Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “PRESSING”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 127 records · Page 7

Performance of Nd-Fe-B Magnets Fabricated by Hot Isostatic Pressing and Low-Temperature Sintering

Magnetic properties and microstructure of Nd-Fe-B sintered magnets fabricated by hot isostatic pressing (HIP) were studied. For comparison, magnets were also fabricated by vacuum sintering. The density reached 7.58 g/cm{sup 3} for the magnets HIP-sintered at 1123 K. The density of the magnets vacuum-sintered at 1123 K was much lower, which is of about 6.92 g/cm{sup 3}. While the density of magnets vacuum-sintered at 1318 K was the same as the HIP-sintered magnets, the sintering temperature was significantly decreased to 1123 K. In addition, the average grain size decreased from 9 to 6 μm, which has enhanced coercivity. Therefore, the coercivity increased from 1067.7 to 1238.5 kA/m, which is 16% higher than the vacuum-sintered magnets. HIP is a promising method to obtain high density and high coercivity Nd-Fe-B sintered magnets.

36 MATERIALS SCIENCE↗

Investigation on Equal-Channel Angular Pressing-Induced Grain Refinement in an Aluminum Matrix Composite Reinforced with Al-Cu-Ti Metallic Glass Particles

In the present study, a homogeneous ultrafine grain structure composite consisting of metallic glass particles reinforcements was developed by equal-channel angular pressing (ECAP) process. The microstructure of composite was characterized using x-ray diffraction (XRD), transmission electron microscopy (TEM) and electron backscatter diffraction (EBSD) techniques. The uniaxial compression test was used to determine the mechanical properties. The mechanisms of grain refinement during ECAP process were discussed based on the microstructural evolutions. A composite was successfully produced after four passes of ECAP, having an average grain size of 610 nm and compressive yield strength of 242 MPa. Also, the yield strength of composite after each pass was quantitatively estimated by considering all the effective strengthening mechanism. The findings showed that the dislocations strengthening mechanism with contribution of more than 50% plays a major role in strengthening the composite. There was a negligible gap between the experimental and theoretical values of yield strength for all ECAP pass numbers.

36 MATERIALS SCIENCE↗

Fabrication, Microstructures, and Properties of 50 vol.% SiCp/6061Al Composites via Hot Pressing

Nearly fully dense 50 vol.% SiCp/6061Al composites were fabricated via hot pressing (HPing) at temperatures ranging from 610 to 650 °C, with the axial load and holding time fixed as 25 MPa and 120 min, respectively. The interfacial reactions, microstructures, and properties of the SiCp/Al alloy were studied. The interface reaction between SiCp and the Al alloy was suppressed at annealing temperatures of 620 °C and below; however, the reaction intensified as the annealing temperature increased, producing Al{sub 4}C{sub 3}, Si, and Mg{sub 2}Si. With an increase in HPing temperature from 610 to 630 °C, the 6061Al alloy melted and gradually filled the pores in the SiC particles under the applied load. The density, bending strength, and thermal conductivity (TC) of the composites increased, whereas the coefficient of thermal expansion (CTE) of the composites decreased. With an increase in HPing temperature increased from 630 to 650 °C, the 6061Al alloy melt leaked through the sintered bodies, resulting in the microstructural degradation and property reduction of the composites. The 50 vol.% SiCp/6061Al composites fabricated by HPing at 630 °C exhibited optimal comprehensive properties [bending strength, 332.4 MPa; TC, 186.3 W(m K){sup −1}; and CTE, 7.9 × 10{sup −6}/°C (20-100 °C)], which were attributed to the highest relative density and the best SiCp/Al interfacial structure of the composites.

36 MATERIALS SCIENCE↗

Development of Texture in Ultrafine-Grained Low-Carbon Steel Processed through Equal-Channel Angular Pressing

