Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “ISOTHERMS”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 1,225 records · Page 68

The ternary system cerium-rhodium-silicon

Phase relations have been established in the ternary system Ce-Rh-Si for the isothermal section at 800 deg. C based on X-ray powder diffraction and EPMA on about 80 alloys, which were prepared by arc melting under argon or by powder reaction sintering. From the 25 ternary compounds observed at 800 deg. C 13 phases have been reported earlier. Based on XPD Rietveld refinements the crystal structures for 9 new ternary phases were assigned to known structure types. Structural chemistry of these compounds follows the characteristics already outlined for their prototype structures: tau{sub 7}-Ce{sub 3}RhSi{sub 3}, (Ba{sub 3}Al{sub 2}Ge{sub 2}-type), tau{sub 8}-Ce{sub 2}Rh{sub 3-x}Si{sub 3+x} (Ce{sub 2}Rh{sub 1.35}Ge{sub 4.65}-type), tau{sub 10}-Ce{sub 3}Rh{sub 4-x}Si{sub 4+x} (U{sub 3}Ni{sub 4}Si{sub 4}-type), tau{sub 11}-CeRh{sub 6}Si{sub 4} (LiCo{sub 6}P{sub 4}-type), tau{sub 13}-Ce{sub 6}Rh{sub 30}Si{sub 19.3} (U{sub 6}Co{sub 30}Si{sub 19}-type), tau{sub 18}-Ce{sub 4}Rh{sub 4}Si{sub 3} (Sm{sub 4}Pd{sub 4}Si{sub 3}-type), tau{sub 21}-CeRh{sub 2}Si (CeIr{sub 2}Si-type), tau{sub 22}-Ce{sub 2}Rh{sub 3+x}Si{sub 1-x} (Y{sub 2}Rh{sub 3}Ge-type) and tau{sub 24}-Ce{sub 8}(Rh{sub 1-x}Si{sub x}){sub 24}Si (Ce{sub 8}Pd{sub 24}Sb-type). For tau{sub 25}-Ce{sub 4}(Rh{sub 1-x}Si{sub x}){sub 12}Si a novel bcc structure was proposed from Rietveld analysis. Detailed crystal structure data were derived for tau{sub 3}-CeRhSi{sub 2} (CeNiSi{sub 2}-type) and tau{sub 6}-Ce{sub 2}Rh{sub 3}Si{sub 5} (U{sub 2}Co{sub 3}Si{sub 5}-type) by X-ray single crystal experiments, confirming the structure types. The crystal structures of tau{sub 4}-Ce{sub 22}Rh{sub 22}Si{sub 56}, tau{sub 5}-Ce{sub 20}Rh{sub 27}Si{sub 53} and tau{sub 23}-Ce{sub 33.3}Rh{sub 58.2-55.2}Si{sub 8.5-11.5} are unknown. High temperature compounds with compositions Ce{sub 10}Rh{sub 51}Si{sub 33} (U{sub 10}Co{sub 51}Si{sub 33}-type) and CeRhSi (LaIrSi-type) have been observed in as-cast alloys but these phases do not participate in the phase equilibria at 800 deg. C. - Graphical abstract: Phase relations in the ternary system Ce-Rh-Si have been established for the isothermal section at 800 deg. C based on X-ray powder and single-crystal diffraction, metallography, SEM and EMPA techniques on about 80 alloys. 25 ternary compounds were observed.

36 MATERIALS SCIENCE↗

Polytypic transformations during the thermal decomposition of cobalt hydroxide and cobalt hydroxynitrate

The isothermal decomposition of cobalt hydroxide and cobalt hydroxynitrate at different intervals of temperature leads to the formation of Co{sub 3}O{sub 4}. The phase evolution during the decomposition process was monitored using powder X-ray diffraction. The transformation of cobalt hydroxide to cobalt oxide occurs via three phase mixture while cobalt hydroxynitrate to cobalt oxide occurs through a two phase mixture. The nature of the sample and its preparation method controls the decomposition mechanism. The comparison of topotactical relationship between the precursors to the decomposed product has been reported in relation to polytypism. - Graphical abstract: Isothermal thermal decomposition studies of cobalt hydroxide and cobalt hydroxynitrate at different intervals of temperature show the metastable phase formed prior to Co{sub 3}O{sub 4} phase.

36 MATERIALS SCIENCE↗

p(O{sub 2})-stability of LaFe{sub 1-x}Ni{sub x}O{sub 3-{delta}}solid solutions at 1100 {sup o}C

LaFe{sub 1-x}Ni{sub x}O{sub 3-{delta}}(x=0.1-1.0) perovskites were synthesized via citrate route. The p(O{sub 2})-stability of the perovskite phases LaFe{sub 1-x}Ni{sub x}O{sub 3-{delta}}has been evaluated at 1100 {sup o}C based on the results of XRD analysis of powder samples annealed at various p(O{sub 2}) and quenched to room temperature. The isothermal LaFeO{sub 3-{delta}-}'LaNiO{sub 3-{delta}'} cross-section of the phase diagram of the La-Fe-Ni-O system has been proposed in the range of oxygen partial pressure -15<log p(O{sub 2})/atm{<=}0.68. The unit cell parameters of orthorhombic perovskites O-LaFe{sub 1-x}Ni{sub x}O{sub 3-{delta}}increase with decrease in p(O{sub 2}) at fixed composition x. This behavior is explained on the basis of size factor. The decomposition temperatures of rhombohedral phases R-LaFe{sub 1-x}Ni{sub x}O{sub 3-{delta}}for x=0.7, 0.8, 0.9 and 1.0 in air were determined as 1137, 1086, 1060 and 995 {sup o}C, respectively. - Graphical abstract: Isothermal LaFeO{sub 3-{delta}-}'LaNiO{sub 3-{delta}'} section of the phase diagram of the La-Fe-Ni-O system at 1100 {sup o}C. The hatched areas represent single phase regions: O-LaFe{sub 1-x}Ni{sub x}O{sub 3-{delta}}(x{<=}0.4) with orthorhombically distorted perovskite structure and R-LaFe{sub 1-x}Ni{sub x}O{sub 3-{delta}}(0.6{<=}x<0.8) with rhombohedral one.

