Structure and Magnetic Properties of Graded (001)-Oriented FePt Films Prepared by Magnetron Sputtering and Rapid Thermal Annealing

L1{sub 0}-FePt/[Fe/Pt]{sub 27} multilayer films were prepared on (100)-oriented single-crystal MgO substrates. Structural analysis indicates epitaxial growth of the L1{sub 0}-FePt films during high-temperature deposition. The room-temperature-deposited [Fe/Pt]{sub 27} multilayer exhibits the fcc-FePt structure grown epitaxially on the L1{sub 0}-FePt base layer. The degree of chemical order and thereby the anisotropy of the top layer has been controlled by varying the temperature of a post-deposition annealing process. Compared with the as-deposited films, coercivities of the films annealed below 400 {sup ∘}C are substantially decreased by introducing the formation of a graded anisotropy in the partially ordered top layer. Coercivities decrease for annealing temperatures that are greater than 400 {sup ∘}C due to improved ordering of the top layer.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Magnetic Properties of (Pr{sub 1−x}Sm{sub x}){sub 2}Fe{sub 14}B Melt-Spun Ribbons

The magnetic properties of (Pr{sub 1−x}Sm{sub x}){sub 2}Fe{sub 14}B melt-spun ribbons with varying x from 0 to 1.0 have been studied. The optimum magnetic property of Pr{sub 2}Fe{sub 14}B ribbon could be obtained with the surface velocity of copper wheel of 30 m/s. By melt spinning method, the formation of α-Fe impurity phase in the (Pr{sub 1−x}Sm{sub x}){sub 2}Fe{sub 14}B samples could be inhibited, and the grain could be aligned. Sm element could be incorporated into Pr{sub 2}Fe{sub 14}B main crystalline phase and formed (Pr,Sm){sub 2}Fe{sub 14}B phase with space group P4{sub 2}/mnm. The Curie temperature (T{sub c}) of the (Pr{sub 1−x}Sm{sub x}){sub 2}Fe{sub 14}B ribbons increases gradually from 555 to 617 K with the increase of Sm content x. Both the coercivity (H{sub c}) and remanence ratio (M{sub r}/M{sub s}) decrease firstly and then increase with the Sm content increasing. As long as the Sm content x does not exceed 0.1, the squareness of demagnetization curve remains good. The critical value of transition from easy c-axis to easy plane for (Pr{sub 1−x}Sm{sub x}){sub 2}Fe{sub 14}B ribbons is x= 0.6. When the Sm content x is up to 0.6, all the H{sub c} and M{sub r}/M{sub s} achieved the minimum value, i.e., 243 Oe and 0.346, respectively.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Martensitic Transformation and Magnetic Properties of the CuAl, CuAlMn, and CuAlMnZn Alloys

In the present work, the effect of alloying elements on the phase transformation which are formed by cooling effect in CuAl, CuAlMn, and CuAlMnZn (wt%) alloys are investigated using scanning electron microscopy (SEM) and vibrating sample magnetometer (VSM) characterization techniques. From SEM observations, the martensite formation with different morphologies is observed in these alloys. But the results of the scanning electron microscope investigations presented in this work have not formed the precipitates in the CuAl alloy with Mn or Zn additions. We found that magnetic saturation and coercivity values decreased with the addition of Mn and Zn elements to the CuAl alloy. The findings confirmed the variation in magnetic properties, which occurred in the result of adding different alloying elements.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Exchange Coupling in MnAlC/α-Fe Nanocomposite Magnets

