Engineering Papers⌕ Search

SEARCH · Engineering Papers

Results for “severity”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 1,207 records · Page 67

Deformation textures of aluminum in a multilayered Ti/Al/Nb composite severely deformed by accumulative roll bonding

The accumulative roll bonding process was carried out to produce multilayered Ti/Al/Nb composites up to four cycles. Scanning electron microscopy, transmission electron microscopy electron backscattered diffraction and nanoindentation were employed to investigate the microstructural and texture evolution. A homogenous distribution of Ti/Nb necking layers in Al matrix was achieved after four ARB cycles. Grain refinement was observed to increase with increasing number of ARB cycles. The fraction of high-angle grain boundaries as also increased. Strong recrystallization texture appeared for high number of ARB cycles due to the adiabatic heat that occurs during ARB processing. The shear band at the Ti/Al interface reduced the intensity of the cold rolling fiber textures of Al. There was no evidence of shear component from the orientation distribution function results.

36 MATERIALS SCIENCE↗

Influence of alloying element Zn on the microstructural, mechanical and corrosion properties of binary Mg-Zn alloys after severe plastic deformation

Highlights: • Mg-Zn alloys are processed by equal channel angular pressing with back-pressure. • The α-Mg matrix consists of highly deformed and partially recrystallized areas. • Zn concentration varies in the α-Mg matrix by up to 2 at.%. • The alloys exhibit mechanical anisotropy and a significant increase in strength. • Equal channel angular pressing increases corrosion rate of Mg-Zn alloys. - Abstract: This work presents an analysis of the microstructural, mechanical and corrosion properties of two binary Mg-Zn alloys. Mg-6 wt%Zn and Mg-12 wt%Zn cast alloys were subjected to annealing followed by quenching and processed via equal channel angular pressing with applied back-pressure (ECAP-BP). After ECAP-BP, both alloys were thoroughly examined and showed partially recrystallized and highly deformed areas. High-angle annular dark-field imaging revealed a difference in Zn content across the α-Mg matrix of the Mg-12 wt%Zn after ECAP-BP due to the growth of MgZn{sub 2} nanoparticles. Electron energy-loss spectroscopy (EELS) was carried out to qualify an average Zn content in these areas, and a variation in Zn content up to 2 at.% was found. Compression tests revealed mechanical anisotropy and a significant increase in the strength of both alloys after ECAP-BP. The yield strength, σ{sub 02}, was in the range from 269 to 385 MPa depending on the composition and compression axis. The initial state alloys showed yield strengths, σ{sub 02}, of only 75–150 MPa but improved ductility. The corrosion rates of the Mg-Zn alloys in the initial state, evaluated using a hydrogen evolution method in NaCl solution, were higher for Mg-12 wt%Zn. The corrosion rates of both alloys after ECAP-BP were higher than those of the initial state. Light microscopy observations did not reveal any preference for corrosion propagation, including transcrystalline, intercrystalline or interphase corrosion, in any of the materials.

36 MATERIALS SCIENCE↗

Dynamic restoration of severely predeformed, ultrafine-grained pure Cu at 373 K observed in situ

Highlights: • Discontinuous grain coarsening during tension at 373 K generated new grains exceeding significantly grain size of UFG Cu. • The coarsening was preferentially located at shear bands. • There are indications that the grain coarsening occurs by recrystallization. - Abstract: Microstructure changes of ultrafine-grained pure copper prepared by equal-channel angular pressing were investigated during in situ tensile testing inside a scanning electron microscope at constant total strain rate of 10{sup −4} s{sup −1} at 373 K (~ 0.28 T{sub m}). After fast work hardening the flow stress saturated at an inelastic strain of 0.06. Significant local coarsening of grains was observed to start at about 2/3 of the maximum flow stress. However, these localized events did not significantly change the mean grain size up to an inelastic strain of 0.09. Surface observations showed that the coarsening was preferentially located at shear bands.

36 MATERIALS SCIENCE↗