Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “joining”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 1,225 records · Page 68

Effect of laser welding parameters on the austenite and martensite phase fractions of NiTi

Although laser welding is probably the most used joining technique for NiTi shape memory alloys there is still a lack of understanding about the effects of laser welding parameters on the microstructural induced changes: in both the heat affected and fusion zones martensite may be present, while the base material is fully austenitic. Synchrotron X-ray diffraction was used for fine probing laser welded NiTi joints. Through Rietveld refinement the martensite and austenite phase fractions were determined and it was observed that the martensite content increases towards the weld centreline. This is related to a change of the local transformation temperatures on these regions, which occurs due to compositional variation in those regions. The martensite phase fraction in the thermally affected regions may have significant implications on functional properties on these joints. - Highlights: •Synchrotron X-ray diffraction was used for fine probing of the microstructure in laser welded NiTi joints. •Rietveld refinement allowed to determine the content of martensite along the heat affected and fusion zones. •The martensite content increases from the base material towards the weld centreline.

36 MATERIALS SCIENCE↗

Microstructural characterization of laser micro-welded Nitinol wires

Highlights: • FIB technique was used in the preparation of TEM foils of laser micro-welded joint. • Phase content in various zones of laser micro-welded Nitinol wires was revealed. • Welding induces the R-phase formation in HAZ and intermetallics precipitation in FZ. - Abstract: Laser micro-welding has been considered one of the most promising joining methods of manufacturing Nitinol biomedical devices. However, there is still a lack of understanding about how laser micro-welding influences the microstructure. This work attempts to reveal the phase content within various microstructural zones of laser micro-welded crossed Nitinol wires by transmission electron microscopy (TEM) with the assistance of the focused ion beam (FIB) technique. The base metal is composed of a single austenite phase (B2). The fusion zone exhibits the coexistence of austenite matrix and several intermetallics (T{sub 2}Ni, TiNi{sub 3} and Ti{sub 3}Ni{sub 4}). The precipitation of R-phase was observed in HAZ with B2 matrix due to thermally induced stresses during welding.

36 MATERIALS SCIENCE↗

The facile synthesis, crystallization behavior and magnetic property of FeNiP amorphous nanoparticles

Highlights: • A facile chemistry method was proposed to synthesize amorphous FeNiP nanoparticle. • Phase transformation happened during sintering the amorphous nanoparticle. • Ni nanospheres and monoclinic (Ni,Fe){sub 3}[PO4]{sub 2} nanorods appeared at 800 °C. • Crystallization behavior is α-FeNiP → Ni + FeNi{sub 3} + Ni{sub 3}P → Ni + (Ni,Fe){sub 3}[PO{sub 4}]{sub 2}. • Sintered powders have varied magnetic properties due to phase proportion change. - Abstract: Amorphous FeNiP nanoparticles with homogeneous composition are synthesized by reduction of aqueous Fe{sup 2 +} and Ni{sup 2 +} with sodium borohydride (NaBH{sub 4}) and hypophosphite at room temperature. These amorphous nanoparticles can be crystallized by heating up to 300 °C to form FeNi{sub 3} and Ni{sub 3}P crystals. Ni phase appeared at the sintering temperature of 500 °C, and a special net structure was formed at 700 °C due to the joining and diffusion among different nanoparticles. At a higher temperature of 800 °C, phase transformation happened and only pure Ni nanospheres and monoclinic ((Ni, Fe){sub 3}[PO{sub 4}]{sub 2}) nanorods can be observed, which should be governed by the long-range diffusion in the net structure. The amorphous FeNiP nanoparticles have excellent soft magnetic property with Ms of 13.2 emu/g and Hc of 0.7 Oe. However, the sintered mixing nanoparticles show varied magnetic properties due to the phase transformation and proportion change among different phases involved in.

