Laser‐Powder Melt Pool Solidification Dynamics and Microstructural Engineering of Ti‐5553 Microlattices

The fine geometric and topological control afforded by additive manufacturing technologies has enabled the manufacture of architected materials across length scales, and enabling tunable mechanical performance as a function of local and global design. Progress has been made to tune the mechanical response of architected materials through geometry, but understanding how the geometry and processing conditions will inform the microstructure remains a challenge due to the rapid solidification in laser powder bed fusion. This study uses in situ X-ray imaging and electron backscatter diffraction microscopy to demonstrate that the melt pool size, microstructure morphology, and elastic strain distribution is influenced by a combination of lattice geometry and laser processing conditions. These results indicate that within larger melt pools the local thermal gradients are sufficient to enable a columnar-to-equiaxed transition across the melt pool. Furthermore, the solidification mechanisms producing these microstructures are examined across the first 5 ms of melting and solidification, described via in situ high-speed X-ray imaging and mirrored via multiphysics simulation.

additive manufacturing↗

Microstructure and Hard Magnetic Properties of Sm 1-x Zr x (Fe,Co) 11.3-y Ti 0.7 By Ingots and Thick Melt-Spun Ribbons

Permanent magnets made from Sm(Fe,Co) 12 -based compounds are being actively pursued through nanostructuring and powder metallurgy. This study was aimed at the development of hard magnetic properties in bulk as-cast alloys and in melt-spun alloys for very low wheel speeds. Slower solidification rates and alloying with Zr promote the tetragonal ThMn 12 -type crystal structure, whereas higher solidification rates and alloying with B replace the ThMn 12 structure type with the TbCu 7 structure type. When introduced simultaneously, Zr and B dramatically reduce the alloy solidification rates required for both the refinement of the 1:12 crystallites and their replacement with the 1:7 phase. In bulk arc-melted alloys, this allowed for a microstructure of separated 1:12 crystallites 1–3 μm in size, although, because of the ferromagnetic nature of a minority phase, the coercivity of these fine-grained alloys reached only 0.73 kOe. A moderately accelerated solidification further refined the 1:12 crystallites and increased the coercivity; a Sm 0.7 Zr 0.4 (Fe,Co) 10.8 Ti 0.7 B 0.5 alloy exhibited a coercivity of 1.5 kOe and a maximum energy product of 3.4 MGOe when it was melt-spun into a 0.26-mm-thick ribbon. A more rapid solidification suppressed the 1:12 phase and after annealing at 800–850 °C, the alloys modified with Zr and B developed reasonably high coercivity and maximum energy product even when melt-spun at a wheel speed of 6 m/s. For the above-mentioned alloy, these values were 4.1 kOe and 7.8 MGOe, respectively. Further, a similarly processed very-Sm-lean Sm 0.5 Zr 0.6 (Fe,Co) 10.6 Ti 0.7 B 0.7 alloy exhibited a remanence of 8.8 kG and an energy product of 7.4 MGOe.

36 MATERIALS SCIENCE↗

In Situ X-ray Radiography and Computational Modeling to Predict Grain Morphology in $\beta$-Titanium during Simulated Additive Manufacturing

