Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “Diffusion rate”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 127 records · Page 7

Sublimation and oxidation measurements of graphite and carbon black at high temperatures in a shock tube using absorption imaging and thermal emission

Surface mass loss rates due to sublimation and oxidation at temperatures of 3000–7000 K have been measured in a shock tube for graphite and carbon black (CB) particles. Diagnostics are presented for measuring surface mass loss rates by diffuse backlit illumination extinction imaging and thermal emission. Here, the surface mass loss rate is found by regression fitting extinction and emission signals with an independent spherical primary particle assumption. Measured graphite sublimation and oxidation rates are reported to be an order of magnitude greater than CB sublimation and oxidation rates. It is speculated that the difference between CB and graphite surface mass loss rates is largely due to the primary particle assumption of the presented technique which misrepresents the effective surface area of an aggregate particle where primary particles overlap and shield inner particles. Measured sublimation rates are compared to sublimation models in the literature, and it is seen graphite shows fair agreement with the models while CB underestimates, likely a result of the particle shielding affect not being considered in the sublimation model.

36 MATERIALS SCIENCE↗

Cobalt Carbonyl Clusters Enable Independent Control of Two Proton Transfer Rates in the Mechanism for Hydrogen Evolution

Abstract Metal carbonyl clusters (MCC's) are atomically defined nanomaterials which can be characterized using the precise tools of molecular (electro)chemistry. HER mechanisms involve two proton transfer (PT) steps in the catalytic cycle. For HER catalyzed by [Co 11 C 2 (CO) 23 ] 3− ( 1 3− ), cyclic voltammetry measurements were used to determine the rate for PT1 as k PT1 =3×10 8 M −1 s −1 , whereas the rate for PT2 is k PT2 =3.7×10 3 M −1 s −1 . The fast, diffusion‐limited rate for PT1 is consistent with a previous report describing [Co 13 C 2 (CO) 24 ] 4− ( 2 4− ), with PT=2.9×10 9 M −1 s −1 . In both cases rate enhancement in PT1 is promoted by the many Co−Co bonds on the surface of the MCC that serve as PT sites: a statistical enhancement of rate akin to the effects of proton relays. In contrast, k PT2 varies and is five orders of magnitude slower for 1 2− compared with 2 4− . Thus, MCC's and nanomaterials offer an opportunity to enhance the rate for PT1 while maintaining thermochemical or kinetic control of PT2.

Pattanayak, Santanu↗

Modeling the Contribution of Precipitation Loss to a Radiation Belt Electron Dropout Observed by Van Allen Probes

A drift-diffusion model is used to simulate the low-altitude electron distribution, accounting for azimuthal drift, pitch angle diffusion, and atmospheric backscattering effects during a rapid electron dropout event on 21st August 2013, at L = 4.5. Additional external loss effects are introduced during times when the low-altitude electron distribution cannot be reproduced by diffusion alone. Here, the model utilizes low-altitude electron count rate data from five POES/MetOp satellites to quantify pitch angle diffusion rates. Low-altitude data provides critical constraint on the model because it includes the drift loss cone region where the electron distribution in longitude is highly dependent on the balance between azimuthal drift and pitch angle diffusion. Furthermore, a newly derived angular response function for the detectors onboard POES/MetOp is employed to accurately incorporate the bounce loss cone measurements, which have been previously contaminated by electrons from outside the nominal field-of-view. While constrained by low-altitude data, the model also shows reasonable agreement with high-altitude data. Pitch angle diffusion rates during the event are quantified and are faster at lower energies. Precipitation is determined to account for all of the total loss observed for 450 keV electrons, 88% for 600 keV and 38% for 900 keV. Predictions made in the MeV range are deemed unreliable as the integral energy channels E3 and P6 fail to provide the necessary constraint at relativistic energies.

