At least 1,225 records · Page 68

Ultra-stable, low phase noise dielectric resonator stabilized oscillators for military and commercial systems

EPSD has designed, fabricated and tested, ultra-stable, low phase noise microwave dielectric resonator oscillators (DRO's) at S, X, Ku, and K-bands, for potential application to high dynamic range and low radar cross section target detection radar systems. The phase noise and the temperature stability surpass commercially available DROs. Low phase noise signals are critical for CW Doppler radars, at both very close-in and large offset frequencies from the carrier. The oscillators were built without any temperature compensation techniques and exhibited a temperature stability of 25 parts per million (ppm) over an extended temperature range. The oscillators are lightweight, small and low cost compared to BAW & SAW oscillators, and can impact commercial systems such as telecommunications, built-in-test equipment, cellular phone and satellite communications systems. The key to obtaining this performance was a high Q factor resonant structure (RS) and careful circuit design techniques. The high Q RS consists of a dielectric resonator (DR) supported by a low loss spacer inside a metal cavity. The S and the X-band resonant structures demonstrated loaded Q values of 20,300 and 12,700, respectively.

Mizan, Muhammad↗

Ion-beam-induced magnetic and structural phase transformation of Ni-stabilized face-centered-cubic Fe films on Cu(100)

Metastable face-centered cubic (fcc) Fe/Cu(100) thin films are good candidates for ion-beam magnetic patterning due to their magnetic transformation upon ion-beam irradiation. However, pure fcc Fe films undergo spontaneous transformation when their thickness exceeds 10 ML. This limit can be extended to approximately 22 ML by deposition of Fe at increased CO background pressures. We show that much thicker films can be grown by alloying with Ni for stabilizing the fcc γ phase. The amount of Ni necessary to stabilize nonmagnetic, transformable fcc Fe films in dependence on the residual background pressure during the deposition is determined and a phase diagram revealing the transformable region is presented.

36 MATERIALS SCIENCE↗

The NASA/GSFC hydrogen maser program: A review of recent data

Data is presented on the phase and frequency stability, over time periods extending to one week, of the new NR field operable hydrogen masers developed by the Applied Physics Laboratory (APL) and the older NX and NP field operable hydrogen masers developed by Goddard Space Flight Center and maintained and upgraded by Bendix Field Engineering Corporation (BFEC). Data is presented on the NR masers in the laboratory showing frequency stabilities well into the 10 to the -15th power range and phase stabilities well into the 100 ps range for periods of up to one day. Data is presented on upgraded NP masers in the laboratory showing that the frequency stability has been improved substantially to virtually the NR level. VLBI data is presented on the phase difference between NX-2 at Owens Valley, California and NR-2 at Fort Davis, Texas for a one week period showing, after removal of a constant frequency drift, a 350 ps RMS phase stability.

Chiu, M.↗

Taming the stability of Pd active phases through a compartmentalizing strategy toward nanostructured catalyst supports

The design and synthesis of robust sintering-resistant nanocatalysts for high-temperature oxidation reactions is ubiquitous in many industrial catalytic processes and still a big challenge in implementing nanostructured metal catalyst systems. Herein, we demonstrate a strategy for designing robust nanocatalysts through a sintering-resistant support via compartmentalization. Ultrafine palladium active phases can be highly dispersed and thermally stabilized by nanosheet-assembled γ-Al2O3 (NA-Al2O3) architectures. The NA-Al2O3 architectures with unique flowerlike morphologies not only efficiently suppress the lamellar aggregation and irreversible phase transformation of γ-Al2O3 nanosheets at elevated temperatures to avoid the sintering and encapsulation of metal phases, but also exhibit significant structural advantages for heterogeneous reactions, such as fast mass transport and easy access to active sites. This is a facile stabilization strategy that can be further extended to improve the thermal stability of other Al2O3-supported nanocatalysts for industrial catalytic applications, in particular for those involving high-temperature reactions.

