Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “difference”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 1,225 records · Page 68

Microstructural characterization and dry sliding wear resistance of MoO{sub 2}-strengthened {gamma}/NiMo alloys with different primary phases

Two {gamma}/NiMo alloys strengthened by a refractory metal oxide MoO{sub 2} phase were fabricated by a laser melting deposition process. Microstructural transformation of the alloys with different primary phases was identified and the crystal structure of the primary phases was confirmed by both X-ray diffraction and transmission electron microscopy. Meanwhile, room-temperature dry sliding wear behavior and mechanism difference of the alloys were also investigated mainly by scanning electron microscopy. Microstructures of the alloys varied from hypoeutectic to hypereutectic, as the molybdenum content increases. The hypoeutectic alloy was solidified on the basis of a Ni-base solid solution {gamma} primary phase, whereas the hypereutectic alloy was grown based on an intermetallic compound with NiMo primary phase. The {gamma}, NiMo primary phases and MoO{sub 2} strengthening phase were confirmed to have face-centered cubic, orthorhombic and monoclinic structures, respectively. Compared with the hypoeutectic alloy, the hypereutectic alloy exhibited higher wear resistance under the same condition. The predominant wear mechanism of the {gamma}/NiMo alloys transformed from micro-cutting to microcracking.

36 MATERIALS SCIENCE↗

Microstructural characterization of high-manganese austenitic steels with different stacking fault energies

Microstructures of tensile-deformed high-manganese austenitic steels exhibiting twinning-induced plasticity were analyzed by electron backscatter diffraction pattern observation and X-ray diffraction measurement to examine the influence of differences in their stacking fault energies on twinning activity during deformation. The steel specimen with the low stacking fault energy of 15 mJ/m{sup 2} had a microstructure with a high population of mechanical twins than the steel specimen with the high stacking fault energy (25 mJ/m{sup 2}). The <111> and <100> fibers developed along the tensile axis, and mechanical twinning occurred preferentially in the <111> fiber. The Schmid factors for slip and twinning deformations can explain the origin of higher twinning activity in the <111> fiber. However, the high stacking fault energy suppresses the twinning activity even in the <111> fiber. A line profile analysis based on the X-ray diffraction data revealed the relationship between the characteristics of the deformed microstructures and the stacking fault energies of the steel specimens. Although the variation in dislocation density with the tensile deformation is not affected by the stacking fault energies, the effect of the stacking fault energies on the crystallite size refinement becomes significant with a decrease in the stacking fault energies. Moreover, the stacking fault probability, which was estimated from a peak-shift analysis of the 111 and 200 diffractions, was high for the specimen with low stacking fault energy. Regardless of the difference in the stacking fault energies of the steel specimens, the refined crystallite size has a certain correlation with the stacking fault probability, indicating that whether the deformation-induced crystallite-size refinement occurs depends directly on the stacking fault probability rather than on the stacking fault energies in the present steel specimens. - Highlights: {yields} We studied effects of stacking fault energies on deformed microstructures of steels. {yields} Correlations between texture and occurrence of mechanical twinning are discussed. {yields} Evolutions of dislocations and crystallite are analyzed by line profile analysis.

36 MATERIALS SCIENCE↗

La{sub 0.7}Sr{sub 0.3}MnO{sub 3} nanopowders: Synthesis of different powders structures and real magnetic properties of nanomanganites

The difference in the magnetic properties between two lanthanum manganite nanopowders with identical phase and chemical composition is discussed in terms of the influence of nanopowder synthesis conditions on their properties. The aim of this investigation was to show the influence of precursor type and structure on the structure and properties of final La{sub 0.7}Sr{sub 0.3}MnO{sub 3} nanopowders obtained by precipitation technique. The forming of a complex structure of precursor materials during drying and inheritance at firing stage led to the formation of bimodal particle size distribution and magnetic properties typical of coarse powders. The correct choice of precursor material and the technological conditions of the drying and firing stage were allowed for the creation of a uniform powder structure with special magnetic properties. We showed that the magnetic properties of nanopowders were not always determined by chemical or phase composition and mean particle size of synthesized powders. The difference in precipitation process can lead to unpredictable and catastrophic results, and masked the effect of nanoparticles on the magnetic properties of the material. - Highlights: • Precursor’s structure has a strong influence on LSM nanoparticles structure. • Amorphous precursor structure led to uniform LSM nanoparticles formation. • Crystal precursors led to the formation of bimodal LSM particles distribution. • Decrease the single-domain LSM NP size led to decrease the powder’s magnetization.