79 ASTRONOMY AND ASTROPHYSICS↗

Fast Proton Transfer and Hydrogen Evolution Reactivity Mediated by [Co 13 C 2 (CO) 24 ] 4–

A common approach to speeding up proton transfer (PT) by molecular catalysts is manipulation of the secondary coordina-tion sphere with proton relays and these enhance overall reaction rates by orders of magnitude. In contrast, heterogenous electrocatalysts have band structures that promote facile PT concerted with electron transfer (ET), known as the Volmer mechanism. Here in this paper, we show that [Co 13 C 2 (CO) 24 ] 4– , containing multiple Co-Co bonds to statistically enhance observed rates of PT, promotes PT on the order of 2.3 × 10 9 M -1 s -1 which suggests a diffusion-limited rate. The fast ET and PT chemistry is at-tributed to the delocalized electronic structure of [Co 13 C 2 (CO) 24 ] 4– . Electrochemical characterization of [Co 13 C 2 (CO) 24 ] 4– in the presence and absence of protons reveals ET kinetics and diffusion behavior similar to other small clusters such as nano-materials and fullerenes.

08 HYDROGEN↗

Triplet Excitons in Pentacene Are Intrinsically Difficult to Dissociate via Charge Transfer

Singlet fission (SF) has the potential to bypass the Shockley–Queisser limit for solar cell efficiency through the production of two electron–hole pairs per photon. However, in polycrystalline pentacene this goal is hindered by slow charge transfer from triplets (=10 7 s –1 ) after SF. In this paper we demonstrate that slow charge transfer is an intrinsic property of triplet states in this material and most likely not connected with the triplet pair states that may result from singlet fission. We compare two perylene diimide/pentacene charge transfer systems that differ only by triplet generation mechanism: SF versus intersystem crossing (ISC), sensitized by using a soluble lead phthalocyanine derivative. We use time-resolved microwave conductivity (TRMC) to measure the charge yield in each system and transient absorption (TA) to follow the triplet population dynamics. These experiments are described by a single global kinetic model, with most of its parameters fixed via control experiments. While we observe modest differences in the charge-transfer rate constants between each sample, 4–10× as a function of triplet generation mechanism, all samples remain far below the predicted diffusion-limited rate constant of 10 7 –10 8 s –1 .

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Collapse of Jahn-Teller phonons in La 1−x Sr x MnO 3 with weak magnetoresistance

Perovskite manganites are quantum materials exhibiting competing interactions inducing colossal magnetoresistance (CMR). The prevailing theory of CMR highlights the essential role of electron-phonon coupling (EPC), but mounting evidence suggests the underlying mechanism is more complicated. Here, we investigate phonons and spin-phonon coupling in ferromagnetic CMR manganites La 1−x Sr x MnO 3 (x=0.2,0.3) with relatively small CMR associated with melting of the magnetic order above room temperature. High-resolution neutron scattering experiments combined with density functional theory (DFT) show that the low-temperature ferromagnetic phase is conventional: neutron scattering from phonons agrees with DFT predictions and magnons follow sinusoidal dispersions. Fluctuating magnetic moments and low-energy phonons remain conventional in the high-temperature paramagnetic phase, indicating the Mn and La/Sr sublattices are not strongly perturbed by melting of ferromagnetism. In contrast, the Jahn–Teller-active optical oxygen vibrations collapse entirely above the Curie temperature, despite low CMR in these compositions, with some of the lost spectral weight reappearing as quasielastic scattering. We attribute this highly anomalous behavior to giant EPC in the charge and/or orbital channel. It drives cooperative diffusive motion of quasistatic carrier-trapping oxygen sublattice distortions once ferromagnetism disappears. We hypothesize the magnitude of magnetoresistance correlates with the rate of diffusion rather than with the strength of Jahn–Teller EPC.