Developments of microstructures and texture are investigated for a low-carbon steel deformed by equal-channel angular pressing (ECAP) at room temperature for equivalent strain (ε{sub vm}) of 16.8. ECAP at ε{sub vm} = 0.6 reduces grain size by two orders of magnitude. With increasing strain, grain size reduces further and high-angle grain boundary (HAGB) fraction improves by grain subdivision and its change in orientation. ECAP of low-carbon steel up to ε{sub vm} = 16.8 can produce ultrafine grains of 0.2 µm size with HAGB fraction of 82%. The as-received steel has low texture index. Microstructural changes strongly influence texture development. It increases with equivalent strain as grain subdivision continues. Texture index fluctuates at intermediate strain range due to randomization of initial texture. Texture index reaches saturation at the high equivalent strain. On ECAP at low to intermediate strain ε{sub vm} = 0.6-6, components of both α (F{sub θ}, J{sub θ}, and J-bar {sub θ}) and γ (D{sub 1θ}, D{sub 2θ}, and E{sub θ}) fibers are developed though all of them deviate from their ideal positions. At higher strain (ε{sub vm} = 9-16.8), the γ fiber components (D{sub 1θ}, D{sub 2θ}, E{sub θ}) are strengthened, and the E{sub θ} component reaches the highest intensity of ≈ 17 at ε{sub vm} = 12. There is no texture symmetry at low to high strain level. The presence of pearlite in low-carbon steel enhances strongly the deviation of texture components from their ideal positions in Euler’s space as well as it increases the intensities of the components more than that of IF steel for a similar equivalent strain.

36 MATERIALS SCIENCE↗

An Investigation on Microstructure Evolution, Mechanical Properties, and Strain Aging of Mg-1.8Zn-0.7Si-0.4Ca Biomedical Alloy Processed by Equal Channel Angular Pressing

The influence of equal channel angular pressing (ECAP) on microstructure and mechanical behavior, as well as, strain aging during ECAP and post-ECAP of Mg-1.8Zn-0.7Si-0.4Ca biomedical alloy was examined. The alloy in solid solution heat-treated condition was processed by ECAP with route B{sub C} at 350 and 400 °C. The specimens ECAPed at 350 °C were aged at 125 and 150 °C for different times. The hardness and shear punch test results indicated that performing ECAP at 350 °C for 4 passes increases the hardness and shear strength of the alloy from 48 HV and 110 MPa to 71 HV and 188 MPa, respectively. It was revealed that the average grain size of the alloy decreases from 78 µm to about 3 µm after 4 passes of ECAP. Three precipitates of CaMgSi, Ca{sub 2}Mg{sub 6}Zn{sub 3}, and Mg{sub 2}Si were detected in the solid solution specimen. After 4 passes of ECAP at 350 °C, Ca{sub 2}Mg{sub 6}Zn{sub 3} was completely dissolved and the morphology of Mg{sub 2}Si changed from Chinese script to fiber-shaped particles. Dynamic strain aging occurred at high-temperature ECAP, and the specimens were overaged during post-ECAP aging. Small MgZn particles were detected in the overaged sample.

36 MATERIALS SCIENCE↗

An innovative radial gradient material design using hot isostatic pressing for applications in extreme environments

Functionally graded materials (FGMs) are highly advanced continuous or discontinuous structures whose structural and material properties vary along a singular geometric dimension either in the axial or radial direction. Here, the radial gradient FGM design makes for an optimal structural design to incorporate a bi-metallic structure with a copper-based high entropy alloy (Cu-HEA) with good mechanical properties and high irradiation resistance, and Chromium (Cr) with great corrosion resistance. This study focuses on the experimental design of a metal powder loading mechanism to fabricate a bi-metallic radial gradient structure using Cu-HEA and 99.9 % pure Cr metal powders. The powder loading strategy uses custom-designed concentric cylindrical dividers to separate the individual compositions. Two benchtop trial runs were performed for design optimization. The optimized design was then implemented to eventually load the HEA and Cr powders for consolidation via powder metallurgy hot isostatic pressing (PM-HIP). The electron microscopy analysis reveals the successful fabrication of the radial gradient structure with the chemical mapping analysis, demonstrating the gradual composition shift from the HEA at the center to the pure-Cr at the periphery via a three-step gradient.

High Entropy Alloys (HEAs)↗

Binder-jetted AISI M2 tool steel during hot isostatic pressing: Densification and carbide transformation