36 MATERIALS SCIENCE↗

Generation of electric-field stabilized zirconium monoxide secondary phase within cubic zirconia

Flash sintering of cubic yttria-stabilized zirconia has been studied via in situ energy dispersive diffraction. A secondary rocksalt-phase zirconium monoxide was observed emerging from the primary fluorite-phase zirconium dioxide, previously only observed as a thin interlayer at metal-oxide interfaces, upon application of a direct current electric field. The average secondary phase intensity rose over extended flow of direct current through the ceramic, faded upon removal of the field and disappeared entirely upon application of an alternating current electric field. The results indicate that the sustained application of a direct current electric field can result in significant electrochemical reduction of zirconia under high current density conditions. Poor sinterability and cracking under direct current is apparent and potential mechanisms discussed therein.

36 MATERIALS SCIENCE↗

An adaptive DC-bus stabilizer for single-phase grid-connected renewable energy source system

This paper proposes an adaptive DC-bus stabilizer for single-phase grid-connected voltage source converter (VSC) with small-scale renewable energy integration. To enhance converter's power density, the conventional active power decoupling (APD) techniques were adopted to reduce the DC capacitance by compensating the inherent second-order harmonic power ripples in the single-phase VSC. However, it would potentially make the DC voltage vulnerable to transient power ripples, which is a critical issue for the grid-connected renewable energy source (RES) system during grid faults. The proposed DC-bus stabilizer can not only compensate the second-order harmonic power ripples at normal operation, but also enhance the fault ride-through capability of the converter. The circuit topology and its corresponding control strategy are presented, and then simulation results are provided to demonstrate the feasibility and validity of the proposed DC-bus stabilizer under normal operation and grid fault condition.

Zeng, Rong↗

Performance Testing of TRL4-6 LISA Laser System

The Laser Interferometer Space Antenna (LISA) is an ESA-led future mission to measure gravitational waves from astronomical sources in space. LISA has been adopted as a formal mission by ESA in January 2024, and is expected to become a formal project at NASA within 2024. The laser system (LS), which includes four laser heads (LH) each containing a laser optical module (LOM) and laser electronics module (LEM), a frequency reference system (FRS, optical frequency reference) and four power monitor detectors (PMON), is one of the three U.S. contributions to LISA from NASA. The Lasers and Electro-Optics Branch at NASA GSFC has been developing and managing the design of the LISA LS. Currently, the TRL (technology readiness level) of the NASA LISA laser system is transitioning from 4 to 6. TRL 4/5 LISA LOM was sent to ESA in early 2023 and has undergone optical performance testing. [1] By late summer of 2024, NASA plans to deliver the TRL 6 LOM to ESA for performance evaluation. Since the delivery of the TRL4/5 LOM to ESA, we have taken steps to advance the TRL of the overall LS and have also started end-to-end system level testing involving other subsystems. They include 1) optical performance test of TRL6 LOM and TRL 5 LEM under thermal cycling, 2) end-to-end test of the laser head (LH) and the GSE (ground support equipment) FRS, driven by TRL 4 FRS electronics (FRS-E) provided by Ball Aerospace, 3) end-to-end test of the laser head (LH) with the GSE phase meter system (PMS) provided by Albert Einstein Institute, and 4) optical performance test of the LH with the PMON subsystem developed by NASA. The FRS, PMS, and PMON provide necessary frequency stability, relative phase stability between lasers, and output power stability, respectively. Since they are all vital for the sensitive laser interferometry performed in LISA, it is necessary to perform these system level testing by combining the LH and other subsystems, and to prove the optical performance at an early stage during the LS development. Our recent work has successfully demonstrated the intra-connectivity of the LS, as well as critical external interface with the PMS to meet the LISA’s performance requirements. In this talk, we will report on the latest status of the LH testing and system level test. We will also discuss the paths to bring each subsystem to TRL6+ and plans for future system level testing.

