Multiphysics Simulation of Palladium Hydride Isotope Exchange in Non-Uniform Particle Beds.
Abstract not provided.
SEARCH · Engineering Papers
Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.
Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.
Abstract not provided.
Explore the source record for details and available documents.
Abstract not provided.
Abstract not provided.
Explore the source record for details and available documents.
Abstract not provided.
The purpose of this project was to investigate and evaluate the attractiveness of using a magnesium chemical hydride slurry as a hydrogen storage, delivery, and production medium for automobiles. To fully evaluate the potential for magnesium hydride slurry to act as a carrier of hydrogen, potential slurry compositions, potential hydrogen release techniques, and the processes (and their costs) that will be used to recycle the byproducts back to a high hydrogen content slurry were evaluated. A 75% MgH 2 slurry was demonstrated, which was just short of the 76% goal. This slurry is pumpable and storable for months at a time at room temperature and pressure conditions and it has the consistency of paint. Two techniques were demonstrated for reacting the slurry with water to release hydrogen. The first technique was a continuous mixing process that was tested for several hours at a time and demonstrated operation without external heat addition. Further work will be required to reduce this design to a reliable, robust system. The second technique was a semi-continuous process. It was demonstrated on a 2 kWh scale. This system operated continuously and reliably for hours at a time, including starts and stops. This process could be readily reduced to practice for commercial applications. The processes and costs associated with recycling the byproducts of the water/slurry reaction were also evaluated. This included recovering and recycling the oils of the slurry, reforming the magnesium hydroxide and magnesium oxide byproduct to magnesium metal, hydriding the magnesium metal with hydrogen to form magnesium hydride, and preparing the slurry. We found that the SOM process, under development by Boston University, offers the lowest cost alternative for producing and recycling the slurry. Using the H2A framework, a total cost of production, delivery, and distribution of $4.50/kg of hydrogen delivered or $4.50/gge was determined. Experiments performed at Boston University have demonstrated the technical viability of the process and have provided data for the cost analyses that have been performed. We also concluded that a carbothermic process could also produce magnesium at acceptable costs. The use of slurry as a medium to carry chemical hydrides has been shown during this project to offer significant advantages for storing, delivering, and distributing hydrogen: • Magnesium hydride slurry is stable for months and pumpable. • The oils of the slurry minimize the contact of oxygen and moisture in the air with the metal hydride in the slurry. Thus reactive chemicals, such as lithium hydride, can be handled safely in the air when encased in the oils of the slurry. • Though magnesium hydride offers an additional safety feature of not reacting readily with water at room temperatures, it does react readily with water at temperatures above the boiling point of water. Thus when hydrogen is needed, the slurry and water are heated until the reaction begins, then the reaction energy provides heat for more slurry and water to be heated. • The reaction system can be relatively small and light and the slurry can be stored in conventional liquid fuel tanks. When transported and stored, the conventional liquid fuel infrastructure can be used. • The particular metal hydride of interest in this project, magnesium hydride, forms benign byproducts, magnesium hydroxide (“Milk of Magnesia”) and magnesium oxide. • We have estimated that a magnesium hydride slurry system (including the mixer device and tanks) could meet the DOE 2010 energy density goals. During the investigation of hydriding techniques, we learned that magnesium hydride in a slurry can also be cycled in a rechargeable fashion. Thus, magnesium hydride slurry can act either as a chemical hydride storage medium or as a rechargeable hydride storage system. Hydrogen can be stored and delivered and then stored again thus significantly reducing the cost of storing and delivering hydrogen. Further evaluation and development of this concept will be performed as follow-on work under another project. However, since the cost of reducing magnesium from magnesium oxide makes up 85% of the cost of the slurry, if hydrogen can be stored many times in the slurry, then the cost of storing hydrogen can be spread over many units of hydrogen and can be significantly reduced from the costs of a chemical hydride system. This may be the most important finding of this project. If the slurry is used to carry a rechargeable hydride, the slurry can be stored in a conventional liquid fuel tank and delivered to a release system as hydrogen is needed. The release system will contain only the hydride needed to produce the hydrogen desired. This is in contrast to conventional designs proposed for other rechargeable hydride systems that store all the hydride in a large and heavy pressure and heat transfer vessel.