36 MATERIALS SCIENCE↗

The electrochemical performance of ordered mesoporous carbon/nickel compounds composite material for supercapacitor

A series of high performance ordered mesoporous carbon/nickel compounds composites have been synthesized by a combination of incipient wetness impregnation and hydrothermal method for the first time. X-ray diffraction (XRD), N{sub 2} adsorption/desorption isotherms and transmission electron microscopy (TEM) are used to characterize the composites derived at the hydrothermal temperature of 125, 150, 175, 200, 250, 275 and 300 {sup o}C. The formation of nanosized nickel compounds, fully inside the mesopore system, was confirmed with XRD and TEM. An N{sub 2} adsorption/desorption isotherms measurements still revealed mesoporosity for the host/guest compounds. It is noteworthy that an OMC/nickel nitrate hydroxide hydrate composite (OMCN-150) exhibits more excellent performance. Based on the various hydrothermal temperatures of the composite, the capacitance of an OMCN-150 delivering the best electrochemical performance is about 2.4 (5 mV s{sup -1}) and 1.5 (50 mV s{sup -1}) times of the pristine OMC. The capacitance retention of an OMCN-150 is 96.1%, which indicates that the electrochemical performance of the supercapacitor is improved greatly, and represents novel research and significant advances in the field of electrode composite materials for supercapacitor. -- Graphical abstract: A series of high performance nickel compound/ordered mesoporous carbon composites were synthesized by a combination of incipient wetness impregnation and hydrothermal method for the first time. Display Omitted

36 MATERIALS SCIENCE↗

Phase equilibria and crystal structure of the complex oxides in the Ln-Ba-Co-O (Ln=Nd, Sm) systems

The phase equilibria in the Ln-Ba-Co-O (Ln=Nd, Sm) systems were systematically studied at 1100 deg. C in air. The homogeneity ranges and crystal structure of the solid solutions: Ln{sub 2-x}Ba{sub x}O{sub 3-{delta}} (0<x{<=}0.1 for Ln=Nd and 0<x{<=}0.3 for Ln=Sm), Nd{sub 3-y}Ba{sub y}Co{sub 2}O{sub 7} (0.70{<=}y{<=}0.80), BaCo{sub 1-z}Sm{sub z}O{sub 3-{delta}} (0.1{<=}z{<=}0.2) were determined by X-ray diffraction of quenched samples. The values of oxygen content (5+{delta}) for slowly cooled LnBaCo{sub 2}O{sub 5+{delta}} (Ln=Nd, Sm) samples were estimated as 5.73 for Ln=Nd, and 5.60 for Ln=Sm. The unit cell parameters were refined using Rietveld full-profile analysis. It was shown that NdBaCo{sub 2}O{sub 5.73} possesses tetragonal structure and SmBaCo{sub 2}O{sub 5.60} - orthorhombic structure. The projections of isothermal-isobaric phase diagrams for the Ln-Ba-Co-O (Ln=Nd, Sm) systems to the compositional triangle of metallic components were presented. - Graphical Abstract: Projections of isobaric isothermal phase diagrams of the Nd-Ba-Co-O system and Sm-Ba-Co-O system. Highlights: > Phase equilibria in the Ln-Ba-Co-O systems (Ln=Nd, Sm). > The homogeneity range for Nd{sub 2-x}Ba{sub x}O{sub 3-{delta}} solid solutions at studied conditions 0<x{<=}0.1. > The homogeneity range for Sm{sub 2-x}Ba{sub x}O{sub 3-{delta}} solid solutions at studied conditions 0<x{<=}0.3. > Nd{sub 3-y}Ba{sub y}Co{sub 2}O{sub 7} solid solutions within the range 0.7{<=}y{<=}0.8. > BaCo{sub 1-z}Sm{sub z}O{sub 3-{delta}} solid solutions within the range 0.1{<=}z{<=}0.2.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

The system Ce-Zn-B at 800 deg. C

The isothermal section for the system Ce-Zn-B has been established at 800 deg. C using electron microprobe analysis and X-ray powder diffraction. No ternary compounds exist and mutual solid solubilities of binary phases are negligible. In the concentration range of 10.0-10.5 at% Ce two structural modifications have been confirmed: high temperature {beta}Ce{sub 2}Zn{sub 17} above {approx}750 deg. C with the Th{sub 2}Zn{sub 17} type (R3-bar m, a=0.90916(4) nm, c=1.3286(1) nm) and low temperature {alpha}CeZn{sub 7} (Ce{sub 1-x}Zn{sub 5+2x}; x{approx}0.33) up to 750 deg. C for which we attributed the TbCu{sub 7} type (P6/mmm, a=0.52424(2), c=0.44274(1) nm). The crystal structure of CeZn{sub 7} was derived from the Rietveld refinement of X-ray powder intensities. Precise data on atom site distribution and positional parameters have been furthermore provided from X-ray single crystal refinements for two compounds, for which crystal structures hitherto have only been derived from X-ray diffraction photographs: Ce{sub 3}Zn{sub 11} (Immm, a=0.45242(2) nm, b=0.88942(3) nm, c=1.34754(4) nm) and Ce{sub 3}Zn{sub 22} (I4{sub 1}/amd; a=0.89363(2) nm, c=2.1804(5) nm). - Graphical abstract: Existence of low temperature modification {alpha}CeZn{sub 7} (Ce{sub 1-x}Zn{sub 5+2x}; x{approx}0.33) of Ce{sub 2}Zn{sub 17} has been verified up to 750 deg. C that is attributed with the TbCu{sub 7} type. Highlights: > Isothermal section of system Ce-Zn-B at 800 deg. C. > In System Ce-Zn, X-ray single crystal intensity data refinement of Ce{sub 3}Zn{sub 11} and Ce{sub 3}Zn{sub 22} and Rietveld refinement of Ce{sub 13}Zn{sub 58}. > Two temperature modifications of Ce{sub 2}Zn{sub 17}, rhombohedral {beta}Ce{sub 2}Zn{sub 17} (hT) and of hexagonal {alpha}CeZn{sub 7} (lT). > No ternary compound in the System Ce-Zn-B (<50 at% Ce) at 800 deg. C.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Physical and electrochemical properties of alkaline earth doped, rare earth vanadates

