At least 127 records · Page 7

Research of the tritium saturation, isotope diffusion and decontamination of stainless steel using magnetic microscopy

The investigations of the tritium distribution in a surface layer and in the depth of samples using a magnetic microscope were carried out. The dependence of a saturation level in the boundary layer for hydrogen was established from a preliminary examination of samples. Conservation of the tritium distribution profile in the depth of the stainless steel samples after completion of their saturation and cooling was assigned. For Inconel-625 substantial tritium redistribution and release during storage (300 K, 15 and 28 months) were experimentally ascertained to a greater degree satisfies the classical characteristics of the diffusion process. The 'braking' effect of tritium diffusion was found by preliminary saturation of samples by hydrogen. Research in tritium decontamination effects for samples saturated with tritium with various technological preparation was carried out and essential increase of its efficiency was founded. The experiments emulated a model of technological operation cycle of the thermonuclear reactor. (authors)

70 PLASMA PHYSICS AND FUSION TECHNOLOGY↗

Effect of radiogenic helium on stainless steel 12Cr18Ni10Ti mechanical properties and hydrogen permeability

Samples of stainless steel 12Cr18Ni10Ti with radiogenic helium were subjected to mechanical tests with a constant extension rate. The presence of {sup 3}He does not markedly affect the strength characteristic, but significantly decreases plasticity of steel. The presence of hydrogen enhances the embrittlement of steel, containing {sup 3}He. The diffusion coefficient of hydrogen does not change significantly in the presence of helium, but the traps for hydrogen, which occur due to the presence of helium, delay the kinetics of a steady state flux onset at helium concentration of 50 appm. (authors)

36 MATERIALS SCIENCE↗

Hydrogen release from ferritic/martensitic stainless steel

Hydrogen release behaviors from the 8Cr2W stainless steel (RAF/M) around RT are examined by using tritium tracer techniques, and trapping effects of bulk and surface are discussed. In the overall release, three different release stages are clearly distinguished giving three different diffusion coefficients and release amounts which indicate the existence of different kinds of trapping. In addition, the appreciable amount of hydrogen (tritium) is trapped on the surface and/or surface oxides of RAF/M, but they are hardly released and show no influence on the overall hydrogen release behavior. At very low hydrogen concentration, almost all hydrogen atoms are trapped at the deepest trapping site, probably M23C6, and the sites are easily saturated. With increasing the hydrogen concentration, the shallower trapping sites are occupied. Remaining hydrogen atoms seem to be in normal (interstitial) sites, whose amount increases with the square root of the hydrogen loading pressure, but they are still influenced by trapping with lattice imperfections and/or grain boundaries. (authors)

36 MATERIALS SCIENCE↗

Hydrogen retention in deposition layers formed from type 316 stainless steel

From the viewpoints of plasma control and radiation safety, tritium retention in deposition layers is an important problem. In this study, deposition layers from type 316 stainless steel were formed by a sputtering method using hydrogen RF plasma at three different temperatures. The behavior of hydrogen release from the deposition layers was observed by a thermal desorption method at argon atmosphere. It was found that hydrogen retention and release behavior greatly change depending on the temperature of a substrate where the layer is formed. The surface structure of the layer also changed depending on the temperature. However, the ratios of metallic atoms such as Fe, Cr and Ni in deposition layers were almost the same as that in type 316 stainless steel. (authors)

36 MATERIALS SCIENCE↗

Microstructure and Mechanical Characterization of Incoloy 925 Welds in the As-Welded and Direct Aged Conditions

The joints of Incoloy 925 obtained from gas tungsten arc welding (GTAW) with pulsating current utilizing ERNiCrMo-3 and ERNiCrMo-10 were investigated under as-welded and direct aged conditions. The microstructure showed the microsegregation of Nb-Mo-, Ti-rich phases in the weld zone of ERNiCrMo-3 in the as-welded condition. Post-weld heat treatment (PWHT) involving direct aging was carried out on the weldments at 732 °C for 4 h followed by air cooling. On direct aging, the tensile strength of the base metal increases by 40% when compared to the as-received ones. The failures were experienced in the parent metal of Incoloy 925 upon tension testing in as-welded conditions. Although the tensile strength was improved considerably, the failures occurred at the fusion zones, for both the fillers in the direct aged conditions. The joint efficiencies of Incoloy 925 welds employing ERNiCrMo-3 and ERNiCrMo-10 were reported as 95 and 86%, respectively. The impact toughness of the weldments in both the as-welded and PWHT conditions was considerably greater compared to that of the candidate metal.

