Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “age”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 1,243 records · Page 69

Hygrothermal aging effects on polyimide and acrylate-based adhesive materials in high-performance flat-flex cable assemblies

Flat-flex assemblies are widely used across a diverse range of technologies, including consumer electronics, automotive systems, aerospace and defense applications, and medical devices, due to their compact form factor and flexibility. However, environmental stressors like temperature and humidity are known to degrade performance over time, though the main mechanisms for degradation remain unknown. Here, in this work, we examined the aging behavior of copper/polyimide/adhesive laminate systems under varying temperature and humidity conditions, focusing on material degradation and its effects on mechanical and dielectric properties. Results show that peel strength and breakdown voltage decrease with exposure time, temperature, and humidity; spectroscopic characterization revealed that the adhesive, and not the polyimide, is the weak link in the material stack-up. The adhesive, identified as a butyl acrylate-acrylonitrile (BA-AN) copolymer, exhibited age-related spectral changes that correlated with exposure severity and duration. Hydrolysis at BA ester and AN nitrile groups was identified as the primary degradation mechanism, producing amides, acids, and alcohols. We developed a mechanistic model that connects kinetic parameters for BA-AN spectral band decay to peel strength and breakdown voltage, and implicates hydrolysis at the AN moiety, not BA, in performance decrements. Modeling predictions at ambient conditions indicate faster decline in peel strength than dielectric strength at early times, followed by plateauing of both properties at longer times. These findings provide critical insights into laminate aging mechanisms and highlight the importance of addressing BA-AN degradation to improve the long-term reliability of these systems in high-humidity environments.

organic↗

Examination of the mechanism for the reversible aging behavior at open circuit when changing the operating temperature of (La 0.8 Sr 0.2 ) 0.95 MnO 3 electrodes

The aging behavior of symmetrical cells, consisting of either (La 0.8 Sr 0.2 ) 0.95 MnO 3 (LSM) or La 0.6 Sr 0.4 Co 0.2 Fe 0.8 O 3 (LSCF) electrodes screen printed on either 8 mol% yttria-stabilized zirconia (YSZ) or Ce 0.8 Gd 0.2 O 2 (GDC) electrolyte substrates, is reported as the symmetrical cell is thermally cycled between 700 °C and 800 °C. For LSM, between 700 °C and 850 °C, the polarization resistance exhibits slow increases or decreases with time (on the order of days) after a quick change in temperature. When increasing the temperature, the polarization resistance decreases with time, and when decreasing the temperature, the polarization resistance slowly increases with time. In a previous work, the authors had explained these results with LSM by connecting the testing conditions to literature reports of surface analysis of LSM thin films which demonstrated a change in the amount of surface cation segregation as a function of temperature. In this work, TEM/EDS/XPS analysis of dense LSM pellets thermally cycled under the same conditions as the symmetrical cells does not indicate any significant reversible change in the surface composition of the LSM pellet between 700 °C and 800 °C. An alternative hypothesis is proposed to explain the relationship between polarization resistance and the LSM cation/anion vacancy concentrations controlled by the Schottky reaction. The timescale of aging behavior is related to the time necessary for the cations to move to or from the LSM surface to adjust to the new equilibrium at each temperature. Furthermore, the relevance in understanding the mechanism behind the aging behavior is emphasized with respect to fuel cell sample/stack modeling as well as to proper testing procedures for reaching reliable conclusions when comparing different electrode samples.

