Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “Intergranular cracks”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 127 records · Page 7

Atomistic Mechanisms of Stress-Dependent Molten Salt Corrosion in NiCr Alloys

Ni-based structural alloys in molten salt environments often experience simultaneous mechanical loading and corrosive attack, yet the mechanisms governing stress-corrosion interactions remain unclear. Prior studies largely emphasize tensile stress, while the role of compressive stress has received limited attention. Here, reactive molecular dynamics simulations are used to investigate the coupled effects of applied strain and corrosion in Ni 0.75 Cr 0.25 exposed to molten FLiNaK at 800 °C. A Σ5(210) grain boundary model is subjected to tensile (+4%) to compressive (−4%) uniaxial strains, and corrosion behavior is evaluated through fluorine adsorption, charge redistribution, and grain boundary evolution. Tensile strain accelerates intergranular corrosion susceptibility by reducing local atomic packing through elastic dilation and increasing excess free volume at the grain boundary, which enhances atomic mobility and salt infiltration. In contrast, compressive strain can suppress corrosion by promoting the formation of a ridge-like surface layer along the grain boundary, limiting salt access to the underlying alloy. These results provide atomistic insight into how stress states influence grain boundary corrosion in molten salts.

36 - MATERIALS SCIENCE↗

A study of hydrogen environment effects on microstructure property behavior of NASA-23 alloy and related alloy systems

This work is part of the overall advanced main combustion chamber (AMCC) casting characterization program of the Materials and Processes Laboratory of the Marshall Space Flight Center. The influence of hydrogen on the tensile properties and ductility behavior of NASA-23 alloy were analyzed. NASA-23 and other referenced alloys in cast and hipped conditions were solution treated and aged under selected conditions and characterized using optical metallography, scanning electron microscopy, and electron microprobe analysis techniques. The yield strength of NASA-23 is not affected much by hydrogen under tensile tests carried at 5000 psig conditions; however, the ultimate strength and ductility properties are degraded. This implies that the physical mechanisms operating would be related to the plastic deformation process. The fracture surfaces characteristics of NASA-23 specimens tensile tested in hydrogen, helium, and air were also analyzed. These revealed surface cracks around specimen periphery with the fracture surface showing a combination of intergranular and transgranular modes of fracture. It is seen that the specimens charged in hydrogen seem to favor a more brittle fracture mode in comparison to air and helium charged specimens. The AMCC casting characterization program is to be analyzed for their hydrogen behavior. As a result of this program, the basic microstructural factors and fracture characteristics in some cases were analyzed.

Diwan, Ravinder M.↗

Elevated temperature crack growth in aluminum alloys: Tensile deformation of 2618 and FVS0812 aluminum alloys

Understanding the damage tolerance of aluminum alloys at elevated temperatures is essential for safe applications of advanced materials. The objective of this project is to investigate the time dependent subcritical cracking behavior of powder metallurgy FVS0812 and ingot metallurgy 2618 aluminum alloys at elevated temperatures. The fracture mechanics approach was applied. Sidegrooved compact tension specimens were tested at 175, 250, and 316 C under constant load. Subcritical crack growth occurred in each alloy at applied stress intensity levels (K) of between about 14 and 25 MPa/m, well below K (sub IC). Measured load, crack opening displacement and displacement rate, and crack length and growth rate (da/dt) were analyzed with several continuum fracture parameters including, the C-integral, C (sub t), and K. Elevated temperature growth rate data suggest that K is a controlling parameter during time dependent cracking. For FVS0812, da/dt is highest at 175 C when rates are expressed as a function of K. While crack growth rate is not controlled by C (sub t) at 175 C, da/dt appears to better correlate with C (sub t) at higher temperatures. Creep brittle cracking at intermediate temperatures, and perhaps related to strain aging, is augmented by time dependent transient creep plasticity at higher temperatures. The C (sub t) analysis is, however, complicated by the necessity to measure small differences in the elastic crack growth and creep contributions to the crack opening displacement rate. A microstructural study indicates that 2618 and FVS0812 are likely to be creep brittle materials, consistent with the results obtained from the fracture mechanics study. Time dependent crack growth of 2618 at 175 C is characterized by mixed transgranular and intergranular fracture. Delamination along the ribbon powder particle boundaries occurs in FVS0812 at all temperatures. The fracture mode of FVS0812 changes with temperature. At 175 C, it is characterized as dimpled rupture, and at 316 C as mixed matrix superplastic rupture and matrix-dipersoid debonding.