Nanostructured composite materials consisting of exchange-coupled hard and soft magnetic phases are proposed as alternative for the development of high-energy product permanent magnets. In this work, we have examined the effects of soft magnetic α-Fe addition on the structure and magnetic properties of powders composed of hard magnetic Mn{sub 54.3}Al{sub 44}C{sub 1.7} compound. The optimum melt-spun ribbon precursor (with τ-phase structure, with magnetization of 88 emu/g and coercive field of 1.6 kOe) was obtained after annealing the ribbons at 500 {sup ∘}C for 20 min. After the combination between the soft and the optimized hard phase, the intensity of τ-phase peaks measured by X-ray diffraction decreases. These changes can also be seen in the magnetic properties. The coercivity (∼ 500 Oe) tends to decrease with the annealing temperature, while the magnetization tends to increase up to 141 emu/g. Evidence of good exchange coupling between particles of Mn{sub 54.3}Al{sub 44}C{sub 1.7} and α-Fe, in the produced composite, was proved by the hysteresis loop and its corresponding Thamm-Hesse analysis.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Quantification of the Interaction Field in Arrays of Magnetic Nanowires from the Remanence Curves

A method is presented that allows quantifying the average value of the interaction field in arrays of magnetic nanowires from the field difference between the isothermal remanence (IRM) and the DC demagnetizing (DCD) remanence curves when the normalized magnetization is equal to one third. Arrays of magnetic nanowires of different diameters and packing fractions are used to experimentally test the method. The results have been compared with those obtained using the method based on the difference between the remanence coercivity fields and with a mean-field expression for the interaction field, providing a very good agreement and thus validating the method. Additionally, it is shown that both the position (m{sub 0}) and the shift along the magnetization axis of the intersection between the remanence curves with respect to the value of one third (δm = m{sub 0} − 1/3) provide qualitative information about the interaction field. The former indicates the type of interaction depending if the intersection is above (m{sub 0} > 1/3) or below (m{sub 0} < 1/3), which corresponds to a ferro or anti-ferro magnetic interaction, respectively. While for the latter, it is shown that the maximum deviation of the Delta-M plot from zero (ΔM{sub max}) corresponds to three times the shift (ΔM{sub max} = 3δm).

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Structural and Magnetic Characteristics of Ferroxplana Co{sub 2}Y Nanoferrites Synthesized via Two Chemical Routes

Barium Y-type hexaferrite Ba{sub 2}Co{sub 2}Fe{sub 12}O{sub 22} nanopowders have been purposefully tailored using two different chemical wet methods, namely sol-gel auto-combustion (SGA) and co-precipitation (CP) routes. The impact of the pre-annealing and the annealing temperature of the formed precursors synthesized using two strategies on the structural, microstructure, and magnetic properties was investigated using x-ray diffraction (XRD), scanning electron microscopic (SEM), Fourier transform infrared spectroscopy (FT-IR), and vibrating sample magnetometer (VSM). For instance, well-defined Ba{sub 2}Co{sub 2}Fe{sub 12}O{sub 22} hexagonal plate-like particles was observed using SGA and CP routes for the precursors pre-annealed at 600 {sup ∘}C for 4 h and then annealed at low temperature 1000 {sup ∘}C for 2 h. The magnetic properties measured at room temperature evinced that hexaferrite Co{sub 2}Y particles have ferromagnetic characteristics. Good magnetic properties involving saturation magnetization (M{sub s}) of 23.64 and 24.37 emu/g and the coercivity (H{sub c}) of 417.76 and 280.92 Oe were accomplished for the samples pre-annealed at 600 {sup ∘}C for 4 h and then annealed at 1000 {sup ∘}C for 2 h for SGA and CP methods, respectively.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Structural and Magnetic Properties of FePt/SiO{sub 2} Core/Shell Nanoparticles

The disorder-order phase transition of FePt/SiO{sub 2} core/shell nanoparticles (NPs) induced by rapid thermal annealing was investigated. The FePt/SiO{sub 2} NPs were synthesized using FePt cores as seeds. For as-prepared FePt/SiO{sub 2} NPs, the average size of the FePt core and the thickness of the SiO{sub 2} shell are about 4.8 and 1.2 nm respectively, and the FePt NPs exhibit a disordered fcc structure. The FePt core NPs show obvious phase transformation from a disordered to an ordered structure after they were annealed at 600 °C for 2 min. Moreover, increasing annealing time can promote effectively the formation of the ordered fct-FePt phase. The relatively large coercivity H{sub c} is obtained for FePt NPs with a thicker SiO{sub 2} shell. The H{sub c} decreases firstly with decreasing temperature from 300 to 100 K and then increases from 100 to 10 K, which is ascribed to the coexistence of magnetically hard fct-FePt and magnetically soft fcc-FePt in the sample, and the incomplete exchange coupling between the hard and soft magnetic phases.