36 MATERIALS SCIENCE↗

Microstructural Investigation of VPPA–GMAW Welded 7A52 Aluminum Alloys

In this study, the microstructural features of 7A52 heat-treatable aluminum alloys welded by variable polarity plasma arc (VPPA) combined with gas metal arc welding (GMAW) (VPPA–GMAW) were investigated and compared with those of 7A52 aluminum alloys welded by GMAW. The grain structures and modification of the precipitates were analyzed by optical microscopy and transmission electron microscopy. Complementary to modification of the precipitates, the precipitation evolution in the heat-affected zone and magnesium loss in the fusion zone were measured by differential scanning calorimetry and inductively coupled plasma spectroscopy. In VPPA–GMAW, the weld only needs one pass by depositing on one side of the 10-mm-thick aluminum alloy plates because of the large penetration capability of VPPA and good fluidity of the molten metal in the weld pool. Accordingly, the effect of excessive heat input on the microstructure can be minimized. The results show that the grain growth is not obvious and the magnesium loss is small in the fusion zone of VPPA–GMAW compared with that of GMAW under the condition of equal heat input to the workpiece. Small precipitates inside the grains remain homogeneously distributed, and a large volume fraction of the η′ phase exists. The VPPA–GMAW weld exhibits less tendency to soften; thus, VPPA–GMAW is appropriate for welding thick-plate aluminum alloys with a high production rate.

36 MATERIALS SCIENCE↗

Effect of Shielding Gas on the Properties of AW 5083 Aluminum Alloy Laser Weld Joints

The paper deals with the evaluation of the shielding gas influence on the properties of AW 5083 aluminum alloy weld joints produced with disk laser. Butt weld joints were produced under different shielding gas types, namely Ar, He, Ar + 5 vol.% He, Ar + 30 vol.% He and without shielding weld pool. Light and electron microscopy, computed tomography, microhardness measurements and tensile testing were used for evaluation of weld joint properties. He-shielded weld joints were the narrowest ones. On the other hand, Ar-shielded weld joints exhibited largest weld width. The choice of shielding gas had significant influence on the porosity level of welds. The lowest porosity was observed in weld joint produced in Ar with the addition of 5 vol.% He shielding atmosphere (only 0.03%), while the highest level of porosity was detected in weld joint produced in pure He (0.24%). Except unshielded aluminum alloy weld joint, the lowest tensile strength was recorded in He-shielded weld joints. On the contrary, the highest average microhardness was measured in He-shielded weld joints.

36 MATERIALS SCIENCE↗

DEVELOPING AND QUANTIFYING PARAMETERS FOR CLOSURE WELDING OVERPACKS CONTAINING RESEARCH REACTOR SPENT NUCLEAR FUEL AT HANFORD

Fluor engineers developed a Gas Tungsten Arc Welding (GTAW) technique and parameters, demonstrated requisite weld quality and successfully closure-welded packaged spent nuclear fuel (SNF) overpacks at the Hanford Site. This paper reviews weld development and qualification activities associated with the overpack closure-welding and provides a summary of the production campaign. The primary requirement of the closure weld is to provide leaktight confinement of the packaged material against release to the environment during interim storage (40-year design term). Required weld quality, in this case, was established through up-front development and qualification, and then verification of parameter compliance during production welding. This approach was implemented to allow for a simpler overpack design and more efficient production operations than possible with approaches using routine post-weld testing and nondestructive examination (NDE). . A series of welding trials were conducted to establish the desired welding technique and parameters. Qualification of the process included statistical evaluation and American Society of Mechanical Engineers (ASME) Section IX testing. In addition, pull testing with a weighted mockup, and thermal calculation/physical testing to identify the maximum temperature the packaged contents would be subject to during welding, was performed. Thirteen overpacks were successfully packaged and placed into interim storage. The closure-welding development activities (including pull testing and thermal analysis) provided the needed confidence that the packaged SNF overpacks could be safely handled and placed into interim storage, and remain leaktight for the duration of the storage term.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Developing and Qualifying Parameters for Closure Welding Overpacks Containing Research Reactor Spent Nuclear Fuel at Hanford

