Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “Ni-rich cathode”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 127 records · Page 7

Impact of Charge Voltage on Factors Influencing Capacity Fade in Layered NMC622: Multimodal X-ray and Electrochemical Characterization

Ni-rich NMC is an attractive Li-ion battery cathode due to its combination of energy density, thermal stability, and reversibility. While higher delivered energy density can be achieved with a more positive charge voltage limit, this approach compromises sustained reversibility. Improved understanding of the local and bulk structural transformations as a function of charge voltage, and their associated impacts on capacity fade are critically needed. Through simultaneous operando synchrotron X-ray diffraction (XRD) and X-ray absorption spectroscopy (XAS) of cells cycled at 3–4.3 or 3–4.7 V, this study presents an in-depth investigation into the effects of voltage window on local coordination, bulk structure, and oxidation state. These measurements are complemented by ex situ X-ray fluorescence (XRF) mapping and scanning electrochemical microscopy mapping (SECM) of the negative electrode, X-ray photoelectron spectroscopy (XPS) of the positive electrode, and cell level electrochemical impedance spectroscopy (EIS). Initially, cycling between 3 and 4.7 V leads to greater delivered capacity due to greater lithium extraction, accompanied by increased structural distortion, moderately higher Ni oxidation, and substantially higher Co oxidation. Continued cycling at this high voltage results in suppressed Ni and Co redox, greater structural distortion, increased levels of transition metal dissolution, higher cell impedance, and 3× greater capacity fade.

capacity fading mechanisms↗

Superionic conducting vacancy-rich β-Li 3 N electrolyte for stable cycling of all-solid-state lithium metal batteries

The advancement of all-solid-state lithium metal batteries requires breakthroughs in solid-state electrolytes (SSEs) for the suppression of lithium dendrite growth at high current densities and high capacities (>3 mAh cm -2 ) and innovation of SSEs in terms of crystal structure, ionic conductivity and rigidness. Here we report a superionic conducting, highly lithium-compatible and air-stable vacancy-rich β-Li 3 N SSE. This vacancy-rich β-Li 3 N SSE shows a high ionic conductivity of 2.14 × 10 -3 S cm -1 at 25 °C and surpasses almost all the reported nitride-based SSEs. A Li- and N-vacancy-mediated fast lithium-ion migration mechanism is unravelled regarding vacancy-triggered reduced activation energy and increased mobile lithium-ion population. All-solid-state lithium symmetric cells using vacancy-rich β-Li 3 N achieve breakthroughs in high critical current densities up to 45 mA cm -2 and high capacities up to 7.5 mAh cm -2 , and ultra-stable lithium stripping and plating processes over 2,000 cycles. The high lithium compatibility mechanism of vacancy-rich β-Li 3 N is unveiled as intrinsic stability to lithium metal. In addition, β-Li 3 N possesses excellent air stability through the formation of protection surfaces. All-solid-state lithium metal batteries using the vacancy-rich β-Li 3 N as SSE interlayers and lithium cobalt oxide (LCO) and Ni-rich LiNi 0.83 Co 0.11 Mn 0.06 O 2 (NCM83) cathodes exhibit excellent battery performance. Extremely stable cycling performance is demonstrated with high capacity retentions of 82.05% with 95.2 mAh g -1 over 5,000 cycles at 1.0 C for LCO and 92.5% with 153.6 mAh g -1 over 3,500 cycles at 1.0 C for NCM83. Utilizing the vacancy-rich β-Li 3 N SSE and NCM83 cathodes, the all-solid-state lithium metal batteries successfully accomplished mild rapid charge and discharge rates up to 5.0 C, retaining 60.47% of the capacity. Notably, these batteries exhibited a high areal capacity, registering approximately 5.0 mAh cm -2 for the compact pellet-type cells and around 2.2 mAh cm -2 for the all-solid-state lithium metal pouch cells.