36 MATERIALS SCIENCE↗

Evolution of microstructural defects with strain effects in germanium nanocrystals synthesized at different annealing temperatures

Ge nanocrystals (Ge-ncs) were produced by implantation of {sup 74}Ge{sup +} into a SiO{sub 2} film on (100) Si, followed by high-temperature annealing from 700 °C to 1100 °C. Transmission electron microscopy (TEM) studies show that the average size of Ge-ncs increases with the annealing temperature. High-resolution TEM (HRTEM) investigations reveal the presence of planar and linear defects in the formed Ge-ncs, whose relative concentrations are determined at each annealing temperature. The relative concentration of planar defects is almost independent of the annealing temperature up to 1000 °C. However, from 1000 °C to 1100 °C, its concentration decreases dramatically. For the linear defects, their concentration varies considerably with the annealing temperatures. In addition, by measuring the interplanar spacing of Ge-ncs from the HRTEM images, a strong correlation is found between the dislocation percentage and the stress field intensity. Our results provide fundamental insights regarding both the presence of microstructural defects and the origin of the residual stress field within Ge-ncs, which can shed light on the fabrication of Ge-ncs with quantified crystallinity and appropriate size for the advanced Ge-nc devices. - Highlights: • Growth of Ge nanocrystals at different annealing temperatures was investigated. • Strain field has great effects on the formation of dislocations. • Different mechanisms are proposed to explain growth regimes of Ge nanocrystals.

36 MATERIALS SCIENCE↗

Microstructural, mechanical and electrochemical behaviour of a 7017 Al–Zn–Mg alloy of different tempers

The aim of the investigation is to assess the microstructural features and associated physical, mechanical and electrochemical properties of a 7017 Al–Zn–Mg alloy of various tempers. A 7017 Al–Zn–Mg alloy was subjected to different ageing schedules to produce under-(T4), peak-(T6), over-(T7) and highly over-aged tempers. Optical microscopy, hardness measurement, electrical conductivity measurement, tensile testing and SEM fractographs, differential scanning calorimetry (DSC), transmission electron microscopy (TEM), and electrochemical polarization studies have been used to characterize the alloy tempers. Hardness measurement and tensile testing showed the characteristic age hardening phenomenon of aluminium alloys. Optical and TEM micrographs have revealed the variation in size of matrix strengthening η′ (MgZn{sub 2}) and also the size and distribution of grain boundary η (MgZn{sub 2}) precipitate with ageing time. DSC thermograms exhibiting exothermic and endothermic peaks indicated the characteristic solid state reaction sequence of the 7017 alloy. Potentiodynamic polarization study of the 7017 alloy of various tempers in 3.5 wt.% NaCl solution at near neutral pH showed typical active metal dissolution behaviour, but at pH 12 an active–passive–transpassive transition behaviour has been observed. - Graphical abstract: TEM micrograph of the 7017 aluminium alloy of various tempers (a, b) under aged (T4), (c, d) peak aged (T6), (e, f) over aged (T7) and (g, h) highly over-aged. Display Omitted - Highlights: • 7017 Al-Zn-Mg alloy was subjected to different artificial ageing treatments. • Characterization of 7017 alloy tempers by hardness, tensile, DSC, TEM and electrochemical behaviour. • Structure-properties relationship of the 7017 Al-Zn-Mg alloy of various tempers.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

The evolution with strain of the stored energy in different texture components of cold-rolled IF steel revealed by high resolution X-ray diffraction

