Degradation Mechanisms in TOPCon/POLO Solar Cells
This presentation shows how Poly-Si/SiO2 contacts show a post firing degradation/regeneration cycle. The following conclusions were made: 1) cycle changes surface passivation (Jo), but not the bulk lifetime; 2) cycle time depends on anneal temperature in light or dark (higher T, faster cycle); 3) 400 degrees Celsius anneal eliminates the cycle - only generation occurs; 4) cycle time and magnitude is not correlated with Tfire; 5) contact passivation is stable after cycling; 6) fundamental nature of defect(s) responsible is not known; 7) TOPCon cells/modules, if constructed well, seem to show minimal degradation issues (PVEL, Jolywood, Jinko, ET Solar), and 8) NREL/ASU are studying TOPCon cells and UC Davis has a molecular dynamics model for TOPCon.