An important aspect of understanding industrial processing is to know the characteristics of the materials used in such processes. A study was performed to determine the effects of hydriding chamber material on the degree of hydriding for the commercial production of thin film hydride targets for various research universities, commercial companies, and government national laboratories. The goal was to increase the degree of hydriding of various thin film hydrides and to study the vacuum environment during air-exposure hydriding. For this purpose, dynamic residual gas analysis during deuterium gas hydride processing was utilized with erbium thin films, employing a special set-up for direct dynamic hydride gas sampling during processing at elevated temperature and full loading gas pressure. Complete process data for (1) a copper–(1.83 wt. %)beryllium wet hydrogen fired passivated (600 °C–1 h) externally heated pipe hydriding chamber are reported. Dynamic residual gas analysis comparisons during hydriding are presented for hydriding chambers made from (2) alumina (99.8 wt. %), (3) copper (with an interior aluminum coating ∼10 k Å thick, and (4) for a stainless-steel air-fired passivated (900 °C–1 h) chamber. Dynamic data with deuterium gas in the chamber at the hydriding temperature (450 °C) showed the presence and growth of water vapor (D{sub 2}O) and related mixed ion species(H{sub 2}O{sup +}, HDO{sup +}, D{sub 2}O{sup +}, and OD{sup +}) from hydrogen isotope exchange reactions during the 1 h process time. Peaks at mass-to-charge ratios (i.e., m/e) of 12(C{sup +}), 16(CD{sub 2}{sup +}), 17(CHD{sub 2}{sup +}), and 18(CD{sub 3}{sup +}, OD{sup +}) increased for approximately the first half hour of a 1 h hydriding process and then approach steady state. Mass-to-charge peaks at 19(HDO{sup +}) and 20(D{sub 2}O{sup +}) continue to increase throughout the process cycle. Using the m/e = 20 (D{sub 2}O{sup +}) peak intensity from chamber (1)–Cu(1.83 wt. %)Be as a standard, the peak intensity from chamber (4)—stainless-steel (air-fired) was 7.1× higher, indicating that the surface of stainless-steel had a larger concentration of reactive oxygen and/or water than hydrogen. The (D{sub 2}O{sup +}) peak intensity from chamber (3)—Cu (interior Al coating) was 1.55× larger and chamber (2)—alumina(99.8%) was 1.33× higher than Cu(1.83 wt. %)Be. Thus copper–(1.83 wt. %)beryllium was the best hydriding chamber material studied followed closely by the alumina (99.8 wt. %) chamber. Gas take-up by Er occluder targets processed in Cu(1.83 wt. %)Be hydriding chambers (i.e., gas/metal atomic ratios) correlate with the dynamic RGA data.
Zirconium alloys are used in fuel cladding and structural components of nuclear power plants. Hydrogen enters the Zr matrix during plant operation and precipitates as hydride particles that degrade the mechanical properties of the alloy, limiting service life. Knowledge of the stress state within hydride precipitates is important to understand stress-induced degradation mechanisms such as delayed hydride cracking, but no direct quantification has yet been reported in the literature. Here, measurements are reported of the average elastic strain tensor within δ zirconium hydride precipitates in Zr2.5%Nb pressure tube material from CANDU power plants. Complete intensity and strain pole figures for the hydride were obtained by synchrotron X-ray diffraction experiments on specimens with hydrogen contents ranging from ~100 wt p.p.m. hydrogen to nearly 100% δ-hydride. Zirconium hydride precipitates by a process involving a martensitic transformation, with two hydride variants possible from a single α-Zr grain. A synthetic model of the hydride crystallographic texture allowed the interpretation of the measured strain pole figures and quantification of the elastic strain tensor for both texture components. It was found that the two variants appear in nearly equal proportion but with different stress states, differing in the sign of the shear strain components (~±3000 µ$\epsilon$). This difference is possibly associated with the shear movement of Zr atoms during the phase transformation. This suggests that hydride clusters are composed of stacks of smaller hydrides in alternating hydride variants. Stresses were estimated from a set of rather uncertain hydride elastic constants. Overall, both variants showed compressive strains along the tube axial direction (~5000 µ$\epsilon$). For low hydrogen concentrations, the hydrides' stress tensor is dominated by compressive stresses of ~300 MPa along the axial direction, probably caused by the elongated morphology of hydride clusters along this direction, and variant-dependent shear stresses of ~±100 MPa, probably from the shear movement of the Zr atoms involved in the phase transformation.