36 MATERIALS SCIENCE↗

Solidification and grain formation in alloys: a 2D application of the grand-potential-based phase-field approach

Solidification is a significant step in the forming of crystalline structures during various manufacturing and material processing techniques. Solidification characteristics and the microstructures formed during the process dictate the properties and performance of the materials. Hence, understanding how the process conditions relate to various microstructure formations is paramount. In this work, a grand-potential-based multi-phase, multi-component, multi-order-parameter phase-field model is used to demonstrate the solidification of alloys in 2D. This model has several key advantages over other multi-phase models such as it decouples the bulk energy from the interfacial energy, removes the constraints for the phase concentration variable, and prevents spurious third-phase formation at the two phase interfaces. Here, the model is implemented in a finite-element-based phase-field modeling code. The role of various modeling parameters in governing the solidification rate and the shape of the solidified structure is evaluated. It is demonstrated that the process conditions such as temperature gradient, thermal diffusion, cooling rate, etc, influence the solidification characteristics by altering the level of undercooling. Furthermore, the capability of the model to capture directional solidification and polycrystalline structure formation exhibiting various grain shapes is illustrated. In both these cases, the process conditions have been related to the growth rate and associated shape of the dendritic structure. As a result, this work serves as a stepping stone towards resolving the larger problem of understanding the process–structure–property–performance correlation in solidified materials.

36 MATERIALS SCIENCE↗

Comparison of plug flow and multi-node stratified tank modeling approaches regarding computational efficiency and accuracy

Residential water heaters contain water stratified by temperature-driven density differences. This implies that a water tank can reach a state in which the top and bottom sections have different temperatures, unless mixing happens. A high degree of thermal stratification can improve the efficiency of some water heaters, by saving the amount of energy required for the heat-up process. Studies of stratification became popular in the 1970s and it remains an active research topic today. The research has led to the development of different models and techniques to better predict and define a stratified tanks behavior. By comparing these models and techniques used previously to describe thermal stratification, the phenomenon could be better understood, exploited, and used to increase efficiency and thermal energy capacity in modern water tanks. From the existing models, we found the one-dimensional standard plug-flow and a multi node model to be appropriate for analyzing the processes of the heat up and cool-down in a water tank. These two models are based on energy balances. This work involved comparing the accuracy and computational effort needed to implement these models. To assess accuracy, we compared both types of existing models to experimental data (also collected in this work) which included a heat up process using an external heat pump. This external process included a layering process that has an eddy diffusivity at five times the rate of thermal diffusion. For this project, we implemented the models in MATLAB, the multi-paradigm numerical computing environment. We quantified model accuracy using the root mean squared error between modeled data and experimental data for six measured tank temperatures. Comparing the accuracy and the computational time taken to run the simulation provides a method to contrast the performance of each model and a way to rate it. The multi node model was run using from 6 to 96 spatial nodes; the plug flow model was run using 1 to 0.001 º C temperature bin sizes. Additionally, timesteps were varied from 4 to 236 s. The results quantify the tradeoff between accuracy and computational time, providing guidance for simulations to intelligently select the best model type and simulation parameters. This research can be used to validate the pre-existing models and possibly improve the modern water tank.

Bulnes, Fernando Karg↗

Data-driven methods for diffusivity prediction in nuclear fuels

The growth rate of structural defects in nuclear fuels under irradiation is intrinsically related to the diffusion rates of the defects in the fuel lattice. The generation and growth of atomistic structural defects can significantly alter the performance characteristics of the fuel. This alteration of functionality must be accurately captured to qualify a nuclear fuel for use in reactors. Predicting the diffusion coefficients of defects and how they impact macroscale properties such as swelling, gas release, and creep is therefore of significant importance in both the design of new nuclear fuels and the assessment of current fuel types. In this article, we apply data-driven methods focusing on machine learning (ML) to determine various diffusion properties of two nuclear fuels—uranium oxide and uranium nitride. We show that using ML can increase, often significantly, the accuracy of predicting diffusivity in nuclear fuels in comparison to current analytical models. We also illustrate how ML can be used to quickly develop fuel models with parameter dependencies that are more complex and robust than what is currently available in the literature. In conclusion, these results suggest there is potential for ML to accelerate the design, qualification, and implementation of nuclear fuels.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Vacancy-Dependent Diffusion Mechanism in Oxygen-Defective SrFeO 3 Perovskite Materials: First-Principles Density Functional Theory and Experimental Approach

