Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “ALUMINIZATION”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 127 records · Page 7

Tailoring the Properties of Calcium Aluminate Macro-Defect-Free Cements: From Brittle to Ductile Behavior

Cementitious macro-defect-free (MDF) materials can be obtained processing a mixture of a water-soluble polymer, namely polyvinyl alcohol (PVA) and the calcium aluminate cement. Based on process techniques typical of plastics, the MDF products can be obtained in complex forms and, thanks to the reduced water to cement ratio, w/c, their strength is very high compared to standard cements. However, these materials show both the sensitivity typical of water-soluble polymers, presenting a low glass transition temperature (T{sub g}), and the brittle behavior typical of ceramic materials and therefore low toughness. The aim of this work is to modify the mechanical properties of MDF cements by tuning their unacceptable brittle behavior. Water solution of carboxylate styrene butadiene rubber is used as reactive additives, and different mixture formulations are tested changing the rubber-like content both with respect to the fixed water content and PVA amounts. It is shown that the modifications of the organic phase imply small or negligible effects on paste formation of different recipes as detected by the torque–time responses. From flexural and fracture toughness tests, a wide range of responses was observed, and depending on the particular recipe, the mechanical behavior can be tuned from a brittle to a ductile behavior.

36 MATERIALS SCIENCE↗

Distinctive features of fluorescence and waveguides in magnesium aluminate spinel crystals driven by structural discrepancy

Transparent polycrystalline ceramics are of significant importance for a wide range of scientific and industrial applications. Developing a deeper understanding of their thermodynamic behavior is essential for achieving their maximum output performance in technological applications. This study provides a systematic investigation into the thermal excitation-induced fluorescence kinetics and waveguide characteristics of Magnesium Aluminate Spinel (MgAl 2 O 4 ) single crystals, with a focus on the intricate relationship between structure and properties. High-temperature extreme environments through irradiation with swift heavy ions 645.0 MeV Xe and 352.8 MeV Fe ions were created; the atomic deposition energy threshold (E th ) associated with disorder morphologies was assessed between 0.91 and 0.99 eV atom –1 . The track prediction model was developed to support the theoretical prediction of track formation. Electronic energy loss (E ele ) disrupts the balance of the initial structure through the thermal spike effect, leading to the formation of absorption-related F and F + color centers. These defects enhance photoluminescence in the visible spectrum and result in an effective modulation of the intrinsic bandgap. Moreover, as ion beams penetrate into the material, the uneven damage distribution induces the formation of waveguide structures. In conclusion, these findings provide valuable insights into the fabrication of functional devices through irradiation technologies and the structural changes of MgAl 2 O 4 at high temperatures within extreme environments.

36 MATERIALS SCIENCE↗

Influence of self heating and Li{sub 2}SO{sub 4} addition on the microstructural development of calcium aluminate cement

Hydrated Calcium Aluminate Cement (CAC) is known to have a complex microstructure involving different phase assemblages strongly dependant on the temperature. This work presents an experimental approach to study the microstructure of CAC pastes from the first minute of hydration with controlled time-temperature histories up to several months of curing. The self heating usually occurring in the CAC concrete is considered and its influence on the growth and assemblage of the hydration products and subsequent space filling is shown. Quantification of the degree of CA hydration by BSE image analysis is used to understand the evolution of phases throughout the hydration process. Lithium sulphate is commonly used to control the setting time of CAC based materials. It is shown that this promotes the formation of more stable hydrates, but slightly reduces the extent of CA hydration.