77 NANOSCIENCE AND NANOTECHNOLOGY↗

Bismuth borate zinc glass braze for bonding sapphire in air

Highlights: • Sapphire was brazed with a novel 50Bi{sub 2}O{sub 3}–40B{sub 2}O{sub 3}–10ZnO (mol.%) glass at temperatures of 600–700 °C for 20 min in air. • Bi{sub 4}B{sub 2}O{sub 9} and Bi{sub 24}B{sub 2}O{sub 39} were formed in the joints brazed at 600 and 625 °C, respectively. • ZnAl{sub 2}O{sub 4} particles were formed in the joints when the brazing temperature was 635 °C. • The maximum shear strength of 85 MPa was obtained for the joints brazed at 650 °C for 20 min. - Abstract: Reliable brazing of sapphire was successfully achieved by using a novel 50Bi{sub 2}O{sub 3}–40B{sub 2}O{sub 3}–10ZnO (mol%) glass braze and joining cycles that peak at temperatures of 600 − 700 °C for 20 min in air. The effect of the brazing temperature on microstructure evolution as well as mechanical properties of the sapphire/sapphire joints was investigated. The results showed that Bi{sub 4}B{sub 2}O{sub 9} and Bi{sub 24}B{sub 2}O{sub 39} were formed in the joints brazed at 600 and 625 °C, respectively. ZnAl{sub 2}O{sub 4} particles were formed in the joints when the brazing temperature was 635 °C due to a reaction between the glass and the sapphire substrate. With the brazing temperature increasing, ZnAl{sub 2}O{sub 4} particles exhibited steady growth, from ~ 160 nm at 635 °C to ~ 455 nm at 700 °C. Besides, ZnAl{sub 2}O{sub 4} particles began to aggregate when the temperature was 675 °C. The strength increased sharply when the brazing temperature increased to 635 °C, which was mainly attributed to the formation of ZnAl{sub 2}O{sub 4} particles in the joint domain. The maximum shear strength of 85 MPa was obtained for the joints brazed at 650 °C for 20 min. The joint shear strength decreased due to the aggregation of ZnAl{sub 2}O{sub 4} particles in the joint.

36 MATERIALS SCIENCE↗

Comparison of microstructural and mechanical properties of friction stir spot welded ultra-high strength dual phase and complex phase steels

Highlights: • The microstructure and mechanical properties of FSSW of ultra high strength DP and CP steels are compared. • The stir zone (SZ) of CP steel mainly consists of bainite and martensite; no bainite is identified in the SZ of DP steel. • The cooling was not fast enough for the CP steel to suppress the effect of chemical composition on phase transformation. - Abstract: The microstructure and mechanical properties of friction stir spot welding of ultrahigh strength dual phase (DP) and complex phase (DP) steels are compared based on the experimental results. For both DP and CP steels, FSSW joints are successfully fabricated using the same process parameter set. While the microstructure of joints are characterized in detail using scanning electron microscopy, electron back scattered diffraction, and transmission electron microscopy, the mechanical property of joints are evaluated by shear tensile tests. The result of the microstructural analysis shows that the stir zone (SZ) of CP steel mainly consists of bainite and martensite, while no bainite is identified in the SZ of DP steel. The existence of bainite in the SZ of CP steel suggests that the cooling rate, which is nearly identical for both CP and DP steels, was not fast enough to suppress the effect of the alloying composition, particularly that of Mn, on the phase transformation. The result of the present study contributes to the development of solid state joining process of the ultrahigh strength steels.

