FEC-generated SEI which is absent from the FEC-free SEI. Adding FEC to the baseline 1 M LiPF 6 in EC:EMC (1:1) electrolyte promotes formation of a thinner and more conformal SEI, and subdues morphology and chemistry changes between consecutive half-cycles. From AFM, morphological stabilization of the FEC-SEI occurs earlier. Furthermore, conventional SEI biproducts such as Li 2 CO 3 and LiEDC appear in reduced quantities in the FEC-SEI implying a reduced quantity of Li-consuming species. The thin polymeric FEC-SEI enables deeper (de)lithiation of silicon. In conclusion, the enhanced mechanical compliance, chemical invariance, and reduced Li inventory consumption of the FEC-SEI are logically the key features underlying the Si cycling enhancement by FEC.
Dynamic Molecular Investigation of the Solid-Electrolyte Interphase of an Anode-Free Lithium Metal Battery Using In Situ Liquid SIMS and Cryo-TEM
Solid electrolyte interphase (SEI) has been widely perceived to play a critical role in the stable cycling of rechargeable batteries. However, associated with the fragile and air-sensitive nature of the SEI layer, delineation of the formation process and the nature of SEI remains a big challenge. Here, we use in situ liquid time-of-flight secondary ion mass spectroscopy (TOF-SIMS), cryo- transmission electron microscope (TEM) and density functional theory (DFT) calculation to delineate molecular process on the formation of SEI layer under the dynamic operating condition. We discover that the onset potential for SEI layer formation and the thickness of the SEI show dependence on the solvation shell structure. Using LiCoO 2 as a cathode and Cu film as an anode, the SEI is noticed to start to form at around 2.0 V and reach its final thickness (irreversible part, ~ 40-50 nm) at about 3.0 V in the 1 M LiPF 6 –EC/DMC electrolyte, while for the case of 1 M LiFSI–DME, the SEI starts to form at around 1.5 V and reaches its final thickness (~ 20 nm) at about 2.0 V. The in situ TOF-SIMS clearly indicates the outer SEI layer formation and dissipation upon charging and discharging, implying a continued evolution of electrolyte structure with extended cycling. In conclusion, the present work establishes a direct correlation between the molecular signature of SEI layer with solvation feature of electrolytes in lithium batteries, providing insights for tailoring SEI layer toward improved electrochemical properties of lithium batteries.
Kinetic pathways of fast lithium transport in solid electrolyte interphases with discrete inorganic components
The transport of lithium ions in the solid electrolyte interphase (SEI) has been previously accepted to proceed in two steps: a fast pore diffusion through the outer, porous organic layer followed by a slow knock-off or vacancy diffusion in the inner, dense inorganic layer. The second step is believed to be the rate-limiting step during fast-charging. In this study, we have intentionally constructed a thicker SEI (SEI-rich) structure on the surface of monoclinic Nb 2 O 5 (H-Nb 2 O 5 ) by adding LiNO 3 into a conventional ethylene carbonate based electrolyte. The electrochemical performance of two electrodes, one SEI-rich and one with few SEI (SEI-lean), was found to be almost the same, including their fast-charging capability and cycling stability, despite the significant difference in their SEI structure. Importantly, analysis using cryogenic scanning/transmission electron microscopy showed the discrete decoration of individual inorganic particles (e.g., Li 2 O) and amorphous species (LiN x O y /organic components) over the surface of H-Nb 2 O 5 . These discrete inorganic particles are in contradiction to the formation of dense inner inorganic layer, which has been commonly postulated. Based on these findings, we propose a new mechanism for Li ion transport through the SEI: one-step pore diffusion, without the second step slow diffusion. This one-step pore diffusion process provides an extremely fast Li ion transport, and effectively removes the kinetic limitation of Li ion transport in the SEI for fast charging. Finally, these results strongly suggest that the influence of SEI structure on the transport kinetics of lithium ions is much less significant than previously accepted. These results offer a new understanding of possible lithium ion transport pathway within SEI and may have implications for the future designs of fast-charging battery materials.