36 MATERIALS SCIENCE↗

Kinetics of calcium sulfoaluminate formation from tricalcium aluminate, calcium sulfate and calcium oxide

The formation kinetics of tricalcium aluminate (C{sub 3}A) and calcium sulfate yielding calcium sulfoaluminate (C{sub 4}A{sub 3}$) and the decomposition kinetics of calcium sulfoaluminate were investigated by sintering a mixture of synthetic C{sub 3}A and gypsum. The quantitative analysis of the phase composition was performed by X-ray powder diffraction analysis using the Rietveld method. The results showed that the formation reaction 3Ca{sub 3}Al{sub 2}O{sub 6} + CaSO{sub 4} → Ca{sub 4}Al{sub 6}O{sub 12}(SO{sub 4}) + 6CaO was the primary reaction < 1350 °C with and activation energy of 231 ± 42 kJ/mol; while the decomposition reaction 2Ca{sub 4}Al{sub 6}O{sub 12}(SO{sub 4}) + 10CaO → 6Ca{sub 3}Al{sub 2}O{sub 6} + 2SO{sub 2} ↑ + O{sub 2} ↑ primarily occurred beyond 1350 °C with an activation energy of 792 ± 64 kJ/mol. The optimal formation region for C{sub 4}A{sub 3}$ was from 1150 °C to 1350 °C and from 6 h to 1 h, which could provide useful information on the formation of C{sub 4}A{sub 3}$ containing clinkers. The Jander diffusion model was feasible for the formation and decomposition of calcium sulfoaluminate. Ca{sup 2+} and SO{sub 4}{sup 2−} were the diffusive species in both the formation and decomposition reactions. -- Highlights: •Formation and decomposition of calcium sulphoaluminate were studied. •Decomposition of calcium sulphoaluminate combined CaO and yielded C{sub 3}A. •Activation energy for formation was 231 ± 42 kJ/mol. •Activation energy for decomposition was 792 ± 64 kJ/mol. •Both the formation and decomposition were controlled by diffusion.

36 MATERIALS SCIENCE↗

Synthesis and hydration behavior of calcium zirconium aluminate (Ca{sub 7}ZrAl{sub 6}O{sub 18}) cement

Calcium zirconium aluminate (Ca{sub 7}ZrAl{sub 6}O{sub 18}) cements were prepared by solid state reaction and polymeric precursor methods, and their phase evolution, morphology, and hydration behavior were investigated. In polymeric precursor method, a nearly single phase Ca{sub 7}ZrAl{sub 6}O{sub 18} was obtained at relatively lower temperature (1200 °C) whereas in solid state reaction, a small amount of CaZrO{sub 3} coexisted with Ca{sub 7}ZrAl{sub 6}O{sub 18} even at higher temperature (1400 °C). Unexpectedly, Ca{sub 7}ZrAl{sub 6}O{sub 18} synthesized by polymeric precursor process was the large-sized and rough-shaped powder. The planetary ball milling was employed to control the particle size and shape. The hydration behavior of Ca{sub 7}ZrAl{sub 6}O{sub 18} was similar to that of Ca{sub 3}Al{sub 2}O{sub 6} (C3A), but the hydration products were Ca{sub 3}Al{sub 2}O{sub 6}·6H{sub 2}O (C3AH6) and several intermediate products. Thus, Zr (or ZrO{sub 2}) stabilized the intermediate hydration products of C3A.

36 MATERIALS SCIENCE↗

X-AFm stabilization as a mechanism of bypassing conversion phenomena in calcium aluminate cements

Phase conversion phenomena are often observed in calcium aluminate cements (CACs), when the water-rich hydrates (e.g., CAH{sub 10}, C{sub 2}AH{sub 8}) formed at early ages, at temperatures ≤ 30 °C, expel water in time to form more compact, less water-rich structures (C{sub 3}AH{sub 6}). The phase conversions follow a path regulated by the thermodynamic stabilities (solubilities) of phases. Based on this premise, it is proposed that conversion phenomena in CACs can be bypassed by provoking the precipitation of phases more preferred than those typically encountered along the conversion pathway. Therefore, X-AFm formation (where in this case, X = NO{sub 3}{sup −}) triggered by the sequential addition of calcium nitrate (Ca(NO{sub 3}){sub 2} = CN) additives is identified as a new means of bypassing conversion. A multi-method approach comprising X-ray diffraction (XRD), thermal analytics, and evaluations of the compressive strength is applied to correlate phase balances and properties of CAC systems cured at 25 °C and 45 °C. The results highlight the absence of the C{sub 3}AH{sub 6} phase across all systems and the curing conditions considered, with enhanced strengths being noted, when sufficient quantities of CN are added. The experimental outcomes are supported by insights gained from thermodynamic calculations which highlight thermodynamic selectivity as a means of regulating and controlling the evolutions of solid phase balances using inorganic salts in CACs, and more generally in cementing material systems.