42 ENGINEERING↗

Yes-associated protein homolog, YAP-1, is involved in the thermotolerance and aging in the nematode Caenorhabditis elegans

The mammalian Hippo pathway comprises mammalian Ste20-like kinases (MST1/2) and large tumor suppressor kinases (LATS1/2). LATS1/2, which are activated by MST1/2, phosphorylate a transcriptional co-activator, yes-associated protein (YAP), and induce the recruitment of YAP by 14-3-3 to cytoplasm, so that the TEAD-dependent gene transcriptions are turned off. Although the core components of the Hippo pathway are well conserved in metazoans, it has been discussed that Caenorhabditis elegans lacks YAP ortholog, we found that F13E6.4 gene encodes a protein that shows sequence similarities to YAP in the N-terminal TEAD-binding domain and in the WW domain. We designated this gene as yap-1. YAP-1 is widely expressed in various cells such as epithelial cells, muscles, hypodermal cells, gonadal sheath cells, spermatheca, and hypodermal cells. YAP-1 is distributed in cytoplasm and nuclei. wts-1 (LATS ortholog) and ftt-2 (14-3-3 ortholog) knockdowns cause nuclear accumulation of YAP-1, supporting that the subcellular localization of YAP-1 is regulated in a similar way as that of YAP. Heat shock also causes the nuclear accumulation of YAP-1 but after heat shock, YAP-1 translocates to cytoplasm. Knockdowns of DAF-21 (HSP90 ortholog) and HSF-1block the nuclear export of YAP-1 during this recovery. YAP-1 overexpression is beneficial for thermotolerance, whereas YAP-1 hyperactivity induced by wts-1 and ftt-2 knockdowns is deleterious on thermal response and yap-1 deficiency promotes health aging. In short, YAP-1 partially shares basal characters with mammalian YAP and plays a role in thermal stress response and healthy aging. - Highlights: ► We named Caenorhabditis elegans F13E6.4 gene yap-1 as a putative YAP homolog. ► The localization of YAP-1 is regulated by WTS-1 and FTT-2. ► YAP-1 is involved in healthy aging and thermosensitivity.

60 APPLIED LIFE SCIENCES↗

Reducing lipofuscin accumulation and cardiomyocytic senescence of aging heart by enhancing autophagy

Highlights: • Lipofuscin accumulation varies in different regions and tissues of the heart. • Lipofuscin accumulation is related to cardiomyocytic senescence. • Enhancement of autophagy alleviates lipofuscin accumulation and myocardial senescence. Cardiomyocytes are particularly prone to lipofuscin accumulation. In the aging heart, lipofuscin accumulation is augmented. This study examined distribution of lipofuscin and senescent cardiomyocytes and evaluated improvement of lipofuscin accumulation and cardiomyocytic senescence of the aging heart after treatment with rapamycin. The results of Schmorl staining, Sudan black staining and autofluorescence detection showed that there was more lipofuscin in the myocardium of the ventricles especially in the left ventricle. The conductive tissue contained less lipofuscin than the myocardium. In the aged hearts, lipofuscin accumulation and senescent cardiomyocytes were increased, and the level of autophagy was reduced. In double staining of Sudan black B and senescence-associated β-galactosidase, 10%–20% lipofuscin-loaded cardiomyocytes became senescent. All senescent cardiomyocytes contained lipofuscin deposits. After enhancing autophagy with feed of rapamycin for six months, lipofuscin accumulation and senescence of cardiomyocytes were improved in old rats. Colocalization of autophagic structure and lipofuscin as well as electron micrographs showed that some lipofuscin-loaded lysosomes were sequestrated by autophagic structures. This study suggests that rapamycin-enhanced autopahgy is effective for reducing lipofuscinogenesis and promoting degradation of lipofuscin. Therefore, enhancing autophagy is a novel therapy for alleviating lipofuscin accumulation and myocardial senescence.