LISA↗

Temperature feedback control for long-term carrier-envelope phase locking

A feedback control module for stabilizing a carrier-envelope phase of an output of a laser oscillator system comprises a first photodetector, a second photodetector, a phase stabilizer, an optical modulator, and a thermal control element. The first photodetector may generate a first feedback signal corresponding to a first portion of a laser beam from an oscillator. The second photodetector may generate a second feedback signal corresponding to a second portion of the laser beam filtered by a low-pass filter. The phase stabilizer may divide the frequency of the first feedback signal by a factor and generate an error signal corresponding to the difference between the frequency-divided first feedback signal and the second feedback signal. The optical modulator may modulate the laser beam within the oscillator corresponding to the error signal. The thermal control unit may change the temperature of the oscillator corresponding to a signal operable to control the optical modulator.

47 OTHER INSTRUMENTATION↗

Impact of Structural Defects and Hydronium Ion Concentration on the Stability of Zeolite BEA in Aqueous Phase

The presence of fluoride anions in the synthesis gel leads to zeolite BEA with high hydrothermal stability. This longer lifetime is caused by a lower concentration of internal silanol defects that are sites of the initial framework hydrolysis eventually destroying the lattice structure. The lifetime of these zeolites was the higher the lower the concentration of framework bridging hydroxyl groups that form hydronium ions was. While lattice hydrolysis was initiated at defect sites in all cases, the role of defects became less important as the concentration of hydronium ions increased. At higher concentration of hydrated hydronium ions, the presence of water associated with the hydrated hydronium ions limits the useful lifetime of zeolite catalysts in water. For such materials, the selective hydrophobization of the external surface extends the lifetime. Acknowledgments: S.P. and M.A.D. acknowledge support by the Materials Synthesis and Simulation Across Scales (MS3 Initiative) conducted under Laboratory Directed Research & Development Program at PNNL. H.S. and H.W. were supported by the Chemical Transformation Initiative (CTI) conducted under Laboratory Directed Research & Development Program at PNNL. J.A.L. was supported by the US Department of Energy, Office of Science, Office of Basic Energy Sciences.

Prodinger, Sebastian↗

Phase evolution and amorphous stability upon solid-state reaction in superlattice like Ge–Sb–Te combinatorial thin-film

In this paper, the superlattice-like (SLL) Ge–Sb–Te combinatorial thin films were prepared by using a high-throughput ion beam sputtering system. The phase evolution and amorphous stability of such films undergoing heat treatment as a function of the coating sequence and modulation period were systematically studied. The composition structure diagram was constructed via an automated process of data obtained by high-throughput synchrotron micro-X-ray diffraction and lab-based micro-X-ray fluorescence. Furthermore, the element distribution and microstructure in the depth direction of the SLL thin films were characterized with time-of-flight secondary ion mass spectrometry and transmission electron microscopy, respectively. These studies demonstrated that the coating sequence has a significant effect on the element distribution in the as-deposited SLL thin films and the structure of the final product upon solid-state reaction. Reducing the modulation period of the SLL thin film improves the stability of the amorphous Ge–Sb–Te phase. This work lays a solid foundation for the rational design of SLL Ge–Sb–Te thin films to improve their performance.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

The stability of two-phase flow over a swept-wing

We use numerical and asymptotic techniques to study the stability of a two-phase air/water flow above a flat porous plate. This flow is a model of the boundary layer which forms on a yawed cylinder and can be used as a useful approximation to the air flow over swept wings during heavy rainfall. We show that the interface between the water and air layers can significantly destabilize the flow, leading to traveling wave disturbances which move along the attachment line. This instability occurs for lower Reynolds numbers than in the case of the absence of a water layer. We also investigate the instability of inviscid stationary modes. We calculate the effective wavenumber and orientation of the stationary disturbance when the fluids have identical physical properties. Using perturbation methods we obtain corrections due to a small stratification in viscosity, thus quantifying the interfacial effects. Our analytical results are in agreement with the numerical solution which we obtain for arbitrary fluid properties.