Leng, Yang↗

Effects of hydrogen partial pressure on crack initiation and growth rate in vintage X52 steel

There is an increasing interest in ensuring compatibility of existing natural gas infrastructure with conveyance of hydrogen, especially for vintage (pre-1970s) pipeline steels. While hydrogen is known to affect the fatigue and fracture resistance of these materials, there is a lack of data on its effects on crack initiation at low hydrogen partial pressure. To address this gap, the current work presents a series of fatigue tests on vintage API Grade X52 steel in pure nitrogen, air and gaseous hydrogen at partial pressures of 1 and 207 bar. Circumferential notch tension (CNT) specimens with direct current potential difference (DCPD) measurements are used to get S–N curves for crack initiation and failure, and compact tension (CT) tests to assess crack growth rates. Results indicate that air accelerates crack initiation, low hydrogen partial pressure affects the crack growth rate, and higher pressures have the largest impact on both. Surprisingly, crack initiation is faster in air than at 1 bar hydrogen partial pressure. The CNT tests also reveal that the orientation of the banded microstructure has no effect on the crack initiation site, but it influences its growth behavior. Moreover, fractography shows that hydrogen also promotes instances of quasi-cleavage and intergranular fracture, linked to embrittlement of the material. Here, these results demonstrate that, while hydrogen may impact the entirety of the fatigue process, its effects on the early stages of damage accumulation become relevant only at larger pressures. More comprehensive studies of crack initiation in hydrogen atmospheres will be critical to future codes and standards for hydrogen infrastructure.

Circumferential notch tension↗

Microstructure and in-service degradation of baffle former bolts – in-core components of light water reactors

This report presents a microstructure evaluation of the baffle former bolt, a commercial pressurized water reactor component. Using SEM, EDS, and EBSD analysis the material was identified as AISI 316 steel with an annealed austenite microstructure. Findings include abnormal grain growth in a fraction of the grains and the absence of retained ferrite. Notable observations include an overlapping of pre- and post-irradiation deformation, including defect-free channel formation as an active deformation mechanism in the near-surface layer of BFB. Specimen surfaces, exposed to high-temperature, high-pressure water, exhibited signs of in-service corrosion degradation. EBSD and EDS analyses highlighted intergranular corrosion, possible grain boundary oxidation with depths less than 3 µm, and, unexpectedly, short cracks filled with Cr-rich oxides measuring around 5-6 µm. The presence of defect-free channels from EBSD data suggests episodes of high mechanical stresses during service. The specimens provide a potentially unique insight into the in-service degradation of NPP components, strain localization, and crack initiation processes. An intact corrosion layer reveals a complex component's in-service history. Further research is underway for a detailed analysis.

22 GENERAL STUDIES OF NUCLEAR REACTORS↗

Fatigue crack propagation behaviour of unidirectionally solidified gamma/gamma-prime-delta eutectic alloys

Fatigue crack propagation studies were carried out on unidirectionally solidified gamma/gamma-prime-delta (Ni-Nb-Al) alloys over an aluminum content range of 1.5-2.5% by weight. The variation of Al content of as-grown alloys did not significantly affect the crack growth behavior of these eutectic composites. The results indicate that the addition of Al to the eutectic dramatically improved the FCP behavior. The gamma/gamma-prime-delta alloy exhibited crack growth rates for a given stress intensity range that are an order of magnitude lower than those for the gamma-delta alloy. It is suggested that this difference in FCP behavior can be explained on the basis of stacking fault energy considerations. Extensive delaminations at the crack tip were also revealed, which contributed to the superior fatigue response. Delamination was predominantly intergranular in nature.

Bretz, P. E.↗

An Abrupt Transition to an Intergranular Failure Mode in the Near-Threshold FCG Regime in Ni-Based Superalloys

Cyclic near-threshold FCG behavior of two disk superalloys was evaluated, and was shown to exhibit an unexpected sudden failure mode transition from a mostly transgranular failure mode at higher stress intensities to an almost completely intergranular failure mode in the threshold regime. The change in failure modes was associated with a crossover effect in which the conditions that produced higher FCG rates in the Paris regime resulted in lower FCG rates and increased ΔKth values in the threshold region. High resolution scanning and transmission electron microscopy was used to carefully characterize the crack tips at these near-threshold conditions. Formation of stable Al-oxide followed by Cr and Ti oxides was found to occur at the crack tip prior to formation of unstable oxides. To contrast with the threshold failure mode regime, a quantitative assessment of the role that the intergranular failure mode has on cyclic FCG behavior in the Paris regime was also performed. It was demonstrated that the even a very limited intergranular failure content dominates the FCG response under mixed mode failure conditions.

fatigue crack growth↗

Intergranular oxidation and oxygen transport in Ni-20Cr during exposure to model dry and wet oxidation environments