The effect of partial substitution of alkaline earth (AE) ions, Sr{sup 2+} and Ca{sup 2+}, for the rare earth (RE) ions, La{sup 3+}, Ce{sup 3+}, Pr{sup 3+}, and Sm{sup 3+}, on the physical properties of REVO{sub 4} compounds were investigated. The use of the Pechini method to synthesize the vanadates allowed for high levels of AE substitution to be obtained. Coulometric titration was used to measure redox isotherms for these materials and showed that the addition of the AE ions increased both reducibility and electronic conductivity under typical solid oxide fuel cell (SOFC) anode conditions, through the formation of compounds with mixed vanadium valence. In spite of their high electronic conductivity, REVO{sub 4}-yttira stabilized zirconia (YSZ) composite anodes exhibited only modest performance when used in SOFCs operating with H{sub 2} fuel at 973 K due to their low catalytic activity. High performance was obtained, however, after the addition of a small amount of catalytically active Pd to the anode. - Graphical abstract: Coulometric titration isotherms for ({open_square}) LaVO{sub 4}, ( White-Circle ) PrVO{sub 4}, ( Lozenge ) CeVO{sub 4}, ( Black-Up-Pointing-Triangle ) Ce{sub 0.7}Sr{sub 0.3}VO{sub 3.85}, and ( Black-Square ) Ce{sub 0.7}Ca{sub 0.3}VO{sub 3.85}, at 973 K. Highlights: Black-Right-Pointing-Pointer Infiltration procedures were used to prepare SOFC anodes from various vanadates. Black-Right-Pointing-Pointer Doping of Alkaline Earth to Rare Earth Vanadates showed to improve conductivity and chemical stability. Black-Right-Pointing-Pointer Alkaline Earth Doped Rare Earth Vanadates-YSZ composites showed conductivities as high as 5 S cm{sup -1} at 973 K. Black-Right-Pointing-Pointer As with other ceramic anodes, the addition of a catalyst was required to achieve low anode impedance.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Phase relations and crystal structures in the system Ce-Ni-Zn at 800 Degree-Sign C

Phase relations have been established for the system Ce-Ni-Zn in the isothermal section at 800 Degree-Sign C using electron microprobe analysis and X-ray powder diffraction. Phase equilibria at 800 Degree-Sign C are characterized by a large region for the liquid phase covering most of the Ce-rich part of the diagram, whereas a Zn-rich liquid is confined to a small region near the Zn-corner of the Gibbs triangle. Whereas solubility of Ce in the binary Ni-Zn phases is negligible, mutual solubilities of Ni and Zn at a constant Ce content are large at 800 Degree-Sign C for most Ce-Zn and Ce-Ni compounds. The solid solution Ce(Ni{sub 1-x}Zn{sub x}){sub 5} with the CaCu{sub 5}-type is continuous throughout the entire section and for the full temperature region from 400 to 800 Degree-Sign C. Substitution of Zn by Ni is found to stabilize the structure of CeZn{sub 11} to higher temperatures. At 800 Degree-Sign C Ce(Ni{sub x}Zn{sub 1-x}){sub 11} (0.03{<=}x{<=}0.22) appears as a ternary solution phase. Similarly, a rather extended solution forms for Ce{sub 2}(Ni{sub x}Zn{sub 1-x}){sub 17} (0{<=}x{<=}0.53). Detailed data on atom site occupation and atom parameters were derived from X-ray structure analyses for single crystals of Ce{sub 2+y}(Ni{sub x}Zn{sub 1-x}){sub 17}, y=0.02, x=0.49 (a=0.87541(3), c=1.25410(4) nm; Th{sub 2}Zn{sub 17} type with space group R3{sup Macron }m,R{sub F{sup 2}}=0.018) and Ce(Ni{sub 0.18}Zn{sub 0.82}){sub 11} (a=1.04302(2), c=0.67624(3)nm, BaCd{sub 11} type with space group I4{sub 1}/amd, R{sub F{sup 2}}=0.049). - Graphical abstract: Ce-Ni-Zn isothermal section at 800 Degree-Sign C. Highlights: Black-Right-Pointing-Pointer Phase relations were determined for the system Ce-Ni-Zn in the section at 800 Degree-Sign C. Black-Right-Pointing-Pointer A continuous solid solution Ce(Ni{sub 1-x}Zn{sub x}){sub 5}, 0{<=}x{<=}1, forms between 400 and 800 Degree-Sign C. Black-Right-Pointing-Pointer Zn/Ni substitution stabilizes the ternary phase Ce(Zn{sub 1-x}Ni{sub x}){sub 11}, 0.03{<=}x{<=}0.22, 800 Degree-Sign C. Black-Right-Pointing-Pointer An extended solution forms for Ce{sub 2}(Ni{sub x}Zn{sub 1-x}){sub 17} (0{<=}x{<=}0.53). Black-Right-Pointing-Pointer Crystal data are given: Ce{sub 2+y}(Ni{sub x}Zn{sub 1-x}){sub 17} (Th{sub 2}Zn{sub 17}), Ce(Ni{sub 0.18}Zn{sub 0.82}){sub 11} (BaCd{sub 11}).