60 APPLIED LIFE SCIENCES↗

Creation of Self-Semi-Interpenetrating Network Structures in PIM-1 Membranes for Enhanced Physical Aging Resistance

A series of self-semi-interpenetrating network (ssIPN) thin films based on PIM-1 structure were developed by end-cross-linking telechelic PIM-1 oligomers end-capped with curable carboxylic acid groups to form model networks, which are penetrated by linear high-molecular-weight PIM-1 chains. ssIPN films with systematically varied network content ranging from 10 to 30 wt % were comprehensively examined on their microstructure and gas permeation properties. Fresh PIM-1 ssIPN films exhibited gas separation performances close to those of as-cast linear PIM-1, where the films closely followed the upper bound trade-off line, gaining as much selectivity as they lose gas permeability as the network content increases. This indicates that gas permeability is largely preserved despite cross-linking. Wide-angle X-ray scattering supported this observation, with peaks shifting toward lower d-spacing as oligomer content increased, suggesting tighter chain packing with higher cross-linkable oligomer loading. In physical aging studies over two months, all ssIPN films outperform linear PIM-1 for H 2 /CH 4 and O 2 /N 2 separations. Notably, the PIM-1 ssIPN with 10 wt % network content showed the best physical aging resistance, with negligible permeability loss even after one month. Finally, these findings highlight a promising macromolecular strategy for enhancing the physical aging resistance of microporous polymer membranes for gas separation.

PIM-1↗

Interplay between Swelling Kinetics and Nanostructure in Perfluorosulfonic Acid Thin-Films: Role of Hygrothermal Aging

Impacts of processing, storage, and operation on thin-film perfluorosulfonic acid (PFSA) ionomer coatings used in electrodes of electrochemical devices remains unestablished. In this work, alteration of structure–function relationship in ionomers is achieved via exposure to elevated temperature and humidity (hygrothermal aging). Findings reflect a strong inverse correlation between aging-induced ionomer thin-film domain orientation and water-transport kinetics evaluated from swelling. Finally, impact of aging is shown to be more pronounced on platinum due to interactions with PFSA, as evidenced by greater increase in nanodomain orientation parallel to substrate accompanied by reduced water transport, in contrast to silicon support.

36 MATERIALS SCIENCE↗

Strong Sensitivity of Simulated Biomass Burning Aerosol Transport and Radiative Effects Over the South Atlantic to Carbonaceous Aerosol Aging and Particle Density

Biomass burning aerosol (BBA) impacts climate through aerosol‐cloud‐radiation interactions, but models disagree on the sign and magnitude of BBA radiative effects. We quantify the sensitivity of BBA radiative effects and transport to three BBA‐relevant processes and properties: parameterized oxidative aging of organic aerosol (OA), a combined change to black carbon (BC) density and the method for calculating aerosol refractive index, and reduction in OA density. We evaluate Unified Model simulations against two aircraft campaigns from summer 2017 over the Southeast Atlantic. The model generally performs well, such that discrepancies between the observational data sets may sometimes limit the precision of the evaluation. Our newly developed aging parameterization reproduces observed OA:BC mass ratios well and allows modeled OA:BC to decrease with smoke age, but increases bias in aerosol extinction and changes the BBA radiative effect little (+0.12 W m -2 ). We calculate aerosol refractive index using either a volume‐weighted component average or the Maxwell‐Garnett (MG) mixing assumption, which represents BC as small inclusions in a host material. Compared to MG mixing, the volume‐weighted average refractive index and reduced BC density increase aerosol absorption, substantially increasing the total BBA radiative effect (+2.66 W m -2 ) and amount of BBA transported across the ocean through BC self‐lofting. Reducing OA density to better match literature values changes the total BBA radiative effect by −1.96 W m -2 . Changes to direct radiative effects exceed changes to cloud radiative effects. Our findings emphasize the sensitivity of aerosol radiative effects and transport to these processes and properties, which we suggest could be improved in climate models.

