Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “Cathode electrolyte interface”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 127 records · Page 7

Stabilizing and understanding the interface between nickel-rich cathode and PEO-based electrolyte by lithium niobium oxide coating for high-performance all-solid-state batteries

The pursuit of high energy density and safe lithium ion batteries (LIBs) is the urgent goal for the development of next-generation electric vehicles (EVs). All-solid-state batteries (ASSBs) with the combination of poly(ethylene oxide) (PEO)-based solid polymer electrolyte (SPE) and Ni-rich lithium nickel manganese cobalt oxide LiNi0.8Mn0.1Co0.1O2 (NMC811) cathode are promising candidates for EVs due to their improved energy density and safety. However, the low electrochemical oxidation window of PEO-based SPE and the instability of NMC811 at the charge/discharge process seriously restrict the battery performance. Herein, a high voltage stable solid-state electrolyte layer lithium niobium oxide (LNO) is coated on the NMC811 electrode surface by atomic layer deposition for stabilizing NMC811-PEO solid polymer batteries. Electrochemical tests show that LNO coating can stabilize the NMC811 active materials and mitigate the decomposition of SPE upon the cycling process, rendering a good performance of NMC811-PEO solid polymer battery. Mechanism studies by SEM, STEM, XAS, and XPS disclose that the uncoated NMC811 suffers from chemomechanical degradations along with oxygen release triggering the decomposition of SPE, which results in unstable cathodic electrolyte interphase. With LNO coating, chemomechanical degradations and oxygen release are inhibited and the decomposition of SPE is mitigated. This paper renders a stable and high-performance high-energy-density SSB for high voltage application, which paves the way toward next-generation solid-state LIBs.

25 ENERGY STORAGE↗

All‐Solid‐State Batteries With Mechanically Stable Interfaces Consisting of a Zero‐Strain Cation‐Disordered Rocksalt Cathode

Interface stabilization is critical to the development of working all‐solid‐state batteries. Rigid cathode/solid electrolyte interfaces often disintegrate due to anisotropic volume change of cathode‐active materials, resulting in irreversible capacity loss. Herein, we demonstrate that Li 1.211 Mo 0.467 Cr 0.3 O 2 (LMCO), a pioneering cation‐disordered rocksalt oxide (DRX) cathode that has intrinsically small volume change upon lithium intercalation, can be integrated with a thiophosphate‐based solid electrolyte for all‐solid‐state batteries. Interface stability of the all‐solid LMCO cell was investigated by electrochemical impedance spectroscopy, X‐ray micro‐computed tomography, and electron microscopy. Since LMCO was initially synthesized as a layered phase exhibiting a large volume change, interface disintegration can be observable in the early cycles. As layered LMCO phase‐transformed into DRX LMCO in subsequent cycles, reintegration of the interfaces occurs within a pressurized cell as a result of its zero‐stain behavior. Consequently, the DRX LMCO cathode maintains interface integrity, and thus electrical wiring, over an extended number of cycles, leading to improved capacity retention with small internal cell resistance.

DRX↗

Probing degradation at solid-state battery interfaces using machine-learning interatomic potential

Solid-state batteries featuring fast ion-conducting solid electrolytes are promising next-generation energy storage technologies, yet challenges remain for practical deployment due to electro-chemo-mechanical instabilities at solid-solid interfaces. These interfaces, which include homogeneous/internal interfaces such as grain boundaries (GBs) and heterogeneous/external interfaces between solid-electrolyte and electrode materials, can impede Li-ion transport, deteriorate performance, and eventually lead to cell failure. Here, in this study, we leverage large-scale molecular simulations, enabled by validated machine-learning interatomic potentials, to directly probe the onset of interfacial degradation at the garnet Li 7 La 3 Zr 2 O 12 (LLZO) solid-electrolyte/LiCoO 2 (LCO) cathode interface. By surveying different interfacial geometries and compositions, it is found that Li-deficient interfaces can lead to severe interfacial disordering with cation mixing and Co interdiffusion from LCO into LLZO. By contrast, Li-sufficient interfaces are less disordered, although elemental segregation with local ordering is observed. As a consequence of Co interdiffusion, Co-rich regions are formed at the GBs of LLZO due to cation segregation and trapping effects. This behavior is independent of the GB tilting axis, degree of disorder at the GBs, and Co concentration, which implies Co clustering at GBs is a general phenomenon in polycrystalline LLZO and can dictate its overall transport and mechanical properties. Our findings elucidate the underlying fundamental mechanisms that give rise to experimentally observed physicochemical properties and provide guidelines for interface design that can mitigate interfacial degradation and improve cycling performance.