During the deformation of low carbon steel by cold-rolling, dislocations are created and stored in grains depending on local crystallographic orientation, deformation, and deformation gradient. Orientation dependent dislocation densities have been estimated from the broadening of X-ray diffraction lines measured on a synchrotron beamline. Different cold-rolling levels (from 30% to 95% thickness reduction) have been considered. It is shown that the present measurements are consistent with the hypothesis of the sole consideration of screw dislocations for the analysis of the data. The presented evolutions show that the dislocation density first increases within the α fiber (=(hkl)<110>) and then within the γ fiber (=(111) ). A comparison with EBSD measurements is done and confirms that the storage of dislocations during the deformation process is orientation dependent and that this dependence is correlated to the cold-rolling level. If we assume that this dislocation density acts as a driving force during recrystallization, these observations can explain the fact that the recrystallization mechanisms are generally different after moderate or large strains. - Highlights: • Dislocation densities are assessed by XRD in main texture components of a steel sheet. • Dislocation densities vary with both strain and texture components. • The analysis relies on the sole presence of screw dislocations. • The measured dislocation densities include the contribution of both SSD and GND.

36 MATERIALS SCIENCE↗

Electrochemical characterization for lithium vanadium phosphate with different calcination temperatures prepared by the sol–gel method

Li{sub 3}V{sub 2}(PO{sub 4}){sub 3}/C (LVP/C) composite materials were synthesized via a sol–gel method with oxalic acid as the chelating agent and polyethylene glycol (PEG) as the supplementary carbon source. The oxalic acid and PEG serve as double carbon sources. This study focused on the effect of different calcination temperatures on the electrochemical properties of Li{sub 3}V{sub 2}(PO{sub 4}){sub 3}. The diffraction peaks for all of the samples are well indexed to monoclinic Li{sub 3}V{sub 2}(PO{sub 4}){sub 3} with a P2{sub 1}/n space group. The TGA data indicate that the residual carbon content of LVP/C-700 is the highest (i.e., 2.31 wt.%), and as the calcination temperature increased, the residual carbon content of the material gradually decreased. SEM and TEM analyses indicated that the LVP particles that were calcined at 700 °C exhibit a uniform particle size distribution and the carbon coating exhibited a complete and orderly moderate thickness. The LVP/C-700 material exhibits the best electrochemical performance in the voltage range of 3.0 to 4.3 V and 0.1 C where the initial discharge capacity can reach 128.98 mAh g{sup −} {sup 1}. Even after 200 cycles, the discharge capacity was 119.31 mAh g{sup −} {sup 1}, and the capacity retention rate was 92.49%. - Highlights: • Li{sub 3}V{sub 2}(PO{sub 4}){sub 3}/C composite materials have been synthesized via a sol–gel method with double carbon sources. • The different calcination temperatures affect the grain growth and crystallinity of the Li{sub 3}V{sub 2}(PO{sub 4}){sub 3}/C materials. • The LVP/C-700 material exhibites the largest lithium ion diffusivity and electronic conductivity.

36 MATERIALS SCIENCE↗

Microstructural changes and strain hardening effects in abrasive contacts at different relative velocities and temperatures

Strain hardening is commonly used to reach the full potential of materials and can be beneficial in tribological contacts. 2-body abrasive wear was simulated in a scratch test, aimed at strain hardening effects in various steels. Different working conditions were examined at various temperatures and velocities. Strain hardening effects and microstructural changes were analysed with high resolution scanning electron microscopy (HRSEM), electron backscatter diffraction (EBSD), micro hardness measurements and nanoindentation. Statistical analysing was performed quantifying the influence of different parameters on microstructures. Results show a crucial influence of temperature and velocity on the strain hardening in tribological contacts. Increased velocity leads to higher deformed microstructures and higher increased surface hardness at a lower depth of the deformed zones at all materials investigated. An optimised surface hardness can be achieved knowing the influence of velocity (strain rate) and temperature for a “tailor-made” surface hardening in tribological systems aimed at increased wear resistance. - Highlights: •Hardening mechanisms and their intensity in tribological contacts are dependent on relative velocity and temperature. •Beneficial surface hardened zones are formed at certain running-in conditions; the scientific background is presented here. •Ferritic-pearlitic steels strain hardens via grain size reduction and decreasing interlamellar distances in pearlite. •Austenitic steels show excellent surface hardening (120% hardness increase) by twinning and martensitic transformation. •Ferritic steels with hard phases harden in the ferrite phase as per Hall-Petch equation and degree of deformation.