36 MATERIALS SCIENCE↗

Influencing mechanism of Al-containing Zn coating on interfacial microstructure and mechanical properties of friction stir spot welded Mg–steel joint

Highlights: • Al-containing Zn coating improved Mg–steel interfacial wettability during friction stir spot welding (FSSW). • Pre-existing Al{sub 5}Fe{sub 2} phase in coating on steel surface promoted Mg–steel metallurgical bonding. • A high tensile-shear load of 4.3 kN was obtained in FSSW AZ31–steel joint. - Abstract: 2.4 mm thick AZ31 Mg alloy sheet and 1.5 mm Q234 steel sheet with a hot-dipped Al-containing Zn coating were friction stir spot welded (FSSW) using a pinless tool. It was shown that the Al-containing Zn coating played a crucial role in joining the Mg alloy and steel during FSSW. The Zn coating observably improved the Mg–steel interfacial wettability during FSSW, and the Al{sub 5}Fe{sub 2} phase in the Zn coating on the steel substrate surface promoted the metallurgical bonding of Mg alloy and steel. It was confirmed that the Al{sub 5}Fe{sub 2} phase on the steel surface resulted from the reaction between the steel substrate and the Al in the Zn coating during hot-dipping, and was not related to the Al-containing Mg alloy substrate. The tensile-shear load of the FSSW Mg–steel joint reached 4.3 kN. The fracture of the joint occurred along the interface on the steel substrate side. The interface between the Al{sub 5}Fe{sub 2} layer and Mg alloy substrate was the weakest region of the Mg–steel joint.

77 NANOSCIENCE AND NANOTECHNOLOGY↗

Interfacial diffusion reactions and mechanical properties of Ti3Al/Ni-based superalloy joints brazed with AgCuPd filler metal

Highlights: • Ti{sub 3}Al alloy to Ni-based superalloy was successfully brazed using Ag-21Cu-25Pd filler metal. • Phases TiPd (fcc), Ti{sub 3}Pd{sub 5} (bct) and AlPd (hcp) formed within the Ti{sub 3}Al/Ni-based superalloy joint. • Diffusion behavior of elements and its influence on joint interfacial microstructure were revealed. • A formation model of interfacial microstructure has been established. • The joint tensile strength at room temperature reached 404MPa, and the strength of 212MPa was maintained at 773 K. - Abstract: Dissimilar joining of a Ti{sub 3}Al-based alloy to a Ni-based superalloy has been conducted using Ag-21Cu-25Pd filler metal. The joint microstructures were analyzed using SEM, EPMA, XRD and TEM. The reaction behaviors between different elements were discussed. Due to the strong affinity, element Pd mainly reacted with Ti{sub 3}Al substrate and formed intermetallic compounds of TiPd, Ti{sub 3}Pd{sub 5} and AlPd. Elements Ni and Ti reacted with each other and caused the formation of Ni{sub 3}Ti in the centre of the joint. Owing to the diffusion effect, element Ag was enriched in the joint central area as (Ag,Cu){sub ss}. With the prolonging of the brazing time varying from 3 min to 15 min at 1253 K, the tensile strength of the joint firstly increased and then decreased. The joints brazed at 1253 K for 10 min presented the maximum strength of 404 MPa at room temperature, and the joint strength of 212 MPa was maintained at 773 K. The total fracture surface covered the most of the reaction zones from the (Ag,Cu){sub ss} to the diffusion effect zone at the Ti{sub 3}Al side.

36 MATERIALS SCIENCE↗

On visualizing material flow and precipitate evolution during probeless friction stir spot welding of an Al-Li alloy

Highlights: • Severe thermal cycle and deformation refined grains and intermetallic particles in SZ. • T{sub 1} phases fully dissolved in SZ followed by re-precipitation of GP zone and δ′ phases. • The predominant flow direction remained in spiral-like pattern during P-FSSW. • Local abrasion existed in the lap-weld interface due to flow difference, forming joining. - Abstract: The precipitate evolution and material flow visualization during probeless friction stir spot welding (P-FSSW) of an Al-Li alloy has been investigated experimentally and numerically in this work. Due to severe heat input during welding, the main strengthening phases of T{sub 1} fully dissolved in the stir zone followed by the re-precipitation of GP zone and δ′ phases, assisted with the refinement of the intermetallic particles and grains. The history of material flow was three-dimensionally visualized with a tracer, studied with X-ray tomography. The experiments and the simulation results provided a consistent interpretation of a circumferential material flow which moved inwards radially near the top surface. Upward flow in the bottom sheet improved with dwell time, causing the interface to bend. Local abrasion between the two sheets due to flow difference led to the disruption of oxide layer, and formed a connection at the interface.