25 ENERGY STORAGE↗

In-situ Multimodal Imaging and Spectroscopy of Mg Electrodeposition at Electrode-Electrolyte Interfaces

We report the study of Mg cathodic electrochemical deposition on Ti and Au electrode using a multimodal approach by examining the sample area in-situ using liquid cell transmission electron microscopy (TEM), scanning transmission X-ray microscopy (STXM) and X-ray absorption spectroscopy (XAS). Magnesium Aluminum Chloride Complex was synthesized and utilized as electrolyte, where non-reversible features during in situ charging-discharging cycles were observed. During charging, a uniform Mg film was deposited on the electrode, which is consistent with the intrinsic non-dendritic nature of Mg deposition in Mg ion batteries. The Mg thin film was not dissolvable during the following discharge process. We found that such Mg thin film is hexacoordinated Mg compounds by in-situ STXM and XAS. This study provides insights on the non-reversibility issue and failure mechanism of Mg ion batteries. Also, our method provides a novel generic method to understand the in situ battery chemistry without any further sample processing, which can preserve the original nature of battery materials or electrodeposited materials. This multimodal in situ imaging and spectroscopy provides many opportunities to attack complex problems that span orders of magnitude in length and time scale, which can be applied to a broad range of the energy storage systems.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Electrochemical-driven green recovery of lithium, graphite and cathode from lithium-ion batteries using water

The expected exponential increase in consumption of lithium-ion batteries (LIBs) would pose a unique challenge to the availability of near-critical resources like lithium and graphite in the upcoming decade. In this work, we present a lithium recovery process that utilizes a degradation mechanism, i.e., lithium plating, as a tool to concentrate metallic lithium at the anode/separator interface for convenient extraction at room temperature – using only water. Electrochemical characterization of fast charged (1–6 C) LIBs yielded a maximum capacity fade of 50% over ten cycles. The lithium plating was confirmed via voltage plateau analysis, coulombic efficiency, and DC resistance measurements. A maximum lithium plating condition was observed to exist between 4C and 5C, thereby limiting the energy consumption in the extraction process. Post-mortem film thickness measurement showed an incrementing film deposition with a maximum of 35 µm thickness. SEM and XPS analysis confirmed increasing concentration of a dense dendritic metallic lithium deposition on the anode/separator interface with C-rate. A green recovery process was adopted to extract the concentrated metallic lithium using distilled water. The lithium from the plated film, solid/electrolyte interface (SEI), electrolyte, anode, and cathode, was extracted as salts. A 37% improvement in lithium recoverability was achieved with fast charging under ambient conditions. XPS analysis showed ~92% of lithium yield with no residual lithium in the graphite. In addition, the battery-grade graphite was recovered with 97% purity after heat treatment of the washed anode film, and concentrated transition metals oxides in the cathode to 93% purity for convenient extraction.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Towards a high-performance garnet-based solid-state Li metal battery: A perspective on recent advances