36 MATERIALS SCIENCE↗

Effect of different stages of deformation on the microstructure evolution of Ti-rich NiTi shape memory alloy

The main objective of this work was to investigate the thermomechanical behavior and microstructural changes of a Ti-rich NiTi shape memory alloy (SMA). The microstructural and texture evolution of aged NiTi alloy at different degrees of deformation were elicited by transmission electron microscopy (TEM). An effort was made to correlate results obtained from the tensile test with results from microstructure studies. The undeformed sample reveals a self-accommodated morphology with straight and well defined twin boundaries. At different stages of deformation, diverse mechanisms were involved. These mechanisms include marstraining, detwinning accompanied by dislocation movement, and finally, severe plastic deformation, subdivision and amorphization of the matrix. Under increasing strains, high density lattice defects were generated and the morphology of B19’ became disordered. - Graphical abstract: The summary of microstructure changes of the martensite twins during tensile deformation in polycrystalline NiTi SMAs. - Highlights: • Initial elastic response, dislocation avalanche and deformation bands were studied. • < 011 > Type II twin accompanied by detwinned area after 2% cold work was observed. • Visible parallel fine stacking faults showed plastic flow of the material. • At higher strains, subgrains changed to recrystallized, finely amorphous structure.

36 MATERIALS SCIENCE↗

Microstructures of chemical vapor deposited high-purity tungsten achieved by two different precursors

Highlights: • CVD tungsten used as electron emitters of thermionic fuel elements was investigated. • Microstructures were characterized with metallography analysis. • The preferred orientation was determined with XRD and EBSD. • The surface morphology was observed with SEM and WLI. • Tungsten via thermolysis of WCl{sub 6} is better for thermionic fuel elements. - Abstract: Chemical vapor deposited (CVD) high-purity tungsten can be manufactured as electron emitters in thermionic fuel elements. Exposed surface planes of the emitter emit electrons and affect the efficiency and load capacity of the thermionic fuel element. In order to determine the electron emission planes of the emitter, the metallurgic structures, the preferred orientation and the as-deposited surface morphology of CVD tungsten have been investigated. In this work, high-purity (over 99.99%) tungsten was achieved by two different precursors: hydrogen reduction of tungsten hexafluoride (WF{sub 6}) and thermolysis of tungsten hexachloride (WCl{sub 6}). The microstructures of CVD tungsten were characterized by metallography analysis, X-ray diffraction (XRD), electron backscattered diffraction (EBSD), and white light interference (WLI). Tungsten fabricated by hydrogen reduction of WF{sub 6} and thermolysis of WCl{sub 6} has <100>-preferred columnar microstructures. However, the latter exhibits larger columnar grains and preferred <100> less. The preferred orientation is caused by the higher growth rate of the <100> orientation and competition between the <100> orientations of different grains. The as-deposited surface consists of tiny pyramids, with <100> axis and {111} side faces. In contrast to tungsten produced by hydrogen reduction of WF{sub 6}, the pyramid on tungsten synthesized via thermolysis of WCl{sub 6} contains small {110} facets on the four edges. Therefore, tungsten made via thermolysis of WCl{sub 6} is a better candidate for thermionic fuel elements, because the higher work function of {110} planes enables better output efficiency.