The catalytic reduction of carbon dioxide to fuels and value-added chemicals is of significance for the development of carbon recycling technologies. One of the main challenges associated with catalytic CO 2 reduction is product selectivity: the formation of carbon monoxide, molecular hydrogen, formate, methanol, and other products occurs with similar thermodynamic driving forces, making it difficult to selectively reduce CO 2 to the target product. Significant scientific effort has been aimed at the development of catalysts that can suppress the undesired hydrogen evolution reaction and direct the reaction toward the selective formation of the desired products, which are easy to handle and store. Inspired by natural photosynthesis, where the CO 2 reduction is achieved using NADPH cofactors in the Calvin cycle, in this study we explore biomimetic metal-free hydride donors as catalysts for the selective reduction of CO 2 to formate. Here, we outline our recent findings on the thermodynamic and kinetic parameters that control the hydride transfer from metal-free hydrides to CO 2 . By experimentally measuring and theoretically calculating the thermodynamic hydricities of a range of metal-free hydride donors, we derive structural and electronic factors that affect their hydride-donating abilities. Two dominant factors that contribute to the stronger hydride donors are identified to be (i) the stabilization of the positive charge formed upon HT via aromatization or by the presence of electron-donating groups and (ii) the destabilization of hydride donors through the anomeric effect or in the presence of significant structural constrains in the hydride molecule. Hydride donors with appropriate thermodynamic hydricities were reacted with CO 2 , and the formation of the formate ion (the first reduction step in CO 2 reduction to methanol) was confirmed experimentally, providing an important proof of principle that organocatalytic CO 2 reduction is feasible. The kinetics of hydride transfer to CO 2 were found to be slow, and the sluggish kinetics were assigned in part to the large self-exchange reorganization energy associated with the organic hydrides in the DMSO solvent. Finally, we outline our approaches to the closure of the catalytic cycle via the electrochemical and photochemical regeneration of the hydride (R–H) from the conjugate hydride acceptors (R + ). We illustrate how proton-coupled electron transfer can be efficiently utilized not only to lower the electrochemical potential at which the hydride regeneration takes place but also to suppress the unwanted dimerization that neutral radical intermediates tend to undergo. Overall, this account provides a summary of important milestones achieved in organocatalytic CO 2 reduction and provides insights into the future research directions needed for the discovery of inexpensive catalysts for carbon recycling.
d-hydride structures in Zr nuclear fuel-rod cladding significantly affect mechanical properties. In this work, a micromechanical phase-field model is developed to investigate the effect of interfacial energy anisotropy and elastic interaction on the nucleation, stacking structure formation, and stacking structure transition of d-hydride precipitates. It is found that the nucleation probability and growth of d-hydride near pre-existing hydrides are strongly spatially dependent. Results show that (1) the d-hydride precipitate has a platelet-like shape. The large shear deformation associated with lattice mismatches and a small interfacial energy of its broad interface cause the orientation of the plate-like d-hydride off the basal plane a small angle of approximately 14.7°. (2) Stress-induced nucleation of d-hydride precipitates near a pre-existing hydride results in the unique stacking structure formation of d-hydride precipitates. (3) The morphology and alignment of hydride stacking structures, called as macroscopic hydrides which consist of microscopic hydrides with certain stacking sequences, change under stresses. The alignment of macroscopic hydrides changes from along the circumferential direction to along the radial direction under tensile hoop stress while the orientation of microscopic hydrides remains parallel to the basal plane. These results are in agreement with experimental observations. The simulations reveal that stress-induced heterogeneous nucleation and growth is the mechanism for the formation and transition of unique macro-hydride stacking structures observed in in Zr nuclear fuel-rod cladding.
Zirconium hydrides precipitate in fuel cladding alloys as a result of hydrogen uptake from the high-temperature corrosion environment of light water reactors. Synchrotron X-ray diffraction was performed at room temperature on stress-relieved Zircaloy-4 cladding with two distributions of hydrides - (1) uniformly distributed hydrides across the entire cladding wall and (2) hydride rim next to the outer surface. The {delta}-hydride phase was found to be the predominant hydride phase to precipitate for hydrogen contents up to 1250 weight parts per million (wt ppm). At a higher content, about 3000 wt ppm, although {delta}-hydride is still the majority phase, a significant amount of {gamma}-hydride is also observed. At even higher hydrogen contents, in excess of approximately 6000 wt ppm, such as can occur in a highly dense hydride layer, peaks associated with the {epsilon}-hydride phase are also observed in the diffraction pattern. The volume fraction of hydrides was estimated as a function of hydrogen content using the integrated intensities of select diffraction peaks corresponding to the {alpha}-Zr matrix and the hydride phases. These estimated values agree well with calculated values from the independently measured concentrations. The results of this study indicate that hydride precipitation in Zircaloy-4 is a complex process of evolving hydride phases with increasing local hydrogen content.