Selective oxidation is a critical component of the proposed internal oxidation mechanism of stress corrosion cracking (SCC) for Ni-based alloys in primary water reactor (PWR) operation. To isolate and study this process, the binary Ni-20Cr was exposed to pressurized water and a CO/CO2 gas mixture. In both environments, the oxygen potential was kept under the Ni/NiO line to stimulate penetrative intergranular attack. A combination of electron microscopy and atom probe tomography was used to study the nanometer-scale details of the passivation and penetrative intergranular oxidation processes at high-energy grain boundaries. Oxygen transport towards the terminating oxidation front is elucidated with dedicated usage of oxygen isotopic tracer exchange experiments to support classical theories of internal oxidation, revealing preferred oxygen transport paths were visualized with sub-nanometer resolution.

Weiser, Martin↗

Evaluation of BISON's Transient Fission Gas Release Model on High-Burnup UO 2 MiniFuel

BISON's fission gas release (FGR) model has been evaluated and tested over several hypothetical thermal transient cases at high burnup and validated against FGR experimental data from an annealing test at high burnup. Diffusion-controlled FGR is accounted for in the model by including several physical mechanisms such as the diffusion of fission gas to grain faces, grain boundary sweeping, grain growth, and intergranular bubble growth. Under temperature variations, FGR is increased due to the development of micro-cracks at grain faces. This existing transient capability, however, was developed based on transient fuel behavior during power ramps and the associated micro-cracking process. Nevertheless, a fraction of the FGR during temperature transients such as LOCA can ensue from different mechanisms (in particular, fuel fragmentation) and present an important dependency on local burnup and high burnup structure formation. It follows that the performance and necessary developments of the existing BISON fission gas model for the analysis of LOCA-type transients need to be investigated through a systematic assessment study. Such a study is performed in this work. The model shows an overall good qualitative agreement with experimental observations on FGR during annealing tests with different temperature conditions. It also accounts well for microstructural effects on FGR. When quantitatively compared to FGR data from previously irradiated 103 MWd/kgU UO 2 discs under thermal annealing, the model shows a less satisfactory agreement with the experimental data.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Slow crack growth in sintered silicon nitride

The strength and crack growth characteristics of a sintered silicon nitride were studied at 1000 C. Fractographic analysis of material failing in dynamic fatigue revealed the presence of slow crack growth (SCG) at stressing rates below 6 ksi/min. This material can sustain a 40-ksi flexural stress at 1000 C for 400 h or more but is susceptible to both SCG and creep deformation at higher stress levels. The crack velocity exponent (N) determined both from dynamic and static fatigue experiments lies in a range from 13 to 22. The subcritical crack growth and creep behavior at 1000 C is primarily controlled by the deformation of an intergranular glassy phase.

Khandelwal, P. K.↗

Fractographic evaluation of creep effects on strain-controlled fatigue-cracking of AISI 304LC and 316 stainless steel

Analysis of high temperature low cycle fatigue of AISI 304LC and 316 stainless steels by the method of strainrange partitioning results in four separate strainrange versus life relationships, depending upon the way in which creep-strain and plastic strain are combined within a cycle. Fractography is used in this investigation of the creep-fatigue interaction associated with these cycles. The PP and PC-cycle fractures were transgranular. The PC-cycle resulted in fewer cycles of initiation and shorter total cyclic life for the same applied inelastic strainrange. The CC-cycle had mixed transgranular and intergranular fracture, fewer cycles of initiation and shorter cycle life than PP or PC. The CP-cycle had fully integranular cracking, and failed in fewer cycles than were required for cracks to initate for PP,PC, and CC.

Oldrieve, R. E.↗

Effects of processing and microstructure on the fatigue behaviour of the nickel-base superalloy Rene95

Forms of the nickel-base superalloy Rene95 produced by three processing methods were evaluated in tensile, low cycle fatigue and fatigue crack propagation tests at 540 and 650 C. Two powder-metallurgy (PM) forms, hot-isostatically-pressed and extruded-and-forged, and a conventionally cast-and-wrought form were all given the same heat treatment. The extruded-and-forged form showed superior fatigue life in low strain range tests though the two PM forms exhibited nearly identical mechanical behavior in all other respects. Further, this life difference could not be explained by significant differences in the types, sizes or shapes of the defects initiating failure. The cast-and-wrought Rene95, however, had lower strength, ductility and fatigue life, but higher fatigue crack propagation resistance because of a larger grain size. It did not exhibit the environmentally-assisted intergranular mode of propagation which occurs in PM Rene95 and other fine-grained superalloys at these test temperatures and frequencies.