36 MATERIALS SCIENCE↗

Microstructure characterization and nano & micro hardness of tri-modal microstructure of titanium alloy under different hot working conditions

Highlights: • The contents and sizes of α{sub p} and α{sub l} are determined by the processing parameters of first and second step. • The morphology of α{sub s} embedded in β phase is determined by the accumulated distortional strain energy and dislocations. • α{sub p} becomes harder as the strain rate of the first step increases due to the constantly enhanced work hardening effect. • β{sub t} is always harder than α{sub p} and α{sub l} due to the interfacial-strengthening effect. • The hardness of α{sub l} makes the greatest contribution in the integrated hardness of tri-modal microstructure. - Abstract: In this work, the dependences of tri-modal microstructure parameters and corresponding nano & micro hardness on through-process processing parameters were quantitatively studied during the three-step thermo-mechanical processing of TA15 titanium alloy. It is found that the processing parameters of first step, especially for the deformation temperature and strain rate, mainly affect primary equiaxed α (α{sub p}) through the α → β phase transformation and the competition between dynamic recovery and dynamic recrystallization. The second processing step primarily affects the content and thickness of lamellar α (α{sub l}). In the third processing step, compared with low-temperature aging, normal annealing provides sufficient driving force for α{sub l} and secondary lamellar α (α{sub s}) growing, which leads to thicker α{sub l} and α{sub s}. As for the nano & micro hardness, in one sample undergoing different process, transformed β matrix (β{sub t}) is always harder than α{sub l} and α{sub s} due to the interfacial-strengthening effect. In addition, with increasing strain rate of the first step, α{sub p} becomes harder due to the constantly enhanced work hardening effect while the hardness of β{sub t} varies little because of the competition between interfacial strengthening and distribution disorder degree. However, the nano hardness of α{sub l} decreases firstly and then increases with strain rate, which presents the same trend with the micro hardness of integrated hardness at different processing conditions.

36 MATERIALS SCIENCE↗

Comparison of aluminium foams prepared by different methods using X-ray tomography

Highlights: • The closed porosity of MF aluminium foam is much lower than GI aluminium foam at a similar overall porosity. • There are more micropores in cell walls of MF aluminium foams than that in GI aluminium foams. • GI method is more suitable to prepare aluminium foams with high porosity under a similar cell size condition. • The thickness difference between normal cell wall and Plateau border is greater in GI foams compared to MF foams. - Abstract: The cell structure and mechanical properties of aluminium foams prepared by melt foaming (MF) method are supposed to be better than the ones produced by gas injection (GI) method. Preparation processes of these two methods have been developed during the last recent years. Mechanical properties of aluminium foams depend strongly on characteristics of the cell structure. Therefore, it is necessary to compare cell structures of the foams fabricated with these two methods quantitatively using X-ray computed tomography and this is the purpose of the present paper. MF and GI foams have thus been prepared. True density measurements and cell structures indicate that the volume fraction of the closed cells of MF foam with high porosity is negligible. By contrast, the majority of cells of GI foam are closed. Results of cell structure analysis show that there are more micropores in cell walls of the foams prepared by MF method compared to the ones prepared by GI method, especially for the MF foams with low porosity. In addition, results of cell size study show that the cell size distribution is wide in dynamic GI foams, and there are usually big holes inside MF foams. GI method is more suitable to prepare aluminium foams with high porosity compared to MF method. Furthermore, the thickness difference between normal cell wall and Plateau border is greater in GI foams, in particular for the ones produced by the static injector.

36 MATERIALS SCIENCE↗

Crystal development during carbonation of lime-based mortars in different environmental conditions

Highlights: • High CO{sub 2} and DiloCarb® treatment favour advanced carbonation and self-healing. • In the lime mortar without ceramics, channel type pores occur in the aggregate border. • In the lime mortars with ceramics, vug type pores are produced in the binder during kneading. • The formation of tabular CaCO{sub 3} polymorphs caused an increase in stress leading to microshrinkage cracks. • The use of a ceramic provoked dissolution and then re-precipitation of more stable polymorphs. - Abstract: This study examines crystal development during the carbonation of lime mortars according to the additives used and curing conditions. Two types of samples were prepared, one with sand and the other one additionally including Roman ceramics. These mortars were cured: 1) by spraying with a carbonation accelerator product under laboratory conditions; 2) in a climate chamber under 20 °C, 60% relative humidity, and 1600 ppm CO{sub 2}; and 3) under laboratory conditions as controls. Polarized light microscopy, SEM-EDS and XRD were used at 28, 90, 120 and 180 days to monitor the carbonation process. Observations indicate the development of different CaCO{sub 3} polymorphs, which appeared as metastable phases. The early nucleation of a well-defined calcite phase as the most stable CaCO{sub 3} polymorph was only identified in the chamber-cured samples. Differences in the pore network were observed depending on the composition and morphology of the mortar components and the environmental curing conditions.