36 MATERIALS SCIENCE↗

Effect of retarders on the early hydration of calcium-sulpho-aluminate (CSA) type cements

The retardation of calcium-sulpho-aluminate (CSA) type cements by three common retarders—sodium gluconate, sodium–potassium tartrate and borax is investigated at a 2% addition rate. Each of the retarders has a different effect on the early-age hydrate assemblage, as shown by quantitative X-ray diffraction, thermogravimetric analysis, scanning electron microscopy and pore solution analysis. Regardless of the retarder used, the hydration starts with mainly the dissolution of ready soluble (calcium) alkali sulphates and ye'elimite, followed by the formation of ettringite and aluminium hydroxide, whereby the specific clinker mineral dissolution as well as ettringite-forming reaction is delayed in different ways depending on the retarder used. The results showed that the retardation is mainly caused by preventing hydrates formation in the case of tartrate and gluconate. Contrary, borax retards the hydration by preventing to a certain extent the dissolution of ye'elimite and lowers the initial pH. Furthermore, the morphology of ettringite is altered depending on the type of the retarder used.

36 MATERIALS SCIENCE↗

A high-pressure X-ray diffraction study of the crystalline phases in calcium aluminate cement paste

Calcium aluminate cement (CAC) has wide application in civil engineering and castable refractory materials. The main binding phases of hardened CAC paste, CaO·Al{sub 2}O{sub 3}·10H{sub 2}O (CAH{sub 10}), inevitably converts to 2CaO·Al{sub 2}O{sub 3}·8H{sub 2}O (C{sub 2}AH{sub 8}), 3CaO·Al{sub 2}O{sub 3}·6H{sub 2}O (C{sub 3}AH{sub 6}) and Al(OH){sub 3} (AH{sub 3}), leading to a significant change in the mechanical properties of the CAC matrix. This work investigates the mechanical properties of the main crystalline components in hydrated and/or converted CAC systems, using synchrotron-radiation-based high-pressure X-ray diffraction. The anisotropic deformations of CaAl{sub 2}O{sub 4} (CA), CAH{sub 10} and C{sub 3}AH{sub 6} along each crystallographic direction are investigated, along with their bulk moduli. The density-driven stiffening hypothesis is validated for the studied phases and other cement-based minerals. An atom-scale topological analysis is proposed to explain the unusually high stiffness of CAH{sub 10}. The results provide fundamental information to understand the mechanical properties of single cement-based phases at molecular level, and enable predicting the changing mechanical properties of converted CAC matrix using homogenization models.

36 MATERIALS SCIENCE↗

Reduction of water content in calcium aluminate cement with/out phosphate modification for alternative cementation technique

Cementation of the secondary aqueous wastes from TEPCO Fukushima Daiichi Nuclear Power Plant is challenging due to the significant strontium content and radioactivity, leading to a potential risk of hydrogen gas generation via radiolysis of water content. The present study investigates the reduction of water content in calcium aluminate cement (CAC) with/out phosphate modification by a heat-treatment during the solidification. The reduction of water in the CAC was found restricted by the rapid formation of crystalline hydration phases, whereas the phosphate-modified system allowed the gradual reduction of water, achieving the reduction of 60% water content at 95 °C. Curing at 60–95 °C also eliminated the significant cracks found at 35 °C in the phosphate system. The possible difference in the amorphous products, NaCaPO{sub 4}·nH{sub 2}O type at 35°C and Ca(HPO{sub 4})·xH{sub 2}O type at 60–95 °C, may have contributed to the improvement in the microstructure together with the change in the pore size distribution.