The continued development of metal additive manufacturing (AM) has expanded the engineering metallic alloys for which these processes may be applied, including beta-titanium alloys with desirable strength-to-density ratios. To understand the response of beta-titanium alloys to AM processing, solidification and microstructure evolution needs to be investigated. In particular, thermal gradients (Gs) and solidification velocities (Vs) experienced during AM are needed to link processing to microstructure development, including the columnar-to-equiaxed transition (CET). In this work, in situ synchrotron X-ray radiography of the beta-titanium alloy Ti-10V-2Fe-3Al (wt.%) (Ti-1023) during simulated laser-powder bed fusion (L-PBF) was performed at the Advanced Photon Source at Argonne National Laboratory, allowing for direct determination of Vs. Two different computational modeling tools, SYSWELD and FLOW-3D, were utilized to investigate the solidification conditions of spot and raster melt scenarios. The predicted Vs obtained from both pieces of computational software exhibited good agreement with those obtained from in situ synchrotron X-ray radiography measurements. The model that accounted for fluid flow also showed the ability to predict trends unobservable in the in situ synchrotron X-ray radiography, but are known to occur during rapid solidification. A CET model for Ti-1023 was also developed using the Kurz–Giovanola–Trivedi model, which allowed modeled Gs and Vs to be compared in the context of predicted grain morphologies. Both pieces of software were in agreement for morphology predictions of spot-melts, but drastically differed for raster predictions. The discrepancy is attributable to the difference in accounting for fluid flow, resulting in magnitude-different values of Gs for similar Vs.

36 MATERIALS SCIENCE↗

Effect of Undercooling in a Low-Gravity Containerless Environment on the Structure and Properties of Alloys

The 30 meter and 100 meter drop tubes at the Marshall Space Flight Center offer a unique opportunity to study solidification in a containerless, microgravity environment. Samples are melted in a furnace at the top of the drop tube and solidify during a 4.5 second free fall in the 100 meter drop tube or a 2.6 second free fall in the 30 meter drop tube. The cooling rate obtained in the drop tubes is lower than cooling rates in atomization and splat-quenching processes. Decoupling the rapid solidification process allows the study of the effects of undercooling and recalescence on alloy morphologies. The research therefore has a three-fold purpose. The first is examination of the limits of undercooling of niobium and niobium-base alloys in the drop tube. The second purpose is the observation of microstructures resulting from the solidification of samples at large undercoolings and moderate cooling rates. The third purpose is the observation of metastable phase formation in highly undercooled samples.

Bayuzick, R. J.↗

Effects of Solidification Cooling Rates on Microstructures and Physical Properties of Fe-6.5%Si Alloys

Compared to the widely used Fe-3.2wt%Si steel, Fe-6.5wt%Si has superior electric and magnetic properties, including higher electrical resistivity, lower iron loss, higher permeability, and near zero magnetostriction. However, Fe-6.5wt%Si sheet is difficult to produce using traditional manufacturing processes as the high silicon content favors the formation of ordered phases that embrittle the material. Fortunately, these ordered phases can be suppressed if the alloy is cooled fast enough from a high temperature kinetically trapping the disordered solid solution or amorphous state. Planar flow casting is known for its rapid solidification rate. In order to consider it as a viable method to manufacture ductile Fe-6.5wt%Si sheets, the effect of cooling rate on physical properties of Fe-6.5wt%Si alloy are systematically investigated. In this work, various cooling rates are achieved by changing melt-spin wheel speeds, which significantly affect the solidification temperature profile and have profound effects on ordering, microstructures, textures, hardness, and magnetic properties. High cooling rates result in refined grains, reduced ordering, enhanced <100> out of the plane texture, decreased hardness, and increased coercivity. This study demonstrates a critical cooling rate at ~1.7 × 10 5 K/s, corresponding to a tangential wheel speed of 5-7 m/s, below which the hardness significantly increases in agreement with the sudden increase of the ordered phases that causes the material embrittlement.

36 MATERIALS SCIENCE↗

Nanoscale interfacial melting enables bonding during high velocity microparticle impacts

Melting during high-velocity particle impact has been understood to be typically detrimental to bonding by lowering the strength at the interface and promoting rebound before solidification can occur. Here we establish a possible remedy to this challenge: by dramatically restricting the volume of molten material, its resolidification is accelerated, effectively forming a nanoscale, braze-type joint during impact. In-situ single particle impact imaging is combined with post-mortem structural and chemical analyses to reveal a regime where adhesion is governed not by extensive plastic deformation, but by the kinetics of melt layer resolidification. Furthermore, these findings redefine the role of melting in impact-based processes, establishing transient melting and rapid solidification as a viable strategy for engineering successful adhesion events.