Coward, Adrian↗

Effect of metal loading processes on the stability and thermal transformation of Co{sup 2+}- and Cu{sup 2+}-zeolite Y prepared from Egyptian kaolin

This paper aims to assess the effect of the transition metals (TM) loading procedure on the incorporation of Co{sup 2+} and Cu{sup 2+} in zeolite Y, and their relevance to stability of the zeolite, particularly with respect to the thermal transformation to the spinel phases. In this work, zeolite Y prepared from Egyptian kaolin was used. XRF, XRD, TEM, UV/visible absorption measurements, and atomic absorption analyses in addition to the visual observations are recorded. XRF has been used to investigate the materials composition. TEM and XRD indicate the presence of nanoparticle spinel upon the calcination of the TM-zeolites at 1000 Degree-Sign C. In addition to spinel particles, XRD shows the formation of metal oxides, SiO{sub 2} and alumino-silicate phases. According to the transition metal and the cation loading process, different phases were detected. UV/visible absorption measurements and the visual observations are used to determine the experimental condition of the highest spinel content. It has been noticed that the experimental conditions of the metal sorption processes greatly affect the phase transformation. Stability and thermal transformation of zeolite depend on the initial concentration of the transition cation solutions and the number of loading cycles. - Highlights: Black-Right-Pointing-Pointer We study the effects of loading procedure in the incorporation of TM in zeolite Y. Black-Right-Pointing-Pointer Synthetic zeolite Y prepared from Egyptian kaolin has been used. Black-Right-Pointing-Pointer The type of TM affects the stability and thermal transformation of zeolite. Black-Right-Pointing-Pointer Loading processes affect the stability and thermal transformation of zeolite.

36 MATERIALS SCIENCE↗

Automated RF Phase Adjustment for Beam Stabilization in the Fermilab Linac

The Fermilab Linac experiences longitudinal beam phase drift, leading to increased particle loss, conventionally corrected through labor-intensive manual RF adjustments. This project explores machine learning-based automation for drift correction, employing a prototype-based classification approach. Our model utilizes a 34-dimensional feature set (RF settings and BPM readings) and leverages a 7x27 response matrix for system modeling. To overcome limited real-world data, we generate synthetic data, enhancing model training and generalizability. Custom loss functions, including a surrogate energy-consistent loss and a temporal smoothness constraint, ensure physically plausible drift predictions. The goal is a robust system for autonomous phase adjustments, ensuring stable beam acceleration and reduced manual intervention.

Chichili, R. R. [Illinois U., Chicago]↗

Automated RF Phase Adjustment for Beam Stabilization in the Fermilab Linac

The Fermilab Linac experiences longitudinal beam phase drift, leading to increased particle loss, conventionally cor- rected through labor-intensive manual RF adjustments. This project explores machine learning-based automation for drift correction, employing a prototype-based classification approach. Our model utilizes a 34-dimensional feature set (RF settings and BPM readings) and leverages a 7x27 response matrix for system modeling. To overcome limited real-world data, we generate synthetic data, enhancing model training and generalizability. Custom loss functions, including a sur- rogate energy-consistent loss and a temporal smoothness constraint, ensure physically plausible drift predictions. The goal is a robust system for autonomous phase adjustments, ensuring stable beam acceleration and reduced manual intervention.

Chichili, R. R. [U. Illinois, Chicago]↗

9R phase enabled superior radiation stability of nanotwinned Cu alloys via in situ radiation at elevated temperature

Nanotwinned metals exhibit outstanding radiation tolerance as twin boundaries effectively engage, transport and eliminate radiation-induced defects. However, radiation-induced detwinning may reduce the radiation tolerance associated with twin boundaries, especially at elevated temperatures. Here we show, via in-situ Kr ion irradiation inside a transmission electron microscope, that 3 at. % Fe in epitaxial nanotwinned Cu (Cu 97 Fe 3 ) significantly improves the thermal and radiation stability of nanotwins during radiation up to 5 displacements-per-atom at 200 °C. Such enhanced stability of nanotwins is attributed to a diffuse 9R phase resulted from the dissociation of incoherent twin boundaries in nanotwinned Cu 97 Fe 3 . The mechanisms for the enhanced stability of twin boundaries in irradiated nanotwinned alloys are discussed. As a result, the stabilization of nano-twins opens up opportunity for the application of nanotwinned alloys for aggressive radiation environments.

36 MATERIALS SCIENCE↗