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Phase relations and structural features in the system Ni-Zn-B

Phase relations for the system Ni-Zn-B have been established in the isothermal section at 800 Degree-Sign C based on X-ray powder diffraction and electron microprobe analyses of about 60 samples, which have been prepared by hot pressing of pre-annealed powder compacts of arc-melted master alloys Ni{sub x}B{sub y} and Zn-filings. Six ternary compounds (labeled {tau}{sub 1} to {tau}{sub 6}) were found to exist, which in some cases exhibit considerable mutual solid solubilities mostly as an exchange of Ni-Zn at constant B-content, but in the case of the so-called {tau}-phase {tau}{sub 1}-(Ni{sub 1-x}Zn{sub x}){sub 21}[Zn{sub 1-y-z}{open_square}{sub y}(B{sub 4}){sub z}]{sub 2}B{sub 6} (0.07{<=}x{<=}0.11, 0.07{<=}y{<=}0.53, 0{<=}z{<=}0.3) also with Zn/B substitution. Single crystal X-ray data analysis for the composition x=0.07, y=0.125, z=0.30, and a=1.05800(3) nm confirmed the Cr{sub 23}C{sub 6} type with space group Fm3{sup Macron }m, but revealed partial replacement of Zn-atoms by B{sub 4}-tetrahedra (R{sub F}=0.014). Whereas Ni/Zn exchange (at constant B-content) ranges at about 4-5 at% for {tau}{sub 4}-Ni{sub 3}ZnB{sub 2} and {tau}{sub 5}-Ni{sub 48}Zn{sub 32}B{sub 20}, it is below 3 at% for {tau}{sub 2}-Ni{sub 12}ZnB{sub 8-x} (x=0.43), {tau}{sub 3}-Ni{sub 21}Zn{sub 2}B{sub 20} and {tau}{sub 6}-Ni{sub 47}Zn{sub 23}B{sub 30}. The crystal structures of {tau}{sub 2}-Ni{sub 12}ZnB{sub 8-x} (x=0.43; Ni{sub 12}AlB{sub 8} type), {tau}{sub 3}-Ni{sub 21}Zn{sub 2}B{sub 20} (own type) and {tau}{sub 4}-Ni{sub 3}ZnB{sub 2} (own type) have been determined in our foregoing paper [8]. Due to the non-availability of suitable single crystals, the crystal structures of {tau}{sub 5}-Ni{sub 48}Zn{sub 32}B{sub 20} (body-centered orthorhombic; a=1.6(2) nm, b=0.63(7) nm, and c=0.27(0) nm, determined from TEM) and of {tau}{sub 6}-Ni{sub 47}Zn{sub 23}B{sub 30} have not been elucidated yet. Phase equilibria at 800 Degree-Sign C are dominated by a large three-phase field ({beta}B)+Ni{sub 2}Zn{sub 11}+{tau}{sub 3}, as practically all ternary compounds form at compositions with less than about 50 at% Ni. Furthermore, precise data on atom site distribution and positional parameters have been provided from X-ray single crystal refinements for Ni-borides, for which crystal structures hitherto have only been derived from X-ray diffraction photographs: o-Ni{sub 4}B{sub 3-x} (x=0.19; Pnma, a=1.9665(4) nm, b=0.29852(1) nm, c=0.65750(2) nm; R{sub F}=0.015) and m-Ni{sub 4}B{sub 3} (C2/c, a=0.64356(3) nm, b=0.48867(3) nm, c=0.78267(3) nm, {beta}=103.288(3) Degree-Sign , R{sub F}=0.021). - Graphical abstract: Ni-Zn-B isothermal section at 800 Degree-Sign C. Highlights: Black-Right-Pointing-Pointer Phase relations were determined for the system Ni-Zn-B at 800 Degree-Sign C. Black-Right-Pointing-Pointer Existence of six ternary compounds ({tau}{sub 1}-{tau}{sub 6}) has been confirmed at 800 Degree-Sign C. Black-Right-Pointing-Pointer Homogeneity range for {tau}{sub 1} with respect to Ni/Zn and Zn/B at 800 Degree-Sign C has been determined. Black-Right-Pointing-Pointer The crystal structures of {tau}{sub 5}-Ni{sub 48}Zn{sub 32}B{sub 20} from TEM (oI, a=1.6(2) nm, b=0.63(7) nm, and c=0.27(0) nm). Black-Right-Pointing-Pointer Precise data on {tau}{sub 1}-(Ni{sub 1-x}Zn{sub x}){sub 21}[Zn{sub 1-y-z{open_square}y}(B{sub 4}){sub z}]{sub 2}B{sub 6} (0.07{<=}x{<=}0.11, 0.07{<=}y{<=}0.53, 0{<=}z{<=}0.3), o-Ni{sub 4}B{sub 3-x} and m-Ni{sub 4}B{sub 3} have been presented.