Additive manufacturing↗

The study of dopant segregation behavior during the growth of GaAs in microgravity

An investigation into the segregation behavior of selenium doped gallium arsenide during directional solidification in the microgravity environment was conducted using the Crystal Growth Furnace (CGF) aboard the first United States Microgravity Laboratory (USML-1). The two crystals grown were 1.5 cm in diameter and 16.5 cm in length with an initial melt length of 14 cm. Two translation periods were executed, the first at 2.5 microns/s and after a specified time, which was different between the two experiments, the translation rate was doubled to 5.0 microns/s. The translation was then stopped and the remaining sample melt was solidified using a gradient freeze technique in the first sample and a rapid solidification in the second experiment. Measurement of the selenium dopant distribution, using quantitative infrared transmission imaging, indicates that the first sample initially achieved diffusion controlled growth as desired. However, after about 1 cm of growth, the segregation behavior was driven from a diffusion controlled growth regime to a complete mixing regime. Measurements in the second flight sample indicated that the growth was always in a complete mixing regime. In both experiments, voids in the center line of the crystal, indicative of bubble entrapment, were found to correlate with the position in the crystal when the translation rates were doubled.

Matthiesen, David H.↗

Transient Effects in Planar Solidification of Dilute Binary Alloys

The initial transient during planar solidification of dilute binary alloys is studied in the framework of the boundary integral method that leads to the non-linear Volterra integral governing equation. An analytical solution of this equation is obtained for the case of a constant growth rate which constitutes the well-known Tiller's formula for the solute transient. The more physically relevant, constant ramping down temperature case has been studied both numerically and analytically. In particular, an asymptotic analytical solution is obtained for the initial transient behavior. A numerical technique to solve the non-linear Volterra equation is developed and the solution is obtained for a family of the governing parameters. For the rapid solidification condition, growth rate spikes have been observed even for the infinite kinetics model. When recirculating fluid flow is included into the analysis, the spike feature is dramatically diminished. Finally, we have investigated planar solidification with a fluctuating temperature field as a possible mechanism for frequently observed solute trapping bands.

Mazuruk, K.↗

Transient Effects in Planar Solidification of Dilute Binary Alloys

The initial transient during planar solidification of dilute binary alloys is studied in the framework of the boundary integral method that leads to the non-linear Volterra integral governing equation. An analytical solution of this equation is obtained for the case of a constant growth rate which constitutes the well-known Tiller's formula for the solute transient. The more physically relevant, constant ramping down temperature case has been studied both numerically and analytically. In particular, an asymptotic analytical solution is obtained for the initial transient behavior. A numerical technique to solve the non-linear Volterra equation is developed and the solution is obtained for a family of the governing parameters. For the rapid solidification condition, growth rate spikes have been observed even for the infinite kinetics model. When recirculating fluid flow is included into the analysis, the spike feature is dramatically diminished. Finally, we have investigated planar solidification with a fluctuating temperature field as a possible mechanism for frequently observed solute trapping bands.

Mazuruk, Konstantin↗

Localized orientation gradients in additively manufactured stainless steel 316H structures

The high solidification rates during additive manufacturing cause highly localized thermal and strain gradients. The effect of these gradients on the evolution of local orientation misorientations within a grain is not well understood. In this study, stainless steel 316H parts were fabricated via laser powder bed fusion using three different energy densities: 43, 71, and 135 J/mm 3 . Electron backscatter diffraction showed that the maximum misorientations of the grains can be up to 25° along the build direction. Misorientation gradients (RM g ) within grains are process-dependent and can change from 0.036°/μm to 0.015°/μm with increased volumetric energy densities. In conclusion, the characterized misorientation gradients are an indication of the level of dislocations and, to an extent, the plastic deformation resulting from the rapid solidification during laser powder bed fusion.