A systematic study of H. B. Robinson (HBR) high burnup spent nuclear fuel (SNF) vibration integrity was performed in Phase I project under simulated transportation environments, using the Cyclic Integrated Reversible-Bending Fatigue Tester (CIRFT) hot cell testing technology developed at Oak Ridge National Laboratory in 2013–14. The data analysis on the as-irradiated HBR SNF rods demonstrated that the load amplitude is the dominant factor that controls the fatigue life of bending rods. However, previous studies have shown that the hydrogen content and hydride morphology has an important effect on zirconium alloy mechanical properties. To address the effect of radial hydrides in SNF rods, in Phase II a test procedure was developed to simulate the effects of elevated temperatures, pressures, and stresses during transfer-drying operations. Pressurized and sealed fuel segments were heated to the target temperature for a preset hold time and slow-cooled at a controlled rate. The procedure was applied to both non-irradiated/prehydrided and high-burnup Zircaloy-4 fueled cladding segments using the Nuclear Regulatory Commission-recommended 400°C maximum temperature limit at various cooling rates. Before testing high-burnup cladding, four out-of-cell tests were conducted to optimize the hydride reorientation (R) test condition with pre-hydride Zircaloy-4 cladding, which has the same geometry as the high burnup fuel samples. Test HR-HBR#1 was conducted at the maximum hoop stress of 145 MPa, at a 400°C maximum temperature and a 5°C/h cooling rate. On the other hand, thermal cycling was performed for tests HR-HBR#2, HR-HBR#3, and HR-HBR#4 to generate more radial hydrides. It is clear that thermal cycling increases the ratio of the radial hydride to circumferential hydrides. The internal pressure also has a significant effect on the radial hydride morphology. This report describes a procedure and experimental results of the four out-of-cell hydride reorientation tests of hydrided Zircaloy-4 cladding, which served as a guideline to prepare in-cell hydride reorientation samples with high burnup HBR fuel segments. This report also provides the Phase II CIRFT test data for the hydride reorientation irradiated samples. The variations in fatigue life are provided in terms of moment, equivalent stress, curvature, and equivalent strain for the tested SNFs. The CIRFT results appear to indicate that hydride reoriented treatment (HRT) have a negative effect on fatigue life, in addition to hydride reorientation effect. For HR4 specimen that had no pressurization procedure applied, the thermal annealing treatment alone showed a negative impact on the fatigue life compared to the HBR rod.
In light water nuclear reactors, waterside corrosion of the cladding material leads to the production of hydrogen, a fraction of which is picked up by the zirconium cladding and precipitates into brittle hydride particles. These nanoscale hydride particles aggregate into mesoscale hydride clusters. The principal stacking direction of the nanoscale hydrides precipitated in the cladding tube changes from circumferential in the absence of applied stress to radial under circumferential applied stress. A quantitative phase field model has been developed to predict the hydride morphology observed experimentally and identify the mechanisms responsible for nanoscale hydride stacking. The model focuses on nanoscale hydride precipitation in a single zirconium grain with a detailed description of the anisotropic elastic contribution. The model predictions concerning the shape, orientation, and stacking behavior of nanoscale hydride are analyzed and compared with experimental observations. The model accurately accounts for the experimentally observed elongated nanoscale hydride shape and the stacking of hydrides along the basal plane of the hexagonal zirconium matrix. When investigating the role of applied stress in hydride morphology, the model challenges some of the mechanisms previously proposed to explain hydride reorientation. Finally, although hydride reorientation has been hypothesized to be caused by a change in nanoscale hydride shape, the current study shows that these mechanisms are unlikely to occur.