Understanding oxygen diffusion at the atomic scale in SrFeO 3−δ perovskites is crucial for developing oxygen storage materials with optimal performance. Such materials are required to have high stability, corrosion resistance, and acceptable oxygen storage capacity at moderate operating temperatures and pressures. Here, in this study, we used first-principles density functional theory and thermogravimetric analysis to study the vacancy-dependent oxygen diffusion in oxygen-deficient SrFeO 3−δ (δ = 0, 0.065, 0.125, 0.25, 0.5) perovskites. The electronic structures, including the partial- and spin-resolved density of states, for different SrFeO 3−δ phases were calculated and compared with available experimental and theoretical results. By mapping the migration pathways, we investigated diffusion mechanisms and calculated the energy barriers for oxygen diffusion in cubic, orthorhombic, and brownmillerite phases of SrFeO 3−δ perovskites. Using the calculated energy barriers, we deduced the diffusion time scales and diffusion coefficients within SrFeO 3−δ . A diffusion coefficient on the order of 10 –8 m 2 /s was obtained for SrFeO 2.875 . We experimentally investigated the roles of temperature and oxygen partial pressures on the redox kinetics and deduced the kinetics rate and diffusion density, which agreed well with the calculated values for the density of diffusing oxygen vacancy in the lattice. Our results showed that the energy barrier tends to reduce at higher oxygen concentrations. Our results serve as an important guideline for designing oxygen storage materials with optimal redox kinetics.

chemical looping with oxygen uncoupling (CLOU)↗

Diffusion-limited hydrolysis in polymeric materials

Polymer degradation under aggressive environmental stressors often develops heterogeneities due to diffusion-limited reaction phenomena. This is well established for diffusion-limited oxidation (DLO), which is known to occur for most polymeric materials at elevated temperatures but has been less summarized for the conditions of diffusion-limited hydrolysis (DLH). Here, an overview of hydrolysis for several materials and a computational model, analogous to the underlying equations for DLO, able to define this diffusion-reaction system is presented. A systematic study of the influence of various parameters, such as water diffusivity, reaction rate and order, and a more in-depth focus on residual isocyanate hydrolysis in a polymeric methylene diphenyl diisocyanate (pMDI) based polyurethane (PU) foam is given. For this system, we present experimental data for model ‘input’ parameters and discuss predictions for different conditions. We conceptually compare the behavior of diffusion-limited oxidation to that of diffusion-limited hydrolysis (DLH). With the mathematical framework and key material properties presented herein, any DLH phenomena following Fickian diffusion behavior can be understood, modeled, and predicted.

36 MATERIALS SCIENCE↗

Modeling of non-equilibrium partitioning in direct metal deposited copper–iron concentrated alloys

The direct metal deposition (DMD) additive manufacturing process produces high cooling rates within a small melt pool and can lead to high amounts of solute trapping. These high cooling rates limit diffusion and lead to the formation of non-equilibrium phases. In this work, we utilize a numerical model to calculate the degree of solute trapping, defined as non-equilibrium partitioning. A theoretical case with overall composition fixed to 50Cu-50Fe at.%. was performed to observe the influence of increasing solidification rates. We then simulate DMD of equimolar Cu-Fe powder printed on mild steel substrate and the calculated non-equilibrium phase compositions were consistent with experimental observations reported earlier on this alloy composition. For a single deposited track, cooling rates are high enough to yield significant solute trapping. Here, the degree of solute trapping is highest near the free surface and has a gradient that correlates with the cooling rate gradient.

36 MATERIALS SCIENCE↗

Moisture ingress in commercial steel drums: Water content determination, diffusion modelling and predicted permeation rates