316H↗

Refining Microstructures in Additively Manufactured Al/Cu Gradients Through TiB 2 Inclusions

Here, the additive manufacture of compositionally graded Al/Cu parts by laser engineered net shaping (LENS) is demonstrated. The use of a blue light build laser enabled deposition on a Cu substrate. The thermal gradient and rapid solidification inherent to selective laser melting enabled mass transport of Cu up to 4 mm from a Cu substrate through a pure Al deposition, providing a means of producing gradients with finer step sizes than the printed layer thicknesses. Divorcing gradient continuity from layer or particle size makes LENS a potentially enabling technology for the manufacture of graded density impactors for ramp compression experiments. Printing graded structures with pure Al, however, was prevented by the growth of Al 2 Cu 3 dendrites and acicular grains amid a matrix of Al 2 Cu. A combination of adding TiB 2 grain refining powder and actively varying print layer composition suppressed the dendritic growth mode and produced an equiaxed microstructure in a compositionally graded part. Material phase was characterized for crystal structure and nanoindentation hardness to enable a discussion of phase evolution in the rapidly solidifying melt pool of a LENS print.

36 MATERIALS SCIENCE↗

Laser Patterning Assisted Devitrification and Domain Engineering of Amorphous and Nanocrystalline Alloys

We have investigated laser-patterning and devitrification as a novel method to realize emergent properties in modified regions at the ribbon surface consisting of periodic localized laser spots thermally treated under rapid heating and cooling conditions. Fe-based amorphous ribbons were annealed for systematically varied laser power. Extremely high heating and cooling rates on the order of 10(exp 8)-10(exp 10)K/s have been estimated by finite element analysis simulations. Observations suggest surface melting followed by rapid solidification fast enough to quench and form an amorphous structure upon cooling. Diffusion of heat occurs from the laser irradiated surface region so that a finite volume of material surrounding this region rises in temperature above the crystallization temperature relevant for conventional isothermal annealing experiments. The underlying mechanism of laser annealing and consequences of heat transients involved are discussed in terms of impacts upon micro/nanostructure, residual stresses, and magnetic domain structure surrounding the laser irradiated region. The study illustrates the potential to exploit spatially optimized phase transformations in a scalable manufacturing process of amorphous and nanocrystalline alloys to locally access otherwise inaccessible extreme heating and cooling rates.

Amorphous ribbons↗

Pitting Corrosion in 316L Stainless Steel Fabricated by Laser Powder Bed Fusion Additive Manufacturing: A Review and Perspective

Abstract 316L stainless steel (316L SS) is a flagship material for structural applications in corrosive environments, having been extensively studied for decades for its favorable balance between mechanical and corrosion properties. More recently, 316L SS has also proven to have excellent printability when parts are produced with additive manufacturing techniques, notably laser powder bed fusion (LPBF). Because of the harsh thermo-mechanical cycles experienced during rapid solidification and cooling, LPBF processing tends to generate unique microstructures. Strong heterogeneities can be found inside grains, including trapped elements, nano-inclusions, and a high density of dislocations that form the so-called cellular structure. Interestingly, LPBF 316L SS not only exhibits better mechanical properties than its conventionally processed counterpart, but it also usually offers much higher resistance to pitting in chloride solutions. Unfortunately, the complexity of the LPBF microstructures, in addition to process-induced defects, such as porosity and surface roughness, have slowed progress toward linking specific microstructural features to corrosion susceptibility and complicated the development of calibrated simulations of pitting phenomena. The first part of this article is dedicated to an in-depth review of the microstructures found in LPBF 316L SS and their potential effects on the corrosion properties, with an emphasis on pitting resistance. The second part offers a perspective of some relevant modeling techniques available to simulate the corrosion of LPBF 316L SS, including current challenges that should be overcome.