36 MATERIALS SCIENCE↗

Oxidation kinetics of aluminum diboride

The oxidation characteristics of aluminum diboride (AlB{sub 2}) and a physical mixture of its constituent elements (Al+2B) were studied in dry air and pure oxygen using thermal gravimetric analysis to obtain non-mechanistic kinetic parameters. Heating in air at a constant linear heating rate of 10 °C/min showed a marked difference between Al+2B and AlB{sub 2} in the onset of oxidation and final conversion fraction, with AlB{sub 2} beginning to oxidize at higher temperatures but reaching nearly complete conversion by 1500 °C. Kinetic parameters were obtained in both air and oxygen using a model-free isothermal method at temperatures between 500 and 1000 °C. Activation energies were found to decrease, in general, with increasing conversion for AlB{sub 2} and Al+2B in both air and oxygen. AlB{sub 2} exhibited O{sub 2}-pressure-independent oxidation behavior at low conversions, while the activation energies of Al+2B were higher in O{sub 2} than in air. Differences in the composition and morphology between oxidized Al+2B and AlB{sub 2} suggested that Al{sub 2}O{sub 3}–B{sub 2}O{sub 3} interactions slowed Al+2B oxidation by converting Al{sub 2}O{sub 3} on aluminum particles into a Al{sub 4}B{sub 2}O{sub 9} shell, while the same Al{sub 4}B{sub 2}O{sub 9} developed a needle-like morphology in AlB{sub 2} that reduced oxygen diffusion distances and increased conversion. The model-free kinetic analysis was critical for interpreting the complex, multistep oxidation behavior for which a single mechanism could not be assigned. At low temperatures, moisture increased the oxidation rate of Al+2B and AlB{sub 2}, but both appear to be resistant to oxidation in cool, dry environments. - Graphical abstract: Isothermal kinetic data for AlB{sub 2} in air, showing a constantly decreasing activation energy with increasing conversion. Model-free analysis allowed for the calculation of global kinetic parameters despite many simultaneous mechanisms occurring concurrently. (a) Time–temperature plots, (b) conversion as a function of time, (c) Arrhenius plots used to calculate activation energies, and (d) activation energy as a function of conversion. Display Omitted - Highlights: • First reported kinetic parameters for AlB{sub 2} and Al+2B oxidation in air and O{sub 2}. • Possible mechanism of enhanced boron combustion presented. • Moisture sensitivity shown to be problematic for AlB{sub 2}, less for Al+2B.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Magnetism and magnetocaloric effect in multicomponent Laves-phase compounds: Study and comparative analysis

This paper presents a review and results of comparative study of the influence of Gd on some physical properties of (R{sub 0.9}R′{sub 0.1}){sub 1−x}Gd{sub x}Co{sub 2} solid solutions with R=Dy, Ho and R′=Er, Ho and x varied from 0.05 to 0.15. Powder X-ray diffraction analysis performed at room temperature revealed that all studied solid solutions solidify with the formation of a Laves-phase MgCu{sub 2}-type structure (space group Fd−3m). The magnetization behavior and the magnetic transition are analyzed in terms of the Landau theory. The studies of magnetic properties and heat capacity showed that a relatively small Gd addition significantly increases T{sub C} of the compounds. The maximum percentage increase in T{sub C}, namely, ∼43% was observed for (Ho{sub 0.9}Er{sub 0.1}){sub 1−x}Gd{sub x}Co{sub 2}. However, the highest temperature was noted for the (Dy{sub 0.9}Ho{sub 0.1}){sub 0.85}Gd{sub 0.15}Co{sub 2} solid solution; it is T{sub C}=183.4 K. Below the ordering temperature, all samples are ferrimagnetically ordered; at high temperatures, they are Curie–Weiss paramagnets. Moreover, a small Gd addition eliminates the field-induced magnetic transition near T{sub C} and, as consequence, transforms the nature of magnetic transition from the first- to second-order. The magnetocaloric effect has been estimated in terms of both isothermal magnetic entropy and adiabatic temperature changes. The highest adiabatic temperature change ΔT{sub ad}=3 K and highest isothermal entropy change ΔS{sub mag}=12.1 J/kg K were observed for (Ho{sub 0.9}Er{sub 0.1}){sub 0.95}Gd{sub 0.05}Co{sub 2} at ∼90 K in magnetic fields of 2 T and 3 T, respectively. A decrease in the entropy change has been observed with increasing Gd content in all studied samples. The smallest values of ΔS{sub mag} were observed for the (Dy{sub 0.9}Ho{sub 0.1}){sub 1−x}Gd{sub x}Co{sub 2} solid solutions. Under an external field change of from 0 to 3 T, the maximum entropy change for (Dy{sub 0.9}Ho{sub 0.1}){sub 1−x}Gd{sub x}Co{sub 2} compounds decreases from 6.9 at x=0.05–4.3 J/kg K at x=0.15. The refrigerant capacity for all solid solutions (with 0.05≤x≤0.15) is reported. The effect of increasing Gd content in the solid solutions on their magnetic and magnetocaloric properties is discussed. - Graphical abstract: Temperature dependencies of ΔT{sub ad} induced by µ{sub 0}H=1 and 2 T in (a) (Ho{sub 0.9}Er{sub 0.1}){sub 1−x}Gd{sub x}Co{sub 2} and (b) (Dy{sub 0.9}Er{sub 0.1}){sub 1−x}Gd{sub x}Co{sub 2} solid solutions. Display Omitted.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Oxygen potentials and phase equilibria in the system Ca–Co–O and thermodynamic properties of Ca{sub 3}Co{sub 2}O{sub 6} and Ca{sub 3}Co{sub 4}O{sub 9.163}