Fluor engineers developed a Gas Tungsten Arc Welding (GTAW) technique and parameters, demonstrated requisite weld quality, and successfully closure-welded packaged spent nuclear fuel (SNF) overpacks at the Hanford Site. This paper reviews weld development and qualification activities associated with the overpack closure-welding and provides a summary of the production campaign. The primary requirement of the closure weld is to provide leak-tight confinement of the packaged material against release to the environment during interim storage (40-year design term). Required weld quality, in this case, was established through up-front development and qualification, and then verification of parameter compliance during production welding. This approach was implemented to allow for a simpler overpack design and more efficient production operations than possible with approaches using routine post-weld testing and nondestructive examination (NDE). A series of welding trials were conducted to establish the desired welding technique and parameters. Qualification of the process included statistical evaluation and American Society of Mechanical Engineers (ASME) Section IX testing. In addition, pull testing with a weighted mockup, and thermal calculation/physical testing to identify the maximum temperature the packaged contents would be subject to during welding, was performed. Thirteen overpacks were successfully packaged and placed into interim storage. The closure-welding development activities (including pull testing and thermal analysis) provided the needed confidence that the packaged SNF overpacks could be safely handled and placed into interim storage, and remain leak-tight for the duration of the storage term. (author)

42 ENGINEERING↗

Characterization of microstructure and texture across dissimilar super duplex/austenitic stainless steel weldment joint by super duplex filler metal

In the present paper, microstructural changes across an as-welded dissimilar austenitic/duplex stainless steel couple welded by a super duplex stainless steel filler metal using gas tungsten arc welding process is characterized with optical microscopy and electron back-scattered diffraction techniques. Accordingly, variations of microstructure, texture, and grain boundary character distribution of base metals, heat affected zones, and weld metal were investigated. The results showed that the weld metal, which was composed of Widmanstätten austenite side-plates and allotriomorphic grain boundary austenite morphologies, had the weakest texture and was dominated by low angle boundaries. The welding process increased the ferrite content but decreased the texture intensity at the heat affected zone of the super duplex stainless steel base metal. In addition, through partial ferritization, it changed the morphology of elongated grains of the rolled microstructure to twinned partially transformed austenite plateaus scattered between ferrite textured colonies. However, the texture of the austenitic stainless steel heat affected zone was strengthened via encouraging recrystallization and formation of annealing twins. At both interfaces, an increase in the special character coincident site lattice boundaries of the primary phase as well as a strong texture with <100> orientation, mainly of Goss component, was observed. - Graphical abstract: Display Omitted - Highlights: • Weld metal showed local orientation at microscale but random texture at macroscale. • Intensification of <100> orientated grains was observed adjacent to the fusion lines. • The austenite texture was weaker than that of the ferrite in all duplex regions. • Welding caused twinned partially transformed austenites to form at SDSS HAZ. • At both interfaces, the ratio of special CSL boundaries of the primary phase increased.