Garnet-based solid-state Li metal batteries have been widely considered one of the most promising next-generation energy storage systems. However, the performance of these batteries is plagued by various limitations caused by the solid-state electrolyte (SSE). The poor wetting of lithium on the garnet surface diminishes the contact between the anode and electrolyte, leading to extremely high anode interfacial resistance. Similarly, the point-to-point contact between the cathode and electrolyte leads to high impedance on the cathode side. Moreover, although the SSE serves a firm barrier separating the anode and cathode, lithium dendrites can still grow through, causing a short circuit. Lastly, the solid/solid interface cannot be well maintained under cycling at high current density and capacity. Recently, remarkable progress has been achieved in garnet electrolyte to resolve these problems towards the aim of a high-performance solid-state Li metal battery. In this perspective, we highlight various recent advances in the field of garnet-based solid-state battery, including improving the anode/electrolyte interface, lithium dendrite detection, reducing cathode impedance, and electrolyte architecture design.

25 ENERGY STORAGE↗

Cathode Interface Compatibility of Amorphous LiMn 2 O 4 (LMO) and Li 7 La 3 Zr 2 O 12 (LLZO) Characterized with Thin-Film Solid-State Electrochemical Cells

Solid-state lithium-ion batteries are a hopeful successor to traditional Li-ion cells that use liquid electrolytes. While a growing body of work has characterized the interfaces between various solid electrolytes and the lithium metal, interfaces with common cathode intercalation compounds are comparatively less understood. In this contribution, the influence of polarization and temperature on interfacial stability between LiMn 2 O 4 (LMO) and Li 7 La 3 Zr 2 O 12 (LLZO) are investigated. Sputtered thin-film LMO electrodes are utilized to permit high-capacity cycling while retaining a large ratio of interfacial area to electrode bulk. Electrochemical impedance spectroscopy (EIS) is compared across a set of full (LMO|LLZO|Li) and symmetric (LMO|LLZO|LMO, Li|LLZO|Li, and Au|LLZO|Au) cells to delineate impedance features that are specific to the evolution of the cathode interface. Furthermore, additional X-ray photoelectron spectroscopy (XPS) provides evidence of a limited interfacial reaction between LMO and LLZO that coincides with an increase in the impedance of the LMO–LLZO interface.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

High Energy Aqueous Lithium-Ion Batteries (Final Report)

Lithium-ion batteries (LIBs) are a widely used energy storage device. For decades, researchers have been studying aqueous electrolytes due to their non-flammability and environmental friendless. However, the hydrogen evolution reaction (HER) and oxygen evolution reaction (OER) of water greatly limit the voltage window of the aqueous electrolyte. The recent concept of ‘solvent-in-salt’ electrolytes, namely ‘water-in-salt’ electrolytes (WISE) for aqueous batteries and ‘super-concentrated’ electrolytes for non-aqueous batteries, greatly expands the electrochemical window of these battery systems and consequently their energy density. This expansion occurs because the large number of salt aggregates in ‘solvent-in-salt’ electrolytes enables preferential salt decomposition over solvent decomposition to form robust interphase layers on electrodes, thus enhancing their stability in a wide range of operating voltages. However, even when the salt concentration reached 63m, regardless of cost, the cathodic potential of the WISE expanded only to 1.75V with an overall electrochemical stability window of <3.25V. To design the next generation of high energy aqueous LIBs, electrolytes that possess a wider electrochemical stability window and lower cost but still maintain the merit of non-flammability are much needed. In this project, we designed the aqueous LIBs with widened voltage window. We reported a cheap and non-flammable ternary eutectic electrolyte that can form a robust solid electrolyte interface (SEI)so that the cathodic limiting potential can be decreased to <1.5 V for Li 4 Ti 5 O 12 anodes, while maintaining both a high ionic conductivity of >10 -3 S cm –1 and a low viscosity. We demonstrated the super-stable2.5V LiMn 2 O 4 ||Li 4 Ti 5 O 12 pouch cell with mass loading of 2.5 mAh/cm. Further, LiCl-LiBr-Graphite/Li full cells were designed with high energy density. Finally, we use a bi-layer design to enlarge the voltage window of aqueous electrolyte, which can endow the stable cycling of aqueous Lithium metal batteries.