Binder jetting (BJ) enables fabrication of complex components from high-alloy steels such as AISI M2; however, residual porosity after sintering limits mechanical performance. This study investigates the coupled effects of binder chemistry, sintering conditions, cooling rate, and subsequent hot isostatic pressing (HIP) on densification, microstructure, and mechanical response in binder-jetted M2 tool steel. HIP increased relative density from ∼93 to 95% to >99% and improved compressive strength by ∼40-70%. Densification was governed by initial pore morphology, where closed porosity was effectively eliminated, while interconnected porosity limited full consolidation. Microstructural analysis (XRD, EBSD, SEM) shows that HIP promotes dissolution of metastable carbides and redistribution of alloying elements (W, Mo, V), transforming heterogeneous carbide networks into finer and more uniformly distributed M 2 C, MC, and M 6 C phases through diffusion-assisted homogenization. Among the investigated conditions, the FluidFuse binder combined with sintering at 1270 °C for 60 min and furnace cooling produced the most balanced response, achieving ∼99.7% density, ∼855 HV hardness, ∼4130 MPa compressive strength, and ∼24% strain. In contrast, higher sintering temperatures promoted carbide coarsening, reducing ductility despite high density. HIP reduces microstructural heterogeneity and drives the system toward a near-equilibrium state with reduced sensitivity to prior processing history. A comparative assessment with conventional and additive manufacturing routes (LPBF, DED, EBM, FFF) shows that the BJ-HIP approach achieves competitive densification and mechanical performance. These findings provide a mechanistic basis for controlling densification and microstructure in high-alloy steels processed via BJAM.

AISI M2 tool steel↗

Growth kinetics and microstructural evolution during hot isostatic pressing of U-10 wt.% Mo monolithic fuel plate in AA6061 cladding with Zr diffusion barrier

Phase constituents and microstructure changes in RERTR fuel plate assemblies as functions of temperature and duration of hot-isostatic pressing (HIP) during fabrication were examined. The HIP process was carried out as functions of temperature (520, 540, 560 and 580 °C for 90 min) and time (45–345 min at 560 °C) to bond 6061 Al-alloy to the Zr diffusion barrier that had been co-rolled with U-10 wt.% Mo (U10Mo) fuel monolith prior to the HIP process. Scanning and transmission electron microscopies were employed to examine the phase constituents, microstructure and layer thickness of interaction products from interdiffusion. At the interface between the U10Mo and Zr, following the co-rolling, the UZr2 phase was observed to develop adjacent to Zr, and the a-U phase was found between the UZr2 and U10Mo, while the Mo2Zr was found as precipitates mostly within the a-U phase. The phase constituents and thickness of the interaction layer at the U10Mo-Zr interface remained unchanged regardless of HIP processing variation. Observable growth due to HIP was only observed for the (Al,Si)3Zr phase found at the Zr/AA6061 interface, however, with a large activation energy of 457 ± 28 kJ/mole. Thus, HIP can be carried to improve the adhesion quality of fuel plate without concern for the excessive growth of the interaction layer, particularly at the U10Mo-Zr interface with the a-U, Mo2Zr, and UZr2 phases.

99 GENERAL AND MISCELLANEOUS↗

Micro-tensile testing of the bond line in hot isostatic pressed aluminum

Considerable effort is being devoted to development and regulatory qualification of low enriched fuels for research and test reactors by many agencies worldwide. One promising fuel configuration being examined for United States higher power research and test reactors (USHPRRs) are plate-type fuels composed of a metallic uranium-molybdenum foil clad in an aluminum alloy. The two pieces of aluminum alloy cladding are bonded using a hot isostatic pressing method. The mechanical properties of the resulting bond line in the aluminum alloy cladding will vary by the HIP'ing parameters, requiring a need to characterize the bond line. Small scale mechanical testing can provide a path for evaluating the mechanical properties and deformation behavior of the bond line both prior to and following irradiation. Here, in this research, room temperature micro-tensile specimens of non-irradiated and irradiated samples containing an Al alloy (AA 6061) bond line were tested to evaluate its strength and deformation behavior. Observations indicated that the strain rate did not affect the deformation behavior or strength and most of the micro-tensile specimens failed in a ductile mode in grains around the bond line. There was no indication that the microstructural features from the bond line affected the mechanical properties of the micro-tensile specimens. An initial examination was performed on irradiated material but further systematic studies of the effects of irradiation can be performed in the future.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Insight into the interfacial microstructure and chemistry of hot isostatically pressed AA6061-AA6061 bonds for U-10Mo fuel cladding application