36 MATERIALS SCIENCE↗

Superplasticizer to layered calcium aluminate hydrate interface characterized using model organic molecules

Ten organic molecule models simulating the chemical functions of commercial superplasticizers used in the cement/concrete industry were intercalated into lamellar calcium aluminate hydrates to synthesize hybrid AFm phases. AFm phases, encountered in cement hydration chemistry, belong to the large Layered Double Hydroxide (LDH) family. The intercalation process was performed using the anion exchange method. The affinities of the model molecules toward the AFm mineral layers, [Ca{sub 2}Al(OH){sub 6}]{sup +}, were compared using several complementary techniques. They display the following tendencies: –PO{sub 3}{sup 2-} > –SO{sub 3}{sup -} > –CO{sub 2}{sup -} for the hydrophilic parts and heptyl-R > phenyl-R > pentyl-R > ethyl-R for the hydrophobic parts. The organic-inorganic interface of the hybrid AFm phases was achieved. The organic molecule arrangement is either perpendicular or parallel to the inorganic main layer, resulting in various connection modes, from intercalation to grafting. The results enable a better understanding of the chemical reactivity of the utilized superplasticizers during the concrete setting process.

36 MATERIALS SCIENCE↗

Evolution of thermo-mechanical properties of concrete with calcium aluminate cement and special aggregates for energy storage

Highlights: • CAC Concrete with stable aggregates is suitable for high temperatures with cycles. • Concrete suffered performance changes after the first thermal cycle (dehydration). • Subsequent thermal cycles showed stabilization and slight performance decreases. With the ever-expanding presence of solar energy, the design of cost-efficient heat energy storage systems is becoming increasingly relevant. Concrete is a potential solid material for these systems but raises questions of its response at high temperatures in operating conditions. This work studies concrete designed with calcium aluminate cement and three types of aggregates that are stable at high temperatures. The designed concrete mixes were exposed to thermal cycles (290–550 °C), and their thermal fatigue response was evaluated with mechanical, cracking, thermal, and microstructural analyses at room temperature after heat cycles. The obtained results show that the main changes are mostly produced after the first thermal cycle and are stabilized during successive thermal cycles, with only a slight decrease in the thermo-mechanical properties. The results showed stabilization of cracking, crack widths between 10 and 80 μm, reduction of compressive strength, around 50–65%, and reduction of the thermal conductivity by 30%.

36 MATERIALS SCIENCE↗

NOx sequestration by calcium aluminate cementitious materials

This study quantifies NO{sub x} uptake efficiency and explores NO{sub x} binding mechanisms in calcium aluminate cementitious (CAC) materials. Comparison between unmodified and TiO{sub 2}-modified CAC separates intrinsic NO{sub x} binding mechanisms from those related to photocatalysis. Attributed to surface-related heterogeneous reactions, the NO{sub x} binding occurs in unmodified CAC at nitrite-to-nitrate ratio of 1: 1.3 and can be increased with surface area. The photocatalytic reactions in TiO{sub 2}-modified CAC increase NO{sub x} uptake, and ~50% of converted NO{sub x} resists releasing back into the environment via dissolution. Compared to previously studied ordinary portland cement (OPC) materials, CAC increases NO{sub x} uptake capacity and demonstrates a more permanent NO{sub x} binding, potentially mitigating concerns related to the release of previously bound N-species in OPC. Examination of the interaction between NO{sub x} and a synthetic pure aluminum-bearing phase shows that the permanent NO{sub x} uptake in CAC could be largely attributed to the chemical binding of converted NO{sub x} within aluminum-bearing phases.