36 MATERIALS SCIENCE↗

CHARACTERIZATION OF DEFECTS IN ALLOY 152, 52 AND 52M WELDS

Defect distributions have been documented by optical metallography, scanning electron microscopy and electron backscatter diffraction in alloy 152 and 52 mockups welds, alloy 52 and 52M overlay mockups and an alloy 52M inlay. Primary defects were small cracks at grain boundaries except for more extensive cracking in the dilution zone of an alloy 52 overlay on 304SS. Detailed characterizations of the dilution zone cracks were performed by analytical transmission electron microscopy identifying grain boundary titanium-nitride precipitation associated with the intergranular separations. I. INTRODUCTION Weldments continue to be a primary location of stress-corrosion cracking (SCC) in light-water reactor systems. While problems related to heat-affected-zone (HAZ) sensitization and intergranular (IG) SCC of austenitic stainless alloys in boiling-water reactors (BWRs) have been significantly reduced, SCC has now been observed in HAZs of non-sensitized materials and in dissimilar metal welds where Ni-base alloy weld metals are used. IGSCC in weld metals has been observed in both BWRs and pressurized water reactors (PWRs) with recent examples for PWR pressure vessel penetrations producing the most concern. This has led to the replacement of alloy 600/182/82 welds with higher Cr, more corrosion-resistant replacement materials (alloy 690/152/52/52M). Complicating this issue has been a known susceptibility to cracking during welding [1-7] of these weld metals. There is a critical need for an improved understanding of the weld metal metallurgy and defect formation in Ni-base alloy welds to effectively assess long-term performance. A series of macroscopic to microscopic examinations were performed on available mockup welds made with alloy 52 or alloy 152 plus selected overlay and inlay mockups. The intent was to expand our understanding of weld metal structures in simulated LWR service components with a focus on as-welded defects. Microstructural features, defect distributions, defect characteristics and weld residual strains were examined by optical metallography, scanning electron microscopy, electron backscatter diffraction and transmission electron microscopy. Industry-supplied mock-up welds were characterized including alloy 52 and 152 weldments, alloy 52M overlay and inlay welds, and an alloy 52 overlay. II. WELDMENTS II.A. Alloy 52 and 152 Weld Mockups The alloy 52 and 152 weld mockups were fabricated by MHI for the Kewaunee reactor and were obtained from the EPRI NDE Center. The mockups were U-groove welds joining two plates of 304SS as shown in Figure 1. Alloy 152 butter (heat 307380) was placed on the U-groove surface for both mockups by shielded metal arc welding (SMAW). For the alloy 152 weld mockup, the alloy 152 fill (heat 307380) was also applied using SMAW while for the alloy 52 weld mockup, the alloy 52 fill (heat NX2686JK) was applied using gas tungsten arc welding (GTAW). Welding parameters for the fill materials were substantially different with the alloy 152 SMAW having a deposition speed of 4-25 cm/min with a current of 95-145 A and the alloy 52 GTAW having a deposition speed of 4-10 cm/min with a current of 150-300 A. One prominent feature in these mockup welds is the presence of a crack starting at the 304SS butt joint at the bottom of the U-groove and extending up into the weld. It appears that the 304SS plate on either side of the butt joint acted as an anchor for the weld resulting in a stress rise across the slit that drove crack formation and extension up into the fill weld. As will be shown in the next section, the extent of the cracking around this stress riser was much greater in the MHI 52 weld mockup.

21 SPECIFIC NUCLEAR REACTORS AND ASSOCIATED PLANTS↗

A New Perspective on Fatigue Performance of Advanced High- Strength Steels (AHSS) GMAW Joints

Weld fatigue performance is a critical aspect for application of advanced high-strength steels (AHSS) in automotive body structures. A comparative study has been conducted to evaluate the fatigue life of AHSS welds. The material studied included seven AHSS of various strength levels - DP 600, DP 780, DP 980, M130, M220, solution annealed boron and fully hardened boron steels. Two conventional steels, HSLA 590 and DR 210, were also included for baseline comparison. Lap fillet welds were made on 2-mm nominal thick sheets by the gas metal arc welding process (GMAW). Fatigue test was conducted under a number of stress levels to obtain the S/N curves of the weld joints. It was found that, unlike in the static and impact loading conditions, the fatigue performance of AHSS is not influenced by the HAZ softening in AHSS. There are appreciable differences in the fatigue lives among different AHSS. Changes in weld parameters can influence the fatigue life of the weld joints, particularly of these of higher strength AHSS. A model is developed to predict the fatigue performance of AHSS welds. The validity of the model is benchmarked with the experimental results. This model is capable to capture the effects of weld geometry and weld microstructure and strength on the fatigue performance experimentally observed. The theoretical basis and application of the newly developed fatigue modeling methodology will be discussed.

36 MATERIALS SCIENCE↗

The Effect of Weld Metal Composition on Microstructural and Mechanical Properties of Dissimilar Welds Between Monel 400 and Inconel 600

The current work was carried out to characterize welding of Inconel 600 superalloy and Monel 400. In the present study, gas tungsten arc welding (GTAW) with four types of filler metals (ENiCu, ENiCu-7, ENiCr-3 and ENiCrFe-3) was utilized. The filler metals were categorized into two groups based on the presence of Cr and Nb in their chemical composition. This paper describes the selection and application of welding consumables in manufacturing dissimilar metal combinations. It was found that (Nb/Cr) ratio and Fe content can affect on the size and amount of carbides. During solidification of ENiCr-3 and ENiCrFe-3 filler metals, Nb leaves dendritic cores and is rejected to inter-dendritic regions because of its high tendency for segregation. However, No brittle Laves phase was detected in the welds. The interface between weld metal and base metal and gradual changes in alloying elements were also investigated by scanning electron microscopy. EDX analysis was also applied for different samples. Microhardness measurements and tensile test were performed on the joints. The average hardness value in the weld metal obtained from ENiCrFe-3 is higher than the other welds. ENiCu-7 weld exhibited the highest tensile strength of 540 MPa and percent elongation of 53% in contrast to ENiCrFe-3 weld with the lowest tensile strength (518 MPa) and percent elongation (39%).