Here, in the present study, hot isostatic pressing (HIP) bonding was carried out using AA6061-AA6061 plates for U-10Mo monolithic fuel cladding application. HIP was performed at 560°C with an applied isostatic pressure of 103 MPa for 90 min. Interfacial microstructure characterizations were performed using scanning electron microscopy (SEM) combined with electron backscatter diffraction (EBSD) to quantify precipitate fractions and study recrystallization, grain growth, and orientation relationships across the interface. EBSD results confirmed that no interfacial grain growth occurred during the HIP process. Transmission electron microscopy (TEM) was also employed to quantify composition and identify phases of various precipitates and an oxide layer that formed at the interface during HIP bonding. Microstructural analyses revealed the formation of a large fraction of Mg 2 Si precipitate and a ~50 nm thick Mg-oxide layer at the interface. Further TEM analysis confirmed that the oxide layer was not continuous, and Mg 2 Al 2 O 5 oxide particles with an average size of 18 nm were present in the oxide layer. Finite element modeling analysis was performed to study the stress distribution at the interface during HIP processing.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Phase transformations of NbCr{sub 2} intermetallics produced by mechanical alloying followed by hot-pressing consolidation

Mechanical alloying followed by hot-pressing consolidation has been used to produce NbCr{sub 2} intermetallics under different conditions. High-purity Nb and Cr crystalline powders, in the relative (molar) ratio of 13:1, were milled for periods up to 100 h. This powder was vacuum-sintered at temperatures ranging from 1423 to 1573 K for 0.5 h under a pressure of 45 MPa. The phase transformations of the NbCr{sub 2} were investigated by X-ray diffraction and scanning electron microscopy; several different phase transformations were observed. Increasing the milling time up to 100 h transforms into a mixture of C14, Nb, Cr and C15. The experimental results show that new evidence based on X-ray diffraction measurements further establishes the existence of a high-temperature C14 Laves polytype; an intermediate C36 structure for NbCr{sub 2}, reported in the literature, was not detected in this study. The relationship between the various phase transformations, based on the atomic radii and different preparation techniques, is discussed.

36 MATERIALS SCIENCE↗

Effect of rapid solidification on the microstructure and mechanical properties of hot-pressed Al-20Si-5Fe alloys

The aim of this work is to study the effect of cooling rate and subsequent hot consolidation on the microstructural features and mechanical strength of Al-20Si-5Fe-2X (X = Cu, Ni and Cr) alloys. Powder and ribbons were produced by gas atomization and melt spinning processes at two different cooling rates of 1 x 10{sup 5} K/s and 5 x 10{sup 7} K/s. The microstructure of the products was examined using optical microscopy, scanning electron microscopy, transmission electron microscopy, and X-ray diffraction. The particles were consolidated by hot pressing at 400 deg. C/250 MPa/1 h under a high purity argon atmosphere and the microstructure, hardness and compressive strength of the compacts were evaluated. Results showed a profound effect of the cooling rate, consolidation stage, and transition metals on the microstructure and mechanical strength of Al-20Si-5Fe alloys. While microstructural refining was obtained at both cooling rates, the microstructure of the atomized powder exhibited the formation of fine primary silicon ({approx} 1 {mu}m), eutectic Al-Si phase with eutectic spacing of {approx} 300 nm, and {delta}-iron intermetallic. Supersaturated Al matrix containing 5-7 at.% silicon and nanometric Si precipitates (20-40 nm) were determined in the microstructure of the melt-spun ribbons. The hot consolidation resulted in coarsening of Si particles in the atomized particles, and precipitation of Si and Fe-containing intermetallics from the supersaturated Al matrix in the ribbons. The consolidated ribbons exhibited higher mechanical strength compared to the atomized powders, particularly at elevated temperatures. The positive influence of the transition metals on the thermal stability of the Al-20Si-5Fe alloy was noticed, particularly in the Ni-containing alloy.

36 MATERIALS SCIENCE↗

The role of grain orientation in microstructure evolution of pure aluminum processed by equal channel angular pressing

A new approach describing the role of crystallographic orientation in the microstructural refinement of commercially pure aluminum during the successive passes of equal channel angular pressing (ECAP) is introduced. The study is based on analysis of X-ray diffraction texture data that is used to calculate the geometrical position of crystallographic slip planes with respect to the shearing plane of the ECAP die. The angular deviations of {l_brace}111{r_brace} slip planes from the macroscopic deformation plane for different processing routes were calculated and compared. The microstructure evolution was investigated using electron back-scattered diffraction (EBSD). The grain size and grain boundary character distribution obtained for each processing route are related to the angles between {l_brace}111{r_brace} planes and the shearing plane. It was shown that the more effective routes in grain refinement have higher angles between {l_brace}111{r_brace} slip planes and the shearing plane. - Research Highlights: {yields} The grain refinement of commercially pure aluminum during ECAP highly depends on the processing routes. {yields} The differences between the processing routes could be explained by the crystallographic orientations of the grains which become parallel to the shearing plane and direction. {yields} Texture results could be used to calculate the angle between the slip planes of the grains and the shearing plane of the ECAP die. {yields} The routes making higher angles between {l_brace}111{r_brace} planes and the shearing plane result in better grain refinement during the process.