36 MATERIALS SCIENCE↗

Effect of seawater as mixing water on the hydration behaviour of tricalcium aluminate

This study explored the mechanism of the effect of seawater on tricalcium aluminate (C{sub 3}A) hydration. The results showed that seawater retarded C{sub 3}A hydration and reduced the reaction degree of C{sub 3}A. The co-existence or ion pairing of Ca{sup 2+} and SO{sub 4}{sup 2−} onto the surface of C{sub 3}A poisoning the reactive sites is the main reason for this retardation. Besides, the precipitation of Mg(OH){sub 2} on the surface of C{sub 3}A would prolong the induction period for another 30 min and then consequently decrease the dissolution rate of C{sub 3}A hydration. Trace amounts of MgSO{sub 4}{sup 0} and Mg{sup 2+} present in the alkaline solution had little retardation effect. It was also found that Cl{sup −} would preferentially react with C{sub 3}A to form Friedel's salt, rather than forming hydroxy-AFm as that in the C{sub 3}A-deionized water paste. The direct formation of Friedel's salt resulted in an accumulation of Al{sup 3+} in solution, which would also hinder the subsequent dissolution of C{sub 3}A.

36 MATERIALS SCIENCE↗

Development of MnCoO Coating with New Aluminizing Process for Planar SOFC Stacks

Low-cost, chromia-forming steels find widespread use in SOFCs at operating temperatures below 800°C, because of their low thermal expansion mismatch and low cost. However, volatile Cr-containing species originating from this scale poison the cathode material in the cells and subsequently cause power degradation in the devices. To prevent this, a conductive manganese cobaltite coating has been developed. However, this coating is not compatible with forming hermetic seals between the interconnect or window frame component and ceramic cell. This coating reacts with sealing materials. Thus, a new aluminizing process has been developed for the sealing regions in these parts, as well as for other metallic stack and balance-of-plant components. From this development, the sealing performance and SOFC stack performance became very stable.

30 DIRECT ENERGY CONVERSION↗

Polymorphism of the iron doped strontium aluminate SrAl{sub 1.5}Fe{sub 0.5}O{sub 4}

The partial substitution of Al by Fe atoms in SrAl{sub 2}O{sub 4} allowed to stabilize four stuffed tridymite derivative structures SrAl{sub 1.5}Fe{sub 0.5}O{sub 4}. The different phases have been characterized by TEM and XRPD techniques. Two are isotypes of those observed for the undoped oxides, namely the hexagonal phase with sq root(3)Axsq root(3)AxC (with A and C being the tridymite unit cell parameters) and space group P6{sub 3} and the monoclinic one with Axsq root(3)AxC, {beta}{approx}93{sup o} and space group P2{sub 1}, with a synthesis temperature lower than the one required for SrAl{sub 2}O{sub 4}. By annealing, two original phases, denoted O{sub 1} and O{sub 2}, are obtained; they are metrically similar (3Axsq root(3)AxC and {beta}{approx}90{sup o}) and only differ by their space groups. The TEM study showed that the transitions between the different phases follow topotactic mechanisms, through the formation of twinning boundaries, antiphase boundaries and planar defects. The annealed sample exhibits a mesomorph state and a reversible transition from this semi-ordered state to a crystalline phase. This dynamic transition takes place over a very wide temperature range from 620 to 1120 deg. C. The reversibility of the transition has been studied by DSC measurements. The crystallization energy of the orthorhombic phases is of the order of 10 J/g, at T{approx}622 deg. C as T decreases. The variation of the peak height observed as the annealing temperature increases is explained by the complex microstructures, which create an ill-defined energy barrier. Structural models related to the stuffed tridymite derivative structures are proposed for the new forms of the ferri-aluminate. - Graphical abstract: Four tridymite derivative structures SrAl{sub 1.5}Fe{sub 0.5}O{sub 4} have been characterized. Two phases are isotypes of those observed for SrAl{sub 2}O{sub 4}. Two 'orthorhombic' original phases are characterized by superstructures. The transitions between the different phases follow topotactic mechanisms. The transition LT->HT takes place from 620 to 1120 deg. C, explained by complex microstructures, creating ill-defined energy barriers.