77 NANOSCIENCE AND NANOTECHNOLOGY↗

Effect of RF Power on Structural, Magnetic, and Optical Properties of CoFe{sub 2}O{sub 4} Thin Films

The thin films of CoFe{sub 2}O{sub 4} were deposited on glass substrates by radio-frequency (RF) sputtering. The effect of RF power variation from 60–120 W on the structure, magnetic, and optical properties of the as-deposited films and films annealed at 500 °C was studied. The magnetic parameters of the film, i.e., in-plane coercivity (H{sub c}), saturation magnetization (M{sub s}), and remanence (M{sub r}) increase as RF power is increased from 60 to 80 W followed by a decreasing trend with further increase in RF power to 120 W. Annealing of the film significantly improves the magnetic properties. The largest grain size and the best crystallinity of the film are obtained for the film deposited at 80 W of RF power. The thin films exhibited 70–80% optical transmittance. Optical band gap (E{sub g}) depends on the RF power and grain size, and it varies between 2.08 and 2.16 eV for the as-deposited films and between 2.16 and 2.30 eV for the annealed films. The study shows that RF power used for depositing the film has strong effect on the microstructure and properties of the film.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Structural and Hysteretic Properties of La{sub 0.7}Ca{sub 0.3−x}Sr{sub x}MnO{sub 3} Manganites Using the Hydrothermal Route

Manganitesof La{sub 0.7}Ca{sub 0.3−x}Sr{sub x}MnO{sub 3} have been produced using the hydrothermal method. The influence of the concentration of La, Ca, and Sr on the structural, morphological, and magnetic properties was studied and analyzed. The x-ray diffraction studies showed the occurrence of orthorombic and trigonal symmetries in the crystalline structure, depending on the stoichiometry. X-ray photoelectron spectroscopy studies were performed, showing the presence of the elements La3d, Ca2p, Sr3d, Mn2p, and O1s. In all samples, a deficiency of oxygen was observed and ascribed to hydroxide formation. The FTIR spectra shows the Mn–O–Mn bonds in the stretching vibration mode; on the other hand, a great relative amount of Mn{sup 4+} ions that are not included in the manganite phase was observed. Furthermore, morphology analyses developed using scanning electron microscopy showed cauliflower-type microstructures in all samples. The dependence of magnetization on magnetic field was also studied where a low coercivity and a high-saturation magnetization were evidenced. Values of the squareness ratio coefficient ranged between 0.0587 and 0.0867, indicating that the individual particles exhibit a strong random anisotropy.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Structural, Magnetic and Microwave Absorption Properties of Ba{sub 0.5}Sr{sub 0.5}Ni{sub 2−x} (MgZn) {sub x/2}Fe{sub 16}O{sub 27} Hexaferrite Nanoparticles Prepared by the Sol-Gel Combustion Method

In this study, Sr–Ba hexaferrite nanoparticles (Ba{sub 0.5}Sr{sub 0.5}Ni{sub 2−x}(MgZn){sub (x/2)}Fe{sub 16}O{sub 27}, x = –0.6, in the step of 0.2) was synthesized by the sol-gel method. The influence of Mg–Zn substitution on the structure and microwave absorption properties of Ni–W-type hexaferrite were investigated by technical methods such as x-ray diffraction, vector network analyzer, transmission electron micrograph and vibrating sample magnetometer. TEM images illustrated almost spherical particles with an average size of 35–52 nm. The M–H loops for all samples were measured at room temperature by vibrating sample magnetometer. Saturation magnetization (M{sub s}) and coercivity (H{sub c}) were derived from the hysteresis loops. The maximum field used in this measurement was 9 kilo-Oersted (kOe) Finally, the microwave absorption properties of these samples were investigated in Ku band range. The thickness of the composites was 2 mm in microwave absorption measurements. The results showed that the synthesized samples have a great potential in many fields of industry.