36 MATERIALS SCIENCE↗

Microstructure evolution and mechanical properties of Cu/Sn/Ag TLP-bonded joint during thermal aging

Highlights: • The thermal reliability of the Cu/Sn/Ag TLP-bonded joint was investigated through high-temperature storage. • A diffusion reaction occurred at the interface between Cu{sub 3}Sn and Ag{sub 3}Sn during thermal aging. • The mechanism of the Cu{sub 3}Sn/Ag{sub 3}Sn interfacial reaction was investigated from thermodynamics and kinetics. - Abstract: Low-temperature transient liquid phase (TLP) bonding is a promising joining technology for high-temperature electronic devices packaging. However, the effect of thermal aging on the joint microstructure and performance has been rarely studied so far. In this paper, the relationship between microstructural evolution and mechanical property was developed for the Cu/Sn/Ag TLP-bonded joint during 350 °C aging. Experimental results show that an interfacial reaction occurs between the intermetallic compounds (IMCs) of Cu{sub 3}Sn and Ag{sub 3}Sn, which induces that a great amount of Cu{sub 3}Sn particles or wedges embed into the Ag-Sn phase layer. The reaction process is controlled by a volume diffusion of Cu elements from the Cu substrate, and capable of promoting the transformation from Ag{sub 3}Sn into Ag(Sn) solid solution. Cu{sub 41}Sn{sub 11} phase can be formed at the expense of Cu{sub 3}Sn and Cu, of which transformation process is completely achieved after aging for 480 h, and the Cu(Sn) solid solution intimately contacts with the opposite Ag(Sn) solid solution in many areas after aging for 960 h. The joint mechanical property initially declines due to the formation of Cu{sub 41}Sn{sub 11} phase and Cu-Sn IMCs grain coarsening, and then increases because of the complete depletion of Cu{sub 3}Sn and substantial precipitation of Cu(Sn) solid solution. After aging for nearly 1000 h, the joint still maintains a high shear strength of >40 MPa, indicating an excellent thermal reliability.

36 MATERIALS SCIENCE↗

Multi-scale and multi-technic microstructure analysis of a linear friction weld of the metastable-β titanium alloy Ti-5Al-2Sn-2Zr-4Mo-4Cr (Ti17) towards a new Post-Weld Heat Treatment

Highlights: • Soft joint showing sharp macro-zones and marked by asymmetrical process effects • Gradient of thermomechanical loads identified through progressive stages of transformation • Highly textured recrystallized β grains at the joint core with distorted β lattice • Lattices, phase fractions, microstructures and hardness homogenized after heat treatment - Abstract: Linear Friction Welding (LFW) is a solid-state joining process producing narrow joints mainly developed for the aircraft industry. The Thermo-Mechanical Processing (TMP) loads imposed on the material cause complex microstructure transformations. This study aimed at characterizing the local microstructures and crystallographic configurations to identify the mechanisms impacting the stability and the mechanical properties of a Ti17 LFW joint with the objective of establishing an innovative homogenizing Post-Weld Heat Treatment (PWHT). The process caused a narrow zone of ±2 mm from the friction interface to reach the isothermal α → β transformation temperature under a heating rate of 500 K/s followed by quenching (−100 K/s). The TMP resulted in the formation a ±3 mm wide soft Process Affected Zone (PAZ) delimited by three characteristic zones: the Welding Line (WL width ≈ 400 μm), The Thermo-Mechanically Affected Zone (TMAZ width ≈ 1 mm) and the Heat Affected Zone (HAZ). β TMP resulted in the total dissolution of the α phase in the joint core (WL + TMAZ) and formed strongly textured {110}<111> β recrystallized grains in the WL by continuous dynamic recrystallization of squeezed prior-β grains in the TMAZ. α + β TMP led to a gradual loss of hardness in the HAZ whose microstructure is similar to the one of the base material (BM) but is subject to gradual α laths dissolution due to the local temperatures experienced during LFW. A PWHT consisting in a β annealing followed by an α + β ageing resulted in a uniformly hardened weld with a homogenized Widmanstätten microstructure in the whole assembly.