25 ENERGY STORAGE↗

Accurately constituting robust interfaces for high-performance high-energy lithium metal batteries

High-energy lithium metal batteries (LMBs) have received ever-increasing interest. Among them, coupling lithium metal (Li) with nickel-rich material, LiNi x Mn y Co z O 2 (NMCs, x ≥ 0.6, x + y + z = 1), is promising because Li anodes enable an extremely high capacity (∼3860 mA h g −1 ) and the lowest redox potential (−3.04 V vs. standard hydrogen electrode), while NMCs can achieve a much higher capacity of ∼200 mA h g −1 and lower cost than those of LiCoO 2 . However, the resultant Li‖NMC cells have been hindered from commercialization due to a series of challenges related to the interface stability of both Li anodes and NMC cathodes. Specifically, Li anodes suffer from Li dendritic growth and the formation of solid electrolyte interphase (SEI), while NMC cathodes suffer from the formation of cathode electrolyte interphase (CEI) and other interface-related issues, including transition metal dissolution, oxygen release, cracking, and so on. To tackle these issues, recently, two sister techniques, atomic and molecular layer deposition (ALD and MLD), have emerged and exhibit tremendous capabilities to accurately constitute robust interfaces to achieve high-performance Li‖NMC LMBs. They can uniquely develop uniform and conformal films as surface coatings of LMBs in a precisely controllable mode at the atomic/molecular level, while proceeding with film deposition at low temperatures (e.g., ≤250 °C). In this Feature Article, we review the latest research progress in developing novel surface coatings via ALD and MLD for Li‖NMC LMBs and discuss outcomes for pursuing high performance.

25 ENERGY STORAGE↗

Low temperature sulfur and sodium metal battery for grid-scale energy storage application

A re-chargeable battery comprising a non-dendrite forming sodium (Na)/potassium (K) liquid metal alloy anode, a sulfur and polyacrylonitrile (PAN) conductive polymer composite cathode, a polyethyleneoxide (PEO) solid electrolyte, a solid electrolyte interface (SEI) formed on the PEO solid electrolyte; and a cell housing, wherein the anode, cathode, and electrolyte are assembled into the cell housing with the PEO solid electrolyte disposed between the cathode and anode.

Liu, Gao↗

Molecular Beam Epitaxy (MBE) Growth of Model Cathodes to Study Interfacial Ion Diffusion

Lithium-ion batteries (LIBs) have been the focus of research for decades owing to their superior energy storage potential and wide range of applications. However, long-term stability issues still persist in LIB cathodes as the result of the formation of a solid electrolyte interface (SEI), structural transformations, or the loss of active cathode materials. In nanoscale cathodes, it is often impossible to isolate, let alone mitigate the causes of the observed capacity loss. Herein, a novel approach is presented to synthesizing LIB cathode model systems using thin-film molecular beam epitaxy (MBE). Specifically, 100 nm thick LiMn 2 O 4 (LMO) thin-film cathodes are grown on SrRuO 3 /SrTiO 3 (100) single-crystal substrates and characterized in their pristine and cycled states. The pristine thin films exhibit the electro-chemical cycling behavior and structural evolution previously seen in bulk LMO cathodes. The formation of surface-layer rocksalt MnO and spinel Mn 3 O 4 along with the mass-loss associated with the corrosion of active Mn ions is also reported. It is, therefore, demonstrated that these MBE-grown model systems can be used for detailed studies of their surface structures and the electrode/electrolyte interfacial evolution in LIB cathodes, leading to the development of materials for rechargeable batteries with higher capacity and better stability.