77 NANOSCIENCE AND NANOTECHNOLOGY↗

Enhancement of Magnetization and Tailoring of Blocking Temperatures of Nano-Ni–Zn Ferrite Powder Synthesized Using Microwave-assisted Combustion Method

Single-phase nano-Ni–Zn ferrite samples in the range of 6 to 75 nm were synthesized using microwave-assisted combustion method. Enhancement of saturation magnetization (M{sub s}) was observed in comparison with previously reported results. Minor variation of (M{sub s}) due to composition change can be explained on the basis of strengthening of A–B exchange interaction due to replacement of nonmagnetic Zn ions by Ni ions. Low coercivity (H{sub c}) and retentivity (M{sub r}) indicate low loss in the samples. SQUID analysis showed that the blocking temperature (T{sub B}) of the samples can be tailored in the present work.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Dynamic Magnetization Switching in NiO Nanoparticles: Pulsed Field Magnetometry Study

The dynamic magnetization switching of antiferromagnetic nickel oxide nanoparticles with a characteristic size of 8 nm has been experimentally investigated by pulsed field magnetometry. It is shown that, due to the presence of defects in NiO nanoparticles, as in other antiferromagnetic particles, the uncompensated magnetic moment is induced by the incomplete compensation of spins at the antiferromagnetic ordering. The dynamic magnetic hysteresis loops have been studied in pulsed fields with the maximum field (H{sub max}) of up to 130 kOe and pulse lengths (τ{sub P}) of 4, 8, and 16 ms. According to the results obtained, the coercivity (H{sub C}) depends on both the τ{sub P} and H{sub max} values. The observed increase in the H{sub C} value with decreasing pulse length (i.e., with increasing switching field frequency) is unambiguously related with the relaxation processes typical of single-domain ferromagnetic nanoparticles. However, the observed effect of the maximum applied field (H{sub max}) on the H{sub C} value is assumed to be a feature of antiferromagnetic nanoparticles.

77 NANOSCIENCE AND NANOTECHNOLOGY↗

Effect of the Boron Content on the Amorphization Process and Magnetic Properties of the Mechanically Alloyed Fe{sub 92−x}Nb{sub 8}B{sub x} Powders

The effect of the B content on the microstructural, structural, and magnetic properties of partially amorphous Fe{sub 92−x}Nb{sub 8}B{sub x} (x = 5, 10, 15, and 20) alloys has been investigated by means of scanning electron microscopy, X-ray diffraction, high and low-temperature extraction-type magnetometers. The XRD results reveal the formation of a nanocomposite structure where nanocrystalline bcc α-Fe and Fe{sub 2}B phases are embedded into an amorphous matrix. The FeB boride is observed for higher boron contents (x = 15 and 20), and the crystallite sizes are in the range of 7–24 nm. As the B content increases, the amorphous phase-relative proportion and coercivity increase, whereas the saturation magnetization decreases. An important magnetic hardening occurs by lowering the temperature from 400 to 5 K for x = 20% B. The variation of the Curie temperature can be attributed to the heterogeneity of the amorphous matrix.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Annealing Effects on Microstructure and Magnetic Properties of (NdPr){sub 9.5}(FeNbCoCu){sub 79.5}(BC){sub 11} Nanocomposite Magnets