Miner, R. V.↗

Failure analysis of a Stirling engine heat pipe

Failure analysis was conducted on a heat pipe from a Stirling Engine test rig which was designed to operate at 1073 K. Premature failure had occurred due to localized overheating at the leading edge of the evaporator fin. It was found that a crack had allowed air to enter the fin and react with the sodium coolant. The origin of the crack was found to be located at the inner surface of the Inconel 600 fin where severe intergranular corrosion had taken place.

Moore, Thomas J.↗

Hot Cracking Behavior and Beam-Induced Grain Refinement in Electron Beam Freeform Fabricated Al 7075

Electron beam freeform fabrication (EBF 3 ) is a high deposition rate, wire-based directed energy deposition (DED) additive manufacturing (AM) process used to print metallic parts in a vacuum environment. While high specific strength 7xxx-series Al alloys are of interest in the aerospace and automotive industries, these alloys suffer from hot cracking issues during fusion welding and AM. In this work, linear deposits of Al 7075 were fabricated with EBF 3 to study the effects of baseplate thickness, preheat temperature, and beam focus on hot cracking behavior. Solidification cracks were observed in the first deposition layer, and by the third layer coalesced into large “macrocracks” running vertically through the build height. Fine, intergranular liquation “microcracks” appeared between macrocracks below the root of the final deposit layer fusion zone. Increasing the substrate preheat temperature from 165°C to 320°C deepened the partially melted zone and resulted in a more than twofold increase in the liquation microcrack density. Analysis of Scheil solidification diagrams revealed that fugitive losses of Zn and Mg during deposition increased the susceptibility to solidification cracking and promoted substrate liquation cracking. Focused electron beam (EB) conditions combined with a high aspect ratio elliptical raster pattern resulted in bands of refined, equiaxed grains. The refined microstructure suppressed solidification macrocracking and caused a nearly fivefold reduction in liquation crack density, demonstrating that beam-induced grain refinement may be a promising low-cost method for reducing hot cracking during AM.

aluminum↗

Identifying multiple synergistic factors on the susceptibility to stress relaxation cracking in variously heat-treated weldments

The 347H austenitic stainless steel has been widely used for pressure vessels and pipeline (PVP) applications due to its excellent creep and corrosion resistance, which fit ideally to the harsh conditions in petrochemical industries, fossil fuel or nuclear power plants, and modern energy storages. However, a failure mode has been commonly observed with cracks emerging at the heat affected zone (HAZ) of weldments during post-weld heat treatment (PWHT) or under intermediate to high temperature service conditions. This phenomenon is termed as Stress Relaxation Cracking (SRC) since the purpose of PWHT is to relieve the welding-induced residual stress fields, or as Stress Age Cracking (SAC) if failure happens during service. A leading literature explanation of this failure suggests that the residual stress relaxation and the precipitation dissolution and/or re-precipitation occur in the same temperature range, which can lead to locally high strains and thus to crack at the grain boundaries. Since in situ spatial measurements of residual stress fields, microstructural evolution, and failure processes are nearly infeasible, this work recourses to a micromechanical finite element framework that models the high temperature failure as the nucleation and growth of grain boundary cavities, whereas various parameters such as thermomechanical loading history and its evolution, the competition of grain-interior dislocation creep and grain-boundary diffusion in failure lifetime, and microstructural heterogeneities (such as the precipitate free zone near grain boundaries) can be quantitatively incorporated. It can be concluded from these microstructure-explicit simulations that an accurate knowledge of residual stress evolution and a carefully calibrated set of material constitutive parameters are the essential prerequisites for lifetime predictions. The understanding of individual governing factors also leads to a mechanistic interpretation of the observed SRC susceptibility C-curves. In conclusion, these results suggest that the criticality of residual stress evolution, but not the precipitation-induced local strains, be the leading factor for SRC.

347H stainless steel weldments↗

Complex Dependence of Calcite Crack Kinetics on Salinity: The Role of DLVO and Hydration Forces