36 MATERIALS SCIENCE↗

Characterization of as-welded microstructure of heat-affected zone in modified 9Cr–1Mo–V–Nb steel weldment

Non-equilibrium microstructure of the heat-affected zone (HAZ) in the as-welded modified 9Cr–1Mo–V–Nb pipe steel (P91) weldment deposited by gas tungsten arc welding (GTAW) and flux core arc welding (FCAW) has been characterized by field-emission scanning electron microscope (FESEM) and electron backscatter diffraction (EBSD). The heterogeneous structures in the sub-layers of the as-welded HAZ are attributable to phase transformations caused by the welding thermal cycles and the local structure variations in the as-received base metal. Coarse-grained heat-affected zone (CGHAZ) has a prior austenite grain (PAG) size of 20 μm. Fine uniformly-distributed precipitates and a higher fraction of MX carbonitrides are observed in the CGHAZ. Fine-grained heat-affected zone (FGHAZ) consists of the finest grains (1.22 μm measured by EBSD, 5 μm PAG size), coarse undissolved M{sub 23}C{sub 6} carbides within the PAG boundaries and fine nucleated M{sub 23}C{sub 6} particles within the martensite laths. Inter-critical heat-affected zone (ICHAZ) consists of partially austenitized grains and over-tempered martensite laths. EBSD kernel average misorientation (KAM) map in the FGHAZ close to the ICHAZ illustrates the greatest local strain variations with a moderate normalized KAM value of 0.92°. The majority (88.1%) of the matrix grains in the CGHAZ are classified as deformed grains by EBSD grain average misorientation (GAM) evaluation. The FGHAZ close to the ICHAZ has the most recrystallized grains with an area fraction of 14.4%. The highest density variation of precipitates within grains in the FGHAZ originates from the inhomogeneous chemistry in the base metal. - Highlights: •A comprehensive characterization of the as-welded HAZ of P91 weldment is conducted. •Structural features in the each layer of the HAZ are quantified by EBSD. •Structural heterogenities in HAZ are due to welding cycle and base metal structure. •FGHAZ contains the finest grain structure and largest precipitate density variation.

36 MATERIALS SCIENCE↗

Characterization of microstructure and texture across dissimilar super duplex/austenitic stainless steel weldment joint by austenitic filler metal

The evolution of microstructure and texture across an as-welded dissimilar UNS S32750 super duplex/UNS S30403 austenitic stainless steel joint welded by UNS S30986 (AWS A5.9 ER309LMo) austenitic stainless steel filler metal using gas tungsten arc welding process was evaluated by optical micrography and EBSD techniques. Due to their fabrication through rolling process, both parent metals had texture components resulted from deformation and recrystallization. The weld metal showed the highest amount of residual strain and had large austenite grain colonies of similar orientations with little amounts of skeletal ferrite, both oriented preferentially in the < 001 > direction with cub-on-cube orientation relationship. While the super duplex stainless steel's heat affected zone contained higher ferrite than its parent metal, an excessive grain growth was observed at the austenitic stainless steel's counterpart. At both heat affected zones, austenite underwent some recrystallization and formed twin boundaries which led to an increase in the fraction of high angle boundaries as compared with the respective base metals. These regions showed the least amount of residual strain and highest amount of recrystallized austenite grains. Due to the static recrystallization, the fraction of low degree of fit (Σ) coincident site lattice boundaries, especially Σ3 boundaries, was increased in the austenitic stainless steel heat affected zone, while the formation of subgrains in the ferrite phase increased the content of < 5° low angle boundaries at that of the super duplex stainless steel. - Graphical abstract: Display Omitted - Highlights: • Extensive grain growth in the HAZ of austenitic stainless steel was observed. • Intensification of < 100 > orientated grains was observed adjacent to both fusion lines. • Annealing twins with Σ3 CSL boundaries were formed in the austenite of both HAZ. • Cub-on-cube OR was observed between austenite and ferrite in the weld metal. • Weld metal had the lowest texture intensity and ratio of low angle and CSL boundaries.