Annealing effects on microstructure and magnetic properties of (NdPr){sub 9.5}(FeNbCo){sub 79.5}(BC){sub 11} ribbons were investigated. It was observed that Nd{sub 2}Fe{sub 14}B and Fe{sub 3}B phases were directly formed at low spinning speed. Then, the alloys transformed to an amorphous state at a speed of 20 m/s. Annealed at 700 {sup ∘}C for 10 min, the amorphous alloys as-quenched at 20 m/s crystallized into a nanocomposite composed of Nd{sub 2}Fe{sub 14}B and α-Fe phases. The formation of Fe{sub 3}B phases was inhibited. The magnetic properties firstly increased and then decreased with the increasing of annealing time. The optimum magnetic properties were achieved in the alloys annealed at 700 {sup ∘}C for 10 min. The corresponding coercivity, remanence, and the maximum energy product was 427.5 kA/m, 0.94 T, and 101.2 kJ/m{sup 3}, respectively. In addition, fine and uniform grains were formed. The average grain size was 10 nm.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Preparation and Characterization of NdFeB/PrCo{sub 5} Nanocomposite Magnetic Materials

We first developed NdFeB/PrCo{sub 5} nanocomposite magnetic material by high-energy ball milling, and the influence of the different contents of PrCo{sub 5} on the magnetic properties of NdFeB was studied by means of XRD, DSC, and VSM. The results showed that compared with single-phase NdFeB permanent-magnet material, NdFeB/PrCo{sub 5} nanocomposite magnetic material has superior magnetic properties. When the content of PrCo{sub 5} is 10% and the time of ball milling is 10 h, the magnetic properties for NdFeB/PrCo{sub 5} nanocomposite magnetic material is best: coercivity is 13.2 kOe, which increased by 14.8% over pure NdFeB phase. Remanent magnetization is 96.31 emu/g and the saturation magnetization is 132.29 emu/g. The remanence ratio is 0.728.

36 MATERIALS SCIENCE↗

Single- and Double-Layer Microwave Absorbers of Cobalt Ferrite and Graphite Composite at Gigahertz Frequency

Microwave absorbers of cobalt ferrite and graphite composite have been fabricated to investigate the broadening of absorption frequency by mixing small and large particles and comparing single- and double-layer composites in order to broaden the absorption frequency and to enhance multireflection and scattering of electromagnetic wave. CoO and Fe{sub 2}O{sub 3} precursors were mechanically alloyed and sintered at 800, 900, 1000 and 1100 {sup ∘}C in order to synthesise various particle sizes and shapes. A mixed sample of powders sintered at the above mentioned temperatures was also formed. The morphological, phase, and magnetic properties of these samples were studied. Two series of samples have been synthesised which were single- and double-layer composites. Single-layer composite consisted of mixed particles, and their thickness parameters were varied. Double-layer composite was also prepared with various particle sizes of CoFe{sub 2}O{sub 4} as a layer and graphene as another layer. The effect of these layers as matching and absorbing layer was studied. The degree of crystallinity of CoFe{sub 2}O{sub 4} was increased with increase of sintering temperature. Microstructural study showed the evolution of particle size and shape subjected to sintering temperature. Arrhenius plot showed two stages of growth process with activation energy calculated at 26.85 and 83.091 kJ/mol. The critical size of single domain of this sample plotted from the coercivity against particle size was 63.44 nm. Single-layer composite with mixed particle size was not able to show good electromagnetic (EM)-wave absorption; however double-layer composite showed good return loss. The mechanism of the EM-wave absorption of double-layer composite was discussed in this paper.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Effect of Ce{sup 3+} Ion on Structural and Hyperfine Interaction Studies of Co{sub 0.5}Ni{sub 0.5}Fe{sub 2−x}Ce{sub x}O{sub 4} Ferrites: Useful for Permanent Magnet Applications