Revealing the roles of the solid–electrolyte interphase in designing stable, fast-charging, low-temperature Li-ion batteries
Designing the solid–electrolyte interphase (SEI) is critical for stable, fast-charging, low-temperature Li-ion batteries. Fostering a “fluorinated interphase,” SEI enriched with LiF, has become a popular design strategy. Although LiF possesses low Li-ion conductivity, many studies have reported favorable battery performance with fluorinated SEIs. Such a contradiction suggests that optimizing SEI must extend beyond chemical composition design to consider spatial distributions of different chemical species. In this work, we demonstrate that the impact of a fluorinated SEI on battery performance should be evaluated on a case-by-case basis. Sufficiently passivating the anode surface without impeding Li-ion transport is key. We reveal that a fluorinated SEI containing excessive and dense LiF severely impedes Li-ion transport. In contrast, a fluorinated SEI with well-dispersed LiF (i.e., small LiF aggregates well mixed with other SEI components) is advantageous, presumably due to the enhanced Li-ion transport across heterointerfaces between LiF and other SEI components. An electrolyte, 1 M LiPF 6 in 2-methyl tetrahydrofuran (2MeTHF), yields a fluorinated SEI with dispersed LiF. This electrolyte allows anodes of graphite, μSi/graphite composite, and pure Si to all deliver a stable Coulombic efficiency of 99.9% and excellent rate capability at low temperatures. Pouch cells containing layered cathodes also demonstrate impressive cycling stability over 1,000 cycles and exceptional rate capability down to −20 °C. Through experiments and theoretical modeling, we have identified a balanced SEI-based approach that achieves stable, fast-charging, low-temperature Li-ion batteries.
Lithium Dinitramide as an Additive in Lithium Power Cells
Lithium dinitramide, LiN(NO2)2 has shown promise as an additive to nonaqueous electrolytes in rechargeable and non-rechargeable lithium-ion-based electrochemical power cells. Such non-aqueous electrolytes consist of lithium salts dissolved in mixtures of organic ethers, esters, carbonates, or acetals. The benefits of adding lithium dinitramide (which is also a lithium salt) include lower irreversible loss of capacity on the first charge/discharge cycle, higher cycle life, lower self-discharge, greater flexibility in selection of electrolyte solvents, and greater charge capacity. The need for a suitable electrolyte additive arises as follows: The metallic lithium in the anode of a lithium-ion-based power cell is so highly reactive that in addition to the desired main electrochemical reaction, it engages in side reactions that cause formation of resistive films and dendrites, which degrade performance as quantified in terms of charge capacity, cycle life, shelf life, first-cycle irreversible capacity loss, specific power, and specific energy. The incidence of side reactions can be reduced through the formation of a solid-electrolyte interface (SEI) a thin film that prevents direct contact between the lithium anode material and the electrolyte. Ideally, an SEI should chemically protect the anode and the electrolyte from each other while exhibiting high conductivity for lithium ions and little or no conductivity for electrons. A suitable additive can act as an SEI promoter. Heretofore, most SEI promotion was thought to derive from organic molecules in electrolyte solutions. In contrast, lithium dinitramide is inorganic. Dinitramide compounds are known as oxidizers in rocket-fuel chemistry and until now, were not known as SEI promoters in battery chemistry. Although the exact reason for the improvement afforded by the addition of lithium dinitramide is not clear, it has been hypothesized that lithium dinitramide competes with other electrolyte constituents to react with lithium on the surface of the anode to form a beneficial SEI. Apparently, nitrides and oxides that result from reduction of lithium dinitramide on the anode produce a thin, robust SEI different from the SEIs formed from organic SEI promoters. The SEI formed from lithium dinitramide is more electronically insulating than is the film formed in the presence of an otherwise identical electrolyte that does not include lithium dinitramide. SEI promotion with lithium dinitramide is useful in batteries with metallic lithium and lithium alloy anodes.
Binary Cation Matrix Electrolyte and Its Effect on Solid Electrolyte Interphase Suppression and Evolution of Si Anode
An unstable solid electrolyte interphase (SEI) has been recognized as one of the biggest challenges to commercializing silicon (Si) anodes for high-energy-density batteries. This work thoroughly investigates a binary cation matrix of Mg 2+ +Li + electrolyte and its role in SEI development, suppression, and evolution of a Si anode. Findings demonstrate that introducing Mg ions dramatically reduces the SEI growth before lithiation occurs, primarily due to the suppression of solvent reduction, particularly ethylene carbonate (EC) reduction. The Mg 2+ alters the Li + cation solvation environment as EC preferably participates in the oxophyllic Mg 2+ solvation sheath, thereby altering the solvent reduction process, resulting in a distinct SEI formation mechanism. The initial SEI formation before lithiation is reduced by 70% in the electrolyte with the presence of Mg 2+ cations. While the SEI continues to develop in the postlithiation, the inclusion of Mg ions results in an approximately 80% reduction in the postlithiation SEI growth. Continuous electrochemical cycling reveals that Mg 2+ plays a crucial role in stabilizing the deep-lithiated Si phases, which effectively mitigates side reactions, resulting in controlled SEI growth and stable interphase while eliminating complex Li x Si y formation. Mg ions promote the development of a notably more rigid and homogeneous SEI, characterized by a reduced dissipation (ΔD) in the Mg 2+ +Li + ion matrix compared to the solely Li + system. In conclusion, this report reveals how the Mg 2+ +Li + ion matrix affects the SEI evolution, viscoelastic properties, and electrochemical behavior at the Si interface in real time, laying the groundwork for devising strategies to enhance the performance and longevity of Si-based next-generation battery systems.