36 MATERIALS SCIENCE↗

Low temperature synthesis of nanocrystalline magnesium aluminate with high surface area by surfactant assisted precipitation method: Effect of preparation conditions

Highlights: ► MgAl{sub 2}O{sub 4} showed a high surface area and nanocrystalline structure. ► Addition of polymeric surfactant affected the structural properties of MgAl{sub 2}O{sub 4}. ► MgAl{sub 2}O{sub 4} prepared with surfactant showed a hollow cylindrical shape. -- Abstract: A surfactant assisted co-precipitation method was employed for the low temperature synthesis of magnesium aluminate spinel with nanocrystalline size and high specific surface area. Pluronic P123 triblock copolymer and ammonia solution were used as surfactant and precipitation agent, respectively. The prepared samples were characterized by thermal gravimetric and differential thermal gravimetric analyses (TG/DTG), X-ray diffraction (XRD), N{sub 2} adsorption (BET) and transmission electron microscopy (TEM) techniques. The effects of several process parameters such as refluxing temperature, refluxing time, pH, P123 to metals mole ratio (P123/metals) and calcination temperature on the structural properties of the samples were investigated. The obtained results showed that, among the process parameters pH and refluxing temperature have a significant effect on the structural properties of samples. The results revealed that increase in pH from 9.5 to 11 and refluxing temperature from 40 °C to 80 °C increased the specific surface area of prepared samples in the range of 157–188 m{sup 2} g{sup −1} and 162–184 m{sup 2} g{sup −1}, respectively. The XRD analysis showed the single-phase MgAl{sub 2}O{sub 4} was formed at 700 °C.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Nanoscale calcium aluminate coated graphite for improved performance of alumina based monolithic refractory composite

Graphical abstract: - Highlights: • Sol–gel Ca-doped γ-Al{sub 2}O{sub 3} accomplished graphite retention. • Nanocoating considerably improved matrix-aggregate bonding. • Less porous simulated matrix upgraded slag resistance. - Abstract: The synthesis and properties of high alumina castable containing nanostructured calcium aluminate coated graphite were studied in terms of slag resistance and overall physical characteristics. Raman spectroscopy, BET surface area and field emission scanning electron microscopy (FESEM) were performed to exclusively understand the coating characteristics and its compatibility in refractory composite. The coating not only secured graphite in castable for prolonged period but also noticeably improved matrix to aggregate contact. The microstructural aspects of castables were investigated, with special emphasis on a representative matrix prepared and infiltrated with slag at elevated temperature. Scanning electron microscopy (SEM) and energy dispersive spectroscopy (EDS) of fired composite containing surface-treated graphite was quite prospective. It circumvented the problems of incorporating as-received graphite in castables and should be in the attention of refractory researchers and producers.

36 MATERIALS SCIENCE↗

Thermochemical Capture of Carbon Dioxide on Lithium Aluminates (LiAlO{sub 2} and Li{sub 5}AlO{sub 4}): A New Option for the CO{sub 2} Absorption

Lithium aluminates (LiAlO{sub 2} and Li{sub 5}AlO{sub 4}) were synthesized, characterized, and tested as possible CO{sub 2} captors. LiAlO{sub 2} did not seem to have good qualities for the CO{sub 2} absorption. On the contrary, Li{sub 5}AlO{sub 4} showed excellent behavior as a possible CO{sub 2} captor. Li{sub 5}AlO{sub 4} was thermally analyzed under a CO{sub 2} flux dynamically and isothermically at different temperatures. These results clearly showed that Li5AlO{sub 4} is able to absorb CO{sub 2} in a wide temperature range (200-700{sup o}C). Nevertheless, an important sintering effect was observed during the thermal treatment of the samples, which produced an atypical behavior during the CO{sub 2} absorption at low temperatures. However, at high temperatures, once the lithium diffusion is activated, the sintering effect did not interfere with the CO{sub 2} absorption. Eyring's model was used to determine the activation enthalpies of the CO{sub 2} absorption (15.6 kJ/mol) and lithium diffusion (52.1 kJ/mol); the last one is the limiting process.

01 COAL, LIGNITE, AND PEAT↗