Oxygen potentials established by the equilibrium between three condensed phases, CaO{sub ss}+CoO{sub ss}+Ca{sub 3}Co{sub 2}O{sub 6} and CoO{sub ss}+Ca{sub 3}Co{sub 2}O{sub 6}+Ca{sub 3}Co{sub 3.93+α}O{sub 9.36−δ}, are measured as a function of temperature using solid-state electrochemical cells incorporating yttria-stabilized zirconia as the electrolyte and pure oxygen as the reference electrode. Cation non-stoichiometry and oxygen non-stoichiometry in Ca{sub 3}Co{sub 3.93+α}O{sub 9.36−δ} are determined using different techniques under defined conditions. Decomposition temperatures and thermodynamic properties of Ca{sub 3}Co{sub 2}O{sub 6} and Ca{sub 3}Co{sub 4}O{sub 9.163} are calculated from the results. The standard entropy and enthalpy of formation of Ca{sub 3}Co{sub 2}O{sub 6} at 298.15 K are evaluated. Using thermodynamic data from this study and auxiliary information from the literature, phase diagram for the ternary system Ca–Co–O is computed. Isothermal sections at representative temperatures are displayed to demonstrate the evolution of phase relations with temperature. - Graphical abstract: Isothermal section of the phase diagram of the system Ca–Co–O at 1250 K. - Highlights: • Improved definition of cation and oxygen nonstoichiometry of Ca{sub 3}Co{sub 3.93+α}O{sub 9.36−δ}. • Measurement of Δμ{sub O{sub 2}} associated with two 3-phase fields as a function of temperature. • Use of solid-state electrochemical cells for accurate measurement of Δμ{sub O{sub 2}}. • Decomposition temperatures and thermodynamic properties for ternary oxides. • Characterization of ternary phase diagram of the system Ca–Co–O.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Mo{sub 2}NiB{sub 2}-type (Gd, Tb, Dy){sub 2}Ni{sub 2.35}Si{sub 0.65} and La{sub 2}Ni{sub 3}-type (Dy, Ho){sub 2}Ni{sub 2.5}Si{sub 0.5} compounds: Crystal structure and magnetic properties

The crystal structure of new Mo{sub 2}NiB{sub 2}-type (Gd, Tb, Dy){sub 2}Ni{sub 2.35}Si{sub 0.65} (Immm, No. 71, oI10) and La{sub 2}Ni{sub 3}-type (Dy, Ho){sub 2}Ni{sub 2.5}Si{sub 0.5} (Cmce No. 64, oC20) compounds has been established using powder X-ray diffraction studies. Magnetization measurements show that the Mo{sub 2}NiB{sub 2}-type Gd{sub 2}Ni{sub 2.35}Si{sub 0.65} undergoes a ferromagnetic transition at ~66 K, whereas isostructural Tb{sub 2}Ni{sub 2.35}Si{sub 0.65} shows an antiferromagnetic transition at ~52 K and a field-induced metamagnetic transition at low temperatures. Neutron diffraction study shows that, in zero applied field, Tb{sub 2}Ni{sub 2.35}Si{sub 0.65} exhibits c-axis antiferromagnetic order with propagation vector K=[1/2, 0, 1/2] below its magnetic ordering temperature and Tb magnetic moment reaches a value of 8.32(5) μ{sub B} at 2 K. The La{sub 2}Ni{sub 3}-type Dy{sub 2}Ni{sub 2.5}Si{sub 0.5} exhibits ferromagnetic like transition at ~42 K with coexisting antiferromagnetic interactions and field induced metamagnetic transition below ~17 K. The magnetocaloric effect of Gd{sub 2}Ni{sub 2.35}Si{sub 0.65}, Tb{sub 2}Ni{sub 2.35}Si{sub 0.65} and Dy{sub 2}Ni{sub 2.5}Si{sub 0.5} is calculated in terms of isothermal magnetic entropy change and it reaches a maximum value of −14.3 J/kg K, −5.3 J/kg K and −10.3 J/kg K for a field change of 50 kOe near 66 K, 52 K and 42 K, respectively. Low temperature magnetic ordering with enhanced anisotropic effects in Tb{sub 2}Ni{sub 2.35}Si{sub 0.65} and Dy{sub 2}Ni{sub 2.35}Si{sub 0.65} is accompanied by a positive magnetocaloric effect with isothermal magnetic entropy changes of +12.8 J/kg K and ~+9.9 J/kg K, respectively at 7 K for a field change of 50 kOe. - Graphical abstract: The (Gd, Tb, Dy){sub 2}Ni{sub 2.35}Si{sub 0.65} supplement the series of Mo{sub 2}NiB{sub 2}-type rare earth compounds, whereas the (Dy, Ho){sub 2}Ni{sub 2.5}Si{sub 0.5} supplement the series of La{sub 2}Ni{sub 3}-type rare earth compounds. The variation of alloy’s composition by ~3 at% i.e. from Dy{sub 2}Ni{sub 2.35}Si{sub 0.65} to Dy{sub 2}Ni{sub 2.5}Si{sub 0.5} leads to significant transformation of crystal structure of compound with different variant of distortion of Po-type rare earth sublattice, as in Gd–Co–Ga and Er–Ni–In systems: the Mo{sub 2}NiB{sub 2}-type Gd{sub 2}Co{sub 2}Ga and La{sub 2}Ni{sub 3}-type Gd{sub 2}Co{sub 2.9}Ga{sub 0.1}, and Mo{sub 2}FeB{sub 2}-type Er{sub 2}Ni{sub 1.78}In and Mn{sub 2}AlB{sub 2}-type Er{sub 2}Ni{sub 2}In. Magnetization measurements indicate collinear ferromagnetic ordering of Mo{sub 2}NiB{sub 2}-type Gd{sub 2}Ni{sub 2.35}Si{sub 0.65} and a complex antiferromagnetic ordering with low-temperature metamagnetic nature for Mo{sub 2}NiB{sub 2}-type Tb{sub 2}Ni{sub 2.35}Si{sub 0.65} compounds. However, neutron diffraction study in zero applied field of Tb{sub 2}Ni{sub 2.35}Si{sub 0.65} reveals c-axis pure antiferromagnetic ordering of terbium sublattice with K=[1/2, 0, 1/2] propagation vector. Magnetization measurements indicate ferromagnetic order with coexisting antiferromagnetic interactions and low-temperature metamagnetic state for La{sub 2}Ni{sub 3}-type Dy{sub 2}Ni{sub 2.5}Si{sub 0.5}. We suggest possible polymorphism in other Mo{sub 2}FeB{sub 2}-type, Mo{sub 2}NiB{sub 2}-type, La{sub 2}Ni{sub 3}-type and Mn{sub 2}AlB{sub 2}-type rare earth compounds with corresponding change in their magnetic properties. - Highlights: • (Gd, Tb, Dy){sub 2}Ni{sub 2.35}Si{sub 0.65} compounds crystallize in the Mo{sub 2}NiB{sub 2}-type structure. • (Dy, Ho){sub 2}Ni{sub 2.5}Si{sub 0.5} compounds crystallize in the La{sub 2}Ni{sub 3}-type structure. • Gd{sub 2}Ni{sub 2.35}Si{sub 0.65} shows pure ferromagnetic type ordering. • Tb{sub 2}Ni{sub 2.35}Si{sub 0.65} and Dy{sub 2}Ni{sub 2.5}Si{sub 0.5} show mixed ferro-antiferromagnetic ordering. • Tb{sub 2}Ni{sub 2.35}Si{sub 0.65} and Dy{sub 2}Ni{sub 2.5}Si{sub 0.5} exhibit low-temperature metamagnetic behaviour.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