25 ENERGY STORAGE↗

A Bilayer Electrolyte Design to Enable High-Areal-Capacity Composite Cathodes in Polymer Electrolytes Based Solid-State Lithium Metal Batteries

High-areal-capacity cathodes are needed for energy-dense solid-state batteries. Here, we demonstrate a bilayer polymer electrolyte design for cycling 3–6 mAh/cm 2 NMC811 composite cathodes. In this work, the bilayer electrolyte comprises a cross-linked poly(ethylene oxide) (PEO)-based electrolyte layer and a linear-PEO-based electrolyte layer. The former provides dendritic resistance, and the latter provides a seamless interface with the cathode during cycling. Using a single layer of either membrane led to severe shorting or extremely low Coulombic efficiency (CE) in the first cycle. The general concept of a rigid dendrites-inhibiting electrolyte facing Li anode and a softer, cathode-integrated electrolyte that ensures contact with the cathodes during cycling may present a pattern for enabling high-energy-density cathodes.

25 ENERGY STORAGE↗

Understanding Platinum Ionomer Interface Properties of Polymer Electrolyte Fuel Cells

A well-designed cathode catalyst layer with optimal ionomer distribution is critical to minimizing amount of Platinum (Pt) content in polymer electrolyte fuel cells (PEFCs). The impact of Pt loading, ionomer content and carbon support types on the catalyst/ionomer interface were also investigated at dry and wet conditions. Higher Pt loadings resulted in higher double layer capacity (C dl ) and similar electrochemical surface area (ECSA) due to well dispersed ionic phase material. Higher ionomer content resulted in higher ionic conductivity but also showed similar SO 3 − group coverage. High surface area (HSA) carbon support had larger ECSA and C dl at both dry and wet conditions, as less agglomerated Pt was well dispersed in the meso-pores of the support. Lower SO 3 − group coverages were observed for HSA carbon than for Vulcan carbon due to Pt particles being buried within the porous HSA carbon support. The effect of cell conditioning and voltage recovery on the PEFC cathode catalyst layer was shown to have minimal impact on SO 3 − group coverage despite a decrease in C dl and ECSA due to the size increase of Pt particles. At dry condition, a significant increases in SO 3 − group coverage were observed for all MEAs due to higher adsorptivity of ionomer in dry conditions.

25 ENERGY STORAGE↗

Atomic- and Molecular-Scale Interphase Engineering for High-Performance Solid-State Batteries

Solid-state batteries (SSBs) promise a decisive advance beyond conventional Li-ion systems, yet their development remains constrained by persistent solid–solid interfacial instabilities that degrade performance and durability. Interfaces between solid electrolytes and both cathodes and Li metal often exhibit poor wettability, limited physical contact, and high charge–transfer resistance, leading to chemical decomposition, mechanical failure, and impedance growth. Overcoming these limitations requires interphase engineering with atomic-scale precision—capabilities that conventional coating methods cannot reliably deliver. Atomic layer deposition (ALD) and molecular layer deposition (MLD) uniquely meet this need by enabling ultrathin, conformal, and composition-tunable films that stabilize reactive surfaces, suppress parasitic reactions, and regulate Li-metal morphology. Importantly, this Perspective highlights ALD/MLD systems that have already demonstrated effectiveness in liquid-electrolyte cells and discusses how these validated strategies can be deliberately translated to solid-state architectures. By grounding future directions in experimentally proven concepts rather than speculative hypotheses, we outline how atomic- and molecular-scale design principles can accelerate the development of robust, high-performance SSB technologies.

atomic and molecular layer deposition↗

Hydrogen bonds enhanced composite polymer electrolyte for high-voltage cathode of solid-state lithium battery

Polymer electrolyte is one of the important components for developing advanced solid-state lithium batteries (SSLBs). However, the narrow electrochemical stability window restricts the practical application with high-voltage cathodes. In this study, a series of composite solid electrolytes (CSEs), possessing both wide electrochemical stability window (up to 5.0 V vs. Li + /Li) and high ionic conductivity (over 1.35×10 -3 S/cm at 25 °C), were reported by integrating SiO 2 nanoparticles into poly(vinyl ethylene carbonate) polymer electrolyte. The enhanced anti-oxidation performances are mainly caused and confirmed by the local intermolecular interactions of hydrogen bonds in CSE. Based on this CSE, the SSLBs with LiCoO 2 cathode present good cycle stability at high voltage, and the capacity retention with 4.5 V cut-off voltage is about 94% after 200 cycles. This work not only proves the importance of intermolecular interactions in CSE, but also provides an effective method for achieving high-energy SSLBs with enhanced interface compatibility between polymer electrolyte and highvoltage cathodes