36 MATERIALS SCIENCE↗

Rapid grain refinement and compositional homogenization in a cast binary Cu50Ni alloy achieved by friction stir processing

Friction stir processing (FSP) has been increasingly adopted for joining and processing materials in automotive, aerospace and industrial construction. During FSP a dynamic competition between high-speed shear deformation and deformation-induced heating brings about a complex competition between multiple dynamic microstructural evolution mechanisms making it difficult to predict the microstructural evolution pathway. Hence, improved understanding of microstructural evolution mechanisms during FSP can be beneficial for continued growth in the adoption of FSP for demanding applications of future. Towards this goal, this study uses a model binary Cu – 50 at.% Ni alloy to clarify the effect of single and double pass FSP on the microstructural evolution of a coarse grained and compositionally heterogeneous cast microstructure. High energy synchrotron X-ray diffraction, electron backscatter diffraction, and nanoindentation are used to clarify the microstructural evolution due to FSP. The process of compositional homogenization of as-cast segregations is studied by energy dispersive spectroscopy and atom probe tomography. Our results show that a single fast FSP pass at 30 mm.s -1 produces a 100 µm deep layer of submicrometric and hall-petch hardened CuNi grains. The initial cast compositional heterogeneities in a micrometric scale is rapidly transformed to nano-sized domains, mainly confined at grain boundaries. Double pass FSP increases the penetration depth of the processed layer and leads to a 2.9 times grain growth relative to single pass FSP. Grain fragmentation, discontinuous dynamic recrystallization, grain growth, and twinning mechanisms are discussed. In conclusion, these results highlight the value of FSP for ultrafast grain refinement and compositional homogenization of cast alloys.

36 MATERIALS SCIENCE↗

Microstructure and mechanical properties of friction stir weld performed on neutron-irradiated 304L steel with helium

As nuclear power plants (NPPs) approach or exceed 40–60 years of service, it may become necessary to repair damaged neutron-irradiated components to prolong longevity. However, fusion welding repair of irradiated steels and metallic materials is challenging because of helium-induced cracking. This study used friction stir welding (FSW) to address helium-related issues, such as helium bubble formation and grain boundary cracking. The microstructure, helium-induced degradation, and mechanical properties of a friction stir weld produced on neutron-irradiated 304L stainless steel with approximately 5.2 appm of helium were characterized. The analysis focused on variations in grain size, texture, and the morphology of helium-induced damage in the friction stir weld. Mechanical properties were characterized on the irradiated base metal (BM) and metallurgical zones of the friction stir weld: the stir zone (SZ), the thermo-mechanically affected zone (TMAZ), and the heat affected zone (HAZ). Only minor scattered porosity in the SZ and TMAZ and a few short microcracks (below 20 μm in length) in the TMAZ were observed, indicating limited helium-induced degradation. Tensile tests revealed good mechanical properties and fractography analysis demonstrated predominantly ductile fracture. In conclusion, the results highlight the immediate and substantial benefits of the FSW approach for repairing or joining helium-containing irradiated materials in NPPs.