RNi{sub 8}Si{sub 3} (R=Gd,Tb): Novel ternary ordered derivatives of the BaCd{sub 11} type

The title compounds have been synthesized and characterized both from the structural and magnetic point of view. Both crystallize in a new monoclinic structure strictly related to the tetragonal BaCd{sub 11} type. The structure was solved by means of X-ray single-crystal techniques for GdNi{sub 8}Si{sub 3} and confirmed for TbNi{sub 8}Si{sub 3} on powder data; the corresponding lattice parameters (obtained from Guinier powder patterns) are a=6.3259(2), b=13.7245(5), c=7.4949(3) Å, β=113.522(3)°, V{sub cell}=596.64(3) Å{sup 3} and a=6.3200(2), b=13.6987(4), c=7.4923(2) Å, β=113.494(2)°, V{sub cell}=594.88(2) Å{sup 3}. The symmetry relationship between the tI48-I4{sub 1}/amd BaCd{sub 11} aristotype and the new ordered mS48-C2/c GdNi{sub 8}Si{sub 3} derivative is described via the Bärnighausen formalism within the group theory. The large Gd–Gd (Tb–Tb) distances, mediated via Ni–Si network, likely lead to weak magnetic interactions. Low-field magnetization vs temperature measurements indicate weak and field-sensitive antiferromagnetic ground state, with ordering temperatures of 3 K in GdNi{sub 8}Si{sub 3} and about 2–3 K in TbNi{sub 8}Si{sub 3}. On the other hand, the isothermal field-dependent magnetization data show the presence of competing interactions in both compounds, with a field-induced ferromagnetic behavior for GdNi{sub 8}Si{sub 3} and a ferrimagnetic-like behavior in TbNi{sub 8}Si{sub 3} at the ordering temperature T{sub C/N} of about (or slightly higher than) 3K. The magnetocaloric effect, quantified in terms of isothermal magnetic entropy change ΔS{sub m}, has the maximum values of –19.8 J(kg K){sup −1} (at 4 K for 140 kOe field change) and −12.1 J(kg K){sup −1} (at 12 K for 140 kOe field change) in GdNi{sub 8}Si{sub 3} and TbNi{sub 8}Si{sub 3}, respectively. - Graphical abstract: GdNi{sub 8}Si{sub 3} and TbNi{sub 8}Si{sub 3} compounds are isostructural, and crystallize in a new monoclinic type strictly related to the tetragonal BaCd{sub 11} structure. The large R–R interatomic distances mediated via Ni–Si network lead to a weak magnetism in both compounds. - Highlights: • Novel RNi{sub 8}Si{sub 3} (R=Gd, Tb) compounds have been synthesized and characterized. • GdNi{sub 8}Si{sub 3} and TbNi{sub 8}Si{sub 3} are isostructural compounds, belonging to a new monoclinic structure type. • The monoclinic GdNi{sub 8}Si{sub 3} type is an ordered derivative of the tetragonal BaCd{sub 11} type. • The large R–R interatomic distances mediated via Ni–Si network lead to a weak magnetism. • Both compounds GdNi{sub 8}Si{sub 3} and TbNi{sub 8}Si{sub 3} show antiferromagnetic-like order around 3 K.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Phase equilibria in the NaF-CdO-NaPO{sub 3} system at 873 K and crystal structure and physico-chemical characterizations of the new Na{sub 2}CdPO{sub 4}F fluorophosphate