25 ENERGY STORAGE↗

Stabilizing electrode–electrolyte interfaces to realize high-voltage Li||LiCoO 2 batteries by a sulfonamide-based electrolyte

High-voltage lithium-metal batteries (LMBs) with LiCoO 2 (LCO) as the cathode have high volumetric and gravimetric energy densities. However, it remains a challenge for stable cycling of LCO >4.5 V Li . Here we demonstrate that a rationally designed sulfonamide-based electrolyte can greatly improve the cycling stability at high voltages up to 4.7 V Li by stabilizing the electrode–electrolyte interfaces (EEIs) on both the Li-metal anode (LMA) and high-voltage LCO cathode. With the sulfonamide-based electrolyte, commercial LCO cathodes retain 89% and 85% of their capacities after 200 and 100 cycles under high charging voltages of 4.55 V Li and 4.6 V Li , respectively, significantly outperforming traditional carbonate-based electrolytes. The surface degradation, impedance growth, and detrimental side reactions in terms of gas evolution and Co dissolution are well suppressed. Our work demonstrates a promising strategy for designing new electrolytes to realize high-energy Li||LCO batteries.

25 ENERGY STORAGE↗

Investigation of electrode-electrolyte interfaces to enable non-flammable Li-ion batteries operating up to 125°C with liquid electrolyte

Non-flammable and high-temperature stable ionic liquid (IL)-based electrolytes could eliminate catastrophic battery failures and improve battery safety, but their poor electrochemical interaction with the LiNi x Mn y Co z O 2 (NMC) family of cathodes is a long-standing problem due to severe parasitic reactions at high temperature. Understanding surface and bulk structural mechanisms of NMC-type cathodes at elevated operational temperature is of paramount importance to facilitate stable electrochemical performance. Here, we report a non-flammable phosphonium IL-based cell chemistry that offers stable electrode-electrolyte interfaces, leading to electrochemical performance up to 125°C and high-temperature safety. We combine electrochemistry with multimodal X-ray spectroscopy methods to understand interfaces at elevated temperature (100°C). This nanoscale understating enables a proof-of-concept high-temperature cylindrical cell (14500), and the design achieves an average Coulombic efficiency of ≈99.5% up to 300 cycles at 100°C. The results ascertain the significance of depth-dependent degradation at the interface, guiding room-temperature Li-ion technology toward extreme-temperature applications.

36 MATERIALS SCIENCE↗

Cross-scale modeling and experimental integration for advancing cathode electrolyte interphase studies in high energy density lithium-ion batteries

Electrochemical interfaces are critical to the performance and durability of lithium-ion batteries (LIBs). The solid electrode-electrolyte interphase (SEI and CEI) structures that form during cycling can passivate reactive surfaces, ensuring safe operation, but also may contribute to performance degradation. Understanding the microscopic factors influencing interphase formation, growth, and evolution is essential for balanced battery design. While significant research has focused on the anode-electrolyte interphase (SEI), the cathode-electrolyte interphase (CEI) remains less explored, despite its importance in high-voltage and advanced battery technologies. Challenges in conducting in-situ or operando experiments arise from the occluded nature of these interfaces and the long timescales involved, often leading to biased interpretations. A validated multi-scale, multi-physics modeling approach, integrated with advanced characterization techniques, can effectively elucidate the intrinsic stability of electrolyte and cathode surfaces, the impact of chemical heterogeneity, and the role of microstructural features on CEI performance. In conclusion, this article reviews current modeling and simulation strategies for studying CEI in advanced LIBs and highlights opportunities for future methodological advancements and experimental integration.

Cathode-electrolyte interphase↗