Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “materials aging”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 1,225 records · Page 68

A Spatially Resolved Evaluation of Accelerated Environmental Aging on Emerging Polypropylene-Based Photovoltaic Backsheets Using Raman Spectroscopy

For this work, accelerated aging was used to assess environmental degradation in emerging co-extruded polypropylene (PP)-based backsheets under three different environmental conditions (65°C/20% relative humidity (RH), 75°C/20% RH, and 75°C/50% RH). Although differential scanning calorimetry did not measure crystallinity changes with exposure, spatially resolved Raman spectroscopy identified crystallinity increases in the core layer of aged samples, indicating a heterogeneous postcrystallization process. The Raman results were in agreement with synchrotron-based microfocused wide-angle X-ray scattering measurements. Cross-sectional nanoindentation was used to correlate localized crystallinity shifts with changes in Young's modulus. A similar trend was found where increased modulus was measured in the core layer, supporting the relationship between modulus and crystallinity. Finally, dielectric characterization was used to assess the impact of these material property changes on performance. While changes in the backsheet material properties and dielectric performance were observed with accelerated aging, these shifts generally equilibrated with time, indicating overall stability in response to environmental stressors. Additionally, the identified heterogeneous material property changes indicate that spatially resolved crystallinity measurements may be a valuable early failure indicator to be used in the assessment of PV backsheet long-term durability.

36 MATERIALS SCIENCE↗

New Experimental Data in DC745U [Slides]

The objectives of this project are: (1) study the molecular and mechanical properties of DC745U - (a) DC745U is a silicone elastomer used in several weapons systems, (b) depending on their chemistry and formulation, polymers can be susceptible to damage and failures due to weak chemical linkages and physical interactions, (c) inefficient production processes can generate heterogeneities throughout the material that can contribute negatively to the overall performance and lifetime of the polyer, (d) aging, long-term thermal and radioactive conditions, and mechanical strains can affect the materials network structure and contribute to the degradation of the production; (2) characterization of DC745U materials cured under different conditions to determine possible differences to the polymer structure; and (3) this work is relevant to mission-critical programs and for supporting programmatic work for weapon research.

36 MATERIALS SCIENCE↗

CALPHAD-based ICME design of single-step aging to enhance mechanical strength of WAAM Haynes 282

To match the strength of wire-arc additive manufactured Haynes 282 to its wrought counterpart via a single-step aging heat treatment, the CALPHAD (Calculation of Phase Diagrams) method is integrated with physics-based process-structure-property models and experimental validation. The integrated computational materials engineering (ICME) framework simulates the effects of aging on γ′ and M 23 C 6 precipitation and the resulting yield strength. To improve simulation reliability, the interfacial energies between γ/γ′ and γ/M 23 C 6 carbides were estimated by comparison with precipitation kinetic modeling and measured precipitate sizes. γ′ and M23C6 were found to precipitate simultaneously between 640 and 860 °C, producing microstructures similar to those produced by two-step aging. The optimal γ′ size for peak yield stress was calculated to be 20–23 nm. WAAM Haynes 282 aged at 780 °C for 50 h exceeded the mechanical performance of its wrought counterpart subjected to two-step aging, though desired properties can also be achieved at 800 °C for 16 h or less. The error in yield strength is less than 20 MPa, demonstrating good agreement between the modeling framework and experiments. Creep studies showed that WAAM Haynes 282 exceeded the calculated rupture time, reaching 481 h. This proposed methodology can accelerate the design of aging heat treatments for any γ′-strengthened nickel-base alloy, minimizing the resources required for trial-and-error experiments.

CALPHAD↗

Compact modeling of total ionizing dose and aging effects in MOS technologies

This paper presents a physics-based compact modeling approach that incorporates the impact of total ionizing dose (TID) and stress-induced defects into simulations of metal-oxide-semiconductor (MOS) devices and integrated circuits (ICs). This approach utilizes calculations of surface potential (ψs) to capture the charge contribution from oxide trapped charge and interface traps and to describe their impact on MOS electrostatics and device operating characteristics as a function of ionizing radiation exposure and aging effects. The modeling approach is demonstrated for bulk and silicon-on-insulator (SOI) MOS device. The formulation is verified using TCAD simulations and through the comparison of model calculations and experimental I-V characteristics from irradiated devices. The presented approach is suitable for modeling TID and aging effects in advanced MOS devices and ICs.