Nanoparticles of Co{sub 0.5}Ni{sub 0.5}Fe{sub 2−x}Ce{sub x}O{sub 4} (where x = 0.0, 0.01, 0.015 and 0.02) ferrites are prepared by the modified solution combustion method using a mixture of fuels and are characterized to understand their structural, microstructural and magnetic properties. The X-ray diffraction is used to confirm the formation of a single-phase cubic spinel structure. The average crystallite sizes are calculated using the Scherrer formula and are found to be less than 50 nm. The microstructural features are obtained by the scanning electron microscopy, and the compositional analysis is done by using the energy-dispersive spectroscopy. The transmission electron microscopy (TEM) investigations show that the synthesized ferrites are made up of very fine spherical nanoparticles. The influence of a rare-earth element (Ce{sup 3+}) on the magnetic properties of the samples was studied using the Mössbauer spectroscopy. The Mössbauer spectroscopy reveals the formation of broadened Zeeman lines and quadrupole-split lines and the presence of the Fe{sup 3+} charge state at B sites in the samples. The quadrupole splitting shows that the orientation of the magnetic hyperfine field with respect to the principle axes of the electric field gradient was random. The magnetic hyperfine field values indicate that the A sites have more A-O-B superexchange interactions than the B sites. The coexistence of magnetic sextet and a doublet component on the room-temperature spectra suggests superparamagnetic properties of the nanoparticles. The low-temperature (15 K) Mössbauer spectroscopy explores the paramagnetic relaxation in the nanoparticles. The area under the sextet refers to Fe{sup 3+} concentrations in the tetrahedral and octahedral sites of the ferrite. This study confirms that the Ce{sup 3+} substitution of Fe{sup 3+} only for octahedron sites causes the decrease in Fe-O-Fe arrangement. The effect of Ce{sup 3+} doping on the magnetic properties of Co{sub 0.5}Ni{sub 0.5}Fe{sub 2}O{sub 4} is examined from the vibrating sample magnetometry (VSM) spectra. Saturation magnetization values are decreased initially and then increased, as result of Ce{sup 3+} doping. This can be explained by Neel’s two-sub-lattice model. Further, the value of coercivity is found to be increasing with increasing Ce{sup 3+} concentration. The obtained results of M-H loop with improved coercivity (from 851 to 1039 Oe) by Ce{sup 3+} doping of Co{sub 0.5}Ni{sub 0.5}Fe{sub 2}O{sub 4} demonstrate the usefulness for permanent magnet applications.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Development of Room-Temperature Ferromagnetism in Nanocomposite CdO Codoped with Al and Gd: Treatment in Hydrogen Atmosphere

Cadmium oxide codoped with Al and Gd ion powders was synthesised by thermal codecomposition of a mixture of complexes of cadmium acetate dihydrate, gadolinium acetate hydrate, and aluminum nitrate nonahydrate. The mass ratio of Al/Cd was fixed while the mass ratio of Gd/Cd varied systematically. The purpose of the present study is to synthesise and study the transparent conducting oxide (TCO) CdO powder having room-temperature ferromagnetic (RT-FM) properties. To realize that purpose, the synthesised Al/Gd-codoped CdO powder was annealed under hydrogen gas with certain conditions. The X-ray diffraction (XRD) method confirmed the formation of a single nanocrystalline structure; thus, both Al/Gd ions were incorporated into CdO lattice forming solid solutions. Magnetic measurements revealed that some of the doped CdO powders gained paramagnetic (PM) properties where the susceptibility increases with increasing dopant Gd content; the measured effective magnetic moment of dopant Gd{sup 3+} was around 8 μ{sub B}. Furthermore, the magnetic energy of the created RT-FM of the codoped CdO samples by hydrogenation was found to be dependent on the Gd% doping level. For hydrogenated CdO powder doped with 3% Gd, the coercivity (H{sub c}) was 195.9 Oe, the remanence (M{sub r}) was 0.77 memu/g, the saturation magnetisation (M{sub s}) was 5.05 memu/g, and the energy product (U{sub m}) was 150.6 merg/g. Thus, the possibility of production of TCO CdO with RT-FM, where magnetic characteristics can be tailored by doping and post treatment under H{sub 2} gas, was proven. Thus, a new potential candidate to be used as a dilute magnetic semiconductor (DMS) was successfully synthesised.

77 NANOSCIENCE AND NANOTECHNOLOGY↗