36 MATERIALS SCIENCE↗

Active interlocking metasurfaces enabled by shape memory alloys

Interlocking metasurfaces (ILMs) are a newly developed joining technology that relies on arrays of interlocking features that transmit force and constrain motion between adjoining bodies in one or more directions. This study explores harnessing the shape memory effect (SME) in Nickel-Titanium shape memory alloys (NiTi SMAs) in structures fabricated using additive manufacturing (AM) to advance the development of active ILMs by creating unit cells that open or close at specific temperatures. The study encompasses designing and fabricating two distinct interlocking array configurations using near-equiatomic NiTi powder and the laser powder bed fusion (L-PBF) AM technique, following a previously developed AM process optimization framework to manufacture defect-free parts. To guide the design process, finite element analysis (FEA) was employed to predict strain values during engage-disengage cycles. The martensitic transformation characteristics of the ILMs were characterized. Thermomechanical testing revealed that the ILMs demonstrate high locking force once engaged, coupled with complete shape recovery and good cyclic stability. Digital image correlation (DIC) was also employed to validate the FEA predictions during the engage-disengage cycles. The results indicate that NiTi SMA-based ILMs can be designed and fabricated into complex shapes using L-PBF. By leveraging the SME, the functionality of an ILM can be improved upon. The combination of computational modeling, additive manufacturing, and thermomechanical and physical property characterization provides a framework for designing future ILMs out of active materials.

Additive manufacturing↗

Vibration mitigation in interlocking metasurfaces

Interlocking metasurfaces (ILMs) are a new class of mechanical metamaterials with patterned surface features that enable joining of two adjacent bodies, serving as an alternative to welds, fasteners, or adhesives. While the strength of ILMs has been explored previously, it is also possible to envision ILMs that possess the ability to dampen vibration or tailor energy transmission across the interface. In this study, we explore the vibration transmission under frequency sweep and random excitation of three ILM designs. This is the first study to characterize the response of ILMs under vibration. We find that ILMs which are tightly coupled (e.g., small interference fit) behave as a linear system and depart only marginally from the behavior of a solid body. However, through strategic manipulation of the ILM topology, and in particular the fit clearances, we show that vibrations can be damped by over an order of magnitude. Design strategies to employ ILMs for vibration mitigation are developed using a first-order model.

Bolmin, O. [Carnegie Mellon Univ., Pittsburgh, PA ↗

Directed energy deposition of functionally graded V-4Cr-4Ti to Fe-9Cr transition for fusion power systems

This study proposes a graded structure via additive manufacturing for divertor and first wall blanket applications in fusion reactors. Materials were selected based on thermodynamic calculations to operate from 1100 °C at the plasma-facing level to 550 °C at the structural steel level. Conventional joining methods often lead to failures due to discrete reaction layers with significant mechanical property differences. Using laser beam-directed energy deposition (LB-DED), this study demonstrates the fabrication of a VCrTi-Gr91 steel functionally graded component through a novel process parameter optimization framework. A systematic approach included powder characterization, single-track depositions, and construction of printability maps. Near full-density specimens of each interlayer were additively manufactured, and a transition from V-based alloys to reduced activation ferritic martensitic steels was achieved. Computational material selection of interlayer alloys and thermodynamic/diffusion kinetics simulations prevented most interface incompatibilities. A brittle intermetallic formed at one interface, causing cracking, which was not predicted by current thermodynamic models. Transition alloy design approach was updated with a more recent database and a mitigation strategy has been proposed to eliminate the formation of deleterious intermetallic phases. Ultimately, LB-DED has proven effective for producing multi-material graded systems for fusion applications, with the demonstrated process parameter optimization framework applicable to various materials.

Additive manufacturing↗

Controlling homogenization length scales and microstructure in additively manufactured Ti-Ta functionally graded materials