25 ENERGY STORAGE↗

Lithium-compatible and air-stable vacancy-rich Li 9 N 2 Cl 3 for high–areal capacity, long-cycling all–solid-state lithium metal batteries

Attaining substantial areal capacity (>3 mAh/cm 2 ) and extended cycle longevity in all–solid-state lithium metal batteries necessitates the implementation of solid-state electrolytes (SSEs) capable of withstanding elevated critical current densities and capacities. In this study, we report a high-performing vacancy-rich Li 9 N 2 Cl 3 SSE demonstrating excellent lithium compatibility and atmospheric stability and enabling high–areal capacity, long-lasting all–solid-state lithium metal batteries. The Li 9 N 2 Cl 3 facilitates efficient lithium-ion transport due to its disordered lattice structure and presence of vacancies. Notably, it resists dendrite formation at 10 mA/cm 2 and 10 mAh/cm 2 due to its intrinsic lithium metal stability. Furthermore, it exhibits robust dry-air stability. Incorporating this SSE in Ni-rich LiNi 0.83 Co 0.11 Mn 0.06 O 2 cathode-based all–solid-state batteries, we achieve substantial cycling stability (90.35% capacity retention over 1500 cycles at 0.5 C) and high areal capacity (4.8 mAh/cm 2 in pouch cells). These findings pave the way for lithium metal batteries to meet electric vehicle performance demands.

25 ENERGY STORAGE↗

Ni-Rich Li[Ni x MnyCo 1– x – y ]O 2 Single Crystals as Superior Fast Charge Cathodes for Lithium-Ion Batteries

The utilization of single-crystal (SC) Li[Ni x MnyCo 1-x-y ]O 2 (NMC) cathodes has facilitated unparalleled performance in commercial high-energy lithium-ion batteries (LIBs). In the current study, we evaluate the application of SC cathodes in fast charge (FC)-LIBs where particle cracking is a predominant failure mechanism. Ni-rich SC-NMC samples with various compositions, sizes, and shapes are synthesized and investigated for their influence on FC performance. We reveal the necessity of utilizing smaller SCs (<1 μm) as larger sizes (>2 μm) experience significant particle-level lithium concentration gradients under FC conditions. To improve lithium transport and minimize side reactivities, we strategically expose the (104) crystal facets on the surface. Exceptional performance was observed on an optimized SC-LiNi 0.80 Mn 0.05 Co 0.15 O 2 , delivering a discharge capacity of 165 mAh/g even after 150 cycles at 6C charge. Our study not only demonstrates the promise of SC-NMC but also provides the key insights for the design and optimization of advanced cathodes for FC-LIBs.

25 ENERGY STORAGE↗

Degradation in Ni-Rich LiNi 1– x – y Mn x Co y O 2 /Graphite Batteries: Impact of Charge Voltage and Ni Content

Ni-rich LiNi 1– x–y Mn x CoyO 2 (NMC) materials are attractive as cathodes for Li-ion batteries due to their high energy density and low Co content. However, these materials may display poor electrochemical reversibility relating to structural and interfacial instabilities. The influence of Ni content and level of delithiation during charge on degradation mechanisms and relevance to electrochemical cycling behavior are probed for LiNi 0.6 Mn 0.2 Co 0.2 O 2 (NMC622) and LiNi 0.8 Mn 0.1 Co 0.1 O 2 (NMC811) cathode materials in a full cell configuration under two upper voltage limits (4.1 and 4.3 V). The combined use of dQ/dV analysis of electrochemical voltage profiles, operando XRD, and postcycling scanning electron microscopy (SEM) measurements indicates that a major contributor to capacity fade is the large anisotropic volume change from an H2 $\leftrightarrows$ H3 phase transition and associated mechanical degradation particularly for NMC811. Notably, transition metal dissolution and deposition on the negative electrode are found to correlate with the structural changes occurring in the cathode under high voltage charge. X-ray photoelectron spectroscopy (XPS) analyses of the cycled cathodes reveal a more organic-rich cathode–electrolyte interphase (CEI) when cycling to 4.3 V with lower relative amounts of LiF. Surface reconstruction is not a significant factor under these cycling conditions as determined by soft X-ray absorption spectroscopy (sXAS) analysis. The results emphasize the opportunity to match the electrochemical test parameters with the specific NMC active material to mitigate degradation and extend cycle life.