36 MATERIALS SCIENCE↗

Evaluation of a low temperature hardening Inorganic Phosphate Cement for high-temperature applications

Phase and mechanical changes of Inorganic Phosphate Cement (IPC) are identified along with changes in macro properties as functions of temperature and time. In addition to amorphous phases, the presence of significant amounts of brushite and wollastonite in the reference IPC is confirmed using X-ray diffraction. The thermal behavior of IPC up to 1000 {sup o}C shows that contraction of the solid phase in IPC due to chemical transformations causes reduction in the volume of the material. Also the ongoing meta-stable calcium phosphate transformations and reactions over a long time contribute significantly to the phase instability of the material at ambient conditions. It is found that the strength of IPC increases with ageing at ambient conditions but the formation microcracks below 105 {sup o}C causes a sharp reduction in the mechanical performance of IPC. According to the results obtained by Mercury intrusion porosimetry, the pore system of the reference IPC is dominated by mesopores.

36 MATERIALS SCIENCE↗

Review of nuclear power plant safety cable aging studies with recommendations for improved approaches and for future work.

Many U. S. nuclear power plants are approaching 40 years of age and there is a desire to extend their life for up to 100 total years. Safety-related cables were originally qualified for nuclear power plant applications based on IEEE Standards that were published in 1974. The qualifications involved procedures to simulate 40 years of life under ambient power plant aging conditions followed by simulated loss of coolant accident (LOCA). Over the past 35 years or so, substantial efforts were devoted to determining whether the aging assumptions allowed by the original IEEE Standards could be improved upon. These studies led to better accelerated aging methods so that more confident 40-year lifetime predictions became available. Since there is now a desire to potentially extend the life of nuclear power plants way beyond the original 40 year life, there is an interest in reviewing and critiquing the current state-of-the-art in simulating cable aging. These are two of the goals of this report where the discussion is concentrated on the progress made over the past 15 years or so and highlights the most thorough and careful published studies. An additional goal of the report is to suggest work that might prove helpful in answering some of the questions and dealing with some of the issues that still remain with respect to simulating the aging and predicting the lifetimes of safety-related cable materials.

21 SPECIFIC NUCLEAR REACTORS AND ASSOCIATED PLANTS↗

Moisture Outgassing Rates from TATB-Formulations: Experiments and Kinetic Model Development

Moisture outgassing rates from materials are of interest and importance to a variety of different fields. Because water can attack and accelerate decomposition, aging, or rusting of various parts, the assembly of an apparatus with 'wet' materials can shorten the lifetime of the apparatus. Outgassing of moisture from materials can be quite slow and a material that is seemingly dry at the time of assembly may slowly release water over years. This slow release of water will compromise the other constituents of the apparatus (e.g. electrical components, metals, organic materials) and shorten the lifetime of the apparatus. For apparatuses that are expensive or laborious to construct, it is especially important to understand and be able to predict the mechanisms and rates of water release from various materials. Such an understanding can support the development of accurate estimates of the apparatus's serviceable age and may allow for mitigation strategies in order to protect other parts from water. Energetic materials such as TATB based PBX-9502 (95% TATB, 5% Kel-F 800) and LX-17 (92.5% TATB and 7.5% Kel-F) pose a particularly challenging problem because they are heterogeneous materials with potentially many different sources and mechanisms of water release. Water molecules could be adsorbed into the polymeric binder matrix, trapped in occlusions within the polymer and the TATB crystals/particles, or trapped within defect sites in the TATB crystal. Finally, many studies indicate that water is a decomposition product under rapid heating conditions, at high temperatures and/or high pressure. Previous studies have measured the water release rate(s) from LX-17 or PBX-9502 prill/powder in order to establish oven drying times prior to use. These studies limited their time frame to a few days or a week of drying. Other studies have looked at the rate of water release of large pressed parts contained in sealed containers. Finally, some studies have looked at the rate of water diffusion through pressed parts, or the effects of wet vs. dry machining, or the influence of the synthesis methods in the amount of water present. There are a few different models that have been developed to predict the rate of water release from LX-17 or PBX-9502. These models are, to some extent, limited by the limitations of the experiments. Because all these experiments looked at water release over a relatively short period of time and left the samples relatively undamaged, they serve as a lower bound. In this work, we perform experiments and develop models that can serve as an upper bound on the rate and amount of water that can be released. Our experimental approach is to use temperature programmed desorption (TPD) and monitor the rate and amount of water release as a function of temperature. We analyzed our experimental data using two different kinetic analysis methods (isoconversional analysis and nth-order Arrhenius kinetic fits) and used the results to make predictions. The suitability of these kinetic analysis methods as well as the applicability of these experiments to long term aging (e.g. years) issues are discussed. Using the kinetics from our experiments, we predict the water release at temperature and timescales relevant to the existing literature. Based on our analysis and comparison with older data, the kinetic model(s) developed in this work serve as a relatively accurate (i.e. order of magnitude) method for predicting the water release under a variety of thermal histories.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Sm-Nd Isotopic Studies of Ureilite Novo Urei