Materials with smooth compositional gradients or functionally grade materials (FGMs) produced via additive manufacturing (AM), enables joining dissimilar materials and optimizing multiple properties in advanced engineering applications. However, as-printed AM microstructures exhibit micro-segregation and solidification defects which, when combined with controlling macroscale gradient properties, complicates necessary post-processing. Here, we use CALPHAD-informed diffusion modelling to design post-processing heat treatments for lightweight to refractory FGMs. Ti-Ta (0 to 85 at. % Ta) FGMs were fabricated using laser-based directed energy deposition AM. Post-processing heat treatments at 1000° C and 1500° C were designed to promote homogenization across specific length scales and experimentally validated. Investigation of chemical segregation and microstructures demonstrated that the length scale of homogenization is controlled as a function of time, temperature, and local composition. Ta-rich regions exhibited incomplete homogenization compared to Ti-rich layers. Unmelted Ta particles were found to completely dissolve at 1500 °C. By controlling cooling rate (200 °C/min), martensitic structures were produced between 14–36 at. % Ta, consistent with martensite-start temperatures calculations, while furnace cooling (2 °C/min) produced α+β morphologies. This work establishes a validated predictive framework for designing post-processing to tailor microstructure and chemical architecture in AM FGMs, facilitating their deployment in demanding environments.

Materials science↗

Structural study by X-ray diffraction and transmission electron microscopy of the misfit compound (SbS{sub 1-x}Se{sub x}){sub 1.16}(Nb{sub 1.036}S{sub 2}){sub 2}

In the Sb-Nb-S-Se system, a new misfit layer compound (MSL) has been synthesized and its structure was determined by combining single crystal X-ray diffraction (XRD) and transmission electron microscopy (TEM) techniques. It presents a composite crystal structure formed by (SbS{sub 1-x}Se{sub x}) slabs stacking alternately with double NbS{sub 2} layers and both can be treated as separate monoclinic subsystems. The (SbS{sub 1-x}Se{sub x}) slabs comprise a distorted, two-atom-thick layer with NaCl-type structure formed by an array of {l_brace}SbX{sub 5}{r_brace} square pyramids joined by edges (X: S, Se); the NbS{sub 2} layers consist of {l_brace}NbS{sub 6}{r_brace} trigonal prisms linked through edge-sharing to form sheets, just as in the 2H-NbS{sub 2} structure type. Both sublattices have the same lattice parameters a = 5.7672(19) A, c = 17.618(6) A and {beta} = 96.18(3){sup o}, with incommensurability occurring along the b direction: b{sub 1} = 3.3442(13) A for the NbS{sub 2} subsystem and b{sub 2} = 2.8755(13) A for the (SbS{sub 1-x}Se{sub x}) subsystem. The occurrence of diffuse scattering intensity streaked along c{sup *} indicates that the (SbS{sub 1-x}Se{sub x}) subsystem is subjected to extended defects along the stacking direction.

36 MATERIALS SCIENCE↗

Synthesis, characterization, and anomalous dielectric and conductivity performance of one-dimensional (bdaH)InSe{sub 2} (bda = 1,4-butanediamine)

Graphical abstract: Anomalous dielectric and conductivity performance have been observed in the organic-containing indium selenide (bdaH)InSe{sub 2}, which are attributed to the water molecules existing in the crystal boundary rather than phase transition. Highlights: {yields} The title compound is the first example of organic-containing one-dimensional indium selenide. {yields} The anomalous dielectric peak is attributed to water molecules in crystal boundary. {yields} The inorganic and organic components of the title compound are connected via hydrogen bonding to form a supramolecular three-dimensional network. -- Abstract: A new indium selenide, namely (bdaH)InSe{sub 2} (1) (bda = 1,4-butanediamine) has been solvothermally synthesized and structurally characterized. It belongs to the non-centrosymmetric space group Fdd2. Its structure features an infinite one-dimensional anionic chain of [InSe{sub 2}]{sub n}{sup n-} with monoprotonated [bdaH]{sup +} as charge compensating cation. The organic [bdaH]{sup +} cations are joined into a supramolecular one-dimensional chain via N-H...N hydrogen bonding, which further interacts with the inorganic chain via N-H...Se and C-H...Se hydrogen bonding, forming a supramolecular three-dimensional network. Based on such a well-defined structure, the thermal stability, optical, conductivity, and dielectric properties were systematically investigated, showing that dielectric constant, as well as conductivity, had a hump at about 95 {sup o}C, which could be attributed to water molecules in the crystal boundary.

36 MATERIALS SCIENCE↗