36 MATERIALS SCIENCE↗

Resistance spot welding of ultra-fine grained steel sheets produced by constrained groove pressing: Optimization and characterization

Constrained groove pressing as a severe plastic deformation method is utilized to produce ultra-fine grained low carbon steel sheets. The ultra-fine grained sheets are joined via resistance spot welding process and the characteristics of spot welds are investigated. Resistance spot welding process is optimized for welding of the sheets with different severe deformations and their results are compared with those of as-received samples. The effects of failure mode and expulsion on the performance of ultra-fine grained sheet spot welds have been investigated in the present paper and the welding current and time of resistance spot welding process according to these subjects are optimized. Failure mode and failure load obtained in tensile-shear test, microhardness, X-ray diffraction, transmission electron microscope and scanning electron microscope images have been used to describe the performance of spot welds. The region between interfacial to pullout mode transition and expulsion limit is defined as the optimum welding condition. The results show that optimum welding parameters (welding current and welding time) for ultra-fine grained sheets are shifted to lower values with respect to those for as-received specimens. In ultra-fine grained sheets, one new region is formed named recrystallized zone in addition to fusion zone, heat affected zone and base metal. It is shown that microstructures of different zones in ultra-fine grained sheets are finer than those of as-received sheets. - Highlights: Black-Right-Pointing-Pointer Resistance spot welding process is optimized for joining of UFG steel sheets. Black-Right-Pointing-Pointer Optimum welding current and time are decreased with increasing the CGP pass number. Black-Right-Pointing-Pointer Microhardness at BM, HAZ, FZ and recrystallized zone is enhanced due to CGP.

36 MATERIALS SCIENCE↗

Microstructure stability of ultra-fine grained magnesium alloy AZ31 processed by extrusion and equal-channel angular pressing (EX–ECAP)

Thermal stability of the ultra-fine grained (UFG) microstructure of magnesium AZ31 alloy was investigated. UFG microstructure was achieved by a combined two-step severe plastic deformation process: the extrusion (EX) and subsequent equal-channel angular pressing (ECAP). This combined process leads to refined microstructure and enhanced microhardness. Specimens with UFG microstructure were annealed isochronally at temperatures 150–500 °C for 1 h. The evolution of microstructure, mechanical properties and dislocation density was studied by electron backscatter diffraction (EBSD), microhardness measurements and positron annihilation spectroscopy (PAS). The coarsening of the fine-grained structure at higher temperatures was accompanied by a gradual decrease of the microhardness and decrease of dislocation density. Mechanism of grain growth was studied by general equation for grain growth and Arrhenius equation. Activation energies for grain growth were calculated to be 115, 33 and 164 kJ/mol in temperature ranges of 170–210 °C, 210–400 °C and 400–500 °C (443–483 K, 483–673 K and 673–773 K), respectively. - Highlights: • Microhardness of UFG AZ31 alloy decreases with increasing annealing temperature. • This fact has two reasons: dislocation annihilations and/or grain growth. • The activation energies for grain growth were calculated for all temperature ranges.

36 MATERIALS SCIENCE↗

Characterization of hot-pressed short ZrO{sub 2} fiber toughened ZrB{sub 2}-based ultra-high temperature ceramics