36 MATERIALS SCIENCE↗

Multi-Pass Hybrid Laser Arc Welding of Alloy 740H

The presentation reviews the progress made toward reducing the joining time of an advanced nickel-based alloy, Alloy 740H by a factor of two using a novel two step fusion welding approach. In the first step, a high powered laser is used to rapidly join thick weld groove lands (~10-12 mm thick) during a single pass. Hybrid laser arc welding (HLAW) is then used to fill the remaining weld groove and complete the joint. This sequential process also utilizes laser wobble in both steps to reduce welding defects and refine the weld microstructure to obtain improved properties compared to conventional gas tungsten or gas metal arc welds, GTAW and GMAW, respectively. The creep behavior of laser-only thick weld groove land welds and HLAW welds were found to be the same or slightly improved compared to conventional GMAW or GTAW welds in this alloy. Creep tests have been started to verify the long-term creep behavior (~10,000 hrs) of these welds. Modeling results on deep penetration laser welding are presented and the initial simulations of laser welding with laser wobble are shown. The next phase of the project will combine the two processes to make complete welds - deep penetration laser welds of thick weld groove lands followed by rapid filling of the remaining weld groove by HLAW - in thick plates (32 mm thick) Alloy 740H plate and entails development of narrow weld groove welding to further decrease the joining time of this alloy.

36 MATERIALS SCIENCE↗

Microstructure of a safe-end dissimilar metal weld joint (SA508-52-316L) prepared by narrow-gap GTAW

The microstructure, residual strain and interfacial chemical composition distribution of a safe-end dissimilar metal weld joint (DMWJ, SA508-52-316L) prepared by narrow-gap gas-tungsten arc welding (NG-GTAW) were studied by optical microscope (OM) and scanning electron microscope equipped with an energy dispersive X-ray microanalysis (SEM/EDX) and an electron back scattering diffraction (EBSD) system. Complex microstructure and chemical composition distribution are found, especially at the SA508-52 interface and the 52-316L interface. In brief, a complicated microstructure transition exists within the SA508 heat affected zone (HAZ); the residual strain, the fraction of high angle random grain boundaries and low angle boundaries decrease with increasing the distance from the fusion boundary in 316L HAZ; neither typical type II boundary nor obvious carbon-depleted zone is found near the SA508-52 interface; dramatic and complicated changes of the contents of the main elements, Fe, Cr and Ni, are observed at the distinct interfaces, especially at the SA508-52 interface. No carbon concentration is found at the SA508-52 interface. - Highlights: •Residual strain and GBCD change as a function of the distance from FB in 316L HAZ. •Neither type II boundary nor obvious carbon-depleted zone is found in SA508 HAZ. •No carbon concentration is found at the SA508-52 interface. •The middle part of the DMWJ has the highest residual strain.

36 MATERIALS SCIENCE↗

Welding Heat Input Influence on UNS S82441 Lean Duplex Stainless Steel Corrosion Resistance Assessed by Scanning Vibrating Electrode Technique (SVET)

The precipitation of the intermetallic phases can impair mechanical and corrosion properties. In the case of lean duplex stainless steels, they present solidification mode as primary ferrite, with austenite precipitation in the solid state, during cooling. This means the heat-affected zone balanced microstructure can be changed during the welding by the cooling rate, which is associated to the welding heat input, the thickness of the plate and the physical properties of the material. This work intends to present the influence of welding heat input on the corrosion resistance of UNS S82441 lean duplex stainless steel. The gas metal arc welding process was used to make the weld beads, using ER2209 as filler metal, which characterizes a dissimilar welded joint. The corrosion resistance of these specimens was analyzed through scanning vibrating electrode technique. It was observed that welding heat input variation distinctly influences corrosion in different zones of the weld beads over the specimen exposure time. The weld bead under intermediate welding heat input showed the highest corrosion rate and the one under the highest welding heat input, the lowest corrosion rate intensity.

36 MATERIALS SCIENCE↗