36 MATERIALS SCIENCE↗

Microstructure and texture evolution of duplex stainless steels with different molybdenum contents

Highlights: • The 3.05Mo steel has higher resistance to strain-induced transformation than the 0.28Mo steel. • The increased Mo content affects the grain growth of austenite and ferrite due to the effects of segregation and anchoring. • At high annealing temperatures, this Mo retarding effect is weakened. • The suppression of γ-fiber development in the ferrite texture is associated with the increased Mo content. • High amounts of Mo generate unfavorable conditions for the formation of CSL boundaries. - Abstract: The microstructure and texture evolution of duplex stainless steels with different molybdenum contents were studied. For this purpose, hot-rolled 2205 and 2304 samples were solution-annealed at 1100 °C for 1800 s and then cold-rolled to a 75% thickness reduction. This was followed by an isothermal annealing at 900 and 1100 °C for 180 s. The EBSD technique was used to determine the phase ratio, crystallographic texture, and microstructural characteristics. The hot-rolled steel had a work hardened microstructure and the samples submitted to intermediate annealing presented mainly deformation-free grains. Cold rolling resulted in a substantial reduction in the phase spacing with the formation of the strain-induced α′-martensite (SIM) from the metastable austenite. After annealing at 900 °C, the ferrite grains retained the elongated shape of the cold-rolled condition and the primary recrystallization progressed in the austenite phase. Increasing the Mo content increased the resistance to strain-induced martensitic transformation and inhibited the grain growth of austenite phase during annealing at 900 °C. Increasing annealing temperature to 1100 °C promoted the coarsening of both bcc and fcc structures with the formation of annealing twins in the austenitic grains. The recrystallization kinetics and subsequent grain growth occur earlier in ferrite than in austenite phase. Differences in Mo content did not significantly alter the evolution of austenite texture, whereas in the ferrite phase the increase in Mo content suppressed the γ-fiber development. Oriented nucleation was the predominant mechanism observed during the recrystallization of ferritic grains in the 2205 samples. The development of ∑19a boundaries was associated with the selected growth of {554}<225>{sub α} grains in the annealed 2304 samples. Annealing twins were associated with the formation of Σ3 boundaries after the heat treatments. Grain coarsening resulted in a larger fraction of the special boundaries in ferrite phase but inhibited the CSL formation in the austenite phase.

36 MATERIALS SCIENCE↗

Characterization of the effects of different tempers and aging temperatures on the precipitation behavior of Al-Mg (5.25at.%)-Mn alloys

We investigated the effects of different tempers (H131 and H116) and different aging temperatures (50 and 70 °C) on the precipitation behavior of Al-Mg (5.25 at.%)-Mn (Al 5083) alloys aged for a long time (41 and 30 months) using electron backscatter diffraction(EBSD), scanning transmission electron microscopy(STEM), energy-dispersive X-ray spectroscopy(EDS), atom probe tomography (APT), and small angle neutron scattering (SANS). Results for the GP zones and β'' phases were found in Al 5083 H116 aged at 50 °C for 24 months using APT. EDS and SANS revealed that a phase transformation process from GP zones to β'/β phases occurred for precipitates formed in both Al 5083 H131 and H116 aged at 70 °C. The effective diffusion coefficient of Mg in Al 5083 H131 is 1.8 times of that in Al 5083 H116 aged at 70 °C. The precipitation process in Al 5083 H116 aged at 50 °C is much slower than that in the sample aged at 70 °C. Finally, we identified the coarsening process in Al 5083 H131 and H116 aged at 70 °C for > 9 months.