In an attempt to mitigate the hazards associated with storing large quantities of reactive metal hydrides, polymer composite materials were synthesized and tested under simulated usage and accident conditions. The composites were made by polymerizing vinyl monomers using free-radical polymerization chemistry, in the presence of the metal hydride. Composites with vinyl-containing siloxane oligomers were also polymerized with and without added styrene and divinyl benzene. Hydrogen capacity measurements revealed that addition of the polymer to the metal hydride reduced the inherent hydrogen storage capacity of the material. The composites were found to be initially effective at reducing the amount of heat released during oxidation. However, upon cycling the composites, the mitigating behavior was lost. While the polymer composites we investigated have mitigating potential and are physically robust, they undergo a chemical change upon cycling that makes them subsequently ineffective at mitigating heat release upon oxidation of the metal hydride. Acknowledgements The authors would like to thank the following people who participated in this project: Ned Stetson (U.S. Department of Energy) for sponsorship and support of the project. Ken Stewart (Sandia) for building the flow-through calorimeter and cycling test stations. Isidro Ruvalcaba, Jr. (Sandia) for qualitative experiments on the interaction of sodium alanate with water. Terry Johnson (Sandia) for sharing his expertise and knowledge of metal hydrides, and sodium alanate in particular. Marcina Moreno (Sandia) for programmatic assistance. John Khalil (United Technologies Research Corp) for insight into the hazards of reactive metal hydrides and real-world accident scenario experiments. Summary In an attempt to mitigate and/or manage hazards associated with storing bulk quantities of reactive metal hydrides, polymer composite materials (a mixture of a mitigating polymer and a metal hydride) were synthesized and tested under simulated usage and accident conditions. Mitigating the hazards associated with reactive metal hydrides during an accident while finding a way to keep the original capability of the active material intact during normal use has been the focus of this work. These composites were made by polymerizing vinyl monomers using free-radical polymerization chemistry, in the presence of the metal hydride, in this case a prepared sodium alanate (chosen as a representative reactive metal hydride). It was found that the polymerization of styrene and divinyl benzene could be initiated using AIBN in toluene at 70°C. The resulting composite materials can be either hard or brittle solids depending on the cross-linking density. Thermal decomposition of these styrene-based composite materials is lower than neat polystyrene indicating that the chemical nature of the polymer is affected by the formation of the composite. The char-forming nature of cross-linked polystyrene is low and therefore, not an ideal polymer for hazard mitigation. To obtain composite materials containing a polymer with higher char-forming potential, siloxane-based monomers were investigated. Four vinyl-containing siloxane oligomers were polymerized with and without added styrene and divinyl benzene. Like the styrene materials, these composite materials exhibited thermal decomposition behavior significantly different than the neat polymers. Specifically, the thermal decomposition temperature was shifted approximately 100 °C lower than the neat polymer signifying a major chemical change to the polymer network. Thermal analysis of the cycled samples was performed on the siloxane-based composite materials. It was found that after 30 cycles the siloxane-containing polymer composite material has similar TGA/DSC-MS traces as the virgin composite material indicating that the polymer is physically intact upon cycling. Hydrogen capacity measurements revealed that addition of the polymer to the metal hydride in the form of a composite material reduced the inherent hydrogen storage capacity of the material. This reduction in capacity was observed to be independent of the amount of charge/discharge cycles except for the composites containing siloxane, which showed less of an impact on hydrogen storage capacity as it was cycled further. While the reason for this is not clear, it may be due to a chemically stabilizing effect of the siloxane on the metal hydride. Flow-through calorimetry was used to characterize the mitigating effectiveness of the different composites relative to the neat (no polymer) material. The composites were found to be initially effective at reducing the amount of heat released during oxidation, and the best performing material was the siloxane-containing composite which reduced the heat release to less than 50% of the value of the neat material. However, upon cycling the composites, all mitigating behavior was lost. The combined results of the flow-through calorimetry, hydrogen capacity, and thermogravimetric analysis tests lead to the proposed conclusion that while the polymer composites have mitigating potential and are physically robust under cycling, they undergo a chemical change upon cycling that makes them ineffective at mitigating heat release upon oxidation of the metal hydride.
This study examines the use of transition-metal hydride complexes that can be generated by the heterolytic cleavage of H 2 gas to form B–H bonds. Specifically, these studies are focused on providing a reliable and quantitative method for determining when hydride transfer from transition-metal hydrides to three-coordinate BX 3 compounds will be favorable. This involves both experimental and theoretical determinations of hydride transfer abilities. Thermodynamic hydride donor abilities (ΔG° H- ) were determined for HRh(dmpe) 2 and HRh(depe) 2 , where dmpe = 1,2-bis(dimethylphosphinoethane) and depe = 1,2-bis(diethylphosphinoethane), on a previously established scale in acetonitrile. This hydride donor ability was used to determine the hydride donor ability of [HBEt 3 ]⁻ on this scale. Isodesmic reactions between [HBEt 3 ]⁻ and various BX 3 complexes to form BEt 3 and [HBX 3 ]⁻ were examined computationally to determine the relative hydride affinities of various BX 3 compounds. The use of these scales of hydride donor abilities and hydride affinities for transition-metal hydrides and BX 3 compounds is illustrated with a few selected reactions relevant to the regeneration of ammonia borane. Our findings indicate that it is possible to form B-H bonds from B-X bonds, and the extent to which BX 3 compounds are reduced by transition-metal hydride complexes forming species containing multiple B-H bonds depends on the heterolytic B-X bond energy. An example is the reduction of B(SPh) 3 using HRh(dmpe) 2 in the presence of triethylamine to form Et 3 N-BH 3 in high yields. Pacific Northwest National Laboratory is operated by Battelle for the US Department of Energy.