Lithium-ion battery physics and statistics-based state of health model
A pseudo-2d model using COMSOL Multiphysics® software is developed to simulate performance and performance degradation of Li-ion batteries consisting of layered and olivine cathodes with graphite anode when subjected to peak shaving grid service. Multiple degradation pathways are considered, including solid electrolyte interphase (SEI) formation and breakdown at the anode, cathode dissolution and its synergistic effect on SEI formation at the anode. The model is validated by simulating commercial cylindrical cell performance. A global model is developed to simulate performance across all chemistries, along with individual chemistry models using global model parameters as initial values. There is good agreement between these models for various optimization parameters such as SEI equilibrium potential, cathode dissolution exchange current density, solvent diffusivity in the SEI and SEI ionic conductivity. To circumvent time constraints related to the COMSOL model, a 0d global model is developed which fits data well and provides more clarity on differences in cathode dissolution exchange current density. Again, good agreement for various optimization parameters is obtained among the COMSOL global & individual chemistry models and the 0-d model. The lessons learned from the physics-based model is used to develop a top down statistics-based model using current, voltage and anode volumetric change per mole lithium intercalated, along with their interactions as degradation predictors. This model predicts out of sample degradation for multiple grid services and electric vehicle drive cycle with high accuracy and provides the pathway to develop an efficient battery management system combining machine learning and findings from physics-based computationally intensive algorithms.
Multi-modal characterization methods of solid-electrolyte interphase in silicon-graphite composite electrodes
Composite silicon-graphite (Si-Gr) anodes can improve battery energy density, due to Si's high gravimetric capacity, while mitigating mechanical degradation of the anode and solid-electrolyte interphase (SEI) caused by Si volumetric expansion. Optimizing these anodes is challenging, in part due to difficulty characterizing the SEI structure and composition. In this work, we present multi-modal characterization of the SEI on composite Si-Gr anodes to relate SEI chemical composition and structure to functional properties. Discrepancies in elemental concentrations from X-ray photoelectron spectroscopy, Auger electron spectroscopy, and energy-dispersive X-ray spectroscopy (EDS) are attributed to varying information depth and lateral resolution of the individual probes. However, by combining quantitative composition information with spatially resolved element mapping from scanning transmission electron microscopy, EDS, and electron energy loss spectroscopy, a holistic picture of the SEI emerges. We observe the bilayer SEI structure and a direct correlation between elemental Li and F, suggesting that most Li in the SEI exists as lithium fluoride (LiF). Further, LiF concentration is directly proportional to the maximum SEI resistivity, as determined by scanning spreading resistance microscopy. Lastly, there is an inverse relationship between lithium carbonate and LiF concentration in the SEI, providing insight into the detailed chemistry of SEI formation and evolution.
Sweeping potential regulated structural and chemical evolution of solid-electrolyte interphase on Cu and Li as revealed by cryo-TEM
A fundamental understanding of solid-electrolyte interphase (SEI) is paramount importance for controlling the cycling performance of rechargeable lithium metal batteries. The structural and chemical evolution of SEI with respect to electrochemical operating condition remains barely established. Here we develop a unique method for imaging the evolution of SEI formed on the Cu foil under sweeping electrochemical potential. By using cryogenic TEM imaging combined with energy dispersive X-ray spectroscopy and X-ray photoelectron spectroscopy electronic structure analyses, we reveal that, for the vinylene carbonate (VC)-free electrolyte, the SEI formed at 1.0 V is a monolithic amorphous structure, which evolves to amorphous matrix embedded with Li 2 O particles as the voltage decreases to 0 V. In the case of VC-containing electrolyte, the SEI is featured by an amorphous matrix with Li 2 O particles from 1.0 V to 0 V. The thickness of SEI formed on Cu foil increases with decreasing voltage. Associated with the localized charge modulation by the surface topographic feature and defects in the Cu foil, the SEI layer shows direct spatial correlation with these structural defects in the Cu. In addition, upon Li deposition, the SEI formed on the Li metal has similar thickness with, but different composition from the SEI formed on the Cu foil at 0 V. Furthermore, those results provide insight toward SEI engineering for enhanced cycling stability of Li metal.