Voisin, T. (ORCID:0000000287462659)↗

Laser Powder Bed Fusion of ODS 14YWT from Gas Atomization Reaction Synthesis Precursor Powders

Abstract Laser powder bed fusion (LPBF) additive manufacturing (AM) is a promising route for the fabrication of oxide dispersion strengthened (ODS) steels. In this study, 14YWT ferritic steel powders were produced by gas atomization reaction synthesis (GARS). The rapid solidification resulted in the formation of stable, Y-containing intermetallic Y 2 Fe 17 on the interior of the powder and a stable Cr-rich oxide surface. The GARS powders were consolidated with LPBF. Process parameter maps identified a stable process window resulting in a relative density of 99.8%. Transmission electron microscopy and high-energy x-ray diffraction demonstrated that during LPBF, the stable phases in the powder dissociated in the liquid melt pool and reacted to form a high density (1.7 × 10 20 /m 3 ) of homogeneously distributed Ti 2 Y 2 O 7 pyrochlore dispersoids ranging from 17 to 57 nm. The use of GARS powder bypasses the mechanical alloying step typically required to produce ODS feedstock. Preliminary mechanical tests demonstrated an ultimate tensile and yield strength of 474 MPa and 312 MPa, respectively.

36 MATERIALS SCIENCE↗

Suppressing Ordering in Equiatomic Fe-Co via Laser Powder Bed Fusion

Neutron and electron diffraction was employed to evaluate the effectiveness of thermal management strategies in suppressing the formation of the equilibrium-ordered B2 (CsCl) phase in equiatomic binary Fe-Co specimens fabricated by laser powder bed fusion additive manufacturing. Specimens with a tensile dogbone geometry were fabricated using various combinations of process parameters (laser power and raster speed) and thermal management strategies (no support struts, struts only in the top gauge section, and struts throughout the gauge section). Diffraction results demonstrate that the rapid solidification during PBF-L effectively minimized B2 formation, with laser power and effective scan velocity having no significant impact on the degree of ordering. Furthermore, the inclusion of support struts in the top grip region had no perceivable impact on ordering, whereas specimens with support struts in the gauge region exhibited no detectable ordering. Results are discussed in the context of thermal finite element analysis predictions.

Laser Material Processing↗

Laser powder bed fusion of Inconel 718 on 316 stainless steel

The joining of Inconel 718 and 316 stainless steel has notable industrial importance. However, traditional arc-welding has many issues. In particular, the formation of the detrimental Nb-rich Laves phase in the heat affected zone can promote crack initiation and propagation, which leads to poor mechanical properties. The small heat input and the rapid solidification of laser powder bed fusion (PBF) has the potential to suppress this problem. Despite the infancy of the multi-material PBF, it is of interest to investigate the relationship among the process parameter, the microstructure at the materials joining point, and the mechanical performance. In this study, we used high-speed x-ray imaging to in-situ monitor the printing of Inconel 718 tracks on a 316H SS substrate via laser powder bed fusion, followed by post-build characterization and testing with SEM, XRD and nanoindentation. We observed that a higher linear energy density resulted in a more diffused interface and a smaller compositional gradient, but as a trade-off, generated more keyhole pores and thermal cracks. Furthermore, we also showed that the built layer exhibited chemical inhomogeneity at two length scales: a tens-of-mu m-scale compositional vortex due to the melt flow, and a sub-mu m-scale Nb-rich dendritic structure due to the non-equilibrium solidification that led to the formation of the Laves phase. It was inferred that the chemical inhomogeneity may benefit the mechanical properties at the interface by providing more interlocking between the two materials and also by limiting the effect of the brittle Laves phase to potentially short range.