Commercial steel drums underpin the global economy, playing a pivotal role in the storage and transportation of critical materials. Transported and stored materials, such as food, chemical and nuclear waste, can be sensitive to ambient conditions, particularly moisture that can enhance negative effects such as corrosion and material degradation. Although international standards and regulations are in place for the qualification of steel drums, there are no current testing requirements, established limits or boundaries for the permeation of moisture into the drums during transportation or storage. This work aims to provide insights into the moisture ingress over time into properly sealed steel drums and provides estimated moisture ingress rates over time through extrapolation. Water vapour transmission rate (WVTR) measurements through the gasket material at 10–40°C were 0.11–2.1 g/m 2 /day resulting in a permeation activation energy of 30.2 kJ/mol. Water sorption measurements and Karl Fischer titration (KFT) on ethylene propylene diene monomer (EPDM) gasket material revealed a decrease in equilibrium moisture saturation with increasing temperature. KFT measurements also revealed the presence of moisture within the adhesive and drum wall after exposure to ambient conditions. KFT and Fourier transform infrared spectroscopy (FTIR) show that moisture will desorb from the EPDM and drum wall after exposure to desiccating conditions, although a minimal amount of moisture will remain present. When sealed to the manufacturer's recommendations, the steel drums are effective in minimizing moisture ingress. In conclusion, in sealed empty drums, moisture ingress rates for 19-L drums were 0.4–1.5 mg/day at 25°C 15% relative humidity (RH) and increased to 7.1–8.8 mg/day at 40°C 90% RH, and moisture ingress rates for 210-L drums were 2.5 and 3.5 mg/day at field deployment conditions of 15.5°C 51.5% RH and 23°C 40% RH, respectively.

42 ENGINEERING↗

Optimized utilization of COMB3 reactive potentials in LAMMPS

An investigation to optimize the application of the third-generation charge optimized many-body (COMB3) interatomic potential and associated input parameters was carried out through the study of solid–liquid interactions in classical molecular dynamics simulations. The rates of these molecular interactions are understood through the wetting rates of water nano-droplets on a bare copper (111) surface. Implementing the Langevin thermostat, the influence of simulation time step, the number of atoms in the system, the frequency at which charge equilibration is performed, and the temperature relaxation rate are all examined. The results indicate that time steps of 0.4 fs are possible when using longer relaxation times for the system temperature, which is almost double the typical time step used for reactive potentials. Additionally, the use of the charge equilibration allows for a fewer atomic layers to be used in the Cu slab. In addition, charge equilibrium schemes do not need to be performed every time step to ensure accurate charge transfer. Interestingly, the rate of wetting for the nanodroplets is dominantly dependent on the temperature relaxation time, which is predicted to significantly change the viscosity of the water droplets. This work provides a pathway for optimizing simulations using the COMB3 reactive interatomic potential.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Advanced Electrochemical Separations of Actinide/Fission Products via the Control of Nucleation and Growth of Electrodeposits. Final Report

This is the final report to the NEUP regarding the “Advanced Electrochemical Separations of Actinide/Fission products via the Control of Nucleation and Growth of Electrodeposits” project. This report describes the project activities conducted during the period October 01, 2016 through September 30, 2019. The report includes a brief statement of the project objectives and approach, followed by the details of the performed research activities and suggestion for the future work. It is well known that according to current knowledge the pyroprocessing of spent nuclear fuels invariably leads to the dendritic form of electrodeposits, which from technological point of view is undesirable for many reasons. The aim of this research was to study and preclude the formation of electrodeposits with dendritic morphology (of essential importance to FC-1 Program). This project is characterized with four novel study categories: (1) exploring electrodeposit morphology control by controlling the electrochemical deposition reaction rate, (2) the use of rotating disk electrode technique to distinguish the electrodeposition control modes (reaction rate vs. diffusion), (3) morphology studies of lanthanides (La) and actinides (U) in characteristic stages of nucleation and growth, (4) exploring the need for separation of electrochemical cell in compartments for cathodic and anodic reactions. All these study categories were applied on two distinct electrolyte systems (a) high temperature ionic liquids, i.e. molten LiCl-KCl salts, and (b) room temperature ionic liquids (compounds exclusively made of organic cations, and organic/inorganic anions). Because the quality (dense and smooth) of electrodeposits is a direct function of the electrochemical reduction rate (slower the better), the major expectation was that addition of organic molecules would provide the desired slowing down of electroreduction effect, avoiding the undesired dependence on mass transfer. What was learned is summarized in seven key areas.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