Ureilites are ultramafic (harzburgitic) achondrites composed predominantly of olivine and pyroxenes, abundant carbon (graphites and shock-produced diamonds), some metal and sulfides. These rocks probably represent ultramafic mantles of differentiated parent asteroidal bodies. Age determinations of these rocks by Rb-Sr and Sm-Nd methods have been difficult because of their extremely low abundances of these parent-daughter elements. Nevertheless, Sm-Nd isochron ages were reported for Kenna, Goalpara, MET 78008 and PCA 82506 yielding ages of 3.74+/-0.02 Ga, approx.3.7 Ga, 4.09+/-0.08 Ga, 4.23+/-0.06 Ga, respectively [1-4]. These "young" Sm-Nd ages may represent secondary metasomatism events [1] related to impacts [5], as indicated by the similarly young Ar-39-Ar-40 degassing ages of 3.3-4.1 Ga for ureilites Kenna, Novo Urei and Havero [6]. Alternatively, it has been suggested that these rocks may have been contaminated with terrestrial crustal materials and the isochrons do not have any age significance [2,7]. Indications of old approx.4.56 Ga ages for ureilites were reported from the U-Pb and Sm-Nd model ages for MET 78008 [8]. More reliable evidences for old formation ages of ureilites were reported recently using the short-lived chronometers Hf-182-W-182, Al-26-Mg-26 and Mn-53-Cr-53. The deficits of 182W in ureilites suggest the metal-silicate segregation occurred very early, approx.1-2 Ma after CAI [9]. The Al-26-Mg-26 and Mn-53-Cr-53 studies for a feldspathic lithology [10] and the Mn-53-Cr-53 for olivine- and pyroxene-dominant lithologies [11] in ureilites revealed that they crystallized approx.5.4 Ma after CAI, i.e., at 4563.8+/-0.5 Ma relative to D.Orbigny. In this report, we present Sm-Nd isotopic data for a relatively fresh ureilite, Novo Urei, a rare ureilite fall (1886). We compare these data to Sm-Nd data for other ureilites, and discuss Novo Urei's petrogenesis

Shih, C.-Y.↗

Dislocation density evolution in the process of high-temperature treatment and creep of EK-181 steel

X-ray diffraction has been used to study the dislocation structure in ferrite-martensite high-chromium steel EK-181 in the states after heat treatment and high-temperature creep. The influence of heat treatment and stress on evolution of lath martensite structure was investigated by and electron back-scattered diffraction. The effect of nitrogen content on the total dislocation density, fraction of edge and screw dislocation segments are analyzed. - Highlights: •Fraction of edge dislocation in quenched state depends on nitrogen concentration. •Nitrogen affects the character of dislocation structure evolution during annealing. •Edge dislocations fraction influences on dislocation density after aging and creep.

36 MATERIALS SCIENCE↗

Evaluation of Nonmetallic Components in the Hanford Waste Transfer System - 17287

Nonmetallic materials are currently being used in the United States Department of Energy's Hanford Site Tank Farm waste transfer system. These materials include the inner primary hoses in the hose-in-hose transfer lines (HIHTLs), Garlock{sup R} gaskets, ethylene propylene diene monomer (EPDM) O-rings. These materials are exposed to a number of stressors and the synergistic effects are not well understood. Florida International University (FIU) engineers have developed an experimental test loop to determine how the nonmetallic materials react to both individual and simultaneous stressors. The initial phase of testing includes exposure of coupons and components to caustic material at various temperatures for varying lengths of time. The coupons are manufactured from EPDM and Garlock{sup R} sheets and will be used to evaluate changes in material data from baseline data. Components (inner hoses, O-rings and gaskets) will also be used to determine the effects from an environment similar to its operational environment. The test loop utilizes a 25% NAOH solution as the fluid and can accommodate eighteen component assemblies, each consisting of one EPDM HIHTL, EPDM O-ring and Garlock{sup R} gasket. There are three assembly aging sets, one for each temperature (37.78 deg. C, 54.44 deg. C and 79.44 deg. C) and each set contains six assemblies; three for each of the two time periods (6 months and 1 year). Prior to aging, a sample set of the components had baseline mechanical properties tested and a sample set of the coupons had baseline material properties determined as per ASTM standards. After the aging is completed the mechanical and material properties of the aged samples will be measured and compared with the bass-line data to obtain an understanding of the synergistic effects of the two stressors. (authors)