Abstract Subcritical crack growth (SCG) plays an important role in many geological processes such as delayed earth rupture and rock weathering. The complex dependency of SCG on the in‐crack fluid chemistry, however, is still poorly understood. In this study, we utilize the newly developed surface force‐based fracture theory (SFFT) to elucidate the relative contributions of surface forces and solute transport to the crack growth kinetics of calcite in NaCl solutions. Expanding on Barenblatt's cohesive crack model, SFFT introduces an effective stress intensity at the crack tip that encompasses all the relevant intermolecular forces across the crack in addition to the external far‐field stresses. The nonlinear system of equations portraying the crack opening profile, the solute distribution in a propagating crack, and the crack growth velocity are numerically solved via an implicit scheme. After carefully calibrating the model for calcite‐water systems, the SFFT is used to predict the SCG response of calcite at different NaCl concentrations, based on various hypotheses. These predictions are then compared to existing SCG data from the literature. We demonstrate that the experimentally observed variation of SCG rate with NaCl concentration cannot be explained solely by DLVO forces (electrostatic and Van der Waals interactions). This can be remediated by introducing an exponentially decaying hydration force with a nonlinear, nonmonotonic dependence on NaCl concentration. Furthermore, we demonstrate that accounting for both diffusive and advective transport of ions is important in explaining the absence of a stage‐II SCG response for calcite in electrolyte solutions. Plain Language Summary Subcritical crack growth (SCG) refers to the slow propagation of cracks in materials under a stress below the threshold for catastrophic failure. SCG is a key process in many geological events, for example, delayed earth ruptures and rock weathering. New initiatives such as underground CO 2 and H 2 storage in carbonate reservoirs further call for better understanding of SCG in carbonate minerals subjected to varying fluid chemistry. This study examines the SCG of calcite, a key mineral found in carbonate rocks, intergranular cement in sandstones, and filling material in mineral veins and faults, determining their deformation and strength. A mathematical model is developed to describe how the crack opens and propagates, how solutes (like salts) distribute within the crack, and how the crack surfaces interact with each other. We used the model to predict calcite SCG in water at different salt concentrations and compared it with experimental data. Our results revealed that the hydration force is the dominating factor in determining the complex, non‐linear dependency of SCG on salinity. We also found that both the movement of ions by diffusion and by bulk water flow are crucial for explaining the SCG rates, especially when the cracks grow quickly. Key Points Surface Force‐Based Fracture Theory predicts the complex subcritical crack growth patterns of calcite crystals immersed in NaCl solutions Results highlight the dominant role of hydration forces in altering the fracture behavior of calcite compared to VdW and electric double‐layer forces Advective solute transport explains the absence of stages‐II and ‐III subcritical crack growth responses in solid‐liquid systems

DLVO↗

Slow plastic strain rate compressive flow in binary CoAl intermetallics

Constant-velocity elevated temperature compression tests have been conducted on a series of binary CoAl intermetallics produced by hot extrusion of blended prealloyed powders. The as-extruded materials were polycrystalline, and they retained their nominal 10-micron grain size after being tested between 1100 and 1400 K at strain rates ranging from 2 x 10 to the -4th to 2 x 10 to the -7th per sec. Significant plastic flow was obtained in all cases; while cracking was observed, much of this could be due to failure at matrix-oxide interfaces along extrusion stringers rather than to solely intergranular fracture. A maximum in flow strength occurs at an aluminum-to-cobalt ratio of 0.975, and the stress exponent appears to be constant for aluminum-to-cobalt ratios of 0.85 or more. It is likely that very aluminum-deficient materials deform by a different mechanism than do other compositions.

Whittenberger, J. D.↗

Fatigue-crack propagation behavior in a high-carbon chromium SUJ2 bearing steel: Role of microstructure

High-carbon chromium martensite steels are commonly selected for bearing components in the power generation, automotive and aerospace industries where fatigue failure is a major concern. Accordingly, it is of importance to elucidate the structure-property relationships governing the fatigue properties of such bearing steels. Here, the role of microstructure in influencing the fatigue-crack propagation behavior of a high-carbon chromium SUJ2 bearing steel is examined with emphasis on three martensitic structures: (i) a fine-grained (~10 μm) structure with intragranular (but no intergranular) carbides, (ii) a coarser-grained (~25 μm) structure with discontinuous grain-boundary carbides primarily near triple junctions, and (iii) a coarse-grained (~31 μm) structure with continuous grain-boundary carbides. Although growth rates were fairly similar above ~10 -8 m/cycle, significant differences in behavior were observed at lower, near-threshold growth rates; specifically at a load ratio of 0.1, the ΔKth fatigue threshold was increased from 3.8 MPa m ½ in the fine-grained structure to 5.9 to 6.3 MPa m ½ in the two coarser-grained structures. The dominant factor governing such near-threshold behavior was found to be crack-tip shielding from roughness-induced crack closure, which was most pronounced in the coarser-grained structures; additionally, shielding from crack deflection and branching was apparent in these structures as the crack propagated through the network of intersecting martensite lamellae within the coarse grains. Compared to high-strength stainless steels and low-strength carbon steels, the fine-grained SUJ2 steel displays an exceptional combination of high strength and fatigue-crack growth resistance and is considered to be a superior structural alloy for bearing applications.

36 MATERIALS SCIENCE↗