Isothermal sections of the diagram representing phase relationships in the NaF-CdO-NaPO{sub 3} system have been investigated by solid state reactions and powder X-ray diffraction. This phase diagram investigation confirms the polymorphism of the NaCdPO{sub 4} side component and the structure of the ß high temperature polymorph (orthorhombic, space group Pnma and unit cell parameters a=9.3118(2), b=7.0459(1), c=5.1849(1) Å has been refined. A new fluorophosphate, Na{sub 2}CdPO{sub 4}F, has been discovered and its crystal structure determined and refined from powder X-ray diffraction data. It exhibits a new 3D structure with orthorhombic symmetry, space group Pnma and unit cell parameters a=5.3731(1), b=6.8530(1), c=12.2691(2) Å. The structure is closely related to those of the high temperature polymorph of the nacaphite Na{sub 2}CaPO{sub 4}F and the fluorosilicate Ca{sub 2}NaSiO{sub 4}F but differs essentially in the cationic repartition since the structure is fully ordered with one Na site (8d) and one Cd site (4c). Relationships with other Na{sub 2}M{sup II}PO{sub 4}F (M{sup II}=Mg, Ca, Mn, Fe, Co, Ni) have been examined and the crystal-chemical and topographical analysis of these fluorophosphates is briefly reviewed. IR, Raman, optical and {sup 19}F, {sup 23}Na, {sup 31}P MAS NMR characterizations of Na{sub 2}CdPO{sub 4}F have been investigated. - Graphical abstract: The structure of the compound Na{sub 2}CdPO{sub 4}F, discovered during the study of the phase relationships in the NaF-CdO-NaPO{sub 3} system, has been determined and compared with other Na{sub 2}M{sup II}PO{sub 4}F fluorophosphates. - Highlights: • XRD analysis of the isothermal section of the NaF-CdO-NaPO{sub 3} system at 923 K. • Rietveld refinement of the high temperature polymorph β-NaCdPO{sub 4}. • Crystal structure of the new Na{sub 2}CdPO{sub 4}F fluorophosphate determined from powder XRD. • Crystal structure - composition relationships of Na{sub 2}M{sup II}PO{sub 4}F compounds are reviewed. • IR, Raman, optical and {sup 19}F, {sup 23}Na, {sup 31}P MAS NMR characterizations of Na{sub 2}CdPO{sub 4}F.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Dehydration-driven evolution of topological complexity in ethylamonium uranyl selenates

Single crystals of four novel uranyl selenate and selenite-selenate oxysalts with protonated ethylamine molecules, (C{sub 2}H{sub 8}N){sub 2}[(UO{sub 2})(SeO{sub 4}){sub 2}(H{sub 2}O)](H{sub 2}O) (I), (C{sub 2}H{sub 8}N){sub 3}[(UO{sub 2})(SeO{sub 4}){sub 2}(HSeO{sub 4})] (II), (C{sub 2}H{sub 8}N)[(UO{sub 2})(SeO{sub 4})(HSeO{sub 3})] (III), and (C{sub 2}H{sub 8}N)(H{sub 3}O)[(UO{sub 2})(SeO{sub 4}){sub 2}(H{sub 2}O)] (IV) have been prepared by isothermal evaporation from aqueous solutions. Uranyl-containing 1D and 2D units have been investigated using topological approach and information-based complexity measurements that demonstrate the evolution of structural units and the increase of topological complexity with the decrease of H{sub 2}O content. - Graphical abstract: Single crystals of four novel uranyl selenate and selenite-selenate oxysalts with protonated ethylamine molecules have been prepared by isothermal evaporation from aqueous solutions. Structural analysis and information-based topological complexity calculations points to the possible sequence of crystalline phases formation, showing both topological and structural branches of evolution. - Highlights: • Single crystals of four novel uranyl oxysalts were prepared by evaporation method. • The graph theory was used for investigation of topologies of structural units. • Dehydration processes drives the evolution of topological complexity of 1D and 2D structural units.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Sigma phase morphologies in cast and aged super duplex stainless steel

Solution annealed and water quenched duplex and super duplex stainless steels are thermodynamically metastable systems at room temperature. These systems do not migrate spontaneously to a thermodynamically stable condition because an energy barrier separates the metastable and stable states. However, any heat input they receive, for example through isothermal treatment or through prolonged exposure to a voltaic arc in the welding process, cause them to reach a condition of stable equilibrium which, for super duplex stainless steels, means precipitation of intermetallic and carbide phases. These phases include the sigma phase, which is easily identified from its morphology, and its influence on the material's impact strength. The purpose of this work was to ascertain how 2-hour isothermal heat treatments at 920 deg. C and 980 deg. C affect the microstructure of ASTM A890/A890M GR 6A super duplex stainless steel. The sigma phase morphologies were found to be influenced by these two aging temperatures, with the material showing a predominantly lacy microstructure when heat treated at 920 deg. C and block-shaped when heat treated at 980 deg. C.

36 MATERIALS SCIENCE↗

Aging behavior and mechanical properties of maraging steels in the presence of submicrocrystalline Laves phase particles

Cold rolling and annealing of homogenized Fe-Ni-Mn-Mo-Ti-Cr maraging steels resulted in the formation of submicrocrystalline Fe{sub 2}(Mo,Ti) Laves phase particles. Optical and scanning electron microscopy, X-ray diffraction, tensile and hardness tests were used to study the microstructure, aging behavior and mechanical properties of the annealed steels. The annealed microstructures showed age hardenability during subsequent isothermal aging at 753 K. Ultrahigh fracture stress but poor tensile ductility was obtained after substantial age hardening in the specimens with 2% and 4% chromium. Increasing chromium addition up to 6% toughened the aged microstructure at the expense of the fracture stress by increasing the volume fraction of retained austenite. The Laves phase particles acted as crack nucleation sites during tensile deformation. - Highlights: {yields} Laves phases dispersed in a BCC iron matrix by annealing of cold rolled samples. {yields} The samples showed age hardenability during subsequent isothermal aging at 753 K. {yields} Ultrahigh fracture stress but poor ductility was obtained after age hardening. {yields} Increasing chromium addition toughened the aged microstructure. {yields} Laves phase particles acting as crack nucleation sites during tensile deformation.

36 MATERIALS SCIENCE↗