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Ultra-high performance wearable thermoelectric coolers with less materials

Thermoelectric coolers are attracting significant attention for replacing age-old cooling and refrigeration devices. Localized cooling by wearable thermoelectric coolers will decrease the usage of traditional systems, thereby reducing global warming and providing savings on energy costs. Since human skin as well as ambient air is a poor conductor of heat, wearable thermoelectric coolers operate under huge thermally resistive environment. The external thermal resistances greatly influence thermoelectric material behavior, device design, and device performance, which presents a fundamental challenge in achieving high efficiency for on-body applications. Here, we examine the combined effect of heat source/sink thermal resistances and thermoelectric material properties on thermoelectric cooler performance. Efficient thermoelectric coolers demonstrated here can cool the human skin up to 8.2 °C below the ambient temperature (170% higher cooling than commercial modules). Cost-benefit analysis shows that cooling over material volume for our optimized thermoelectric cooler is 500% higher than that of the commercial modules.

36 MATERIALS SCIENCE↗

Electrochemical Characterization of Biomolecular Electron Transfer at Conductive Polymer Interfaces

Bio-electrochemical systems (BESs) are promising for renewable energy generation but remain hindered by inefficient electron transfer at electrode surfaces. As the toolbox of bio-anode materials increases, rigorous electrochemical characterization of emerging materials is needed. Here, we holistically characterize the electrochemical interaction of flavin mononucleotide (FMN), an electron shuttle in biological systems and a cofactor for oxidoreductase enzymes, with the bio-inspired mixed conducting polymer poly{3-[6'-(N-methylimidazolium)hexyl]thiophene} (P3HT-Im + ). The behavior of this polymer is compared to the equivalent polymer without the histidine-like imidazolium. We find improved conductivity and charge storage in imidazolium-containing polymers beyond what is explained by differences in the electroactive area. The P3HT-Im + further shows internal charge storage but with negligible faradaic contribution, indicating that charge storage capacity may translate to improved biocatalysis non-intuitive ways. Finally, one-electron transfer is observed between FMN and glassy carbon, while a bio-similar two-electron transfer is observed for the P3HT-Im + . To our knowledge, this is the first example of a concerted two-electron transfer between FMN and an electrode interface, which we attribute to the bio-inspired, histidine-like imidazolium functional groups in the polymer. These studies demonstrate the importance of bio-relevant materials characterization when such materials are deployed in BESs.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

AGING MODEL FOR CANE FIBERBOARD OVERPACK IN THE 9975 SHIPPING PACKAGE

Many radioactive material shipping packages incorporate a cane fiberboard overpack for thermal insulation and impact resistance. Mechanical, thermal and physical properties have been measured on cane fiberboard following thermal aging in several temperature/humidity environments. Several of the measured properties change significantly over time in the more severe environments, while other properties are relatively constant. Changes in each of the properties have been fit to a model to allow predictions of degradation under various storage scenarios. Additional data continue to be collected to provide for future refinements to the model.

42 ENGINEERING↗

Technical Letter Report on the Cracking of Irradiated Cast Stainless Steels with Low Ferrite Content

Crack growth rate and fracture toughness J-R curve tests were performed on CF-3 and CF-8 cast austenite stainless steels (CASS) with 13-14% of ferrite. The tests were conducted at ~320°C in either high-purity water with low dissolved oxygen or in simulated PWR water. The cyclic crack growth rates of CF-8 were higher than that of CF-3, and the differences between the aged and unaged specimens were small. No elevated SCC susceptibility was observed among these samples, and the SCC CGRs of these materials were comparable to those of CASS alloys with >23% ferrite. The fracture toughness values of unirradiated CF-3 were similar between unaged and aged specimens, and neutron irradiation decreased the fracture toughness significantly. The fracture toughness of CF-8 was reduced after thermal aging, and declined further after irradiation. It appears that while lowering ferrite content may help reduce the tendency of thermal aging embrittlement, it is not very effective to mitigate irradiation-induced embrittlement. Under a combined condition of thermal aging and irradiation, neutron irradiation plays a dominant role in causing embrittlement in CASS alloys.