36 MATERIALS SCIENCE↗

Critical differences between electron beam melted and selective laser melted Ti-6Al-4 V

Effective optimization of the production of Ti-6Al-4 V using AM requires a fundamental understanding of the relative importance of different microstructural features to the deformation and failure mechanisms, particularly features that vary between production methods. In this study, the tensile response and deformation mechanisms of electron beam melted (EBM) AM Ti-6Al-4 V material loaded in different orientations and produced using various powder sizes were compared to those of selective laser melted (SLM) AM Ti-6Al-4 V material. The density and morphology of pores, phase fractions, prior-β grains, and defect microstructures were evaluated using scanning electron microscopy, X-ray computed tomography, electron backscatter diffraction, and transmission electron microscopy before and after deformation. The results were used to evaluate the relative importance of each feature on strengthening, deformation, and failure initiation mechanisms. Results focused primarily on coarse-powder EBM materials indicated that phase distribution and defect density were most influential for determining material yield strength as well as maximum possible strain to failure. Porosity was lower overall in EBM Ti-6Al-4 V than in SLM, allowing for occasional increases in part strain to failure, but remained a limiting factor determining overall part ductility.

36 MATERIALS SCIENCE↗

Synthesis of c-axis oriented AlN thin films on different substrates: A review

Highly c-axis oriented AlN thin films have been deposited by reactive sputtering on different substrates. The crystallographic properties of layered film structures consisting of a piezoelectric layer, aluminum nitride (AlN), synthesized on a variety of substrates, have been examined. Aluminum nitride thin films have been deposited by reactive pulsed-DC magnetron sputtering using an aluminum target in an Ar/N{sub 2} gas mixture. The influence of the most critical deposition parameters on the AlN thin film crystallography has been investigated by means of X-ray diffraction (XRD) analysis of the rocking curve Full-Width at Half Maximum (FWHM) of the AlN-(0 0 0 2) peak. The relationship between the substrate, the synthesis parameters and the crystallographic orientation of the AlN thin films is discussed. A guide is provided showing how to optimize these conditions to obtain highly c-axis oriented AlN thin films on substrates of different nature.

36 MATERIALS SCIENCE↗

Synthesis, characterization and evaluation of nano-zirconium vanadate ion exchanger by using three different preparation techniques

Sol-gel, homogeneous precipitation and hydrothermal synthesis are three different preparation techniques have been used as an attempt to synthesize nano-zirconium vanadate with properties suitable to be used as ion exchangers. The impact of the synthetic preparation variables such as the reactant concentrations, reaction temperature and reaction time on the ion exchange capacity of the produced ion exchanger has been considered for each preparation technique. One sample from each preparation technique having the largest ion exchange capacity has been selected to be physically and chemically characterized using various analytical techniques such as XRD, TGA, DSC, pH titration, FTIR and SEM in order to determine the properties of the ion exchanger produced from each technique. For all the studied ZrV samples it can be presumed that they have the ion exchange affinity sequences for alkali metal ions K > Na > Li, the order for the alkaline earth metals is Ba > Ca > Mg and their affinity for radioactive metals follow Cs > Sr. Moreover, the prepared materials are of high thermal and radiation stabilities. Also they have high chemical stabilities toward wide concentration ranges of acid, basic as well as polar solvents. It has been deduced from the X-ray analysis that ZrV produced from the sol-gel technique has an amorphous structural. While those produced from the homogeneous precipitation and hydrothermal synthesis techniques, in the nano-scale have semi-crystalline structural. Furthermore, SEM confirms that particle size of the all studied prepared ZrV samples have nano-diameters of range 50-60 nm. Specific surface area of the three different prepared ion exchangers are found to be equal to 187, 192 and 320 m{sup 2}/g for sol-gel, homogeneous precipitation and hydrothermal, respectively. A tentative structural formula of Zr(OH){sub 2}(HVO{sub 4}){sub 2}.2H{sub 2}O has been proposed for all studied samples on the basis of on FTIR, DSC and TGA results.

36 MATERIALS SCIENCE↗