36 MATERIALS SCIENCE↗

Perspective—Potential Benefit of Li-Rich Cathode Materials: Reduction of Co and Ni Content Rather than Achievement of Ultra-High Capacities

In the conventional cycling protocol for lithium and manganese rich NMC layered oxides (LMRNMC), the upper cutoff voltage V cut is extended to ~ 4.8, to achieve capacities of similar to 250 mAh g -1 . With this mode of operation, structural rearrangements result in voltage fade upon cycling. Herein, a strategy is proposed to avoid these structural rearrangements based on (a) restricting V cut to values < ~ 4.6 to shut down the bulk instabilities, and (b) application of a (preferably) semi-coherent coating that protects the surface oxygen. The potential benefit of this strategy would be to minimize Co and Ni content, compared to Ni-rich NMC.

25 ENERGY STORAGE↗

The influence of electrochemical cycling protocols on capacity loss in nickel-rich lithium-ion batteries

The transition towards electric vehicles and more sustainable transportation is dependent on lithium-ion battery (LIB) performance. Ni-rich layered transition metal oxides, such as NMC811 (LiNi 0.8 Mn 0.1 Co 0.1 O 2 ), are promising cathode candidates for LIBs due to their higher specific capacity and lower cost compared with lower Ni content materials. However, complex degradation mechanisms inhibit their use. In this work, tailored aging protocols are employed to decouple the effect of electrochemical stimuli on the degradation mechanisms in graphite/NMC811 full cells. Using these protocols, impedance measurements, and differential voltage analysis, the primary drivers for capacity fade and impedance rise are shown to be large state of charge changes combined with high upper cut-off voltage. Focused ion beam-scanning electron microscopy highlights that extensive microscale NMC particle cracking, caused by electrode manufacturing and calendering, is present prior to aging and not immediately detrimental to the gravimetric capacity and impedance. Scanning transmission electron microscopy electron energy loss spectroscopy reveals a correlation between impedance rise and the level of transition metal reduction at the surfaces of aged NMC811. The present study provides insight into the leading causes for LIB performance fading, and highlights the defining role played by the evolving properties of the cathode particle surface layer.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Vibrational Entropy Contribution to Mixing Free Energy of Ni-Rich LiNi 1- y Co y O 2

First principles density-functional-theory calculations are performed of the mixing free energy of the layered oxide LiNi 1-y Co y O 2 , a model Li-ion-battery cathode material, at 1000 K. Analysis of internal energy, LN exchange, configurational entropy and vibrational entropy are combined to obtain the net mixing free energy. The vibrational entropy requires a more indirect treatment than the other terms; analysis based on heat capacity is presented here, to show that the vibrational entropy is of comparable magnitude to the configurational entropy, and it tends to promote solid-solution behavior in LiNi 1-y Co y O 2 .

25 ENERGY STORAGE↗

Understanding Structural and Compositional Evolution during NMC Cathode Direct Recycling via Solid-State NMR

Recycling end-of-life lithium-ion batteries (LIBs) to recover high-value cathode materials such as LiNixMnyCozO2 (NMC) is driven by economical, geopolitical, and sustainability needs. There has been recent interest in direct recycling methods to improve efficiency and recovery of materials, including ionothermal, hydothermal, solid-state, or redox mediator methods. In conjunction with recycling process development, detailed structural characterization is necessary in order to understand the mechanisms and efficacy of cathode recycling steps. Solid-state nuclear magnetic resonance (NMR) spectroscopy is a unique tool that can probe Li coordination, bulk and surface environments, and transition metal ordering in recycled and upcycled NMC cathodes. Here, 6,7Li, 1H, and 19F NMR spectroscopy to probe structural and compositional changes as well as surface impurities that may form during each step in NMC direct recycling is utilized. During relithiation, Li reinsertion into the NMC lattice is observed. During upcycling, where the goal is to increase the Ni content in the NMC, incorporation of Ni-rich phases into the bulk Li environment is observed. Surface impurities formed during processing were also identified. These studies provide valuable information for optimizing recycling processes to reach targeted cathode composition and structure that can enable electrochemical performance comparable to or better than pristine materials.