36 MATERIALS SCIENCE↗

Molecular dynamical simulation of the behavior of early precipitated stage in aging process in dilute Cu-Cr alloy

The aging behaviors of Cu-Cr alloys in the early stage at different temperatures are investigated by molecular dynamics simulations. First principles potentials are used for the interactions between Cu and Cr atoms. The initial behavior of precipitation is characterized by transmission electron microscope and electron energy disperse spectroscopy. The results showed that Cu-Cr supersaturated solid solution is thermodynamically unstable. The mean-square displacements of the atoms are used to describe the diffusivity. At room temperature, the atoms only show harmonic vibrations near the equilibrium positions. The mutual diffusion at 873 K is different from the unidirectional diffusion in low temperatures. The calculation shows that aging process is accelerated with increasing temperature, which is not only due to the lower diffusion activation energy of Cr at higher temperature, but also because Cu atoms are also participated in the aging process. When ''aging'' at 1073 K, the precipitation of Cr element is dissolved again into Cu matrix, which is an ''over-aging'' state of Cu-Cr alloy at high temperature.

36 MATERIALS SCIENCE↗

Crosslink Density and Molecular Weight Effects on the Viscoelastic Response of a Glassy High-Performance Polyimide

Durability and long-term performance are among the primary concerns for the use of advanced polymer matrix composites (PMCs) in modern aerospace structural applications. For a PMC subJected to long-term exposure at elevated temperatures. the viscoelastic nature of the polymer matrix will contribute to macroscopic changes in composite stiffness, strength and fatigue life. Over time. changes in the polymer due to physical aging will have profound effects on tile viscoelastic compliance of the material, hence affecting its long-term durability. Thus, the ability to predict material performance using intrinsic properties, such as crosslink density and molecular weight, would greatly enhance the efficiency of design and development of PMCs. The objective of this paper is to discuss and present the results of an experimental study that considers the effects of crosslink density, molecular weight and temperature on the viscoelastic behavior including physical aging of an advanced polymer. Five distinct variations in crosslink density were used to evaluate the differences in mechanical performance of an advanced polyimide. The physical aging behavior was isolated by conducting sequenced, short-term isothermal creep compliance tests in tension. These tests were performed over a range of sub-glass transition temperatures. The material constants, material master curves and physical aging-related parameters were evaluated as a function of temperature crosslink density and molecular weight using time-temperature and time-aging time superposition techniques.

Nicholson, Lee M.↗

Effect of in-situ (TiC-TiB2) reinforcement on aging and mechanical behavior of AZ91 magnesium matrix composite

Highlights: • Effect of TiC-TiB{sub 2} particles on precipitation behavior of in-situ composite was studied. • The age-hardening rate of in-situ composites is faster than that of alloy. • Faster age hardening rate is due to the presence of high dislocation density in composite. • Post aging treatment improved the mechanical properties of both base and composite. - Abstract: In the present work, influence of in-situ TiC-TiB{sub 2} reinforcement on age hardening behavior and mechanical properties of TiC-TiB{sub 2}/AZ91 composite was investigated. The base and in-situ composite materials were solution treated at 400 °C for 24 h and then aged at different temperatures up to 100 h. The kinetics of age hardening results revealed that the addition of in-situ TiC-TiB{sub 2} reinforcement increase the age hardening kinetics of the composite as compared to AZ91 magnesium alloy. The improvement in age hardening kinetics is attributed to the presence of high dislocation density resulted from the mismatch of coefficients of thermal expansion between in-situ TiC-TiB{sub 2} reinforcement and magnesium matrix. The precipitation behavior of Mg{sub 17}Al{sub 12} phase in both AZ91 alloy and TiC-TiB{sub 2}/AZ91 composites were established. After age hardening, base and in-situ composite materials show significant improvement in ultimate tensile strength by 47.72% and 66.49% respectively as compared with the base monolithic alloy. The enhancement of mechanical properties in the base and in-situ composites is explained in detail by analyzing their fractographs and microstructures.

36 MATERIALS SCIENCE↗