Southeast Atlantic↗

Influence of loblolly pine anatomical fractions and tree age on oil yield and composition during fast pyrolysis

Fast pyrolysis of woody materials is a technology pathway for producing renewable fuels and chemicals. This is a presentation of isolating needles, bark, and stemwood from a single tree as well as isolating stemwood and whole tree samples from the same species of tree with different ages and pyrolyzing each individually as well as in mixtures. This gives insight into the role of tree anatomical fractions on the resulting intermediate oil product as well as into interactions between these components. The highest carbon content oil (45.1 wt% as received) was produced from a one-to-one mixture of stemwood and needles, followed by the pure stemwood (43.4–43.8 wt% as received), while the lowest oil carbon content was from a one-to-one blend of bark and needles (26.7 wt% as received). The pyrolysis oil yield (combining oil and aqueous where separation occurred) varied from 54 wt% as received (needles) to 72.3 wt% as received (stemwood). When comparing trees of different ages, we find the change in the ratio of the anatomical fractions is a dominant factor in the product composition and yields, while the product composition and yields vary slightly with tree age when only the stemwood is pyrolyzed. Here, in this study, we present the bench-scale pyrolysis, yields, and product characterization of loblolly pine feedstocks (13- vs. 23 year-old, residues, air-classified residues, whole tree, needles, bark, and stemwood).

09 BIOMASS FUELS↗

KINETIC STUDY OF AGING IN A URANIUM-TITANIUM EUTECTOID ALLOY USING THERMOELECTRIC POWER MEASUREMENT

Considerable attention has been given to the study of microstructure evolution and mechanical properties of dilute U-Ti alloys. A typical procedure of heat treatment of the eutectoid uranium-titanium alloy consists of solution treatment in the {gamma} phase, obtaining of soft {alpha}{sup '} martensitic metastable structure by water quenching to room temperature and precipitation hardening by aging at 300-550 deg. C. Depending on employed temperature and time the aging results in GP zone formation through the precipitation reaction {alpha}{sup '}{yields}{alpha}+{delta}. The {delta} phase is a hexagonal U{sub 2}Ti intermetallic compound, responsible for the significant increase in the level of the micro-strain in the metastable {alpha}{sup '} matrix. Thermoelectric power (TEP) measurements have recently gained a growing attention for the characterization of metallurgical properties in steels and other alloys. These measurements, which are based on the Seebeck effect, are sensitive to changes in the electronic structure of the material as result of various metallurgical processes. In the current research, TEP measurement technique was applied as a non destructive assessment technique to characterize the aging kinetics of the quenched uranium-titanium binary alloy. Good correlation has been found between measured TEP, micro-strain evolution, as obtained by using XRD, and hardness values at different heat treatment stages. A reasonable explanation of the correlation between the crystallography changes, micro-strain, TEP measurements and properties is presented.

36 MATERIALS SCIENCE↗

Study of tungsten filament aging in hot-wire chemical vapor deposition with silacyclobutane as a source gas and the H{sub 2} etching effect

The tungsten filament aging when using silacyclobutane (SCB) as a source gas in a hot-wire chemical vapor deposition reactor was systematically studied by the characterization of surface morphology using scanning electron microscopy and the chemical composition analysis of the filament surfaces using Auger electron spectroscopy. It is shown that filament aging involves the formation of silicides and under more severe conditions, a pure silicon deposit. At low pressures of SCB samples, e.g., 0.06 and 0.03 Torr, only Si{sub 3}W{sub 5} alloy was formed. Silicon-rich silicide, Si{sub 2}W, was found when using a higher pressure of SCB at 0.12 Torr. At the high SCB pressure of 0.12 Torr and low temperatures, pure silicon was deposited on the W filament surface. It is also demonstrated that H{sub 2} can etch the aged filament at high temperatures above 1900 deg. C. The etching products detected by the 10.5 eV vacuum ultraviolet laser single photon ionization/time-of-flight mass spectrometer include SiH{sub 4}, SiCH{sub x} (x=2-5), and SiC{sub 2}H{sub y} (y=4-7)