Emerging Potassium Metal Anodes: Perspectives on Control of the Electrochemical Interfaces
Potassium metal acts as the anode in emerging potassium metal batteries (KMBs). It further serves as the counter-electrode for potassium ion battery (KIB) half-cells, with its reliable performance being critical for assessing the working electrode material. This first-of-its-kind critical review focuses on the dual challenge of controlling the potassium metal-substrate and the potassium metal-electrolyte interface so as to prevent dendrites. The discussion begins with a comparison of the physical and chemical properties of K metal anodes versus the much oft studied Li and Na metal anodes. Based on established descriptions for root causes of dendrites, the problem should be less severe for K than for Li or Na, while in fact the opposite is observed. The key reason that the K metal surface rapidly becomes dendritic in common electrolytes is its unstable solid electrolyte interphase (SEI). An unstable SEI layer is defined as being non self-passivating. No SEI is perfectly stable during cycling, and all SEI structures are heterogenous both vertically and horizontally relative to the electrolyte interface. The difference between a "stable" and an "unstable" SEI may be viewed as the relative degree to which during cycling it thickens and becomes further heterogeneous. The unstable SEI on K metal leads to a number of interrelated problems, such as low cycling Coulombic efficiency (CE), a severe impedance rise, large overpotentials, and possibly electrical shorting; all of which have been reported to occur as early as in the first ten plating/stripping cycles. Many of the traditional "interface fixes" employed for Li and Na metal anodes, such as various artificial SEIs, surface membranes, barrier layers, the secondary separators, etc. have not been attempted or optimized for the case of K. This is an important area for further exploration, with an understanding that success may come harder than with Li due to K-based SEI reactivity with both ether and ester solvents. The second critical problem with K metal anodes is that they do not thermally or electrochemically wet a standard (untreated) Cu foil current collector. Published experimental and modeling research directly highlights the weak bonding between the K atoms and a Cu surface. Existing surface treatment approaches that achieve improved K wetting are discussed, along with the general design rules for future studies. Also discussed are geometry-based methods to tune nucleation, as well dual approaches where nucleation and SEI structure are tuned through complementary schemes to achieve extended half-cell and full battery stability. We hypothesize that K metal never achieves a planar wetting morphology even at cycle one making the dendrites "baked-in". We propose that classical thin films growth models, Frank van der Merwe (F-M), Volmer Weber (V-W), and Stranski-Krastanov (S-K) can be employed to describe early stage plating behavior. It is demonstrated that island-like V-W growth is the applicable description for the natural plating behavior of K on pristine Cu. Moving forward, there are three inter-related thrusts to be pursued: First, K salt - based electrolyte formulations have to mature and become further tailored to handle the increased reactivity of a metal rather than an ion anode. Second, the K-based SEI structure needs to be further understood and ultimately tuned to be less reactive. Third, the energetics of the K metal - current collector interface must be controlled to promote planar wetting/dewetting throughout cycling.
Resolving Nanoscopic and Mesoscopic Heterogeneity of Fluorinated Species in Battery Solid-Electrolyte Interphases by Cryogenic Electron Microscopy
The stability of lithium batteries is tied to the physicochemical properties of the solid-electrolyte interphase (SEI). Owing to the difficulty in characterizing this sensitive interphase, the nanoscale distribution of SEI components is poorly understood. Here, we use cryogenic scanning transmission electron microscopy (cryo-STEM) to map the spatial distribution of SEI components across the metallic Li anode. We reveal that LiF, an SEI component widely believed to play an important role in battery passivation, is absent within the compact SEI film (~15 nm); instead, LiF particles (100–400 nm) precipitate across the electrode surface. We term this larger length scale as the indirect SEI regime. On the basis of these observations, we conclude that LiF cannot be a dominant contribution to anode passivation nor does it influence Li+ transport across the compact SEI film. We refine the traditional SEI structure derived from ensemble-averaged characterizations and nuance the role of SEI components on battery performance.
Current Density Regulated Atomic to Nanoscale Process on Li Deposition and Solid Electrolyte Interphase Revealed by Cryogenic Transmission Electron Microscopy
Current density has been perceived to play a critical rule for controlling Li deposition morphology and solid electrolyte interphase (SEI). However, the atomic level mechanism of current density on Li deposition and the SEI remains unclear. In this work, based on cryogenic transmission electron microscopy imaging combined with energy dispersive X-ray spectroscopy and electron energy loss spectroscopy electronic structure analyses, we reveal the atomic level correlation of Li deposition morphology and SEI with current density. We discover that increasing current density leads to increased overpotential for Li nucleation and growth, leading to the transition from growth-limited to nucleation-limited mode for Li dendrite. Independence of current density, the electrochemically deposited Li metal (EDLi) exhibits crystalline whisker-like morphology. The SEI formed at low current density (0.1 mA cm -2 ) is monolithic amorphous; while, a current density of above 2 mA cm -2 leads to a mosaic structured SEI, featuring an amorphous matrix with Li 2 O and LiF dispersoids, and the thickness of the SEI increases with the increase of current density. Uniquely, the Li 2 O particles is spatially located at the top surface of the SEI, while LiF is spatially adjacent to the Li-SEI interface. These results highlight the possible tuning of crucial structural and chemical features of EDLi and SEI through altering deposit conditions and consequently direct correlation with electrochemical performance.