36 MATERIALS SCIENCE↗

In-Situ FTIR Detection of Transition Metal (TM)-Ion Dissolution From Cathodes in Li-Ion Batteries

Transition metal (TM) ions, commonly Ni and Mn, play a crucial role in Li-ion battery cathodes as the reaction centers for rapid redox reactions. A major challenge with TM-based cathodes is capacity degradation, particularly at higher operating voltages. This degradation is closely linked to the dissolution of TMs from the cathode materials and their subsequent deposition on the anode. This process not only modifies the surface structure of the cathode but, more significantly, alters the SEI composition on the anode [1-2]. The dissolution of TMs cations into a liquid electrolyte from cathode materials, such as Mn-ion dissolution from Mn-rich cathode (LMR), is detrimental to the cycling performance of Li-ion batteries [3-4]. Much attention has been paid to this issue but there remains a lack of characterization techniques which can detect the TM-ion dissolution from the cathode during electrochemical measurements. In our study, we use in-situ ATR-FTIR as an effective technique to probe the TM-ion dissolution from the cathode. We have first demonstrated the detrimental effects of TM ions on the electrochemical performance of Li-ion batteries by adding a small amount of TM salt (50 mM Mn(PF6)) to the electrolyte of a Li-ion coin cell with LFP and graphite electrode. We observed a rapid capacity fade after the first delithiation cycle. To investigate TM ion dissolution, we established a baseline IR spectrum for various TM solvation states (such as Mn and Ni) by measuring concentration-dependent IR spectra. This baseline spectrum helps us detect TM ion dissolution during battery cycling. In this work, we discuss in detail the effect of TM ions on the electrochemical performance of Li-ion batteries and the detection of TM ions during battery cycling using in-situ FTIR spectroscopy. We will compare TM dissolution between coated and uncoated cathodes to examine the effect of cathode coatings to mitigate degradation due to TM dissolution and cross-over from cathode to anode. References: (1) Zhan, C.; Wu, T.; Lu, J.; Amine, K. Dissolution, migration, anddeposition of transition metal ions in Li-ion batteries exemplified byMn-based cathodes - a critical review. Energy Environ. Sci. 2018, 11,243-257. (2) Jung, R.; Linsenmann, F.; Thomas, R.; Wandt, J.; Solchenbach,S.; Maglia, F.; Stinner, C.; Tromp, M.; Gasteiger, H. A. Nickel,Manganese, and Cobalt Dissolution from Ni-Rich NMC and TheirEffects on NMC622-Graphite Cells. J. Electrochem. Soc. 2019, 166,A378-A389. (3) Zhao, L.; Chenard, E.; Capraz, O. O.; Sottos, N. R.; White, S.R. Direct Detection of Manganese Ions in Organic Electrolyte by UV-Vis Spectroscopy. J. Electrochem. Soc. 2018, 165, A345-A348 (4) Zhang, Y.; Hu, A.; Xia, D.; Hwang, S.; Sainio, S.; Nordlund, D.;Michel, F. M.; Moore, R. B.; Li, L.; Lin, F. Operando characterization and regulation of metal dissolution and redeposition dynamics nearbattery electrode surface. Nat. Nanotechnol. 2023, 18, 790.

25 ENERGY STORAGE↗

First-principles study of the structures and redox mechanisms of Ni-rich lithium nickel manganese cobalt oxides