36 MATERIALS SCIENCE↗

PBX 9404 detonation copper cylinder tests: a comparison of new and aged material

We present detonation copper cylinder test results on aged PBX 9404 (94 wt% HMX, 3 wt% CEF, 2.9 wt% NC, 0.1 wt% DPA) explosive. The charges were newly pressed from 37.5 year-old molding powder. We compare these results to equivalent data performed on the same lot when it was 3.5 years old. Comparison of the detonation energy inferred from detonation speed to that inferred from wall motion suggests that the HMX energy is unchanged but the NC energy has decreased to {approx}25% of its original value. The degradation of explosives and their binders is a subject of continual interest. Secondary explosives such as HMX are sufficiently stable near room temperature that they do not measurably degrade over a period of at least several decades. For formulated systems the bigger concern is binder degradation, for which the three main issues are strength, initiation safety, and (if the binder is energetic) energy content. In this paper we examine the detonation energy of new and aged PBX 9404 (94 wt% HMX, 3 wt% tris-{beta} chloroethylphosphate (CEF), 2.9 wt% nitrocellulose (NC), 0.1 wt% diphenylamine (DPA) [1, 2]), measured via the detonation copper cylinder test. In 1959, two independent PBX 9404 accidents [3] raised serious concerns about the safety of the formulation. Over about a decade's time, Los Alamos pursued a safer, energetically equivalent replacement, which ultimately became PBX 9501. In order to accurately compare the performance of the PBX 9404 and PBX 9501 formulations, W. Campbell and R. Engelke (C & E) developed a stringent cylinder test protocol that they called the Los Alamos Precision Cylinder Test [4]. The present aging study is possible because excellent PBX 9404 data from those qualification tests endures.

66↗

Surface enhanced Raman scattering of aged graphene: Effects of annealing in vacuum

In this paper, we report a simple method to recover the surface enhanced Raman scattering activity of aged graphene. The Raman signals of Rhodamine molecules absorbed on aged graphene are dramatically increased after vacuum annealing and comparable to those on fresh graphene. Atomic force microscopy measurements indicate that residues on aged graphene surface can efficiently be removed by vacuum annealing, which makes target molecule closely contact with graphene. We also find that the hole doping in graphene will facilitate charge transfer between graphene and molecule. These results confirm the strong Raman enhancement of target molecule absorbed on graphene is due to the charge transfer mechanism.

36 MATERIALS SCIENCE↗

Ageing of a neutron shielding used in transport/storage casks

In radioactive materials transport/storage casks, a mineral-filled vinylester composite is used for neutron shielding which relies on its hydrogen and boron atoms content. During cask service life, this composite is mainly subjected to three types of ageing: hydrothermal ageing, thermal oxidation and neutron irradiation. The aim of this study is to investigate the effect of hydrothermal ageing on the properties and chemical composition of this polymer composite. At high temperature (120 Degree-Sign C and 140 Degree-Sign C), the main consequence is the strong decrease of mechanical properties induced by the filler/matrix debonding.

36 MATERIALS SCIENCE↗

A strategy to stabilise the local structure of Ti{sup 4+} and Zn{sup 2+} species against aging in TiO{sub 2}/aluminium-doped ZnO bi-layers for applications in hybrid solar cells

We explore a strategy to counteract aging issues in TiO{sub 2}/aluminium-doped ZnO bi-layers used in hybrid solar cells photo-anodes, mainly related to Zn diffusion in the TiO{sub 2} matrix. Different Ti{sup 4+} and Zn{sup 2+} local structures within the anatase grains and along the film thickness were found as a function of post-deposition annealing treatments in the range between 200 °C and 500 °C by synchrotron radiation extended x-ray absorption fine structure analyses. In particular, in the 500 °C-treated sample, diffusion of zinc species along the TiO{sub 2} grain-boundaries has been observed with aging (3 years). In contrast, a mild thermal budget at 200 °C favours a proper atomic arrangement of the zinc-containing anatase lattice which reduces Zn diffusion, thus guaranteeing a good stability with aging.