3D pattern formation of a protein–membrane suspension

Many essential cellular processes, including cell division and the establishment of cell polarity during embryogenesis, are regulated by pattern-forming proteins. These proteins often need to bind to a substrate, such as the cell membrane, onto which they interact and form two-dimensional (2D) patterns. It is unclear how the membrane’s continuity and dimensionality impact pattern formation. Here, we address this gap using the MinDE system, a prototypical example of pattern-forming membrane proteins. We show that when the lipid substrate is fragmented into submicrometer-sized diffusive liposomes, adenosine triphosphate-driven protein–protein interactions generate three-dimensional (3D) spatially extended patterns, despite the complete loss of membrane continuity. Remarkably, these 3D patterns emerge at scales four orders of magnitude larger than the individual liposomes. By systematically varying protein concentration, liposome size, and density, we observed and characterized a variety of 3D dynamical patterns not seen on continuous 2D membranes, including traveling waves, dynamical spirals, and a coexistence phase. Simulations and linear stability analysis of a coarse-grained model revealed that the physical properties of the dispersed membrane effectively rescale both the protein–membrane binding rates and diffusion, two key parameters governing pattern formation and wavelength selection. These findings highlight the robustness of Min’s pattern-forming ability, suggesting that protein–membrane suspensions could serve as an adaptable template for studying out-of-equilibrium self-organization in 3D, beyond in vivo contexts.

36 MATERIALS SCIENCE↗

Q2 Report for FY25 Theory and Simulation Performance Target: Development of an integrated modeling framework for fusion reactor design and assessment

This report describes the work and activities carried out towards the completion of each of the following milestones in FY25 Q2: 1. Demonstrate workflow for generating self-consistent CESOL plasma profiles + first wall and divertor loading prediction and generate the CAT plasma and neutron loading needed for further engineering analysis: $\circ$ Run CESOL with BOUT++/Hermes-3 and immersed boundary condition to directly map to wall: • Run BOUT++/Hermes-3 through the IPS workflow to find radial particle and energy diffusivities to match either the Eich or the physics-based scaling of the SOL heat flux width, and • Expand source of first wall heat flux to include charged particles, neutrals, and radiation from the core+edge. 2. Generate medium fidelity parametrized CAD: $\circ$ Develop the TRACER tool to read an existing CAD, regenerate the geometry based on vertex location and connectivity information, define vertex translation and parameters needed for scaling the CAD, and $\circ$ Utilize the FreeGS code to determine CAT PF coil placement, including minimizing the number of coils, coil current, and electromechanical stresses. 3. Utilize plasma loading for engineering analysis: $\circ$ Couple the plasma loading to input for OpenFOAM and demonstrate initial test of thermal analysis of CAT first wall loading with typical DCLL blanket component cooling boundary conditions. 4. Demonstrate nuclear analysis: $\circ$ Apply initial analysis of tritium transport in DCLL blanket by evaluating spatially resolved tritium generation rates, tritium diffusion and convection.

70 PLASMA PHYSICS AND FUSION TECHNOLOGY↗

Temperature-Dependent Morphological Evolution during Corrosion of the Ni-20Cr Alloy in Molten Salt Revealed by Multiscale Imaging

Understanding the mechanisms leading to the degradation of alloys in molten salts at elevated temperatures is significant for developing several key energy generation and storage technologies, including concentrated solar and next-generation nuclear power plants. Specifically, the fundamental mechanisms of different types of corrosion leading to various morphological evolution characteristics for changing reaction conditions between the molten salt and alloy remain unclear. Here, in this work, the three-dimensional (3D) morphological evolution of Ni–20Cr in KCl–MgCl 2 is studied at 600 °C by combining in situ synchrotron X-ray and electron microscopy techniques. By further comparing different morphology evolution characteristics in the temperature range of 500–800 °C, the relative rates between diffusion and reaction at the salt–metal interface lead to different morphological evolution pathways, including intergranular corrosion and percolation dealloying. In this work, the temperature-dependent mechanisms of the interactions between metals and molten salts are discussed, providing insights for predicting molten salt corrosion in real-world applications.

36 MATERIALS SCIENCE↗