Two different ZrB{sub 2}-based ultra-high temperature ceramics were produced by hot pressing: ZrB{sub 2} + 20 vol.% SiC particle + 15 vol.% ZrO{sub 2} fiber and ZrB{sub 2} + 20 vol.% SiC whisker + 15 vol.% ZrO{sub 2} fiber. The microstructures were analyzed by using transmission electron microscopy and high-resolution transmission electron microscopy. It was shown that a clean interface without any impurities was identified in ZrB{sub 2}-based hybrid ceramics with SiC whiskers and ZrO{sub 2} fibers, which would significantly improve the toughening mechanism. The results of high-resolution transmission electron microscopy showed that stacking faults in SiC whiskers resulted from an insertion of a (111) layer, which would be one of the main reasons for material anisotropy. However, the interface between the SiC particle and ZrO{sub 2} fiber was found to be ambiguous in ZrB{sub 2}-based hybrid ceramics with SiC particles and ZrO{sub 2} fibers due to the slight reaction. The orientation relationship between t-ZrO{sub 2} and m-ZrO{sub 2} phases obeyed the classical correspondence: (100){sub m}//(100){sub t} and [001]{sub m}//〈001〉{sub t}, which further verified the feasibility of phase transformation toughening mechanism. - Highlights: • ZrB{sub 2}-based ceramics toughened by short ZrO{sub 2} fiber are characterized by TEM and HRTEM. • The orientation relationship of t- and m-ZrO{sub 2} are (100){sub m}//(100){sub t}, [001]{sub m}//〈001〉{sub t} • The clean interface without any impurities leads to improve the toughening mechanism.

36 MATERIALS SCIENCE↗

Development of mechanical properties in a CaO added AZ31 magnesium alloy processed by equal-channel angular pressing

Processing through the application of equal-channel angular pressing (ECAP) is recognized as one of the attractive severe plastic deformation techniques where the processed bulk metals generally achieve ultrafine-grained microstructure leading to improved physical characteristics and mechanical properties. Magnesium has received much attention to date for its lightweight, high strength and excellent elasticity. Mg alloys with addition of CaO is reported to provide the successful casting procedure without usage of greenhouse gas, SF{sub 6}, whereas it is generally used for preventing the oxidation of Mg during casting. In the present investigation, a CaO added AZ31 (AZ31-CaO) magnesium alloy was processed by ECAP at elevated temepratures with a few steps of reduction which result in significant grain refinement to ~ 1.5 μm after 6 passes. Compression testing at room temperature demonstrated the AZ31-CaO alloy after ECAP showed enhanced yield strength more than the as-processed commercial AZ31 alloy while both alloys maintained ductility in spite of significant reduction in grain size. The improved strength in the AZ31-CaO alloy was attributed to the formation of fine Al{sub 2}Ca precipitates which experience breaking-up through ECAP and accelerate the microstructural refinement. Moreover, the preservation of ductility was attributed to the enhancement of strain hardening capability in the AZ31 alloy at room temperature. This study discusses the feasibility of using ECAP to improve both strength and ductility on magnesium alloys by applying the diagram describing the paradox of strength and ductility. - Highlights: • AZ31 and AZ31-CaO magnesium alloys were processed by ECAP up to 6 passes. • AZ31-CaO alloy after ECAP showed improved yield strength without losing ductility. • CaO in AZ31 forms fine Al{sub 2}Ca accelerating microstructural refinement during ECAP. • Feasibility of using ECAP was shown to improve both strength and ductility in Mg.

36 MATERIALS SCIENCE↗

Thermal stability of Cu-Cr-Zr alloy processed by equal-channel angular pressing

Thermal stability of a Cu-Cr-Zr alloy processed by equal-channel angular pressing up to16 passes was investigated using isochronal annealing ranging from 250 to 850 °C for 1 h. The microstructure, crystallographic texture and micro hardness of samples were characterized through electron back scatter diffraction and Vickers micro hardness measurements. The recrystallized grain size was stable between 250 °C and 500 °C then increased quickly. The achieved mean grain size, after 1, 4 and 16 ECAP passes, was around 5.5 μm. A discontinuous mode of recrystallization was found to occur and a Particle Simulated Nucleation mechanism was evidenced. The evolution of the high angle grain boundary fraction increased notably after annealing above 550 °C. The crystallographic texture after isochronal annealing was similar to that of ECAP simple shear, no change of the texture during annealing was observed but only slight intensity variations. Micro hardness of all Cu–Cr–Zr samples showed a hardening with two peaks at 400 and 500 °C associated with precipitation of Cu cluster and Cu{sub 5}Zr phase respectively, followed by a subsequent softening upon increasing the annealing temperature due to recrystallization. - Highlight: •The Cu-1Cr-0.1Zr alloy shows a very good thermal stability up to 550 °C after ECAP. •A discontinuous recrystallization was found to occur and PSN mechanism was evidenced. •The annealing texture was found weak and some new components appear. •Hardening is attributed to the Cr clustering followed by the Cu{sub 51}Zr{sub 14} precipitation. •Softening is a result of recrystallization and grain growth progressing.

36 MATERIALS SCIENCE↗