To reduce the cobalt (Co) content in lithium-ion batteries, Ni-rich (high-Ni) lithium nickel manganese cobalt oxides (NMC) are pursued as one of the next-generation cathode materials. However, there is still debate on the crystal and electronic structures of the baseline, LiNiO 2 . Density Functional Theory (DFT) calculations were performed to provide a theoretical understanding of Ni-rich NMC. First, it was found that the commonly used $R\bar{3}m$ structure for LiNiO 2 is metallic, contrary to the experimentally reported mix-conducting behavior. Among the four different space groups, $R\bar{3}m$, C2/m, P2 1 /c, and P2/c, P2/c with charge disproportionation of Ni 2+ and Ni 4+ is the most energetically stable and semiconducting structure of LiNiO 2 . Therefore, the atomic structures of representative Ni-rich NMC were built by partially replacing Ni with Co or Mn in the P2/c LiNiO 2 to form Li x Ni y Mn z Co 1-y-z O 2 . In the fully lithiated (x=1.0) high Ni content NMC (y>0.5), the oxidation state of all Mn ions becomes 4+, while Co ions still maintain 3+, and part of the Ni ions become 3+ to compensate for the charge. Upon delithiation, the local environment shows more variation of the charge states on the transition metal (TM) ions. The average oxidation on each TM follows a sequence of losing electrons that starts from Ni 2+ to Ni 3+ , then oxidizing Ni 3+ and Co 3+ , while Mn 4+ remains electrochemically inactive till x=0. Finally, a general relationship for the oxidation state change in each TM as a function of x is derived and shows agreement with both modeling and experimental data.

25 ENERGY STORAGE↗

Enhanced cycling stability of Ni-rich Li-metal cells enabled by dual vinylene carbonate and tris(trimethylsilyl)borate electrolyte additives

NMC811 (LiNi 0.8 Co 0.1 Mn 0.1 O 2 ) and other high-Ni chemistries are promising cathode candidates for high-performance electric vehicles, owing to their high energy density and reduced cobalt content. However, their long-term cycling stability is hindered by surface degradation, particularly when paired with conventional electrolytes and a lithium metal anode. Electrolyte additives represent a practical approach to enhance interfacial stability and improve overall battery performance by promoting the formation of a robust electrolyte–electrode interphase (EEI). In this study, we revisit the effects of vinylene carbonate (VC) and tris(trimethylsilyl)borate (TMSB) additives on single-crystal SC-NMC811||Li cells. While TMSB only increases the open-circuit voltage and initial overpotential, it delivers superior capacity retention at C/3 compared to cells containing only VC or a dual additive system (VC and TMSB). Notably, under fast-charging conditions (1C, 2C, and 5C), the dual-additive system significantly outperforms other formulations, achieving markedly enhanced long-term capacity retention. Comprehensive electrochemical and spectroscopic analyses reveal that the VC/TMSB dual-additive system suppresses surface transition in NMC811, mitigates structural degradation by forming a thin, LiF-deficient cathode-electrolyte interface (CEI) layer. Moreover, they promote smooth and dense Li deposition and generate a LiF-deficient solid-electrolyte interphase (SEI). Consequently, the synergistic stabilization of both the CEI and SEI effectively limits the overall cell impedance growth during extended cycling. These findings provide key insights into co-additive strategies for engineering stable interfaces in high-energy Ni-rich Li-metal batteries.

36 MATERIALS SCIENCE↗

Facile synthesis of Co(OH)2 nanoneedle arrays grown on stainless steel for industrial electrochemical oxygen evolution reaction

The electrochemical oxygen evolution reaction (OER) is a critical half-reaction in a variety of energy conversion and storage applications, however, OER suffers from sluggish kinetics due to the four proton-electron transfer processes. To remedy this, interfacial engineering proves an effective strategy to design high active OER catalysts. Herein, we report a facile synthesis of Co(OH)2 nanoneedle (Co-NN) arrays grown on stainless steel (SS) via a one-step hydrothermal reaction, and the resultant impressive OER performance. Particularly, the Co-NN/SS needs 267, 307, and 576 mV overpotentials to reach 10, 100, and 1000 mA cm−2 in 1 M KOH & room temperature, and the overpotentials drop to 199, 257, and 283 mV to achieve the same current densities in 30 wt% KOH & 80 °C. Additionally, an alkaline water electrolysis (AWE) cell coupled with Co-NN/SS anode and PtRu/NiMo cathode only requires 1.65 and 1.73 V iR-free cell voltage to reach 1.0 and 2.0 A cm−2, respectively. The sterling OER performance could be attributed to four possible reasons, the Fe in SS surface tailoring the electronic properties of Co(OH)2, the mixed metal oxides on SS surface accelerating surface reconstruction of Co(OH)2 nanoneedles into CoOOH active species, a Ni-rich surface layer formation cooperatively boosting the OER activity, and a local electric field effect concentrating reactants on the tip surface and accelerating the mass transfer. This work provides a facile approach for synthesizing highly efficient OER catalysts for industrial applications by interfacial engineering.