36 MATERIALS SCIENCE↗

Ultrafine-grained Fe-TiB 2 high-modulus nanocomposite steel with high strength and isotropic mechanical properties by laser powder bed fusion

Fe-TiB 2 metal matrix composite, also called high-modulus steels (HMSs), are of great interest for applications in fuel-efficient transportation infrastructure, aerospace, and wear industries due to their high specific stiffness and yield strength. However, conventional cast Fe-TiB 2 HMSs often contain coarse and sharp-edged TiB 2 particles which easily trigger premature cracking during loading. Here, we synthesized a Fe-TiB 2 nanocomposite HMS via laser powder bed fusion (LPBF) additive manufacturing of mixed micro-sized powders of Fe, Ti, and Fe 2 B. We investigated the microstructure formation and mechanical behavior of the Fe-TiB 2 HMS. We found that in situ chemical reaction of Ti and Fe 2 B enables the formation of TiB 2 particles at nanoscale during rapid solidification of LPBF. These nanoscale TiB 2 particles can serve as heterogeneous nucleation sites and promote the formation of ultrafine and equiaxed α-Fe grains with random crystallographic textures, which differ from many other additively manufactured (AM) metal alloys characteristic of strong crystallographic textures. As such, isotropic mechanical properties were achieved in the AM Fe-TiB 2 nanocomposite HMS with a high elastic modulus of ~ 240 GPa, an exceptional yield strength of ~ 1450 MPa, and a large plasticity of ~ 20% under compression. Quantitative analysis reveals that the high yield strength primarily originates from strengthening contributions of the ultrafine grains with an average grain size of ~450 nm, the nanoscale TiB 2 reinforcing particles of 20–180 nm, and a high density of printing-induced dislocations of the order of 10 15 m –2 . In situ synchrotron high-energy X-ray diffraction unveils the load partitioning from the softer α-Fe matrix to the stiffer and stronger TiB 2 nanoparticles, contributing to the sustained strain hardening during compression. Our work not only provides a general pathway for achieving high-performance metal matrix nanocomposites by in situ chemical reaction and precipitation of ceramic nanoparticles during additive manufacturing, but also offers mechanistic insights into the deformation mechanism of nanoparticle-reinforced HMS composites.

36 MATERIALS SCIENCE↗

Microstructure and strengthening of Al-6Ce-3Ni-0.7Fe (wt%) alloy manufactured by laser powder-bed fusion

In this study, an Al-6Ce-3Ni-0.7Fe (wt%) alloy was fabricated via laser powder-bed fusion and its microstructure, thermal stability, tensile properties, and creep properties are investigated for two rapid-solidification rates with different eutectic spacings. For both faster- and slower-cooled states, the as-fabricated alloy mostly shows elongated grains with very fine eutectic networks (~40 nm lamellar width) comprising a high-volume fraction (~18 %) of intermetallic phases. Faster-cooled samples, however, display a less continuous eutectic network with finer spacing (~100 nm), leading to higher Orowan strengthening and therefore superior microhardness and yield stress up to ~350 °C. Upon aging (300 - 450 °C), micron-size Al 9 (Ni,Fe) 2 needle-like precipitates form within grains, and the Al 11 Ce 3 eutectic network spheroidizes, while retaining a submicron width and spacing, resulting in 33–37 % drop in microhardness after 144 h aging at 400 °C. Limited tensile ductility (~6 %) and creep ductility (~1-2 %) are measured for both faster- and slower-cooled alloys due to an inhomogeneous microstructure, where cavitation preferentially initiates at melt-pool boundaries, precipitate-free zones, and/or denuded zones, eventually leading to local fracture. Denuded zones, induced by stress, form due to diffusional flow with stress-dependent orientations, and are identified as microstructurally weak regions leading to strain localization. The present alloy does not show a significant difference in 300 °C creep resistance between: (i) tensile and compressive loading, (ii) faster- and slower-cooled samples, and (iii) continuous and spheroidized eutectics. Creep resistance at 300 °C is comparable to that of a Ce-richer Al-10.5Ce-3.1Ni-1.2Mn (wt%) alloy, despite the formation of denuded zones and needle-like Al 9 (Ni,Fe) 2 precipitates.

36 MATERIALS SCIENCE↗