36 MATERIALS SCIENCE↗

Chaotic behavior of light-assisted physical aging in arsenoselenide glasses

The theory of strange attractors is shown to be adequately applicable for analyzing the kinetics of light-assisted physical aging revealed in structural relaxation of Se-rich As-Se glasses below glass transition. Kinetics of enthalpy losses is used to determine the phase space reconstruction parameters. Observed chaotic behaviour (involving chaos and fractal consideration such as detrended fluctuation analysis, attractor identification using phase space representation, delay coordinates, mutual information, false nearest neighbours, etc.) reconstructed via the TISEAN program package is treated within a microstructure model describing multistage aging behaviour in arsenoselenide glasses. This simulation testifies that photoexposure acts as an initiating factor only at the beginning stage of physical aging, thus facilitating further atomic shrinkage of a glassy backbone.

71 CLASSICAL AND QUANTUM MECHANICS, GENERAL PHYSIC↗

Assessment of retrogression and re-aging treatment on microstructural and mechanical properties of Al-Zn-Mg-Cu P/M alloy

In order to understand the importance of the retrogression and re-aging as a heat treatment for improving microstructural and mechanical properties of the Al-Zn-Mg-Cu powder metallurgy alloys, Al-Zn-Mg-Cu-Fe-Cr alloys were fabricated from the elemental powders. Green compacts are compressed under compaction pressure about 370 MPa. The sintering process carried out for the samples of aluminum alloys at temperature was 650°C under argon atmosphere for two hours. The sintered compacts were subjected into homogenizing condition at 470°C for 1.5 hours and then aged at 120°C for 24 hours (T6 temper) after that it carried out the retrogressed at 180°C for 30 min., and then re-aged at 120°C for 24 hours (RRA). Observations microstructures were examined using optical, scanning electron microscopy coupled with energy dispersive spectroscopy and X-ray diffraction. Density and porosity content was conducted for the samples of alloys. The result showing that the highest Vickers hardness exhibited for an Al-Zn-Mg-Cu alloy after underwent the retrogression and reaging treatment. Increasing in hardness was because of the precipitation hardening through precipitate the (Mg Zn) and (Mg{sub 2}Zn{sub 11}) phases during matrix of aluminum-alloy.

36 MATERIALS SCIENCE↗

An improved model to estimate trapping parameters in polymeric materials and its application on normal and aged low-density polyethylenes

Trapping parameters can be considered as one of the important attributes to describe polymeric materials. In the present paper, a more accurate charge dynamics model has been developed, which takes account of charge dynamics in both volts-on and off stage into simulation. By fitting with measured charge data with the highest R-square value, trapping parameters together with injection barrier of both normal and aged low-density polyethylene samples were estimated using the improved model. The results show that, after long-term ageing process, the injection barriers of both electrons and holes is lowered, overall trap depth is shallower, and trap density becomes much greater. Additionally, the changes in parameters for electrons are more sensitive than those of holes after ageing.

71 CLASSICAL AND QUANTUM MECHANICS, GENERAL PHYSIC↗

Spectroscopic studies of the physical origin of environmental aging effects on doped graphene

The environmental aging effect of doped graphene is investigated as a function of the organic doping species, humidity, and the number of graphene layers adjacent to the dopant by studies of the Raman spectroscopy, x-ray and ultraviolet photoelectron spectroscopy, scanning electron microscopy, infrared spectroscopy, and electrical transport measurements. It is found that higher humidity and structural defects induce faster degradation in doped graphene. Detailed analysis of the spectroscopic data suggest that the physical origin of the aging effect is associated with the continuing reaction of H{sub 2}O molecules with the hygroscopic organic dopants, which leads to formation of excess chemical bonds, reduction in the doped graphene carrier density, and proliferation of damages from the graphene grain boundaries. These environmental aging effects are further shown to be significantly mitigated by added graphene layers.

71 CLASSICAL AND QUANTUM MECHANICS, GENERAL PHYSIC↗