Hydrogen is proposed as an ideal carrier for storage, transport, and conversion of energy. However, its storage is a key problem in the development of hydrogen economy. Metal hydrides hold promise in effectively storing hydrogen. For this reason, metal hydrides have been the focus of intensive research. The chemical bonds in light metal hydrides are predominantly covalent, polar covalent or ionic. These bonds are often strong, resulting in high thermodynamic stability and low equilibrium hydrogen pressures. In addition, the directionality of the covalent/ionic bonds in these systems leads to large activation barriers for atomic motion, resulting in slow hydrogen sorption kinetics and limited reversibility. One method for enhancing reaction kinetics is to reduce the size of the metal hydrides to nano scale. This method exploits the short diffusion distances and constrained environment that exist in nanoscale hydride materials. In order to reduce the particle size of metal hydrides, mechanical ball milling is widely used. However, microscopic mechanisms responsible for the changes in kinetics resulting from ball milling are still being investigated. The objective of this work is to use metal organic frameworks (MOFs) as templates for the synthesis of nano-scale NaAlH4 particles, to measure the H2 desorption kinetics and thermodynamics, and to determine quantitative differences from corresponding bulk properties. Metal-organic frameworks (MOFs) offer an attractive alternative to traditional scaffolds because their ordered crystalline lattice provides a highly controlled and understandable environment. The present work demonstrates that MOFs are stable hosts for metal hydrides and their reactive precursors and that they can be used as templates to form metal hydride nanoclusters on the scale of their pores (1-2 nm). We find that using the MOF HKUST-1 as template, NaAlH4 nanoclusters as small as 8 formula units can be synthesized inside the pores. A detailed picture of the hydrogen desorption is investigated using a simultaneous thermogravimetric modulated-beam mass spectrometry instrument. The hydrogen desorption behavior of NaAlH4 nano-clusters is found to be very different from bulk NaAlH4. The bulk NaAlH4 desorbs about 70 wt% hydrogen {approx}250 C. In contrast, confinement of NaAlH4 within the MOF pores dramatically increases the rate of H2 desorption at lower temperatures. About {approx}80% of the total H2 desorbed from MOF-confined NaAlH4 is observed between 70 to 155 C. In addition to HKUST-1, we find that other MOFs (e.g. MIL-68 and MOF-5) can be infiltrated with hydrides (LiAlH4, LiBH4) or hydride precursors (Mg(C4H9)2 and LiC2H5) without degradation. By varying pore dimensions, metal centers, and the linkers of MOFs, it will be possible to determine whether the destabilization of metal hydrides is dictated only by the size of the metal hydride clusters, their local environment in a confined space, or by catalytic effects of the framework.
Since hydride microstructure can significantly influence Zr alloy nuclear fuel cladding’s ductility, a new metric has been developed to quantify hydride microstructure in 2D micrographs and relate it to crack propagation. As cladding failure usually results from a hoop stress, this new metric, called the Radial Hydride Continuous Path (RHCP), is based on quantifying the continuity of brittle hydride particles along the radial direction of the cladding tube. Compared to previous metrics, this approach more closely relates to the propensity of a crack to propagate radially through the cladding tube thickness. The RHCP takes into account hydride length, orientation, and connectivity to choose the optimal path for crack propagation through the cladding thickness. The RHCP can therefore be more closely linked to hydride embrittlement of the Zr alloy material, thus creating a relationship between material structure, properties, and performance. The new definition, along with previously proposed metrics such as the Radial Hydride Fraction (RHF), the Hydride Continuity Coefficient (HCC), and the Radial Hydride Continuity Factor (RHCF), have been implemented and automated in MATLAB. These codes are made available with this publication as supplementary materials. These metrics were verified by comparing their predictions of hydride morphology against expected values in simple cases, and the implementation of the new metric was validated by comparing its predictions with manual measurements of hydride microstructure performed on ImageJ. The RHCP was also validated against experimental measurements of fracture behavior and it was shown to correlate with cladding failure better than previous metrics. The information provided by these metrics will help accurately assess cladding integrity during operation, transportation, and storage.