Lyu, Xiang [ORNL] (ORCID:0000000208673248)↗

Decoupling the degradation factors of Ni-rich NMC/Li metal batteries using concentrated electrolytes

Battery degradation results from multiple factors that usually correlate with each other. Electrochemical corrosion of the current collector is one of the main reasons for battery failure, leading to poor internal electrical contact and the dissolution of harmful ions into electrolytes. This phenomenon is especially evident in lithium bistrifluoromethanesulfonimidate (LiTFSI)-based electrolytes, although they have many advantages over conventional lithium hexafluorophosphate (LiPF 6 )-based electrolytes, such as low viscosity, good thermal stability, and stable to water. Recently, highly concentrated electrolytes are found hopeful of inhibiting aluminum's corrosion and boosting new electrolyte development. Here we discuss the solvation structures of liquid electrolytes and decouple the degradation mechanisms of using LiTFSI-based electrolytes in Li(Ni 0.8 Co 0.1 Mn 0.1 )O 2 /Li metal batteries. The results suggest although concentrated electrolytes inhibit the Al corrosion, the growth of lithium dendrites and the protection of the cathode-electrolyte interphase are not significantly improved. Furthermore, this paper provides a paradigm to evaluate the performance of electrolytes comprehensively.

25 ENERGY STORAGE↗

Electrolyte and Cutoff Potential Effects on Cycle Life of Li4Ti5O12/LiNi0.9Mn0.1O2 Batteries for Behind-the-Meter Storage Applications

Behind-the-Meter Storage (BTMS) is a stationary battery energy storage system that is connected to the electrical distribution system on the customer's side of the utility's service meter. BTMS systems are used to store electrical energy from the grid as well as inconstant, renewable energy, such as local solar and wind generation. A successful BTMS system will allow the customer to pair their energy generation and storage to optimize electrical consumption from the grid, improving reliability and minimizing cost. For BTMS applications, batteries must be designed and optimized with different set of criteria from other leading segments of the Li-ion battery market, like transportation, due the system being stationary and proximal to the residential or commercial building it's benefitting. BTMS applications prioritize safety, cost (low/no-critical materials), reliability (20-year calendar life), and durability (10,000 cycle life), while having the ability to (minimally) compromise energy density and rate capability. Lithium titanate (Li4Ti5O12-, LTO) is a promising anode candidate for BTMS applications due to its high safety and capacity retention, while maintaining a reasonable 160 mAhg-1 reversable capacity and composition of relatively abundant materials. (1) Specifically, LTO has a high working voltage which helps to prevent Li dendrite formation, improving safety. Furthermore, LTO also has negligible lithiation-based volume change, leading to less mechanical pulverization, or loss of active material, upon cycling. For the cathode, materials with little or no Co are of high interest due to the high cost and low abundance of Co. LiMn2O4 (LMO) has been paired with LTO for BTMS applications in the past due to its safety, low cost (abundancy), and reasonably high operating voltage. (2-4) However, the low capacity of LMO limits energy density and specific energy. While not the highest priority for BTMS applications, increasing energy density will enable deployment in space constrained BTMS applications and decrease total cost. LiNi0.9Mn0.1O2 (LN-MO) is a recently developed material with promise due to its high operating voltage and relatively low price. (5) However, Ni-rich layered oxides, including LNMO, tend to struggle with capacity retention during high-voltage cycling due to mechanical pulverization, irreversible phase transitions, and unstable solid-electrolyte interphase. The study presented here focuses on building an understanding of how electrolyte solvent and varied cutoff potentials will impact the cycle life of LTO/LN-MO cells. Specifically, a comparison is provided between ethylene carbonate (EC), ethyl methyl carbonate (EMC), fluoroethylene carbonate (FEC), and Gen2 electrolyte solvents with 1M Lithium hexafluorophosphate (LiPF6) salt, cycling to two upper termination potentials, 2.6V and 2.7V. Electrochemical testing and diagnostics (e.g., differential capacity analysis, area specific impedance, constant voltage hold, and rate capability) and post-mortem characterization will be used to understand the aging behavior and failure mechanisms of the 8 cell combinations (four electrolytes and two voltage cutoffs). Cells with FEC electrolyte showed a lower initial capacity compared to cells with Gen2, EMC, and EC cycling at both voltages; however, the cells with FEC showed consistent trends in capacity retention with 2.6V and 2.7V termination potentials, while the cells with the other electrolytes showed much higher rates of capacity loss when cycling to the higher voltage. These results indicate that FEC may play a role in improving durability of high-voltage, Ni-rich electrode systems for use in high-cycle applications, such as BTMS.

electrolyte↗

Fundamental Insights into Cathode Stability: Linking Compositional Tuning and Local Coordination in Complex Metal Oxides under Aqueous Transformations

Compositional tuning of complex metal oxides in Li-ion battery materials influences their performance as well as their end-of-life behavior, in particular, the tendency to release toxic metal cations in aqueous solution. We modeled ternary variants of a parent LiCoO 2 delafossite structure by varying the metal identity and relative amounts. This yielded ten model formulations of Li(A 4/6 B 1/6 C 1/6 )O 2 , where the material is enriched with the A metal and doped with B and C, with Ni, Mn, Co, Fe, Al, V, and Ti as constituent metals. To assess their stability in aqueous conditions, metal release energetics were calculated using a combination of Density Functional Theory calculations and thermodynamics. Metal release in ternary oxides is dictated by subtle variations in the coordination environment of the leaving group. To identify governing chemical features across diverse compositions with varying local coordination environments, we leverage random forest regression and descriptor importance analysis. A key result is that metal–oxygen orbital hybridization, quantified using a projected density-of-states-derived descriptor, H d/p , provides a physically grounded measure of interaction strength that governs metal release energetics. This refined perspective goes beyond conventional oxidation state considerations and offers more robust insights for materials science. Finally, we model defect surface-bound O 2 dimer formation as a proxy for reactive oxygen species (ROS) generation. The results show that Ni-rich compositions more readily stabilize spin-polarized O 2 dimers, corroborating experimental reports of an increased ROS-driven biological response. In conclusion, our results establish a compositional and electronic basis for metal release and surface oxygen reactivity that form a rationale for complex metal oxide design principles.

36 MATERIALS SCIENCE↗

Facet-Dependent Ni Segregation in a Micron-Sized Single-Crystal Li 1.2 Ni 0.2 Mn 0.6 O 2 Cathode

Elemental surface segregation in cathode materials is critical for determining the phase and interfacial reaction between electrode and electrolyte, which consequently affects the electrochemical properties. Single-crystal cathode of Li 1.2 Ni 0.2 Mn 0.6 O 2 and Li 1.2 Ni 0.2 Mn 0.6 O 1.95 F 0.05 with an octahedral morphology of (102) and (003) dominated facets have been manifested to show enhanced electrochemical properties. However, the surface structural features of such single crystals have not been investigated. Herein, using scanning transmission electron microscopy, energy dispersive X-ray spectroscopy, and electron energy loss spectroscopy, we probe the elemental surface segregation characteristics in these single-crystal cathode. We reveal that Ni surface segregation shows dependence on the crystal facet such that it occurs on crystal facets with a mix of cations and anions, but not on the facets with only cations or anions. Furthermore, facet-dependent surface reconstructions are observed, featuring a spinel-like structure at the Ni-rich facet but rock-salt structure at the facet without Ni segregation. The commonly known Mn reduction appears at the single crystal surfaces, more pronounced at the facet without Ni segregation. We further reveal that fluorination leads to the stabilization of surface oxygens. In conclusion, this study provides detailed structural and chemical information about the facet-dependent Ni surface segregation and the resulted phase formation in the rather less explored micron-sized octahedral Li 1.2 Ni 0.2 Mn 0.6 O 2 and Li 1.2 Ni 0.2 Mn 0.6 O 1.95 F 0.05 single crystals, which is key to further exploration of electrochemical properties of cathode in the form of micro-sized single crystal.

25 ENERGY STORAGE↗